Material grade directory
5855 grades and 14528 source records with numerical compositions. Standards, editions and conditions are retained separately; these records do not establish interchangeability or a supply guarantee.
- 008CR27MO · 6 source records
- 008CR30MO2 · 1 source record
- 00CR19NI10 · 2 source records · Original-source verification pending
- 015CR20NI18MO6CUN · 1 source record
- 015CR21NI26MO5CU2 · 1 source record
- 015CR24NI22MO8MN3CUN · 5 source records
- 019CR18MOTI · 1 source record
- 019CR19MO2NBTI · 1 source record
- 022CR11NBTI · 5 source records
- 022CR11TI · 8 source records
- 022CR12 · 2 source records
- 022CR12NI · 1 source record
- 022CR12NI9CU2NBTI · 1 source record
- 022CR17NBTI · 3 source records · Original-source verification pending
- 022CR17NI12MO2 · 14 source records
- 022CR17NI12MO2N · 12 source records
- 022CR17NI13MO2 · 1 source record · Original-source verification pending
- 022CR17NI7 · 1 source record
- 022CR17NI7N · 1 source record
- 022CR18NBTI · 1 source record
- 022CR18NI14MO2CU2 · 1 source record
- 022CR18NI14MO3 · 1 source record
- 022CR18NI15MO3N · 1 source record
- 022CR18TI · 10 source records
- 022CR19NI10 · 16 source records
- 022CR19NI10N · 11 source records
- 022CR19NI13MO3 · 11 source records
- 022CR19NI13MO4N · 1 source record
- 022CR19NI16MO5N · 1 source record
- 022CR19NI5MO3SI2N · 11 source records
- 022CR19NI9 · 1 source record · Original-source verification pending
- 022CR21MN2NI2MON · 1 source record · Original-source verification pending
- 022CR22MN3NI2MON · 2 source records · Original-source verification pending
- 022CR22NI5MO3N · 13 source records
- 022CR23NI4MOCUN · 1 source record
- 022CR23NI5MO3N · 12 source records
- 022CR24NI17MO5MN6NBN · 1 source record
- 022CR25NI22MO2N · 1 source record
- 022CR25NI6MO2N · 7 source records
- 022CR25NI7MO3WCUN · 1 source record
- 022CR25NI7MO4N · 10 source records
- 022CR25NI7MO4WCUN · 1 source record
- 03CR18NI16MO5 · 1 source record
- 03CR21MN5NI1MOCUN · 1 source record · Original-source verification pending
- 03CR21NI1MOCUN · 1 source record · Original-source verification pending
- 03CR22MN5NI2CUMON · 1 source record · Original-source verification pending
- 03CR22NI2MOCUN · 1 source record · Original-source verification pending
- 03CR25NI6MO3CU2N · 1 source record
- 04CR13NI5MO · 1 source record
- 04CR13NI8MO2AL · 1 source record
- 05CR15NI5CU4NB · 1 source record
- 05CR17NI4CU4NB · 12 source records
- 05CR19NI10SI2CEN · 1 source record
- 06CR11TI · 1 source record
- 06CR13 · 12 source records
- 06CR13AL · 13 source records
- 06CR15NI25TI2MOALVB · 6 source records
- 06CR16NI18 · 1 source record
- 06CR17NI12MO2 · 21 source records
- 06CR17NI12MO2N · 1 source record
- 06CR17NI12MO2NB · 1 source record
- 06CR17NI12MO2TI · 13 source records
- 06CR17NI7ALTI · 5 source records
- 06CR18NI11NB · 15 source records
- 06CR18NI11TI · 20 source records
- 06CR18NI12 · 1 source record
- 06CR18NI12MO2CU2 · 1 source record
- 06CR18NI13SI4 · 2 source records
- 06CR18NI9CU2 · 1 source record
- 06CR18NI9CU3 · 1 source record
- 06CR19NI10 · 24 source records
- 06CR19NI10N · 12 source records
- 06CR19NI13MO3 · 2 source records
- 06CR19NI9 · 2 source records · Original-source verification pending
- 06CR19NI9NBN · 1 source record
- 06CR20NI11 · 1 source record
- 06CR23NI13 · 14 source records
- 06CR25NI20 · 15 source records
- 06NI3MODG · 1 source record · Original-source verification pending
- 06NI9DR · 5 source records · Original-source verification pending
- 07CR12NI4MN5MO3AL · 1 source record
- 07CR15NI7MO2AL · 1 source record
- 07CR17NI12MO2 · 1 source record
- 07CR17NI7AL · 11 source records
- 07CR18NI11NB · 1 source record
- 07CR19NI10 · 14 source records
- 07CR19NI11TI · 1 source record
- 07CR25NI20 · 1 source record · Original-source verification pending
- 07CR25NI21 · 2 source records · Original-source verification pending
- 08 · 2 source records
- 08AL · 2 source records
- 08B · 1 source record
- 08F · 1 source record
- 08NI3DR · 5 source records · Original-source verification pending
- 09CR17NI5MO3N · 1 source record
- 09DG · 1 source record · Original-source verification pending
- 09Х17Н7Ю · 1 source record · Original-source verification pending
- 0CR17NI4CU4NB · 2 source records · Original-source verification pending
- 0CR18NI11NB · 1 source record · Original-source verification pending
- 0CR18NI12MO2TI · 2 source records · Original-source verification pending
- 1.0425 · 2 source records · Original-source verification pending
- 1.0456 · 1 source record · Original-source verification pending
- 1.0481 · 1 source record · Original-source verification pending
- 1.0487 · 1 source record · Original-source verification pending
- 1.0565 · 1 source record · Original-source verification pending
- 1.0575 · 1 source record · Original-source verification pending
- 1.0580 · 1 source record · Original-source verification pending
- 1.0599 · 1 source record · Original-source verification pending
- 1.0644 · 1 source record · Original-source verification pending
- 1.1127 · 1 source record · Original-source verification pending
- 1.1151 · 1 source record · Original-source verification pending
- 1.4104 · 1 source record
- 1.4306 · 1 source record · Original-source verification pending
- 1.4307 · 1 source record · Original-source verification pending
- 1.4311 · 1 source record · Original-source verification pending
- 1.4362 · 1 source record · Original-source verification pending
- 1.4404 · 2 source records · Original-source verification pending
- 1.4410 · 1 source record · Original-source verification pending
- 1.4418 · 1 source record
- 1.4432 · 1 source record · Original-source verification pending
- 1.4439 · 2 source records · Original-source verification pending
- 1.4462 · 1 source record · Original-source verification pending
- 1.4501 · 1 source record · Original-source verification pending
- 1.4507 · 1 source record · Original-source verification pending
- 1.4529 · 1 source record · Original-source verification pending
- 1.4541 · 1 source record · Original-source verification pending
- 1.4550 · 1 source record · Original-source verification pending
- 1.4558 · 1 source record
- 1.4571 · 2 source records · Original-source verification pending
- 1.4954 · 1 source record · Original-source verification pending
- 1.6526 · 1 source record · Original-source verification pending
- 1.7014 · 1 source record · Original-source verification pending
- 1.7030 · 1 source record · Original-source verification pending
- 1.7035 · 1 source record
- 1.7036 · 1 source record · Original-source verification pending
- 1.7220 · 2 source records
- 1.7225 · 1 source record · Original-source verification pending
- 1.7319 · 1 source record · Original-source verification pending
- 1.7320 · 1 source record · Original-source verification pending
- 1.7323 · 1 source record · Original-source verification pending
- 1.7333 · 1 source record · Original-source verification pending
- 1.7380 · 1 source record · Original-source verification pending
- 1.7383 · 2 source records · Original-source verification pending
- 10 · 5 source records
- 10-D · 3 source records
- 1002 · 2 source records
- 1003 · 1 source record
- 1004 · 1 source record
- 1005 · 8 source records
- 1006 · 8 source records
- 1007 · 1 source record
- 1008 · 16 source records
- 1009 · 2 source records
- 100CR6 · 4 source records
- 100CRMNMOSI8-4-6 · 4 source records
- 100CRMNSI4-4 · 4 source records
- 100CRMNSI6-4 · 4 source records
- 100CRMNSI6-6 · 4 source records
- 100CRMO 7 · 2 source records · Original-source verification pending
- 100CRMO7 · 5 source records
- 100CRMO7-3 · 8 source records
- 100CRMO7-4 · 4 source records
- 1010 · 18 source records
- 1011 · 2 source records
- 1012 · 8 source records
- 1013 · 6 source records
- 1015 · 17 source records
- 1016 · 18 source records
- 1017 · 8 source records
- 1018 · 9 source records
- 1018 CLASS A · 1 source record
- 1018B · 1 source record
- 1018B-M · 1 source record
- 1019 · 6 source records
- 1020 · 17 source records
- 1021 · 21 source records
- 1021B · 1 source record
- 1021B-M · 1 source record
- 1021BA · 1 source record
- 1022 · 15 source records
- 1023 · 7 source records
- 1023B-M · 1 source record
- 1025 · 14 source records
- 1026 · 14 source records
- 1028B-M · 1 source record
- 1029 · 7 source records
- 102CR17MO · 5 source records
- 102CR6 · 3 source records
- 1030 · 17 source records
- 1030B · 1 source record
- 1033 · 2 source records
- 1033B · 1 source record
- 1034 · 5 source records
- 1035 · 21 source records
- 1035 CLASS A · 2 source records
- 1035B · 1 source record
- 1037 · 10 source records
- 1038 · 10 source records
- 1038B · 1 source record
- 1038H · 3 source records
- 1039 · 9 source records
- 1040 · 20 source records
- 1042 · 9 source records
- 1043 · 11 source records
- 1044 · 9 source records
- 1045 · 17 source records
- 1045 CLASS A · 2 source records
- 1045 CLASS B · 2 source records
- 1045H · 3 source records
- 1046 · 9 source records
- 1049 · 11 source records
- 1050 · 24 source records
- 1050 CLASS A · 2 source records
- 1050 CLASS B · 2 source records
- 1050A · 3 source records
- 1050SH · 1 source record
- 1053 · 9 source records
- 1055 · 10 source records
- 1059 · 3 source records
- 105V · 2 source records
- 1060 · 10 source records
- 1064 · 3 source records
- 1065 · 7 source records
- 1069 · 5 source records
- 1070 · 20 source records
- 1070A · 1 source record
- 1071 · 3 source records
- 1074 · 6 source records
- 1075 · 6 source records
- 1078 · 7 source records
- 1080 · 7 source records
- 1084 · 6 source records
- 1085 · 4 source records
- 1086 · 7 source records
- 108CR17 · 1 source record
- 1090 · 7 source records
- 1095 · 7 source records
- 10B · 1 source record
- 10B16 · 2 source records
- 10B20 · 1 source record
- 10B21 · 4 source records
- 10B21-1 · 1 source record
- 10B21-2 · 1 source record
- 10B21-3 · 1 source record
- 10B21-D · 3 source records
- 10B21M · 2 source records
- 10B21(D) · 1 source record
- 10B22 · 2 source records
- 10B23 · 1 source record
- 10B23-D · 3 source records
- 10B23M · 1 source record
- 10B28 · 1 source record
- 10B29 · 3 source records
- 10B30 · 5 source records
- 10B30-D · 3 source records
- 10B33 · 6 source records
- 10B33-1 · 1 source record
- 10B33-D · 3 source records
- 10B33M · 1 source record
- 10B35 · 3 source records
- 10B35-D · 3 source records
- 10B38 · 2 source records
- 10B38-D · 3 source records
- 10B40 · 3 source records
- 10CR12NI3MO2VN · 1 source record
- 10CR15 · 1 source record
- 10CR17 · 12 source records
- 10CR17MN9NI4N · 1 source record
- 10CR17MO · 1 source record
- 10CR17MONB · 3 source records
- 10CR18NI12 · 1 source record
- 10CRMO 9 10 · 1 source record · Original-source verification pending
- 10CRMO 9-10 · 1 source record · Original-source verification pending
- 10CRMO9-10 · 6 source records · Original-source verification pending
- 10F · 1 source record
- 10L10 · 1 source record
- 10MNDG · 1 source record · Original-source verification pending
- 10NICR5-4 · 7 source records
- 10S20 · 3 source records
- 10SPB20 · 3 source records
- 11 CRMO 9-10 TA · 1 source record · Original-source verification pending
- 11 CRMO 9-10 TN+TT · 1 source record · Original-source verification pending
- 1100 · 3 source records
- 1108 · 3 source records
- 1109 · 2 source records
- 1110 · 3 source records
- 1116 · 2 source records
- 1116A · 1 source record
- 1117 · 8 source records
- 1117 CLASS A · 1 source record
- 1118 · 6 source records
- 1119 · 2 source records
- 1120 · 2 source records · Original-source verification pending
- 1126 · 2 source records
- 1132 · 4 source records
- 1137 · 8 source records
- 1137 CLASS A · 1 source record
- 1138 · 2 source records
- 1139 · 3 source records
- 1140 · 6 source records
- 1141 · 8 source records
- 1141 CLASS A · 1 source record
- 1141 CLASS B · 1 source record
- 1144 · 8 source records
- 1144 CLASS A · 1 source record
- 1144 CLASS B · 1 source record
- 1145 · 3 source records
- 1146 · 6 source records
- 1151 · 6 source records
- 11CR23NI18 · 1 source record
- 11CRMO 9-10 · 1 source record · Original-source verification pending
- 11CRMO9-10 · 5 source records · Original-source verification pending
- 11SMN30 · 5 source records
- 11SMN37 · 3 source records
- 11SMNPB30 · 3 source records
- 11SMNPB37 · 3 source records
- 11V41 · 1 source record
- 12 NI 14 · 1 source record · Original-source verification pending
- 1200 · 3 source records
- 1211 · 3 source records
- 1212 · 6 source records
- 1213 · 6 source records
- 1214 · 1 source record
- 1215 · 8 source records
- 1215A · 1 source record
- 1235 · 1 source record
- 125CR2 · 1 source record
- 12CR12 · 1 source record
- 12CR12MO · 2 source records
- 12CR13 · 18 source records
- 12CR16NI35 · 2 source records
- 12CR17MN6NI5N · 1 source record
- 12CR17NI7 · 1 source record
- 12CR18MN12NI2N · 2 source records · Original-source verification pending
- 12CR18MN9NI5N · 1 source record
- 12CR18NI9 · 1 source record
- 12CR18NI9SI3 · 1 source record
- 12CR1MOV · 2 source records
- 12CR1MOVA · 1 source record
- 12CR1MOVE · 1 source record
- 12CR21NI5TI · 1 source record
- 12CR2MO · 2 source records · Original-source verification pending
- 12CR2MOG · 4 source records · Original-source verification pending
- 12CR2NI4 · 3 source records
- 12CR2NI4A · 1 source record
- 12CR2NI4AH · 1 source record
- 12CR2NI4E · 1 source record
- 12CR2NI4H · 2 source records
- 12CR5MO · 2 source records
- 12CRMO · 8 source records
- 12CRMO4 · 6 source records
- 12CRMOA · 1 source record
- 12CRMOE · 1 source record
- 12CRMOG · 4 source records · Original-source verification pending
- 12CRMOV · 2 source records
- 12CRMOVA · 1 source record
- 12CRMOVE · 1 source record
- 12CRNI2 · 3 source records
- 12CRNI2A · 1 source record
- 12CRNI2E · 1 source record
- 12CRNI3 · 3 source records
- 12CRNI3A · 1 source record
- 12CRNI3E · 1 source record
- 12L13 · 2 source records
- 12L14 · 7 source records
- 12L15 · 2 source records
- 12MNV · 1 source record · Original-source verification pending
- 12NI14 · 6 source records · Original-source verification pending
- 12NICR14-6 · 2 source records
- 12NICR3-2 · 6 source records
- 1330 · 5 source records
- 1330H · 3 source records
- 1335 · 7 source records
- 1335H · 3 source records
- 1340 · 6 source records
- 1340H · 3 source records
- 1345 · 5 source records
- 1345H · 3 source records
- 1350 · 1 source record
- 1370 · 1 source record
- 1385 · 2 source records · Original-source verification pending
- 13CR11NI2W2MOV · 2 source records
- 13CR13MO · 5 source records
- 13CR14NI3W2VB · 1 source record · Original-source verification pending
- 13MOCRNI42-16-14 · 2 source records
- 140BH(CR140BH) · 1 source record · Original-source verification pending
- 14CR11MOV · 2 source records
- 14CR12NI2WMOVNB · 2 source records
- 14CR17NI2 · 8 source records
- 14CR18NI11SI4ALTI · 1 source record
- 14MNNB · 1 source record · Original-source verification pending
- 14MNVTIRE · 1 source record · Original-source verification pending
- 14NICRMO13-4 · 1 source record
- 15 · 8 source records
- 1513 · 3 source records
- 1515 · 1 source record
- 1518 · 2 source records
- 1521 · 1 source record
- 1522 · 5 source records
- 1522H · 3 source records
- 1524 · 10 source records
- 1524B · 1 source record
- 1524H · 3 source records
- 1525 · 2 source records
- 1525B · 1 source record
- 1525B-M · 1 source record
- 1525BA · 1 source record
- 1526 · 5 source records
- 1526H · 3 source records
- 1527 · 5 source records
- 153 MA · 1 source record · Original-source verification pending
- 1536 · 8 source records
- 1536B · 1 source record
- 1537BH · 1 source record
- 1541 · 14 source records
- 1541 CLASS A · 2 source records
- 1541 CLASS B · 2 source records
- 1541H · 3 source records
- 1547 · 4 source records
- 1548 · 5 source records
- 1551 · 2 source records
- 1552 · 6 source records
- 1561 · 2 source records
- 1566 · 5 source records
- 1572 · 2 source records
- 158CR12MOV · 1 source record
- 15B · 1 source record
- 15B2 · 4 source records
- 15B21H · 3 source records
- 15B22 · 1 source record
- 15B25 · 1 source record
- 15B25M · 1 source record
- 15B28H · 2 source records
- 15B30H · 2 source records
- 15B35H · 3 source records
- 15B37H · 3 source records
- 15B41 · 1 source record · Original-source verification pending
- 15B41H · 3 source records
- 15B48H · 3 source records
- 15B62H · 3 source records
- 15CR · 8 source records
- 15CR12WMOV · 2 source records
- 15CRA · 2 source records
- 15CRAH · 1 source record
- 15CRE · 1 source record
- 15CRH · 2 source records
- 15CRMN · 2 source records
- 15CRMNA · 1 source record
- 15CRMNBAH · 1 source record
- 15CRMNBH · 2 source records
- 15CRMNE · 1 source record
- 15CRMO · 5 source records
- 15CRMO4 · 2 source records
- 15CRMO4+H · 1 source record
- 15CRMOA · 1 source record
- 15CRMOAH · 1 source record
- 15CRMOE · 1 source record
- 15CRMOH · 2 source records
- 15CRNIMO · 1 source record
- 15CRNIMOA · 1 source record
- 15CRNIMOE · 1 source record
- 15F · 1 source record
- 15MN · 3 source records
- 15MNTI · 1 source record · Original-source verification pending
- 15MNV · 2 source records · Original-source verification pending
- 15MNVB · 2 source records
- 15MNVBA · 1 source record
- 15MNVBE · 1 source record
- 15MNVN · 1 source record · Original-source verification pending
- 15NICR13 · 1 source record
- 15SMN13 · 3 source records
- 16CR20NI14SI2 · 2 source records
- 16CR23NI13 · 2 source records
- 16CR25N · 4 source records
- 16CR25NI20SI2 · 2 source records
- 16CRMNAH · 1 source record
- 16CRMNH · 2 source records
- 16MN · 4 source records · Original-source verification pending
- 16MNCR 5 · 1 source record · Original-source verification pending
- 16MNCR5 · 25 source records
- 16MNCR5H · 1 source record
- 16MNCRB5 · 7 source records
- 16MNCRS5 · 10 source records
- 16MNDG · 1 source record · Original-source verification pending
- 16MNDR · 2 source records · Original-source verification pending
- 16MNNB · 1 source record · Original-source verification pending
- 16MNRE · 1 source record · Original-source verification pending
- 16NICR4 · 2 source records
- 16NICRMO16-5 · 2 source records
- 16NICRMO16-5+H · 1 source record
- 16NICRS4 · 2 source records
- 17-4PH · 3 source records · Original-source verification pending
- 17B2 · 6 source records
- 17CR 3 · 1 source record · Original-source verification pending
- 17CR16NI2 · 2 source records
- 17CR18NI9 · 1 source record
- 17CR2NI2H · 1 source record
- 17CR3 · 15 source records
- 17CRMNBAH · 1 source record
- 17CRMNBH · 2 source records
- 17CRNI6-6 · 7 source records
- 17CRS3 · 12 source records
- 17MN4 · 1 source record · Original-source verification pending
- 17MNB4 · 5 source records
- 17MNCR5 · 4 source records
- 17MNCR5+H · 1 source record
- 17NICRMO6-4 · 2 source records
- 17NICRMOS6-4 · 2 source records
- 17SMN20 · 2 source records
- 180BH(CR180BH) · 1 source record · Original-source verification pending
- 180H1 · 1 source record · Original-source verification pending
- 180H2 · 1 source record · Original-source verification pending
- 18B2 · 4 source records
- 18CR11NIMONBVN · 4 source records
- 18CR12MOVNBN · 2 source records
- 18CR2NI2MOH · 1 source record
- 18CR2NI4W · 2 source records
- 18CR2NI4WA · 2 source records
- 18CR2NI4WE · 1 source record
- 18CRMNNIMO · 1 source record
- 18CRMNNIMOA · 1 source record
- 18CRMNNIMOE · 1 source record
- 18CRMO4 · 14 source records
- 18CRMO4H · 1 source record · Original-source verification pending
- 18CRMOS4 · 12 source records
- 18CRNIMNMOA · 1 source record
- 18CRNIMO7 · 1 source record
- 18CRNIMO7-6 · 4 source records
- 18CRNIMO7-6+H · 1 source record
- 18MNB4 · 6 source records
- 18NB · 1 source record · Original-source verification pending
- 18NICR5-4 · 1 source record
- 18NICRMO14-6 · 4 source records
- 18NICRMO14-6+H · 1 source record
- 19MN6 · 1 source record
- 19MNB4 · 2 source records
- 19MNCR5 · 2 source records
- 19MNCR5+H · 1 source record
- 19MNV6 · 2 source records
- 19MNVS6 · 2 source records
- 1A30 · 1 source record
- 1A80 · 1 source record
- 1A80A · 1 source record
- 1A85 · 1 source record
- 1A90 · 1 source record
- 1A93 · 1 source record
- 1A95 · 1 source record
- 1A97 · 1 source record
- 1A99 · 1 source record
- 1CR12NI2WMOVNB · 1 source record · Original-source verification pending
- 1CR13 · 2 source records · Original-source verification pending
- 1CR17 · 3 source records · Original-source verification pending
- 1CR17NI2 · 1 source record · Original-source verification pending
- 1J06 · 1 source record · Original-source verification pending
- 1J13 · 1 source record · Original-source verification pending
- 1J50 · 2 source records · Original-source verification pending
- 1J54 · 2 source records · Original-source verification pending
- 1J67 · 2 source records · Original-source verification pending
- 1J83 · 2 source records · Original-source verification pending
- 1J85 · 2 source records · Original-source verification pending
- 1J86 · 2 source records · Original-source verification pending
- 1J91 · 1 source record · Original-source verification pending
- 2.4686 · 1 source record · Original-source verification pending
- 20 · 15 source records
- 2004 · 1 source record
- 2011 · 3 source records
- 2014 · 3 source records
- 2014A · 3 source records
- 2017 · 3 source records
- 2017A · 3 source records
- 2024 · 9 source records
- 2024T72 · 1 source record · Original-source verification pending
- 2024T81 · 1 source record · Original-source verification pending
- 2024T851 · 1 source record · Original-source verification pending
- 2030 · 2 source records
- 20B · 1 source record
- 20CR · 12 source records
- 20CR13 · 2 source records
- 20CR13MN9NI4 · 1 source record
- 20CR15MN15NI2N · 1 source record
- 20CR1AH · 1 source record
- 20CR1H · 2 source records
- 20CR25NI20 · 2 source records
- 20CR2NI4 · 3 source records
- 20CR2NI4A · 1 source record
- 20CR2NI4E · 1 source record
- 20CR3 · 2 source records
- 20CR3+H · 1 source record
- 20CR4 · 12 source records
- 20CR4+H · 1 source record
- 20CR4H · 1 source record · Original-source verification pending
- 20CRA · 1 source record
- 20CRAH · 1 source record
- 20CRE · 1 source record
- 20CRH · 4 source records
- 20CRMN · 2 source records
- 20CRMNA · 1 source record
- 20CRMNAH · 1 source record
- 20CRMNE · 1 source record
- 20CRMNH · 2 source records
- 20CRMNMO · 6 source records
- 20CRMNMOA · 1 source record
- 20CRMNMOAH · 1 source record
- 20CRMNMOE · 1 source record
- 20CRMNMOH · 4 source records
- 20CRMNSI · 5 source records
- 20CRMNSIA · 1 source record
- 20CRMNSIE · 1 source record
- 20CRMNTI · 5 source records
- 20CRMNTIA · 1 source record
- 20CRMNTIAH · 1 source record
- 20CRMNTIE · 1 source record
- 20CRMNTIH · 3 source records
- 20CRMO · 4 source records
- 20CRMO4 · 2 source records
- 20CRMO4+H · 1 source record
- 20CRMOA · 2 source records
- 20CRMOAH · 1 source record
- 20CRMOE · 1 source record
- 20CRMOH · 5 source records
- 20CRMOVTIB4-10 · 2 source records
- 20CRNI · 3 source records
- 20CRNI2MOAH · 1 source record
- 20CRNI2MOH · 2 source records
- 20CRNI3 · 3 source records
- 20CRNI3A · 1 source record
- 20CRNI3AH · 1 source record
- 20CRNI3E · 1 source record
- 20CRNI3H · 2 source records
- 20CRNIA · 1 source record
- 20CRNIE · 1 source record
- 20CRNIMO · 2 source records
- 20CRNIMOA · 1 source record
- 20CRNIMOAH · 1 source record
- 20CRNIMOE · 1 source record
- 20CRNIMOH · 4 source records
- 20CRS4 · 9 source records
- 20G · 5 source records · Original-source verification pending
- 20MN · 4 source records
- 20MN2 · 4 source records
- 20MN2A · 1 source record
- 20MN2E · 1 source record
- 20MN5 · 4 source records
- 20MNB4 · 11 source records
- 20MNB4-D · 3 source records
- 20MNB5 · 5 source records
- 20MNCR4-2 · 2 source records
- 20MNCR4-2+H · 1 source record
- 20MNCR5 · 5 source records
- 20MNCRMO4-2 · 2 source records
- 20MNCRMO4-2+H · 1 source record
- 20MNCRS5 · 9 source records
- 20MNG · 4 source records · Original-source verification pending
- 20MNMOB · 2 source records
- 20MNMOBA · 1 source record
- 20MNMOBE · 1 source record
- 20MNMONI4-5 · 1 source record
- 20MNNICRMO3-2 · 2 source records
- 20MNNICRMO3-2+H · 1 source record
- 20MNTIB · 2 source records
- 20MNTIBA · 1 source record
- 20MNTIBAH · 1 source record
- 20MNTIBE · 1 source record
- 20MNTIBH · 2 source records
- 20MNV · 3 source records
- 20MNVA · 1 source record
- 20MNVB · 2 source records
- 20MNVBA · 1 source record
- 20MNVBAH · 1 source record
- 20MNVBE · 1 source record
- 20MNVBH · 2 source records
- 20MNVE · 1 source record
- 20MNVS6 · 1 source record
- 20MOCR 4 · 1 source record · Original-source verification pending
- 20MOCR3 · 3 source records
- 20MOCR4 · 15 source records
- 20MOCRS3 · 3 source records
- 20MOCRS4 · 13 source records
- 20NICRMO13-4 · 1 source record
- 20NICRMO2 · 1 source record
- 20NICRMO2-2 · 16 source records
- 20NICRMO7 · 5 source records
- 20NICRMO7+H · 1 source record
- 20NICRMOS2 · 1 source record
- 20NICRMOS2-2 · 13 source records
- 20NICRMOS6-4 · 7 source records
- 20NIMO9-7 · 2 source records
- 20R · 1 source record · Original-source verification pending
- 20SIMN2MOV · 2 source records
- 20SIMN2MOVA · 1 source record
- 20SIMN2MOVE · 1 source record
- 2117 · 3 source records
- 2124 · 1 source record
- 21CR12MOV · 3 source records
- 21CRMOV5-7 · 2 source records
- 21MNCR5 · 2 source records
- 21NICRMO 2 · 1 source record · Original-source verification pending
- 21NICRMO2 · 1 source record · Original-source verification pending
- 21NICRMOS2 · 1 source record · Original-source verification pending
- 22 MNB4 · 1 source record
- 2205 · 14 source records · Original-source verification pending
- 2205 GRADE 420 · 2 source records
- 2205 GRADE 520 · 2 source records
- 2205 GRADE 550 · 2 source records
- 2205 GRADE 60 · 2 source records
- 2205 GRADE 75 · 2 source records
- 2205 GRADE 80 · 2 source records
- 220BH(CR220BH) · 1 source record · Original-source verification pending
- 2214 · 1 source record
- 2218 · 1 source record
- 2219 · 2 source records
- 22CR12NIWMOV · 2 source records
- 22CR20MN10NI2SI2N · 2 source records
- 22CR21NI12N · 2 source records
- 22CRMOAH · 1 source record
- 22CRMOH · 2 source records
- 22CRMOS 3-5 · 2 source records · Original-source verification pending
- 22CRMOS3-5 · 5 source records
- 22CRNIMOH · 1 source record
- 22MNB4 · 5 source records
- 22NICRMO12-5 · 1 source record
- 2304 · 10 source records · Original-source verification pending
- 2304 GRADE 420 · 1 source record
- 2304 GRADE 520 · 1 source record
- 2304 GRADE 550 · 1 source record
- 2304 GRADE 60 · 1 source record
- 2304 GRADE 75 · 1 source record
- 2304 GRADE 80 · 1 source record
- 23B2 · 5 source records
- 23MNB3 · 5 source records
- 23MNB4 · 7 source records
- 23MNB4-D · 3 source records
- 23MNB5 · 2 source records
- 23MNNIMOCR5-4 · 1 source record
- 23MNNIMOCR54 · 1 source record
- 24CR18NI8W2 · 1 source record
- 24CRMO13-6 · 1 source record
- 24CRMO4 · 1 source record · Original-source verification pending
- 24CRMOS4 · 1 source record · Original-source verification pending
- 24MNV6 · 1 source record
- 24NICRMO15-5 · 1 source record
- 25 · 10 source records
- 2507 · 11 source records · Original-source verification pending
- 25B · 1 source record
- 25CR2MO1V · 1 source record
- 25CR2MO1VA · 2 source records
- 25CR2MO1VE · 1 source record
- 25CR2MOV · 1 source record
- 25CR2MOVA · 2 source records
- 25CR2MOVE · 1 source record
- 25CR2NI4W · 2 source records
- 25CR2NI4WA · 2 source records
- 25CR2NI4WE · 1 source record
- 25CRH · 1 source record
- 25CRMNSI · 5 source records
- 25CRMNSIA · 1 source record
- 25CRMNSIE · 1 source record
- 25CRMO · 1 source record
- 25CRMO4 · 14 source records
- 25CRMOA · 1 source record
- 25CRMOE · 1 source record
- 25CRMOS4 · 10 source records
- 25MN · 4 source records
- 25MN4 · 1 source record
- 25MNB · 1 source record
- 25MNBA · 1 source record
- 25MNBE · 1 source record
- 25MNTIBRE · 2 source records
- 25MNTIBREA · 1 source record
- 25MNTIBREE · 1 source record
- 25SIMN2MOV · 2 source records
- 25SIMN2MOVA · 1 source record
- 25SIMN2MOVE · 1 source record
- 260BH(CR260BH) · 2 source records · Original-source verification pending
- 2618 · 1 source record
- 26CR18MN12SI2N · 2 source records
- 26MN5 · 1 source record · Original-source verification pending
- 26MNB5 · 5 source records
- 26NICRMO14-6 · 1 source record
- 27CRNIMOH · 1 source record
- 27MNB4 · 5 source records
- 27MNCRB5-2 · 6 source records
- 27NICRMOV15-6 · 1 source record
- 27SIMN · 4 source records
- 27SIMNA · 2 source records
- 27SIMNE · 2 source records
- 28B2 · 10 source records
- 28B2-D · 3 source records
- 28CR4 · 7 source records
- 28CRH · 1 source record
- 28CRS4 · 7 source records
- 28MN6 · 2 source records
- 28NICRMOV8-5 · 1 source record
- 28SIMNB · 1 source record
- 2A01 · 1 source record
- 2A02 · 1 source record
- 2A04 · 1 source record
- 2A06 · 1 source record
- 2A10 · 5 source records
- 2A11 · 1 source record
- 2A12 · 1 source record
- 2A13 · 1 source record
- 2A14 · 1 source record
- 2A16 · 1 source record
- 2A17 · 1 source record
- 2A20 · 1 source record
- 2A21 · 1 source record
- 2A25 · 1 source record
- 2A49 · 1 source record
- 2A50 · 1 source record
- 2A70 · 1 source record
- 2A80 · 1 source record
- 2A90 · 1 source record
- 2B11 · 1 source record
- 2B12 · 1 source record
- 2B16 · 1 source record
- 2B50 · 1 source record
- 2B70 · 1 source record
- 2CR12MOV · 1 source record · Original-source verification pending
- 2J12 · 1 source record · Original-source verification pending
- 2J21 · 1 source record · Original-source verification pending
- 2J212C · 1 source record · Original-source verification pending
- 2J212Y · 1 source record · Original-source verification pending
- 2J32 · 1 source record · Original-source verification pending
- 2J51 · 1 source record · Original-source verification pending
- 2J64 · 1 source record · Original-source verification pending
- 2J67 · 1 source record · Original-source verification pending
- 30 · 8 source records
- 3003 · 8 source records
- 3004 · 1 source record
- 3005 · 1 source record
- 300BH(CR300BH) · 1 source record · Original-source verification pending
- 302 · 2 source records
- 30347 · 1 source record · Original-source verification pending
- 303CU · 1 source record
- 304 · 26 source records
- 304H · 10 source records
- 304L · 20 source records
- 304LN · 9 source records
- 304N · 9 source records
- 304N1 · 1 source record
- 305 · 2 source records
- 309S · 8 source records
- 30CR · 7 source records
- 30CR13 · 11 source records
- 30CR2NI2MO · 1 source record
- 30CR2NI2MOA · 1 source record
- 30CR2NI2MOE · 1 source record
- 30CR2NI4MO · 1 source record
- 30CR2NI4MOA · 1 source record
- 30CR2NI4MOE · 1 source record
- 30CRA · 1 source record
- 30CRE · 1 source record
- 30CRMNSI · 6 source records
- 30CRMNSIA · 8 source records
- 30CRMNSIE · 1 source record
- 30CRMNSINI2A · 5 source records
- 30CRMNTI · 2 source records
- 30CRMNTIA · 1 source record
- 30CRMNTIE · 1 source record
- 30CRMO · 3 source records
- 30CRMOA · 2 source records
- 30CRMOE · 1 source record
- 30CRMOV9 · 2 source records
- 30CRNI3 · 3 source records
- 30CRNI3A · 1 source record
- 30CRNI3E · 1 source record
- 30CRNIMO · 1 source record
- 30CRNIMO8 · 8 source records
- 30CRNIMOA · 1 source record
- 30CRNIMOE · 1 source record
- 30MN · 3 source records
- 30MN2 · 2 source records
- 30MN2A · 1 source record
- 30MN2E · 1 source record
- 30MNB4 · 6 source records
- 30MNB4-D · 2 source records
- 30MNB5 · 5 source records
- 30MNCRB5-2 · 3 source records
- 30MNVS6 · 5 source records
- 30MNVS6MOD · 1 source record
- 30MOB1 · 5 source records
- 30MOCRV20-7 · 3 source records
- 30NICRMO16-6 · 3 source records
- 30SI2MNCRMOVE · 1 source record
- 30W4CR2V · 1 source record
- 3102 · 1 source record
- 3103 · 2 source records
- 3104 · 1 source record
- 3105 · 1 source record
- 310H · 4 source records · Original-source verification pending
- 310HCBN · 1 source record
- 310S · 10 source records
- 316 · 24 source records
- 316H · 1 source record
- 316L · 19 source records
- 316LN · 8 source records
- 316LN GRADE 420 · 1 source record
- 316LN GRADE 520 · 1 source record
- 316LN GRADE 550 · 1 source record
- 316LN GRADE 60 · 1 source record
- 316LN GRADE 75 · 1 source record
- 316LN GRADE 80 · 1 source record
- 316TI · 8 source records
- 317L · 11 source records
- 317LM · 2 source records · Original-source verification pending
- 317LMN · 4 source records · Original-source verification pending
- 31CRMOB2-1 · 4 source records
- 31NICRMO13-4 · 1 source record
- 31SI2MNCRMOVE · 1 source record
- 321 · 18 source records
- 321H · 2 source records
- 329 · 7 source records
- 32CR13MO · 1 source record
- 32CR2 · 1 source record
- 32CRB4 · 5 source records
- 32CRMO12 · 1 source record
- 32CRMOV12-28 · 2 source records
- 32CRS2 · 1 source record
- 3310 · 1 source record · Original-source verification pending
- 334 · 3 source records · Original-source verification pending
- 33B2 · 10 source records
- 33CRMOV12-9 · 2 source records
- 33MNCRB5-2 · 5 source records
- 33NICRMOV14-5 · 1 source record
- 33SIMNB7-3 · 1 source record
- 347 · 15 source records
- 347H · 6 source records
- 347HFG · 1 source record
- 34CR2NI2MO · 1 source record
- 34CR2NI2MOA · 1 source record
- 34CR2NI2MOE · 1 source record
- 34CR4 · 11 source records
- 34CRMO4 · 23 source records
- 34CRMOS4 · 12 source records
- 34CRNI2 · 1 source record
- 34CRNI2A · 1 source record
- 34CRNI2E · 1 source record
- 34CRNIMO6 · 15 source records
- 34CRS4 · 5 source records
- 34MNB5 · 2 source records
- 35 · 5 source records
- 350WT · 2 source records · Original-source verification pending
- 35B2 · 2 source records
- 35CR · 6 source records
- 35CR2NI4MO · 1 source record
- 35CR2NI4MOA · 1 source record
- 35CR2NI4MOE · 1 source record
- 35CRA · 1 source record
- 35CRE · 1 source record
- 35CRMNSI · 4 source records
- 35CRMNSIA · 2 source records
- 35CRMNSIE · 1 source record
- 35CRMO · 10 source records
- 35CRMO-D · 3 source records
- 35CRMO7 · 2 source records
- 35CRMOA · 2 source records
- 35CRMOE · 1 source record
- 35CRMOH · 1 source record
- 35CRMOV · 3 source records
- 35CRMOVA · 1 source record
- 35CRMOVE · 1 source record
- 35MN · 3 source records
- 35MN2 · 3 source records
- 35MN2A · 1 source record
- 35MN2E · 1 source record
- 35MNB · 1 source record
- 35MNBA · 1 source record
- 35MNBE · 1 source record
- 35NICR6 · 1 source record
- 35S20 · 3 source records
- 35SIMN · 3 source records
- 35SIMNA · 1 source record
- 35SIMNE · 1 source record
- 35SMN20 · 2 source records
- 35SMNPB20 · 2 source records
- 35SPB20 · 3 source records
- 36CRB4 · 4 source records
- 36CRNIMO4 · 5 source records
- 36MN6 · 1 source record · Original-source verification pending
- 36MNB4 · 6 source records
- 36NICRMO16 · 2 source records
- 36SMN14 · 3 source records
- 36SMNPB14 · 3 source records
- 37CR4 · 19 source records
- 37CRMO4 · 5 source records
- 37CRNI3 · 3 source records
- 37CRNI3A · 1 source record
- 37CRNI3E · 1 source record
- 37CRS4 · 13 source records
- 37CRV3 · 1 source record
- 37MN · 1 source record · Original-source verification pending
- 37MNB5 · 7 source records
- 37MO2 · 5 source records
- 37SIMN2MOV · 2 source records
- 37SIMN2MOVA · 1 source record
- 37SIMN2MOVE · 1 source record
- 380W · 2 source records · Original-source verification pending
- 384 · 1 source record
- 38B2 · 5 source records
- 38CR2 · 8 source records
- 38CRCOWV18-17-17 · 2 source records
- 38CRMOAL · 4 source records
- 38CRMOALA · 1 source record
- 38CRMOALE · 1 source record
- 38CRS2 · 1 source record
- 38CRSI · 3 source records
- 38CRSIA · 1 source record
- 38CRSIE · 1 source record
- 38MNB5 · 1 source record
- 38MNVS6 · 2 source records
- 38SI 7 · 1 source record · Original-source verification pending
- 38SI2 · 1 source record
- 38SI7 · 4 source records
- 38SMN28 · 3 source records
- 38SMNPB28 · 3 source records
- 39MNB5 · 2 source records
- 39MNCRB6-2 · 3 source records
- 39MNCRB6-4 · 1 source record
- 39NICRMO3 · 1 source record
- 3A21 · 1 source record
- 3CR13 · 2 source records · Original-source verification pending
- 3CR2MNNIMO · 4 source records · Original-source verification pending
- 3J09 · 2 source records · Original-source verification pending
- 3J21 · 1 source record · Original-source verification pending
- 3J240 · 1 source record · Original-source verification pending
- 3J60 · 2 source records · Original-source verification pending
- 40 · 8 source records
- 4004 · 1 source record
- 400W · 2 source records · Original-source verification pending
- 400WT · 2 source records · Original-source verification pending
- 4012 · 2 source records
- 4023 · 6 source records
- 4024 · 2 source records
- 4027 · 6 source records
- 4027H · 3 source records
- 4028 · 2 source records
- 4028H · 3 source records
- 4032 · 3 source records
- 4032H · 3 source records
- 4037 · 7 source records
- 4037B · 1 source record
- 4037H · 3 source records
- 4042 · 2 source records
- 4042H · 3 source records
- 4043A · 1 source record
- 4047 · 7 source records
- 4047A · 1 source record
- 4047H · 3 source records
- 405 · 8 source records
- 409 · 4 source records
- 40ACR · 1 source record
- 40ACR-D · 3 source records
- 40B · 4 source records
- 40B37 · 1 source record
- 40BA · 1 source record
- 40BE · 1 source record
- 40CR · 13 source records
- 40CR10SI2MO · 4 source records
- 40CR13 · 1 source record
- 40CRA · 1 source record
- 40CRAH · 1 source record
- 40CRE · 1 source record
- 40CRH · 4 source records
- 40CRMN · 2 source records
- 40CRMNA · 1 source record
- 40CRMNE · 1 source record
- 40CRMNMO · 3 source records
- 40CRMNMOA · 1 source record
- 40CRMNMOE · 1 source record
- 40CRMNNIMO8-6-4 · 3 source records
- 40CRMOV · 1 source record
- 40CRMOV13-9 · 1 source record
- 40CRMOV4-6 · 3 source records
- 40CRNI · 3 source records
- 40CRNI2MO · 1 source record
- 40CRNI2MOA · 4 source records
- 40CRNI2MOE · 1 source record
- 40CRNI2MOH · 1 source record
- 40CRNI2SI2MOVA · 1 source record
- 40CRNIA · 1 source record
- 40CRNIE · 1 source record
- 40CRNIMO · 6 source records
- 40CRNIMOA · 4 source records
- 40CRNIMOE · 1 source record
- 40CRV · 3 source records
- 40CRVA · 1 source record
- 40CRVE · 1 source record
- 40MN · 4 source records
- 40MN2 · 3 source records
- 40MN2A · 1 source record
- 40MN2E · 1 source record
- 40MNB · 3 source records
- 40MNBA · 1 source record
- 40MNBAH · 1 source record
- 40MNBE · 1 source record
- 40MNBH · 2 source records
- 40MNVB · 3 source records
- 40MNVBA · 1 source record
- 40MNVBE · 1 source record
- 40NICRMO7-3 · 3 source records
- 40SICRMNMO7-6-6 · 1 source record
- 40SIMNVBE · 1 source record
- 410 · 15 source records
- 410S · 6 source records
- 410X · 1 source record · Original-source verification pending
- 4118 · 12 source records
- 4118H · 4 source records
- 4120 · 8 source records
- 4120H · 2 source records
- 4121 · 3 source records
- 4130 · 6 source records
- 4130H · 3 source records
- 4135 · 11 source records
- 4135H · 3 source records
- 4137 · 12 source records
- 4137H · 3 source records
- 4140 · 17 source records
- 4140-D · 3 source records
- 4140H · 3 source records
- 4142 · 11 source records
- 4142H · 3 source records
- 4145 · 6 source records
- 4145H · 3 source records
- 4147 · 2 source records
- 4147H · 3 source records
- 415/F6NM · 1 source record
- 4150 · 6 source records
- 4150H · 3 source records
- 416 · 1 source record
- 4161 · 2 source records
- 4161H · 3 source records
- 41CR · 1 source record
- 41CR4 · 19 source records
- 41CRNIMO2 · 4 source records
- 41CRNIMOS2 · 4 source records
- 41CRS4 · 19 source records
- 41GR4 · 1 source record · Original-source verification pending
- 41NICRMO7-3-2 · 6 source records
- 420 · 1 source record
- 420J2 · 1 source record
- 429 · 1 source record
- 42CR9SI2 · 2 source records
- 42CRMO · 11 source records
- 42CRMO-D · 3 source records
- 42CRMO1NB · 2 source records
- 42CRMO4 · 33 source records
- 42CRMO4(H) · 1 source record · Original-source verification pending
- 42CRMO4-D · 2 source records
- 42CRMO5-6 · 2 source records
- 42CRMO6 · 1 source record
- 42CRMOA · 1 source record
- 42CRMOAH · 1 source record
- 42CRMOE · 1 source record
- 42CRMOH · 2 source records
- 42CRMOS 4 · 1 source record
- 42CRMOS4 · 16 source records
- 42CRMOV · 1 source record
- 42CRMOV(B440V) · 1 source record
- 42CRNI2SI2MOVA · 1 source record
- 42MN6 · 1 source record · Original-source verification pending
- 42NISICRMO8-7-3 · 2 source records
- 42SIMN · 3 source records
- 42SIMNA · 1 source record
- 42SIMNE · 1 source record
- 430 · 13 source records
- 430F · 1 source record
- 430TI · 1 source record · Original-source verification pending
- 431 · 11 source records
- 4320 · 6 source records
- 4320H · 4 source records
- 4330 MOD. · 1 source record · Original-source verification pending
- 4335 MOD. · 1 source record · Original-source verification pending
- 4340 · 15 source records
- 4340H · 3 source records
- 439 · 8 source records
- 43CRMNMO4-4 · 1 source record
- 43CRMO4 · 6 source records
- 43MNB5-3 · 1 source record
- 43MNB6-3 · 1 source record
- 440A MOD · 1 source record · Original-source verification pending
- 440C · 1 source record
- 441 · 1 source record · Original-source verification pending
- 4419 · 2 source records
- 4419H · 1 source record
- 4422 · 2 source records
- 4427 · 2 source records
- 443 · 1 source record · Original-source verification pending
- 44CRMNMO4-4 · 1 source record
- 44SMN28 · 3 source records
- 44SMNPB28 · 3 source records
- 45 · 15 source records
- 45/55 NICU RESISTANCE WIRE · 1 source record
- 45AH · 1 source record
- 45B · 3 source records
- 45BA · 1 source record
- 45BE · 1 source record
- 45CR · 4 source records
- 45CR14NI14W2MO · 2 source records
- 45CR9SI3 · 2 source records
- 45CRA · 1 source record
- 45CRAH · 1 source record
- 45CRE · 1 source record
- 45CRH · 2 source records
- 45CRNI · 3 source records
- 45CRNIA · 1 source record
- 45CRNIE · 1 source record
- 45CRNIMO1VA · 1 source record
- 45CRNIMOV · 2 source records
- 45CRNIMOVA · 2 source records
- 45CRNIMOVE · 1 source record
- 45H · 2 source records
- 45MN · 3 source records
- 45MN2 · 3 source records
- 45MN2A · 1 source record
- 45MN2E · 1 source record
- 45MNB · 3 source records
- 45MNBA · 1 source record
- 45MNBAH · 1 source record
- 45MNBE · 1 source record
- 45MNBH · 2 source records
- 45NICRMO16 · 2 source records
- 45SICRV6-2 · 1 source record
- 4615 · 5 source records
- 4617 · 3 source records
- 4620 · 11 source records
- 4620H · 4 source records
- 4621 · 2 source records
- 4621H · 1 source record
- 4626 · 2 source records
- 4626H · 1 source record
- 46CR2 · 8 source records
- 46CRS2 · 1 source record
- 46MNVS3 · 2 source records
- 46MNVS6 · 1 source record
- 46S20 · 3 source records
- 46SI7 · 2 source records
- 46SICRMO6 · 1 source record
- 46SPB20 · 3 source records
- 4715 · 2 source records
- 4718 · 2 source records
- 4718H · 3 source records
- 4720 · 2 source records
- 4720H · 4 source records
- 480WT · 2 source records · Original-source verification pending
- 4815 · 2 source records
- 4815H · 3 source records
- 4817 · 2 source records
- 4817H · 4 source records
- 4820 · 6 source records
- 4820H · 4 source records
- 48SI7 · 1 source record
- 4A01 · 1 source record
- 4A11 · 1 source record
- 4A13 · 1 source record
- 4A17 · 1 source record
- 4CR10SI2MO · 2 source records · Original-source verification pending
- 4CR5W2VSI · 2 source records · Original-source verification pending
- 4CRMN16-4 · 4 source records
- 4J338 · 1 source record · Original-source verification pending
- 4J46 · 1 source record · Original-source verification pending
- 50 · 8 source records
- 5005 · 1 source record
- 501 · 1 source record · Original-source verification pending
- 5015 · 2 source records
- 5019 · 1 source record
- 502 · 2 source records · Original-source verification pending
- 5040B · 1 source record
- 5041 · 1 source record
- 5046 · 2 source records
- 5046H · 3 source records
- 5050 · 3 source records
- 5052 · 3 source records
- 5056 · 3 source records
- 5082 · 1 source record
- 5083 · 3 source records
- 5086 · 3 source records
- 50B · 3 source records
- 50B40H · 3 source records
- 50B44 · 2 source records
- 50B44H · 3 source records
- 50B46 · 6 source records
- 50B46H · 3 source records
- 50B50 · 2 source records
- 50B50H · 3 source records
- 50B60 · 2 source records
- 50B60H · 3 source records
- 50BA · 1 source record
- 50BE · 1 source record
- 50BV30 · 2 source records
- 50CR · 2 source records
- 50CRA · 1 source record
- 50CRE · 1 source record
- 50CRMO · 1 source record
- 50CRMO4 · 7 source records
- 50CRMOA · 1 source record
- 50CRMOE · 1 source record
- 50CRMOV13-15 · 2 source records
- 50CRNI · 2 source records
- 50CRNIA · 1 source record
- 50CRNIE · 1 source record
- 50CRV · 5 source records
- 50CRV4 · 5 source records
- 50CRVA · 7 source records
- 50CRVE · 1 source record
- 50MN · 4 source records
- 50MN2 · 3 source records
- 50MN2A · 1 source record
- 50MN2E · 1 source record
- 50SICRMO6 · 1 source record
- 50WCRV8 · 2 source records
- 5115 · 6 source records
- 5120 · 10 source records
- 5120H · 4 source records
- 5130 · 13 source records
- 5130H · 3 source records
- 5132 · 6 source records
- 5132H · 3 source records
- 5135 · 7 source records
- 5135H · 3 source records
- 5140 · 10 source records
- 5140H · 3 source records
- 5145 · 2 source records
- 5145H · 1 source record
- 5147 · 2 source records
- 5147H · 3 source records
- 5150 · 6 source records
- 5150H · 3 source records
- 5154 · 3 source records
- 5154A · 1 source record
- 5155 · 2 source records
- 5155H · 3 source records
- 5160 · 6 source records
- 5160H · 3 source records
- 5182 · 1 source record
- 5183 · 1 source record
- 51B20-D · 3 source records
- 51B22-D · 3 source records
- 51B60 · 6 source records
- 51B60H · 3 source records
- 51CRMNV · 1 source record
- 51CRV4 · 18 source records
- 52100 · 4 source records
- 5251 · 1 source record
- 52CRMNMOV · 1 source record
- 52CRMOV4 · 3 source records
- 52SICRMNNI · 1 source record
- 52SICRNI5 · 1 source record
- 5356 · 1 source record
- 53CR21MN9NI4N · 2 source records
- 54 SICR 6 · 1 source record · Original-source verification pending
- 540CL · 1 source record · Original-source verification pending
- 5454 · 3 source records
- 5456 · 1 source record
- 54SICR6 · 3 source records
- 54SICRV6 · 2 source records
- 55 · 7 source records
- 5554 · 1 source record
- 55CR3 · 3 source records
- 55CRMN · 1 source record
- 55CRSIA · 1 source record · Original-source verification pending
- 55NICRMOV7 · 2 source records
- 55SICR · 2 source records
- 55SICR6-3 · 1 source record
- 55SICRA · 1 source record · Original-source verification pending
- 55SICRV · 1 source record
- 55SICRV6-3 · 1 source record
- 55SIMNVB · 1 source record
- 56MN4 · 2 source records
- 56SI2MNCR · 1 source record
- 56SI7 · 7 source records
- 56SICR7 · 6 source records
- 5754 · 3 source records
- 5A01 · 1 source record
- 5A02 · 6 source records
- 5A03 · 1 source record
- 5A05 · 1 source record
- 5A06 · 8 source records
- 5A12 · 1 source record
- 5A13 · 1 source record
- 5A30 · 1 source record
- 5A33 · 1 source record
- 5A41 · 1 source record
- 5A43 · 1 source record
- 5A66 · 1 source record
- 5B05 · 1 source record
- 5B06 · 1 source record
- 5CR5MOSIV1 · 1 source record · Original-source verification pending
- 5N02 · 1 source record
- 60 · 6 source records
- 60 SICR 7 · 1 source record · Original-source verification pending
- 6005 · 1 source record
- 6005A · 3 source records
- 6005C · 1 source record
- 6060 · 3 source records
- 6061 · 10 source records
- 6063 · 7 source records
- 6063A · 1 source record
- 6070 · 1 source record
- 6082 · 3 source records
- 60CR3 · 3 source records
- 60CRMN · 1 source record
- 60CRMNB · 1 source record
- 60CRMNMO · 1 source record
- 60CRMO3-1 · 1 source record
- 60CRMO3-2 · 1 source record
- 60CRMO3-3 · 2 source records
- 60MN · 4 source records
- 60SI2CR · 2 source records
- 60SI2CRA · 2 source records · Original-source verification pending
- 60SI2CRV · 2 source records
- 60SI2CRVA · 1 source record · Original-source verification pending
- 60SI2MN · 4 source records
- 60SI2MNA · 4 source records · Original-source verification pending
- 60SI2MNCRV · 1 source record
- 60SICRV7 · 1 source record
- 60WCRV8 · 2 source records
- 6101 · 3 source records
- 6101A · 1 source record
- 6118 · 2 source records
- 6118H · 3 source records
- 6150 · 10 source records
- 6150H · 3 source records
- 6181 · 3 source records
- 61SICR7 · 5 source records
- 6262 · 2 source records
- 630 · 9 source records
- 631 · 9 source records
- 632 · 5 source records · Original-source verification pending
- 634 · 5 source records · Original-source verification pending
- 635 · 6 source records · Original-source verification pending
- 6351 · 1 source record
- 65 · 10 source records
- 65MN · 11 source records
- 65SI2MNWA · 1 source record · Original-source verification pending
- 660 · 1 source record · Original-source verification pending
- 665 · 1 source record · Original-source verification pending
- 66SIMNCRMO6-6-4 · 2 source records
- 68CR17 · 7 source records
- 6A02 · 1 source record
- 6A51 · 1 source record
- 6B02 · 1 source record
- 6J22 · 1 source record · Original-source verification pending
- 6J422 · 1 source record · Original-source verification pending
- 6N01 · 1 source record
- 70 · 3 source records
- 7003 · 3 source records
- 7005 · 1 source record
- 7020 · 3 source records
- 7022 · 1 source record
- 7049A · 2 source records
- 7050 · 3 source records
- 7075 · 14 source records
- 70MN · 3 source records
- 70MN4 · 2 source records
- 70MNMOCR8 · 2 source records
- 70SI2CRA · 2 source records · Original-source verification pending
- 718 · 3 source records · Original-source verification pending
- 7204 · 1 source record
- 72BPG · 1 source record
- 7475 · 1 source record
- 75 · 2 source records
- 75NI8 · 1 source record
- 77BPG · 1 source record
- 7A01 · 1 source record
- 7A03 · 1 source record
- 7A04 · 1 source record
- 7A05 · 1 source record
- 7A09 · 4 source records
- 7A10 · 1 source record
- 7A15 · 1 source record
- 7A19 · 1 source record
- 7A31 · 1 source record
- 7A33 · 1 source record
- 7A52 · 1 source record
- 7CRMOBS4 · 1 source record
- 7MNB8 · 3 source records
- 7N01 · 1 source record
- 80 · 5 source records
- 80/20 NICR RESISTANCE WIRE · 1 source record
- 800H · 11 source records
- 8011 · 1 source record
- 8011A · 1 source record
- 8090 · 1 source record
- 80CR20SI2NI · 2 source records
- 80CRV2 · 1 source record
- 80MOCRV42-16 · 2 source records
- 8115 · 2 source records
- 8115M · 1 source record
- 81B45 · 2 source records
- 81B45H · 3 source records
- 82BPG · 1 source record
- 82BPG-A · 1 source record
- 82BPG-E · 1 source record
- 82BPG-EX · 1 source record
- 82BPG-EY · 1 source record
- 82BPG-KM · 1 source record
- 85 · 3 source records
- 85CR17 · 1 source record
- 8615 · 6 source records
- 8617 · 6 source records
- 8617H · 4 source records
- 8620 · 10 source records
- 8620H · 8 source records
- 8622 · 6 source records
- 8622H · 3 source records
- 8625 · 6 source records
- 8625H · 3 source records
- 8627 · 5 source records
- 8627H · 3 source records
- 8630 · 6 source records
- 8630H · 3 source records
- 8637 · 6 source records
- 8637H · 3 source records
- 8640 · 7 source records
- 8640H · 3 source records
- 8640M · 1 source record
- 8642 · 2 source records
- 8642H · 3 source records
- 8645 · 6 source records
- 8645H · 3 source records
- 8650 · 2 source records
- 8650H · 3 source records
- 8655 · 5 source records
- 8655H · 3 source records
- 8660 · 3 source records
- 8660H · 3 source records
- 86B30H · 3 source records
- 86B45H · 3 source records
- 8720 · 6 source records
- 8720H · 3 source records
- 8740 · 6 source records
- 8740H · 2 source records
- 87BPG-AY · 1 source record
- 8822 · 6 source records
- 8822H · 3 source records
- 8A06 · 1 source record
- 8CR4MO4V · 1 source record · Original-source verification pending
- 8CRMNMO15-4 · 1 source record
- 8CRMNMO16-4 · 1 source record
- 8MNSI7 · 3 source records
- 904L · 9 source records
- 90CR18MOV · 1 source record
- 90MNCRV8 · 2 source records
- 9254 · 5 source records
- 9255 · 2 source records
- 9259 · 5 source records
- 9259H · 2 source records
- 9260 · 6 source records
- 9260H · 3 source records
- 9310H · 2 source records
- 94B15H · 3 source records
- 94B17 · 2 source records
- 94B17H · 3 source records
- 94B30 · 2 source records
- 94B30H · 3 source records
- 95CR18 · 1 source record
- 95MNWCR5 · 2 source records
- 9MN2V · 2 source records · Original-source verification pending
- 9S20 · 1 source record
- A · 3 source records · Original-source verification pending
- A1021 GRADE A CLASS 1 · 2 source records · Original-source verification pending
- A1021 GRADE A CLASS 2 · 2 source records · Original-source verification pending
- A1021 GRADE A CLASS 3 · 2 source records · Original-source verification pending
- A1028 GRADE A CLASS 1 · 1 source record · Original-source verification pending
- A1028 GRADE A CLASS 2 · 1 source record · Original-source verification pending
- A1028 GRADE F CLASS 1 · 1 source record · Original-source verification pending
- A1050P · 1 source record · Original-source verification pending
- A106 CLASSB · 1 source record · Original-source verification pending
- A1070P · 1 source record · Original-source verification pending
- A108 GRADE 1008 · 1 source record · Original-source verification pending
- A108 GRADE 1010 · 1 source record · Original-source verification pending
- A108 GRADE 1015 · 1 source record · Original-source verification pending
- A108 GRADE 1016 · 1 source record · Original-source verification pending
- A108 GRADE 1020 · 1 source record · Original-source verification pending
- A108 GRADE 1022 · 1 source record · Original-source verification pending
- A108 GRADE 1025 · 1 source record · Original-source verification pending
- A108 GRADE 1030 · 1 source record · Original-source verification pending
- A108 GRADE 1035 · 1 source record · Original-source verification pending
- A108 GRADE 1040 · 1 source record · Original-source verification pending
- A108 GRADE 1045 · 1 source record · Original-source verification pending
- A108 GRADE 1050 · 1 source record · Original-source verification pending
- A135 GRADE B · 1 source record · Original-source verification pending
- A178 GRADE C · 1 source record · Original-source verification pending
- A182 F 22 CLASS 1 · 1 source record · Original-source verification pending
- A182 F 22 CLASS 3 · 1 source record · Original-source verification pending
- A182 F 53 CLASS 1 · 1 source record · Original-source verification pending
- A182 F 53 CLASS 2 · 1 source record · Original-source verification pending
- A182 F 6A CLASS 1 · 2 source records · Original-source verification pending
- A182 F 6A CLASS 2 · 2 source records · Original-source verification pending
- A182 F 6A CLASS 3 · 2 source records · Original-source verification pending
- A182 F 6A CLASS 4 · 2 source records · Original-source verification pending
- A182 F22 CLASS 1 · 1 source record · Original-source verification pending
- A182 F22 CLASS 3 · 1 source record · Original-source verification pending
- A193 B6 · 3 source records · Original-source verification pending
- A193 B6X · 3 source records · Original-source verification pending
- A193 B8 CLASS 1 · 4 source records · Original-source verification pending
- A193 B8 CLASS 1D · 4 source records · Original-source verification pending
- A193 B8 CLASS 2 · 4 source records · Original-source verification pending
- A193 B8 CLASS 2B · 4 source records · Original-source verification pending
- A193 B8A CLASS 1A · 4 source records · Original-source verification pending
- A193 B8C CLASS 1 · 4 source records · Original-source verification pending
- A193 B8C CLASS 2 · 4 source records · Original-source verification pending
- A193 B8CA CLASS 1A · 4 source records · Original-source verification pending
- A193 B8LN CLASS 1 · 4 source records · Original-source verification pending
- A193 B8LN CLASS 1D · 4 source records · Original-source verification pending
- A193 B8LNA CLASS 1A · 4 source records · Original-source verification pending
- A193 B8M CLASS 1 · 4 source records · Original-source verification pending
- A193 B8M CLASS 1D · 4 source records · Original-source verification pending
- A193 B8M CLASS 2 · 4 source records · Original-source verification pending
- A193 B8M2 CLASS 2B · 4 source records · Original-source verification pending
- A193 B8M3 CLASS 2C · 4 source records · Original-source verification pending
- A193 B8MA CLASS 1A · 3 source records · Original-source verification pending
- A193 B8MLN CLASS 1 · 4 source records · Original-source verification pending
- A193 B8MLN CLASS 1D · 4 source records · Original-source verification pending
- A193 B8MLNA CLASS 1A · 4 source records · Original-source verification pending
- A193 B8N CLASS 1B · 4 source records · Original-source verification pending
- A193 B8N CLASS 1D · 4 source records · Original-source verification pending
- A193 B8N CLASS 2 · 4 source records · Original-source verification pending
- A193 B8NA CLASS 1A · 4 source records · Original-source verification pending
- A193 B8R CLASS 1C · 4 source records · Original-source verification pending
- A193 B8R CLASS 1D · 4 source records · Original-source verification pending
- A193 B8RA CLASS 1C · 4 source records · Original-source verification pending
- A193 B8T CLASS 1 · 4 source records · Original-source verification pending
- A193 B8T CLASS 2 · 4 source records · Original-source verification pending
- A193 B8TA CLASS 1A · 4 source records · Original-source verification pending
- A194 GRADE 1 · 1 source record
- A194 GRADE 16 · 1 source record
- A194 GRADE 2 · 1 source record
- A194 GRADE 2H · 1 source record
- A194 GRADE 2HM · 1 source record
- A194 GRADE 3 · 5 source records
- A194 GRADE 6 · 5 source records
- A194 GRADE 6F · 2 source records
- A194 GRADE 7 · 1 source record
- A194 GRADE 7M · 1 source record
- A194 GRADE 8 · 5 source records
- A194 GRADE 8A · 5 source records
- A194 GRADE 8C · 5 source records
- A194 GRADE 8CA · 5 source records
- A194 GRADE 8CLN · 1 source record
- A194 GRADE 8CLNA · 1 source record
- A194 GRADE 8F · 2 source records
- A194 GRADE 8FA · 2 source records
- A194 GRADE 8LN · 5 source records
- A194 GRADE 8LNA · 5 source records
- A194 GRADE 8M · 5 source records
- A194 GRADE 8MA · 5 source records
- A194 GRADE 8MLCUN · 1 source record
- A194 GRADE 8MLCUNA · 1 source record
- A194 GRADE 8MLN · 5 source records
- A194 GRADE 8MLNA · 5 source records
- A194 GRADE 8MN · 1 source record
- A194 GRADE 8MNA · 1 source record
- A194 GRADE 8N · 5 source records
- A194 GRADE 8NA · 5 source records
- A194 GRADE 8P · 1 source record
- A194 GRADE 8PA · 1 source record
- A194 GRADE 8R · 5 source records
- A194 GRADE 8RA · 5 source records
- A194 GRADE 8S · 1 source record
- A194 GRADE 8SA · 1 source record
- A194 GRADE 8T · 5 source records
- A194 GRADE 8TA · 4 source records
- A194 GRADE 9C · 5 source records
- A194 GRADE 9CA · 5 source records
- A194 GRADE B8ML4CUN · 1 source record
- A203 GRADE D · 1 source record · Original-source verification pending
- A203 GRADE E · 1 source record · Original-source verification pending
- A203 GRADE F · 1 source record · Original-source verification pending
- A210 GRADE A-1 · 2 source records · Original-source verification pending
- A213 T2 · 2 source records · Original-source verification pending
- A213 T22 · 2 source records · Original-source verification pending
- A213 TP304 · 2 source records · Original-source verification pending
- A213 TP304H · 2 source records · Original-source verification pending
- A213 TP304L · 2 source records · Original-source verification pending
- A213 TP304LN · 2 source records · Original-source verification pending
- A213 TP304N · 2 source records · Original-source verification pending
- A213 TP309S · 2 source records · Original-source verification pending
- A213 TP310H · 2 source records · Original-source verification pending
- A213 TP310S · 2 source records · Original-source verification pending
- A213 TP316 · 2 source records · Original-source verification pending
- A213 TP316L · 2 source records · Original-source verification pending
- A213 TP316LN · 2 source records · Original-source verification pending
- A213 TP316TI · 2 source records · Original-source verification pending
- A213 TP317L · 2 source records · Original-source verification pending
- A213 TP317LM · 2 source records · Original-source verification pending
- A213 TP317LMN · 2 source records · Original-source verification pending
- A213 TP321 · 2 source records · Original-source verification pending
- A213 TP347 · 2 source records · Original-source verification pending
- A213 TP347H · 2 source records · Original-source verification pending
- A213 XM-19 · 2 source records · Original-source verification pending
- A242 TYPE 1 · 2 source records · Original-source verification pending
- A249 ALLOY 20 · 2 source records · Original-source verification pending
- A249 TP304 · 3 source records · Original-source verification pending
- A249 TP304H · 3 source records · Original-source verification pending
- A249 TP304L · 3 source records · Original-source verification pending
- A249 TP304LN · 3 source records · Original-source verification pending
- A249 TP304N · 3 source records · Original-source verification pending
- A249 TP309S · 3 source records · Original-source verification pending
- A249 TP310H · 3 source records · Original-source verification pending
- A249 TP310S · 3 source records · Original-source verification pending
- A249 TP316 · 3 source records · Original-source verification pending
- A249 TP316L · 3 source records · Original-source verification pending
- A249 TP316LN · 3 source records · Original-source verification pending
- A249 TP317L · 3 source records · Original-source verification pending
- A249 TP321 · 3 source records · Original-source verification pending
- A249 TP347 · 3 source records · Original-source verification pending
- A249 TP347H · 3 source records · Original-source verification pending
- A249 TPXM-19 · 3 source records · Original-source verification pending
- A250 GRADE T2 · 1 source record · Original-source verification pending
- A250 GRADE T22 · 1 source record · Original-source verification pending
- A268 TP XM-27 · 2 source records · Original-source verification pending
- A268 TP405 · 2 source records · Original-source verification pending
- A268 TP409 · 2 source records · Original-source verification pending
- A268 TP410 · 2 source records · Original-source verification pending
- A268 TP430 · 1 source record · Original-source verification pending
- A268 TP430 TI · 2 source records · Original-source verification pending
- A268 TP439 · 2 source records · Original-source verification pending
- A268 TP443 · 2 source records · Original-source verification pending
- A269 TP304 · 2 source records · Original-source verification pending
- A269 TP304L · 2 source records · Original-source verification pending
- A269 TP304LN · 2 source records · Original-source verification pending
- A269 TP316 · 2 source records · Original-source verification pending
- A269 TP316L · 2 source records · Original-source verification pending
- A269 TP316LN · 2 source records · Original-source verification pending
- A269 TP321 · 2 source records · Original-source verification pending
- A269 TP347 · 2 source records · Original-source verification pending
- A269 TPXM-19 · 2 source records · Original-source verification pending
- A270 TP304 · 2 source records · Original-source verification pending
- A270 TP304L · 2 source records · Original-source verification pending
- A270 TP316 · 2 source records · Original-source verification pending
- A270 TP316L · 2 source records · Original-source verification pending
- A283 GRADE C · 1 source record · Original-source verification pending
- A312 800H · 1 source record
- A312 ALLOY 20 · 1 source record · Original-source verification pending
- A312 TP304 · 1 source record · Original-source verification pending
- A312 TP304H · 1 source record · Original-source verification pending
- A312 TP304L · 1 source record
- A312 TP304LN · 1 source record · Original-source verification pending
- A312 TP304N · 1 source record · Original-source verification pending
- A312 TP309S · 1 source record · Original-source verification pending
- A312 TP310H · 1 source record · Original-source verification pending
- A312 TP310S · 1 source record · Original-source verification pending
- A312 TP316 · 1 source record · Original-source verification pending
- A312 TP316L · 1 source record
- A312 TP316LN · 1 source record · Original-source verification pending
- A312 TP316TI · 1 source record · Original-source verification pending
- A312 TP317L · 1 source record · Original-source verification pending
- A312 TP321 · 1 source record · Original-source verification pending
- A312 TP347 · 1 source record · Original-source verification pending
- A312 TP347H · 1 source record · Original-source verification pending
- A312 TPXM-19 · 1 source record · Original-source verification pending
- A320 B8 CLASS 1 · 4 source records · Original-source verification pending
- A320 B8 CLASS 2 · 4 source records · Original-source verification pending
- A320 B8A CLASS 1A · 4 source records · Original-source verification pending
- A320 B8C CLASS 1 · 4 source records · Original-source verification pending
- A320 B8C CLASS 2 · 4 source records · Original-source verification pending
- A320 B8CA CLASS 1A · 4 source records · Original-source verification pending
- A320 B8LN CLASS 1 · 4 source records · Original-source verification pending
- A320 B8LNA CLASS 1A · 4 source records · Original-source verification pending
- A320 B8M CLASS 1 · 4 source records · Original-source verification pending
- A320 B8M CLASS 2 · 4 source records · Original-source verification pending
- A320 B8MA CLASS 1A · 4 source records · Original-source verification pending
- A320 B8MLN CLASS 1 · 4 source records · Original-source verification pending
- A320 B8MLNA CLASS 1A · 4 source records · Original-source verification pending
- A320 B8T CLASS 1 · 4 source records · Original-source verification pending
- A320 B8T CLASS 2 · 4 source records · Original-source verification pending
- A320 B8TA CLASS 1A · 4 source records · Original-source verification pending
- A320 L43 · 4 source records · Original-source verification pending
- A320 L72 · 4 source records · Original-source verification pending
- A320 L7B · 4 source records · Original-source verification pending
- A322 1330 · 1 source record
- A322 1335 · 1 source record
- A322 1340 · 1 source record
- A322 1345 · 1 source record
- A322 4023 · 1 source record
- A322 4024 · 1 source record
- A322 4027 · 1 source record
- A322 4028 · 1 source record
- A322 4037 · 1 source record
- A322 4047 · 1 source record
- A322 4118 · 3 source records
- A322 4120 · 2 source records · Original-source verification pending
- A322 4121 · 2 source records · Original-source verification pending
- A322 4130 · 1 source record
- A322 4135 · 2 source records · Original-source verification pending
- A322 4137 · 3 source records
- A322 4140 · 3 source records
- A322 4142 · 3 source records
- A322 4145 · 1 source record
- A322 4147 · 1 source record
- A322 4150 · 1 source record
- A322 4161 · 1 source record
- A322 4320 · 1 source record
- A322 4340 · 3 source records
- A322 4615 · 1 source record
- A322 4620 · 3 source records
- A322 4621 · 1 source record
- A322 4626 · 1 source record
- A322 4720 · 1 source record
- A322 4815 · 1 source record
- A322 4817 · 1 source record
- A322 4820 · 1 source record
- A322 50B44 · 1 source record
- A322 50B46 · 1 source record
- A322 50B50 · 1 source record
- A322 50B60 · 1 source record
- A322 5117 · 1 source record
- A322 5120 · 3 source records
- A322 5130 · 3 source records
- A322 5132 · 1 source record
- A322 5135 · 3 source records
- A322 5140 · 3 source records
- A322 5150 · 1 source record
- A322 5155 · 1 source record
- A322 5160 · 1 source record
- A322 51B60 · 1 source record
- A322 6118 · 1 source record
- A322 6150 · 3 source records
- A322 81B45 · 1 source record
- A322 8615 · 1 source record
- A322 8617 · 1 source record
- A322 8620 · 3 source records
- A322 8622 · 1 source record
- A322 8625 · 1 source record
- A322 8627 · 1 source record
- A322 8630 · 1 source record
- A322 8637 · 1 source record
- A322 8640 · 1 source record
- A322 8642 · 1 source record
- A322 8645 · 1 source record
- A322 8655 · 1 source record
- A322 8720 · 1 source record
- A322 8740 · 1 source record
- A322 8822 · 1 source record
- A322 9259 · 1 source record
- A322 9260 · 1 source record
- A322 94B17 · 1 source record
- A322 94B30 · 1 source record
- A322 E4340 · 3 source records
- A322 E51100 · 1 source record
- A322 E52100 · 1 source record
- A322 G41200 · 1 source record
- A322 G41210 · 1 source record
- A322 G47150 · 1 source record
- A333 GRADE 1 · 2 source records · Original-source verification pending
- A333 GRADE 3 · 2 source records · Original-source verification pending
- A333 GRADE 6 · 2 source records · Original-source verification pending
- A335 GRADE P2 · 3 source records · Original-source verification pending
- A335 GRADE P22 · 3 source records · Original-source verification pending
- A350 GRADE LF2 CLASS 1 · 2 source records · Original-source verification pending
- A350 GRADE LF6 CLASS 1 · 2 source records · Original-source verification pending
- A351 CF8M · 2 source records · Original-source verification pending
- A36 · 2 source records · Original-source verification pending
- A387 GRADE22 CLASS1 · 1 source record · Original-source verification pending
- A387 GRADE22 CLASS2 · 1 source record · Original-source verification pending
- A387 GRADE5 CLASS1 · 1 source record · Original-source verification pending
- A387 GRADE5 CLASS2 · 1 source record · Original-source verification pending
- A414 GRADE C · 1 source record · Original-source verification pending
- A414 GRADE D · 1 source record · Original-source verification pending
- A414 GRADE E · 1 source record · Original-source verification pending
- A414 GRADE F · 1 source record · Original-source verification pending
- A485 100CRMNMOSI 8-4-6 · 1 source record · Original-source verification pending
- A485 100CRMO 7 · 1 source record · Original-source verification pending
- A485 100CRMO 7-3 · 1 source record · Original-source verification pending
- A492 304 · 1 source record · Original-source verification pending
- A492 316 · 1 source record · Original-source verification pending
- A492 XM-17 · 1 source record · Original-source verification pending
- A515 GRADE 60 · 2 source records · Original-source verification pending
- A515 GRADE 65 · 2 source records · Original-source verification pending
- A515 GRADE 70 · 2 source records · Original-source verification pending
- A516 GRADE 60 · 2 source records · Original-source verification pending
- A516 GRADE 65 · 2 source records · Original-source verification pending
- A516 GRADE 70 · 2 source records · Original-source verification pending
- A529 GRADE 50 · 2 source records · Original-source verification pending
- A529 GRADE 55 · 2 source records · Original-source verification pending
- A537 CLASS 1 · 1 source record · Original-source verification pending
- A556 GRADE B2 · 2 source records · Original-source verification pending
- A572 GRADE 55 · 1 source record · Original-source verification pending
- A572 GRADE 60 · 1 source record · Original-source verification pending
- A572 GRADE 65 · 1 source record · Original-source verification pending
- A573 GRADE 70 · 2 source records · Original-source verification pending
- A574 GRADE 4137 · 2 source records · Original-source verification pending
- A574 GRADE 4142 · 2 source records · Original-source verification pending
- A574 GRADE 4340 · 2 source records · Original-source verification pending
- A576 1008 · 2 source records
- A576 1010 · 2 source records
- A576 1012 · 1 source record
- A576 1015 · 2 source records
- A576 1016 · 2 source records
- A576 1017 · 1 source record
- A576 1018 · 1 source record
- A576 1019 · 1 source record
- A576 1020 · 2 source records
- A576 1021 · 2 source records
- A576 1022 · 2 source records
- A576 1023 · 1 source record
- A576 1025 · 2 source records
- A576 1026 · 2 source records
- A576 1029 · 1 source record
- A576 1030 · 2 source records
- A576 1035 · 2 source records
- A576 1037 · 2 source records
- A576 1038 · 2 source records
- A576 1039 · 2 source records
- A576 1040 · 2 source records
- A576 1042 · 2 source records
- A576 1043 · 2 source records
- A576 1044 · 2 source records
- A576 1045 · 2 source records
- A576 1046 · 2 source records
- A576 1049 · 2 source records
- A576 1050 · 2 source records
- A576 1053 · 2 source records
- A576 1055 · 2 source records
- A576 1060 · 1 source record
- A576 1070 · 2 source records
- A576 1078 · 1 source record
- A576 1080 · 1 source record
- A576 1084 · 1 source record
- A576 1090 · 1 source record
- A576 1095 · 1 source record
- A576 1109 · 1 source record
- A576 1110 · 1 source record
- A576 1116 · 1 source record
- A576 1117 · 1 source record
- A576 1118 · 1 source record
- A576 1119 · 1 source record
- A576 1132 · 1 source record
- A576 1137 · 1 source record
- A576 1139 · 1 source record
- A576 1140 · 1 source record
- A576 1141 · 1 source record
- A576 1144 · 1 source record
- A576 1145 · 1 source record
- A576 1146 · 1 source record
- A576 1151 · 1 source record
- A576 1211 · 1 source record
- A576 1212 · 1 source record
- A576 1213 · 1 source record
- A576 1215 · 1 source record
- A576 12L14 · 1 source record
- A576 1513 · 1 source record
- A576 1518 · 1 source record
- A576 1522 · 1 source record
- A576 1524 · 2 source records
- A576 1525 · 1 source record
- A576 1526 · 1 source record
- A576 1527 · 1 source record
- A576 1536 · 2 source records
- A576 1541 · 2 source records
- A576 1547 · 1 source record
- A576 1548 · 1 source record
- A576 1551 · 1 source record
- A576 1552 · 1 source record
- A576 1561 · 1 source record
- A576 1566 · 1 source record
- A576 1572 · 1 source record
- A588 GRADE A · 2 source records · Original-source verification pending
- A588 GRADE B · 2 source records · Original-source verification pending
- A588 GRADE K · 2 source records · Original-source verification pending
- A595 GRADE A · 1 source record · Original-source verification pending
- A595 GRADE B · 1 source record · Original-source verification pending
- A597 CM-2 · 1 source record · Original-source verification pending
- A600 M2 · 2 source records · Original-source verification pending
- A633 GRADE C · 2 source records · Original-source verification pending
- A633 GRADE D · 2 source records · Original-source verification pending
- A633 GRADE E · 2 source records · Original-source verification pending
- A638 GRADE 660 · 1 source record · Original-source verification pending
- A656 GRADE 60[415] TYPE 3 · 1 source record · Original-source verification pending
- A656 GRADE 60[415] TYPE 7 · 1 source record · Original-source verification pending
- A656 GRADE 60[415] TYPE 8 · 1 source record · Original-source verification pending
- A656 GRADE 70[485] TYPE 3 · 1 source record · Original-source verification pending
- A656 GRADE 70[485] TYPE 7 · 1 source record · Original-source verification pending
- A656 GRADE 70[485] TYPE 8 · 1 source record · Original-source verification pending
- A662 GRADE A · 1 source record · Original-source verification pending
- A662 GRADE B · 1 source record · Original-source verification pending
- A662 GRADE C · 1 source record · Original-source verification pending
- A681 TYPE D3 · 2 source records · Original-source verification pending
- A681 TYPE H10 · 2 source records · Original-source verification pending
- A681 TYPE H11 · 2 source records · Original-source verification pending
- A681 TYPE O1 · 2 source records · Original-source verification pending
- A681 TYPE P20 · 2 source records · Original-source verification pending
- A709 GRADE 36 · 2 source records · Original-source verification pending
- A709 GRADE 50W · 1 source record · Original-source verification pending
- A709 GRADE HPS 70W · 1 source record · Original-source verification pending
- A710 GRADE A CLASS 2 · 1 source record · Original-source verification pending
- A710 GRADE A CLASS 3 · 1 source record · Original-source verification pending
- A737 GRADE B · 1 source record · Original-source verification pending
- A743 CF8M · 1 source record · Original-source verification pending
- A744 CF8M · 1 source record · Original-source verification pending
- A756 440C · 3 source records · Original-source verification pending
- A756 X30CRMON15-1 · 2 source records · Original-source verification pending
- A774 TP 304L · 2 source records · Original-source verification pending
- A774 TP 316L · 2 source records · Original-source verification pending
- A774 TP 317L · 2 source records · Original-source verification pending
- A774 TP 321 · 2 source records · Original-source verification pending
- A774 TP 347 · 2 source records · Original-source verification pending
- A778 TP 304L · 1 source record · Original-source verification pending
- A778 TP 316L · 1 source record · Original-source verification pending
- A778 TP 317L · 1 source record · Original-source verification pending
- A778 TP 321 · 1 source record · Original-source verification pending
- A778 TP 347 · 1 source record · Original-source verification pending
- A793 TYPE 304 · 1 source record · Original-source verification pending
- A793 TYPE 304L · 1 source record · Original-source verification pending
- A793 TYPE 316 · 1 source record · Original-source verification pending
- A793 TYPE 316L · 1 source record · Original-source verification pending
- A803 TP XM-27 · 2 source records · Original-source verification pending
- A803 TP409 · 2 source records · Original-source verification pending
- A803 TP439 · 2 source records · Original-source verification pending
- A813 TP304 · 1 source record · Original-source verification pending
- A813 TP304H · 1 source record · Original-source verification pending
- A813 TP304L · 1 source record · Original-source verification pending
- A813 TP304LN · 1 source record · Original-source verification pending
- A813 TP304N · 1 source record · Original-source verification pending
- A813 TP309S · 1 source record · Original-source verification pending
- A813 TP310S · 1 source record · Original-source verification pending
- A813 TP316 · 1 source record · Original-source verification pending
- A813 TP316L · 1 source record · Original-source verification pending
- A813 TP316LN · 1 source record · Original-source verification pending
- A813 TP317L · 1 source record · Original-source verification pending
- A813 TP321 · 1 source record · Original-source verification pending
- A813 TP347 · 1 source record · Original-source verification pending
- A813 TP347H · 1 source record · Original-source verification pending
- A813 TPXM-19 · 1 source record · Original-source verification pending
- A814 TP 304 · 1 source record
- A814 TP 304H · 1 source record
- A814 TP 304L · 1 source record
- A814 TP 304LN · 1 source record
- A814 TP 304N · 1 source record
- A814 TP 309S · 1 source record
- A814 TP 310S · 1 source record
- A814 TP 316 · 1 source record
- A814 TP 316L · 1 source record
- A814 TP 316LN · 1 source record
- A814 TP 317L · 1 source record
- A814 TP 321 · 1 source record
- A814 TP 347 · 1 source record
- A814 TP 347H · 1 source record
- A814 TP XM-19 · 1 source record
- A826 TP 316 · 1 source record · Original-source verification pending
- A831 316 · 1 source record · Original-source verification pending
- A837 4620 · 1 source record · Original-source verification pending
- A837 8620 · 1 source record · Original-source verification pending
- A841 GRADE A CLASS 1 · 2 source records · Original-source verification pending
- A841 GRADE B CLASS 1 · 2 source records · Original-source verification pending
- A841 GRADE C CLASS 1 · 2 source records · Original-source verification pending
- A851 TP304 · 1 source record · Original-source verification pending
- A851 TP304L · 1 source record · Original-source verification pending
- A955 GRADE 420 · 1 source record
- A955 GRADE 520 · 1 source record
- A955 GRADE 550 · 1 source record
- A955 GRADE 60 · 1 source record
- A955 GRADE 75 · 1 source record
- A955 GRADE 80 · 1 source record
- A982 GRADE A CLASS 1 · 1 source record · Original-source verification pending
- A982 GRADE A CLASS 2 · 1 source record · Original-source verification pending
- A982 GRADE F CLASS 1 · 1 source record · Original-source verification pending
- ACUZINC5 · 1 source record · Original-source verification pending
- AH32 · 2 source records · Original-source verification pending
- AH36 · 2 source records · Original-source verification pending
- AISI 4140 · 1 source record · Original-source verification pending
- AL-6XN · 1 source record · Original-source verification pending
- ALCU4MG1 · 1 source record · Original-source verification pending
- ALCU6BIPB · 1 source record · Original-source verification pending
- ALCUMG2 · 1 source record · Original-source verification pending
- ALLOY 2 · 2 source records · Original-source verification pending
- ALLOY 20 · 3 source records · Original-source verification pending
- ALLOY 20 CB 3 · 2 source records
- ALLOY 3 · 1 source record · Original-source verification pending
- ALLOY 6B · 1 source record · Original-source verification pending
- ALLOY 7 · 1 source record · Original-source verification pending
- ALLOY 800HT · 1 source record · Original-source verification pending
- ALLOY4750 · 2 source records · Original-source verification pending
- ALMG1SICU · 2 source records · Original-source verification pending
- ALMNCU · 1 source record · Original-source verification pending
- ALZN5.5MGCU · 1 source record · Original-source verification pending
- ALZNMGCU 1.5 · 1 source record · Original-source verification pending
- ALZNMGCU1.5 F48 · 1 source record · Original-source verification pending
- ALZNMGCU1.5 F50 · 2 source records · Original-source verification pending
- ALZNMGCU1.5 F51 · 1 source record · Original-source verification pending
- ALZNMGCU1.5 F52 · 1 source record · Original-source verification pending
- ALZNMGCU1.5 F53 · 1 source record · Original-source verification pending
- AMS 5596 · 1 source record · Original-source verification pending
- ASBO20 · 1 source record
- ASBO25 · 1 source record
- ASBO28 · 1 source record
- ASBO30 · 1 source record
- ASBO33 · 1 source record
- ASBO35 · 1 source record
- ASBO38 · 1 source record
- ASBO40 · 1 source record
- ASBO43 · 1 source record
- ASBO45 · 1 source record
- ASBO48 · 1 source record
- ASBO50 · 1 source record
- ASBO53 · 1 source record
- ASCB435H · 1 source record
- ASCB440H · 1 source record
- ASCM115H · 1 source record
- ASCM118H · 1 source record
- ASCM120H · 1 source record
- ASCM125H · 1 source record
- ASCM315H · 1 source record
- ASCM318H · 1 source record
- ASCM320H · 1 source record
- ASCM325H · 1 source record
- ASCM430H · 1 source record
- ASCR418H · 1 source record
- ASCR423H · 1 source record
- ASCR425H · 1 source record
- ASCR445H · 1 source record
- ASMN420H · 1 source record
- ASMN425H · 1 source record
- ASMN430H · 1 source record
- ASMN435H · 1 source record
- ASMN440H · 1 source record
- ASMN443H · 1 source record
- ASMN448H · 1 source record
- ASMN453H · 1 source record
- ASMNB220H · 1 source record
- ASMNB233H · 1 source record
- ASMNB422H · 1 source record
- ASMNB425H · 1 source record
- ASMNB433H · 1 source record
- ASMNB443H · 1 source record
- ASMNC420H · 1 source record
- ASMNC520H · 1 source record
- ASMNC543H · 1 source record
- ASMNCB440H · 1 source record
- ASTMA36 · 1 source record
- B · 2 source records · Original-source verification pending
- B-10B21 · 1 source record
- B-10B30 · 1 source record
- B-1340 · 1 source record
- B-30MNB4 · 1 source record
- B-40ACR · 1 source record
- B-40CRMO · 1 source record
- B-45MN2 · 1 source record
- B-ML15 · 1 source record
- B-ML20MNTIB · 1 source record
- B-ML20MNVB · 1 source record
- B-ML40CR · 1 source record
- B-MNB120H · 1 source record
- B-S10C · 1 source record
- B-S15C · 1 source record
- B-S20C · 1 source record
- B-S25C · 1 source record
- B-S45C · 1 source record
- B-SCM435 · 1 source record
- B-SCM435H · 1 source record
- B-SCM440 · 1 source record
- B-SCM440H · 2 source records
- B-SCR440 · 1 source record
- B-SWRCH10A · 1 source record
- B-SWRCH15A · 1 source record
- B-SWRCH15K · 2 source records
- B-SWRCH18A · 1 source record
- B-SWRCH22A · 1 source record
- B-SWRCH25K · 2 source records
- B-SWRCH35K · 1 source record
- B-SWRCH38K · 1 source record
- B-SWRCH38K-1 · 2 source records
- B-SWRCH40K · 1 source record
- B-SWRCH40K-1 · 1 source record
- B-SWRCH45K · 1 source record
- B-SWRCH6A · 1 source record
- B-SWRCH8A · 1 source record
- B0.6 · 2 source records
- B103 C51100 · 1 source record · Original-source verification pending
- B16 · 1 verified composition source
- B19 · 2 source records
- B23 · 1 source record
- B241 6063 · 1 source record · Original-source verification pending
- B25 · 2 source records
- B271 C95300 · 1 source record · Original-source verification pending
- B271 C95400 · 1 source record · Original-source verification pending
- B271 C95500 · 1 source record · Original-source verification pending
- B30 · 2 source records
- B316 5052 · 2 source records · Original-source verification pending
- B320L · 1 source record
- B330CL · 1 source record
- B369 C96400 · 2 source records · Original-source verification pending
- B380CL · 1 source record
- B420L · 1 source record
- B440HP · 1 source record
- B440QZR · 1 source record
- B440V · 1 source record
- B480QZR · 1 source record
- B490HP · 1 source record
- B510DL · 1 source record
- B510L · 1 source record
- B520JJ · 1 source record
- B550 R60702 · 2 source records · Original-source verification pending
- B550L · 1 source record
- B55SICR · 1 source record · Original-source verification pending
- B55SICRV · 1 source record · Original-source verification pending
- B574 N06200 · 1 source record · Original-source verification pending
- B574 N06686 · 1 source record · Original-source verification pending
- B575 N06200 · 1 source record · Original-source verification pending
- B581 N06030 · 1 source record · Original-source verification pending
- B590GJ · 1 source record
- B5 (steel) · 3 source records · Includes verified composition sources; other original sources await verification
- B5 (copper alloy) · 7 source records
- B6 · 3 source records · Includes verified composition sources; other original sources await verification
- B6X · 2 source records · Includes verified composition sources; other original sources await verification
- B7 · 1 source record
- B7-D · 2 source records
- B8 · 1 verified composition source
- B861 GRADE 1 · 1 source record · Original-source verification pending
- B861 GRADE 23 · 1 source record · Original-source verification pending
- B861 GRADE 3 · 1 source record · Original-source verification pending
- B861 GRADE 7 · 1 source record · Original-source verification pending
- B861 GRADE 7H · 1 source record · Original-source verification pending
- B8A · 1 verified composition source
- B8C · 1 verified composition source
- B8CA · 1 verified composition source
- B8CLN · 1 verified composition source
- B8CLNA · 1 verified composition source
- B8CLNCuB · 1 verified composition source
- B8CLNCuBA · 1 verified composition source
- B8LN · 1 verified composition source
- B8LNA · 1 verified composition source
- B8M · 1 verified composition source
- B8M2 · 1 verified composition source
- B8M3 · 1 verified composition source
- B8MA · 1 verified composition source
- B8ML4CuN · 1 verified composition source
- B8ML4CuNA · 1 verified composition source
- B8MLCuN · 1 verified composition source
- B8MLCuNA · 1 verified composition source
- B8MLN · 1 verified composition source
- B8MLNA · 1 verified composition source
- B8MN · 1 verified composition source
- B8MNA · 1 verified composition source
- B8N · 1 verified composition source
- B8NA · 1 verified composition source
- B8P · 1 verified composition source
- B8PA · 1 verified composition source
- B8R · 1 verified composition source
- B8RA · 1 verified composition source
- B8S · 1 verified composition source
- B8SA · 1 verified composition source
- B8T · 1 verified composition source
- B8TA · 1 verified composition source
- BAL13-3 · 2 source records
- BAL6-1.5 · 2 source records
- BB503 · 1 source record
- BERYLLIUM COPPER CB 101 · 2 source records
- BFE10-1-1 · 2 source records
- BFE10-1.5-1 · 1 source record
- BFE10-1.6-1 · 1 source record
- BFE16-1-1-0.5 · 1 source record
- BFE30-0.7 · 1 source record
- BFE30-1-1 · 2 source records
- BFE30-2-2 · 1 source record
- BFE5-1.5-0.5 · 2 source records
- BFE7-0.4-0.4 · 1 source record
- BMN3-12 · 2 source records
- BMN40-1.5 · 2 source records
- BMN43-0.5 · 2 source records
- BTMCR12-DT · 1 source record · Original-source verification pending
- BTMCR12-GT · 1 source record · Original-source verification pending
- BTMCR15 · 1 source record · Original-source verification pending
- BTMCR2 · 1 source record · Original-source verification pending
- BTMCR26 · 1 source record · Original-source verification pending
- BTMCR8 · 1 source record · Original-source verification pending
- BTMCR9NI5 · 1 source record · Original-source verification pending
- BTMNI4CR2-DT · 1 source record · Original-source verification pending
- BZN10-41-2 · 1 source record
- BZN12-24 · 1 source record
- BZN12-26 · 1 source record
- BZN12-29 · 1 source record
- BZN12-37-1.5 · 1 source record
- BZN15-20 · 2 source records
- BZN15-21-1.8 · 2 source records
- BZN15-24-1.5 · 2 source records
- BZN18-10 · 1 source record
- BZN18-17 · 1 source record
- BZN18-18 · 2 source records
- BZN18-20 · 1 source record
- BZN18-26 · 2 source records
- BZN22-16 · 1 source record
- BZN25-18 · 1 source record
- BZN40-20 · 1 source record
- BZN9-29 · 1 source record
- C 35 · 1 source record · Original-source verification pending
- C-CH1 · 1 source record
- C-CH1T · 1 source record
- C-CH35ACR · 2 source records
- C-CH40ACR · 1 source record
- C10 · 2 source records
- C100S · 1 source record
- C1022 · 3 source records · Original-source verification pending
- C105U · 2 source records
- C10C · 7 source records
- C10C-D · 3 source records
- C10E · 3 source records
- C10E2C · 6 source records
- C10GC · 2 source records
- C10R · 2 source records
- C120U · 2 source records
- C125S · 1 source record
- C15 · 2 source records
- C15725 · 3 source records · Original-source verification pending
- C15C · 5 source records
- C15E · 3 source records
- C15E2C · 11 source records
- C15E4 · 1 source record
- C15GC · 2 source records
- C15M2 · 1 source record
- C15R · 2 source records
- C16E · 2 source records
- C16R · 2 source records
- C17000 · 2 source records · Original-source verification pending
- C17C · 5 source records
- C17E2C · 6 source records
- C17GC · 2 source records
- C18150 · 1 source record · Original-source verification pending
- C20C · 5 source records
- C20E2C · 6 source records
- C20GC · 2 source records
- C22 · 3 source records
- C22E · 4 source records
- C25 · 2 source records
- C25C · 2 source records
- C25E · 1 source record · Original-source verification pending
- C25GC · 2 source records
- C25R · 1 source record · Original-source verification pending
- C2C · 5 source records
- C30 · 2 source records
- C30E · 2 source records
- C30EC · 2 source records
- C30R · 1 source record · Original-source verification pending
- C30RC · 2 source records
- C34200 · 2 source records · Original-source verification pending
- C35 · 21 source records
- C35E · 16 source records
- C35EC · 5 source records
- C35R · 1 source record · Original-source verification pending
- C35RC · 5 source records
- C40 · 3 source records
- C40E · 2 source records
- C40R · 1 source record · Original-source verification pending
- C45 · 4 source records
- C45E · 17 source records
- C45EC · 5 source records
- C45R · 1 source record · Original-source verification pending
- C45RC · 5 source records
- C45U · 2 source records
- C4C · 8 source records
- C50 · 2 source records
- C50E · 2 source records
- C50R · 1 source record · Original-source verification pending
- C55 · 3 source records
- C55E · 1 source record
- C55S · 1 source record
- C56E2 · 2 source records
- C60 · 3 source records
- C60E · 2 source records
- C60R · 1 source record · Original-source verification pending
- C60S · 1 source record
- C67S · 5 source records
- C70U · 2 source records
- C75S · 1 source record
- C80U · 2 source records
- C85S · 1 source record
- C8C · 6 source records
- C90S · 1 source record
- C90U · 2 source records
- C95400 · 2 source records · Original-source verification pending
- CH0 · 1 source record · Original-source verification pending
- CK 35 · 1 source record · Original-source verification pending
- CK22 · 4 source records
- CK25 · 1 source record
- CK30 · 1 source record
- CK35 · 4 source records
- CK35-D · 2 source records
- CK40 · 1 source record
- CK45 · 4 source records
- CK50 · 1 source record
- CK55 · 1 source record
- CK60 · 1 source record
- CK67 · 1 source record · Original-source verification pending
- CM22 · 1 source record
- CM25 · 1 source record
- CM30 · 1 source record
- CM35 · 1 source record
- CM40 · 1 source record
- CM45 · 1 source record
- CM50 · 1 source record
- CM55 · 1 source record
- CM60 · 1 source record
- COR-TEN® O · 1 source record
- CQ15 · 1 source record · Original-source verification pending
- CR12 · 3 source records · Original-source verification pending
- CR12MO1V1 · 3 source records · Original-source verification pending
- CR4W2MOV · 1 source record · Original-source verification pending
- CR8 · 1 source record · Original-source verification pending
- CRONIDUR30 · 1 source record · Original-source verification pending
- CRXM-19 · 1 source record · Original-source verification pending
- CS41A · 1 source record · Original-source verification pending
- CUAL10NI3FE2-C · 3 source records · Original-source verification pending
- CUNI10ZN27 · 2 source records · Original-source verification pending
- CUNI10ZN42PB2 · 2 source records · Original-source verification pending
- CUNI18ZN19PB1 · 7 source records · Original-source verification pending
- CUNI2BE · 9 source records · Original-source verification pending
- CUSI1 · 2 source records · Original-source verification pending
- CUSN11PB2-C · 3 source records · Original-source verification pending
- CUSN4 · 7 source records · Original-source verification pending
- CUSN6 · 18 source records · Original-source verification pending
- CUSN7ZN2PB3-C · 3 source records · Original-source verification pending
- CUTEP · 8 source records · Original-source verification pending
- CUZN20 · 12 source records · Original-source verification pending
- CUZN20AL2 · 3 source records · Original-source verification pending
- CUZN23AL6MN4FE3 · 3 source records · Original-source verification pending
- CUZN23AL6MN4FE3PB · 6 source records · Original-source verification pending
- CUZN30 · 15 source records · Original-source verification pending
- CUZN31SI1 · 9 source records · Original-source verification pending
- CUZN36 · 15 source records · Original-source verification pending
- CUZN36PB3 · 11 source records · Original-source verification pending
- CUZN37 · 16 source records · Original-source verification pending
- CUZN37PB0.5 · 4 source records · Original-source verification pending
- CUZN37PB1SN1 · 2 source records · Original-source verification pending
- CUZN37PB2 · 5 source records · Original-source verification pending
- CUZN39PB2 · 10 source records · Original-source verification pending
- CUZN39PB3 · 13 source records · Original-source verification pending
- CUZN40 · 14 source records · Original-source verification pending
- CUZN40MN1PB1 · 6 source records · Original-source verification pending
- CUZN40PB2 · 12 source records · Original-source verification pending
- CUZN5 · 6 source records · Original-source verification pending
- CW6MO5CR4V2 · 1 source record
- CW6MO5CR4V3 · 1 source record
- D · 2 source records · Original-source verification pending
- DC05 · 6 source records · Original-source verification pending
- DD402 · 2 source records · Original-source verification pending
- DFSCR440 · 1 source record
- DH36 · 2 source records · Original-source verification pending
- DIN-50CRV4 · 1 source record
- DIN-54SICRV6 · 1 source record
- DIN17CR3 · 1 source record
- DJ02 · 1 source record
- DL05 · 1 source record
- DT4 · 1 source record · Original-source verification pending
- DT4A · 1 source record · Original-source verification pending
- DT4C · 1 source record · Original-source verification pending
- DT4C DT4 DT4E DT4A · 1 source record · Original-source verification pending
- DT4E · 1 source record · Original-source verification pending
- DUPLEX 2205 · 1 source record
- DX51D+Z · 1 source record · Original-source verification pending
- DX52D+Z · 2 source records · Original-source verification pending
- E · 2 source records · Original-source verification pending
- E 275 A · 1 source record · Original-source verification pending
- E 275 B · 1 source record · Original-source verification pending
- E 275 C · 1 source record · Original-source verification pending
- E 275 D · 1 source record · Original-source verification pending
- E 275A · 1 source record · Original-source verification pending
- E 275B · 1 source record · Original-source verification pending
- E 275C · 1 source record · Original-source verification pending
- E 275D · 1 source record · Original-source verification pending
- E 355 C · 1 source record · Original-source verification pending
- E 355 D · 1 source record · Original-source verification pending
- E 355C · 1 source record · Original-source verification pending
- E 355D · 1 source record · Original-source verification pending
- E 460 DD · 1 source record · Original-source verification pending
- E 460 E · 1 source record · Original-source verification pending
- E1038H · 1 source record
- E1045H · 1 source record
- E1522H · 1 source record
- E1524H · 1 source record
- E1526H · 1 source record
- E1541H · 1 source record
- E155 · 4 source records · Original-source verification pending
- E15B21H · 1 source record
- E15B28H · 1 source record
- E15B30H · 1 source record
- E15B35H · 1 source record
- E15B37H · 1 source record
- E15B41H · 1 source record
- E15B48H · 1 source record
- E15B62H · 1 source record
- E190 · 2 source records · Original-source verification pending
- E195 · 4 source records · Original-source verification pending
- E215 · 2 source records · Original-source verification pending
- E220 · 2 source records · Original-source verification pending
- E235 · 7 source records · Original-source verification pending
- E255 · 1 source record · Original-source verification pending
- E260 · 2 source records · Original-source verification pending
- E275 · 5 source records · Original-source verification pending
- E275K2 · 1 source record · Original-source verification pending
- E295 · 1 source record
- E315 · 1 source record · Original-source verification pending
- E320 · 2 source records · Original-source verification pending
- E335 · 3 source records
- E355 · 6 source records · Original-source verification pending
- E355 DD · 1 source record · Original-source verification pending
- E355 E · 1 source record · Original-source verification pending
- E355DD · 2 source records · Original-source verification pending
- E355E · 1 source record · Original-source verification pending
- E360 · 3 source records
- E370 · 2 source records · Original-source verification pending
- E390DD · 1 source record · Original-source verification pending
- E390E · 1 source record · Original-source verification pending
- E410 · 1 source record · Original-source verification pending
- E420 · 1 source record · Original-source verification pending
- E420DD · 2 source records · Original-source verification pending
- E420E · 1 source record · Original-source verification pending
- E4340 · 8 source records
- E4340H · 1 source record
- E460 CC · 1 source record · Original-source verification pending
- E460 DD · 1 source record · Original-source verification pending
- E460 E · 1 source record · Original-source verification pending
- E460CC · 3 source records · Original-source verification pending
- E460DD · 2 source records · Original-source verification pending
- E460E · 1 source record · Original-source verification pending
- E470 · 1 source record · Original-source verification pending
- E50100 · 2 source records
- E51100 · 2 source records
- E52100 · 4 source records
- E9310 · 2 source records
- E9310H · 1 source record
- EH32 · 2 source records · Original-source verification pending
- EH36 · 2 source records · Original-source verification pending
- ELCH2 · 1 source record
- ELCH2S · 1 source record
- EN AW-AL CU4MG1 · 2 source records · Original-source verification pending
- EN AW-AL CU6BIPB · 1 source record · Original-source verification pending
- EN AW-AL MG1SICU · 2 source records · Original-source verification pending
- EN AW-AL ZN5.5MGCU · 1 source record · Original-source verification pending
- EN AW-AL99.99 · 2 source records · Original-source verification pending
- EN AW-ALZN5.5MGCU · 1 source record · Original-source verification pending
- ENI1066 · 1 source record · Original-source verification pending
- ENI6625 · 1 source record · Original-source verification pending
- ER2594 · 2 source records · Original-source verification pending
- ER409 · 1 source record · Original-source verification pending
- ER70S-3 · 1 source record
- ER70S-4 · 1 source record
- ER70S-6 · 1 source record
- ERNICRFE-8 · 2 source records · Original-source verification pending
- ERNICRMO-10 · 2 source records · Original-source verification pending
- ERNICRMO-11 · 1 source record · Original-source verification pending
- ERNICRMO-14 · 2 source records · Original-source verification pending
- ERNICRMO-17 · 2 source records · Original-source verification pending
- ERNICRMO-18 · 1 source record · Original-source verification pending
- ERNICU-7 · 1 source record · Original-source verification pending
- ERNIFECR-2 · 1 source record · Original-source verification pending
- ERNIMO-7 · 1 source record · Original-source verification pending
- F 467MAT TI 1 · 1 source record · Original-source verification pending
- F 467MBN NI 686 GRADE 1 · 1 source record · Original-source verification pending
- F 467MCN NI 686 GRADE 2 · 1 source record · Original-source verification pending
- F 467MDN NI 686 GRADE 3 · 1 source record · Original-source verification pending
- F 467MDT TI 5 · 1 source record · Original-source verification pending
- F 467MEN NI 686 GRADE 4 · 1 source record · Original-source verification pending
- F 467MET TI 7 · 1 source record · Original-source verification pending
- F 467MX AL 2024-T4 · 1 source record · Original-source verification pending
- F194 GRADE 8TA · 1 source record · Original-source verification pending
- F468 AL2024-T4 · 1 source record · Original-source verification pending
- F468 AL7075-T73 · 1 source record · Original-source verification pending
- F468 NI686 GRADE 1 · 1 source record · Original-source verification pending
- F468 NI686 GRADE 2 · 1 source record · Original-source verification pending
- F468 NI686 GRADE 3 · 1 source record · Original-source verification pending
- F468 NI686 GRADE 4 · 1 source record · Original-source verification pending
- F468 TI 1 · 1 source record · Original-source verification pending
- F468 TI 5 CLASS A · 1 source record · Original-source verification pending
- F468 TI 5 CLASS B · 1 source record · Original-source verification pending
- F468 TI 7 · 1 source record · Original-source verification pending
- F468AT TI 1 · 1 source record · Original-source verification pending
- F468BN NI 686 GRADE 1 · 1 source record · Original-source verification pending
- F468CN NI 686 GRADE 2 · 1 source record · Original-source verification pending
- F468DN NI 686 GRADE 3 · 1 source record · Original-source verification pending
- F468DT TI 5 CLASS A · 1 source record · Original-source verification pending
- F468EN NI 686 GRADE 4 · 1 source record · Original-source verification pending
- F468ET TI 7 · 1 source record · Original-source verification pending
- F468HT TI 5 CLASS B · 1 source record · Original-source verification pending
- F468MAT TI 1 · 1 source record · Original-source verification pending
- F468MBN NI 686 GRADE 1 · 1 source record · Original-source verification pending
- F468MCN NI 686 GRADE 2 · 1 source record · Original-source verification pending
- F468MDN NI 686 GRADE 3 · 1 source record · Original-source verification pending
- F468MDT TI 5 CLASS A · 1 source record · Original-source verification pending
- F468MEN NI 686 GRADE 4 · 1 source record · Original-source verification pending
- F468MET TI 7 · 1 source record · Original-source verification pending
- F468MHT TI 5 CLASS B · 1 source record · Original-source verification pending
- F468MX AL 2024-T4 · 1 source record · Original-source verification pending
- F468MZ AL 7075-T73 · 1 source record · Original-source verification pending
- F468X AL 2024-T4 · 1 source record · Original-source verification pending
- F468Z AL 7075-T73 · 1 source record · Original-source verification pending
- F593 304 · 1 source record · Original-source verification pending
- F593 304 L · 1 source record · Original-source verification pending
- F593 316 · 1 source record · Original-source verification pending
- F593 316L · 1 source record · Original-source verification pending
- F593 321 · 1 source record · Original-source verification pending
- F593 347 · 1 source record · Original-source verification pending
- F593 410 · 1 source record · Original-source verification pending
- F593 430 · 1 source record · Original-source verification pending
- F593 431 · 1 source record · Original-source verification pending
- F593 630 · 1 source record · Original-source verification pending
- F594 304 · 1 source record · Original-source verification pending
- F594 304L · 1 source record · Original-source verification pending
- F594 316 · 1 source record · Original-source verification pending
- F594 316L · 1 source record · Original-source verification pending
- F594 321 · 1 source record · Original-source verification pending
- F594 347 · 1 source record · Original-source verification pending
- F594 410 · 1 source record · Original-source verification pending
- F594 430 · 1 source record · Original-source verification pending
- F594 431 · 1 source record · Original-source verification pending
- F594 630 · 1 source record · Original-source verification pending
- F738M CLASS A1-50 304 · 1 source record · Original-source verification pending
- F738M CLASS A1-50 304L · 1 source record · Original-source verification pending
- F738M CLASS A1-70 304 · 1 source record · Original-source verification pending
- F738M CLASS A1-70 304L · 1 source record · Original-source verification pending
- F738M CLASS A1-80 304 · 1 source record · Original-source verification pending
- F738M CLASS A1-80 304L · 1 source record · Original-source verification pending
- F738M CLASS A2-50 321 · 1 source record · Original-source verification pending
- F738M CLASS A2-50 347 · 1 source record · Original-source verification pending
- F738M CLASS A2-70 321 · 1 source record · Original-source verification pending
- F738M CLASS A2-70 347 · 1 source record · Original-source verification pending
- F738M CLASS A2-80 321 · 1 source record · Original-source verification pending
- F738M CLASS A2-80 347 · 1 source record · Original-source verification pending
- F738M CLASS A4-50 316 · 1 source record · Original-source verification pending
- F738M CLASS A4-50 316L · 1 source record · Original-source verification pending
- F738M CLASS A4-70 316 · 1 source record · Original-source verification pending
- F738M CLASS A4-70 316L · 1 source record · Original-source verification pending
- F738M CLASS A4-80 316 · 1 source record · Original-source verification pending
- F738M CLASS A4-80 316L · 1 source record · Original-source verification pending
- F738M CLASS C1-110 410 · 1 source record · Original-source verification pending
- F738M CLASS C1-50 410 · 1 source record · Original-source verification pending
- F738M CLASS C1-70 410 · 1 source record · Original-source verification pending
- F738M CLASS C3-120 431 · 1 source record · Original-source verification pending
- F738M CLASS C3-80 431 · 1 source record · Original-source verification pending
- F738M CLASS F1-45 430 · 1 source record · Original-source verification pending
- F738M CLASS F1-60 430 · 1 source record · Original-source verification pending
- F738M CLASS P1-90 630 · 1 source record · Original-source verification pending
- F836M A1-50 304 · 1 source record · Original-source verification pending
- F836M A1-50 304L · 1 source record · Original-source verification pending
- F836M A1-70 304 · 1 source record · Original-source verification pending
- F836M A1-70 304L · 1 source record · Original-source verification pending
- F836M A1-80 304 · 1 source record · Original-source verification pending
- F836M A1-80 304L · 1 source record · Original-source verification pending
- F836M A2-50 347 · 1 source record · Original-source verification pending
- F836M A2-70 347 · 1 source record · Original-source verification pending
- F836M A2-80 347 · 1 source record · Original-source verification pending
- F836M A4-50 316 · 1 source record · Original-source verification pending
- F836M A4-50 316L · 1 source record · Original-source verification pending
- F836M A4-50 321 · 1 source record · Original-source verification pending
- F836M A4-70 316 · 1 source record · Original-source verification pending
- F836M A4-70 316L · 1 source record · Original-source verification pending
- F836M A4-70 321 · 1 source record · Original-source verification pending
- F836M A4-80 316 · 1 source record · Original-source verification pending
- F836M A4-80 316L · 1 source record · Original-source verification pending
- F836M A4-80 321 · 1 source record · Original-source verification pending
- F836M C1-110 410 · 1 source record · Original-source verification pending
- F836M C1-70 410 · 1 source record · Original-source verification pending
- F836M C3-120 431 · 1 source record · Original-source verification pending
- F836M C3-80 431 · 1 source record · Original-source verification pending
- F836M F1-45 430 · 1 source record · Original-source verification pending
- F836M P1-90 630 · 1 source record · Original-source verification pending
- F837 GROUP 1-AF 304 · 1 source record · Original-source verification pending
- F837 GROUP 1-AF 304L · 1 source record · Original-source verification pending
- F837 GROUP 1-CW 304 · 1 source record · Original-source verification pending
- F837 GROUP 1-CW 304L · 1 source record · Original-source verification pending
- F837 GROUP 1-CW1 304 · 1 source record · Original-source verification pending
- F837 GROUP 1-CW1 304L · 1 source record · Original-source verification pending
- F837 GROUP 2-AF 316 · 1 source record · Original-source verification pending
- F837 GROUP 2-AF 316L · 1 source record · Original-source verification pending
- F837 GROUP 2-CW 316 · 1 source record · Original-source verification pending
- F837 GROUP 2-CW 316L · 1 source record · Original-source verification pending
- F837 GROUP 2-CW1 316 · 1 source record · Original-source verification pending
- F837 GROUP 2-CW1 316L · 1 source record · Original-source verification pending
- F879 GROUP 1-AF 304 · 1 source record · Original-source verification pending
- F879 GROUP 1-AF 304L · 1 source record · Original-source verification pending
- F879 GROUP 1-CW 304 · 1 source record · Original-source verification pending
- F879 GROUP 1-CW 304L · 1 source record · Original-source verification pending
- F879 GROUP 1-CW1 304 · 1 source record · Original-source verification pending
- F879 GROUP 1-CW1 304L · 1 source record · Original-source verification pending
- F879 GROUP 2-AF 316 · 1 source record · Original-source verification pending
- F879 GROUP 2-AF 316L · 1 source record · Original-source verification pending
- F879 GROUP 2-CW 316 · 1 source record · Original-source verification pending
- F879 GROUP 2-CW 316L · 1 source record · Original-source verification pending
- F879 GROUP 2-CW1 316 · 1 source record · Original-source verification pending
- F879 GROUP 2-CW1 316L · 1 source record · Original-source verification pending
- F879M CLASS A1-50 304 · 1 source record · Original-source verification pending
- F879M CLASS A1-50 304L · 1 source record · Original-source verification pending
- F879M CLASS A1-50 316 · 1 source record · Original-source verification pending
- F879M CLASS A1-50 316L · 1 source record · Original-source verification pending
- F879M CLASS A1-55 304 · 1 source record · Original-source verification pending
- F879M CLASS A1-55 304L · 1 source record · Original-source verification pending
- F879M CLASS A1-55 316 · 1 source record · Original-source verification pending
- F879M CLASS A1-55 316L · 1 source record · Original-source verification pending
- F879M CLASS A1-70 304 · 1 source record · Original-source verification pending
- F879M CLASS A1-70 304L · 1 source record · Original-source verification pending
- F879M CLASS A1-70 316 · 1 source record · Original-source verification pending
- F879M CLASS A1-70 316L · 1 source record · Original-source verification pending
- F880 GROUP 1-AF 304 · 1 source record · Original-source verification pending
- F880 GROUP 1-AF 304L · 1 source record · Original-source verification pending
- F880 GROUP 1-AF 316 · 1 source record · Original-source verification pending
- F880 GROUP 1-AF 316L · 1 source record · Original-source verification pending
- F880 GROUP 1-CW 304 · 1 source record · Original-source verification pending
- F880 GROUP 1-CW 304L · 1 source record · Original-source verification pending
- F880 GROUP 1-CW 316 · 1 source record · Original-source verification pending
- F880 GROUP 1-CW 316L · 1 source record · Original-source verification pending
- F901 2024 · 1 source record · Original-source verification pending
- FEP05 · 1 source record · Original-source verification pending
- FH32 · 1 source record · Original-source verification pending
- FH36 · 1 source record · Original-source verification pending
- G-CUAL9NI · 2 source records · Original-source verification pending
- G-CUSN12PB · 2 source records · Original-source verification pending
- G-CUSN6ZNNI · 2 source records · Original-source verification pending
- G-X3CRNIMON 17 13 5 · 1 source record · Original-source verification pending
- G-X5CRNI 13 4 · 1 source record · Original-source verification pending
- G10080 · 5 source records
- G10100 · 4 source records
- G10150 · 6 source records · Original-source verification pending
- G10200 · 3 source records · Original-source verification pending
- G10210 · 1 source record · Original-source verification pending
- G10220 · 1 source record
- G10250 · 4 source records · Original-source verification pending
- G10260 · 1 source record
- G102CR18MO · 1 source record · Original-source verification pending
- G10300 · 4 source records
- G10301 · 1 source record
- G10350 · 4 source records · Original-source verification pending
- G10351 · 1 source record
- G10370 · 3 source records · Original-source verification pending
- G10380 · 1 source record
- G10390 · 3 source records
- G10400 · 2 source records
- G10420 · 1 source record
- G10440 · 6 source records · Original-source verification pending
- G10450 · 3 source records · Original-source verification pending
- G10460 · 1 source record
- G10500 · 4 source records · Original-source verification pending
- G10530 · 3 source records · Original-source verification pending
- G10550 · 3 source records
- G10690 · 2 source records · Original-source verification pending
- G10700 · 3 source records
- G10710 · 1 source record · Original-source verification pending
- G10B18 · 1 source record
- G10B18-A · 1 source record
- G10B18-B · 1 source record
- G10B18-C · 1 source record
- G10B21 · 1 source record
- G10B21-A · 1 source record
- G10B21-B · 1 source record
- G10B21-C · 1 source record
- G10B28 · 1 source record
- G10B28-A · 1 source record
- G10B28-B · 1 source record
- G10B28-C · 1 source record
- G10B30 · 1 source record
- G10B30-A · 1 source record
- G10B30-B · 1 source record
- G10B30-C · 1 source record
- G10B33 · 1 source record
- G10B33-A · 1 source record
- G10B33-B · 1 source record
- G10B33-C · 1 source record
- G10B38 · 1 source record
- G10B38-A · 1 source record
- G10B38-B · 1 source record
- G10B38-C · 1 source record
- G12144 · 3 source records · Original-source verification pending
- G15240 · 3 source records · Original-source verification pending
- G34CRMO4 · 3 source records · Original-source verification pending
- G41180 · 3 source records
- G41200 · 3 source records
- G41210 · 3 source records · Original-source verification pending
- G41350 · 3 source records
- G41370 · 1 source record
- G41400 · 5 source records
- G41420 · 3 source records
- G42CRMO4 · 3 source records · Original-source verification pending
- G43400 · 2 source records
- G43406 · 4 source records
- G46200 · 1 source record
- G51200 · 1 source record
- G51300 · 2 source records
- G51400 · 1 source record
- G61500 · 2 source records
- G86200 · 1 source record
- G95CR18 · 1 source record · Original-source verification pending
- GB-CUPB15SN · 2 source records · Original-source verification pending
- GC-CUSN12PB · 1 source record · Original-source verification pending
- GCR15 · 5 source records · Original-source verification pending
- GCR15Z · 1 source record · Original-source verification pending
- GH 4169 · 1 source record · Original-source verification pending
- GH1131 · 4 source records · Original-source verification pending
- GH2018 · 3 source records · Original-source verification pending
- GH2132 · 8 source records · Original-source verification pending
- GH2706 · 1 source record · Original-source verification pending
- GH3128 · 4 source records · Original-source verification pending
- GH3536 · 2 source records · Original-source verification pending
- GH4090 · 2 source records · Original-source verification pending
- GH4141 · 3 source records · Original-source verification pending
- GH4169 · 3 source records · Original-source verification pending
- GH4708 · 1 source record · Original-source verification pending
- GH4738 · 3 source records · Original-source verification pending
- GH6159 · 2 source records · Original-source verification pending
- GK-CUAL9NI · 1 source record · Original-source verification pending
- GM10MNA · 1 source record
- GML20CR · 1 source record
- GML20CR-A · 1 source record
- GML20CR-B · 1 source record
- GML20CR-C · 1 source record
- GML40CR · 1 source record
- GML40CR-A · 1 source record
- GML40CR-B · 1 source record
- GML40CR-C · 1 source record
- GRADE 1 (titanium) · 2 source records · Original-source verification pending
- GRADE 1 (steel) · 3 source records · Original-source verification pending
- GRADE 23 · 3 source records · Original-source verification pending
- GRADE 3 (titanium) · 2 source records · Original-source verification pending
- GRADE 3 (steel) · 3 source records · Original-source verification pending
- GRADE 410S · 1 source record · Original-source verification pending
- GRADE 439 · 1 source record · Original-source verification pending
- GRADE 5 · 1 source record · Original-source verification pending
- GRADE 58 · 1 source record · Original-source verification pending
- GRADE 65 · 1 source record · Original-source verification pending
- GRADE 660 · 3 source records · Original-source verification pending
- GRADE 665 · 3 source records · Original-source verification pending
- GRADE 6 (titanium) · 2 source records · Original-source verification pending
- GRADE 6 (steel) · 3 source records · Original-source verification pending
- GRADE 718 · 2 source records · Original-source verification pending
- GRADE 7H · 1 source record · Original-source verification pending
- GRADE 7 (titanium) · 1 source record · Original-source verification pending
- GRADE 7 (steel) · 3 source records · Original-source verification pending
- GRADE B · 2 source records · Original-source verification pending
- GRADE B TYPE E · 2 source records · Original-source verification pending
- GRADE B TYPE S · 2 source records · Original-source verification pending
- GRADE C · 3 source records · Original-source verification pending
- GRADE D · 3 source records · Original-source verification pending
- GRADE E · 2 source records · Original-source verification pending
- GRADE F1925N · 2 source records · Original-source verification pending
- GRADE F20 · 2 source records · Original-source verification pending
- GRADE F304 · 2 source records · Original-source verification pending
- GRADE F304H · 2 source records · Original-source verification pending
- GRADE F304L · 2 source records · Original-source verification pending
- GRADE F304LN · 2 source records · Original-source verification pending
- GRADE F304N · 2 source records · Original-source verification pending
- GRADE F310H · 2 source records · Original-source verification pending
- GRADE F316 · 2 source records · Original-source verification pending
- GRADE F316L · 2 source records · Original-source verification pending
- GRADE F316LN · 2 source records · Original-source verification pending
- GRADE F321 · 2 source records · Original-source verification pending
- GRADE F347 · 2 source records · Original-source verification pending
- GRADE F347H · 2 source records · Original-source verification pending
- GRADE F62 · 2 source records · Original-source verification pending
- GRADE F904L · 2 source records · Original-source verification pending
- GRADE FNIC10 · 2 source records · Original-source verification pending
- GRADE FNIC11 · 2 source records · Original-source verification pending
- GRADE FXM-19 · 2 source records · Original-source verification pending
- GRADE NO. 4118 · 1 source record · Original-source verification pending
- GRADE NO. 4137 · 1 source record · Original-source verification pending
- GRADE NO. 4140 · 1 source record · Original-source verification pending
- GRADE NO. 4142 · 1 source record · Original-source verification pending
- GRADE NO. 4340 · 1 source record · Original-source verification pending
- GRADE NO. 4620 · 1 source record · Original-source verification pending
- GRADE NO. 5120 · 1 source record · Original-source verification pending
- GRADE NO. 5130 · 1 source record · Original-source verification pending
- GRADE NO. 5135 · 1 source record · Original-source verification pending
- GRADE NO. 5140 · 1 source record · Original-source verification pending
- GRADE NO. 6150 · 1 source record · Original-source verification pending
- GRADE NO. 8620 · 1 source record · Original-source verification pending
- GRADE NO. E4340 · 1 source record · Original-source verification pending
- GRADE R28 · 3 source records · Original-source verification pending
- GRADE R33 · 3 source records · Original-source verification pending
- GRADE R37 · 3 source records · Original-source verification pending
- GRADE R44 · 3 source records · Original-source verification pending
- GRADE R50 · 3 source records · Original-source verification pending
- GRADE TP405 · 1 source record · Original-source verification pending
- GRADE TP410 · 1 source record · Original-source verification pending
- GS-34CRMO4 · 1 source record · Original-source verification pending
- GS-42CRMO4 · 1 source record · Original-source verification pending
- GSCM420 · 1 source record
- GSCM420-A · 1 source record
- GSCM420-B · 1 source record
- GSCM420-C · 1 source record
- GSCM435 · 1 source record
- GSCM435-A · 1 source record
- GSCM435-B · 1 source record
- GSCM435-C · 1 source record
- GSCM440 · 1 source record
- GSCM440-A · 1 source record
- GSCM440-B · 1 source record
- GSCM440-C · 1 source record
- GSWRCH10A · 1 source record
- GSWRCH10A-A · 1 source record
- GSWRCH10A-B · 1 source record
- GSWRCH10A-C · 1 source record
- GSWRCH10K · 1 source record
- GSWRCH10K-A · 1 source record
- GSWRCH10K-B · 1 source record
- GSWRCH10K-C · 1 source record
- GSWRCH12A · 1 source record
- GSWRCH12A-A · 1 source record
- GSWRCH12A-B · 1 source record
- GSWRCH12A-C · 1 source record
- GSWRCH12K · 1 source record
- GSWRCH12K-A · 1 source record
- GSWRCH12K-B · 1 source record
- GSWRCH12K-C · 1 source record
- GSWRCH15A · 1 source record
- GSWRCH15A-A · 1 source record
- GSWRCH15A-B · 1 source record
- GSWRCH15A-C · 1 source record
- GSWRCH15K · 1 source record
- GSWRCH15K-A · 1 source record
- GSWRCH15K-B · 1 source record
- GSWRCH15K-C · 1 source record
- GSWRCH16A · 1 source record
- GSWRCH16A-A · 1 source record
- GSWRCH16A-B · 1 source record
- GSWRCH16A-C · 1 source record
- GSWRCH16K · 1 source record
- GSWRCH16K-A · 1 source record
- GSWRCH16K-B · 1 source record
- GSWRCH16K-C · 1 source record
- GSWRCH17K · 1 source record
- GSWRCH17K-A · 1 source record
- GSWRCH17K-B · 1 source record
- GSWRCH17K-C · 1 source record
- GSWRCH18A · 1 source record
- GSWRCH18A-A · 1 source record
- GSWRCH18A-B · 1 source record
- GSWRCH18A-C · 1 source record
- GSWRCH18K · 1 source record
- GSWRCH18K-A · 1 source record
- GSWRCH18K-B · 1 source record
- GSWRCH18K-C · 1 source record
- GSWRCH19A · 1 source record
- GSWRCH19A-A · 1 source record
- GSWRCH19A-B · 1 source record
- GSWRCH19A-C · 1 source record
- GSWRCH20K · 1 source record
- GSWRCH20K-A · 1 source record
- GSWRCH20K-B · 1 source record
- GSWRCH20K-C · 1 source record
- GSWRCH22A · 1 source record
- GSWRCH22A-A · 1 source record
- GSWRCH22A-B · 1 source record
- GSWRCH22A-C · 1 source record
- GSWRCH22K · 1 source record
- GSWRCH22K-A · 1 source record
- GSWRCH22K-B · 1 source record
- GSWRCH22K-C · 1 source record
- GSWRCH24K · 1 source record
- GSWRCH24K-A · 1 source record
- GSWRCH24K-B · 1 source record
- GSWRCH24K-C · 1 source record
- GSWRCH25K · 1 source record
- GSWRCH25K-A · 1 source record
- GSWRCH25K-B · 1 source record
- GSWRCH25K-C · 1 source record
- GSWRCH27K · 1 source record
- GSWRCH27K-A · 1 source record
- GSWRCH27K-B · 1 source record
- GSWRCH27K-C · 1 source record
- GSWRCH30K · 1 source record
- GSWRCH30K-A · 1 source record
- GSWRCH30K-B · 1 source record
- GSWRCH30K-C · 1 source record
- GSWRCH33K · 1 source record
- GSWRCH33K-A · 1 source record
- GSWRCH33K-B · 1 source record
- GSWRCH33K-C · 1 source record
- GSWRCH35K · 1 source record
- GSWRCH35K-A · 1 source record
- GSWRCH35K-B · 1 source record
- GSWRCH35K-C · 1 source record
- GSWRCH38K · 1 source record
- GSWRCH38K-A · 1 source record
- GSWRCH38K-B · 1 source record
- GSWRCH38K-C · 1 source record
- GSWRCH40K · 1 source record
- GSWRCH40K-A · 1 source record
- GSWRCH40K-B · 1 source record
- GSWRCH40K-C · 1 source record
- GSWRCH41K · 1 source record
- GSWRCH41K-A · 1 source record
- GSWRCH41K-B · 1 source record
- GSWRCH41K-C · 1 source record
- GSWRCH43K · 1 source record
- GSWRCH43K-A · 1 source record
- GSWRCH43K-B · 1 source record
- GSWRCH43K-C · 1 source record
- GSWRCH45K · 1 source record
- GSWRCH45K-A · 1 source record
- GSWRCH45K-B · 1 source record
- GSWRCH45K-C · 1 source record
- GSWRCH48K · 1 source record
- GSWRCH48K-A · 1 source record
- GSWRCH48K-B · 1 source record
- GSWRCH48K-C · 1 source record
- GSWRCH50K · 1 source record
- GSWRCH50K-A · 1 source record
- GSWRCH50K-B · 1 source record
- GSWRCH50K-C · 1 source record
- GSWRCH6A · 1 source record
- GSWRCH6A-A · 1 source record
- GSWRCH6A-B · 1 source record
- GSWRCH6A-C · 1 source record
- GSWRCH8A · 1 source record
- GSWRCH8A-A · 1 source record
- GSWRCH8A-B · 1 source record
- GSWRCH8A-C · 1 source record
- GX25CRNISI18-9 · 3 source records · Original-source verification pending
- GX25CRNISI20-14 · 3 source records · Original-source verification pending
- GZ-CUAL9NI · 1 source record · Original-source verification pending
- GZ-CUSN12PB · 1 source record · Original-source verification pending
- H59 · 7 source records
- H62 · 2 source records
- H63 · 2 source records
- H65 · 2 source records
- H66 · 1 source record
- H68 · 2 source records
- H68A · 1 source record
- H70 · 2 source records
- H70A · 1 source record
- H80 · 2 source records
- H85 · 2 source records
- H85A · 1 source record
- H86200 · 2 source records · Original-source verification pending
- H90 · 2 source records
- H95 · 1 source record
- H96 · 1 source record
- HAL59-3-2 · 2 source records
- HAL60-1-1 · 2 source records
- HAL61-4-3-1 · 2 source records
- HAL61-4-3-1.5 · 1 source record
- HAL64-5-4-2 · 1 source record
- HAL66-6-3-2 · 2 source records
- HAL67-2.5 · 2 source records
- HAL77-2 · 2 source records
- HAS68-0.04 · 1 source record
- HAS70-0.05 · 1 source record
- HAS85-0.05 · 1 source record
- HASTELLOY ALLOY C-4 · 1 source record · Original-source verification pending
- HASTELLOY B-2 · 1 source record
- HASTELLOY B-3 · 2 source records
- HASTELLOY C-2000 · 2 source records
- HASTELLOY C-22 · 2 source records
- HASTELLOY C-276 · 2 source records
- HASTELLOY C-4 · 2 source records
- HASTELLOY F · 2 source records · Original-source verification pending
- HASTELLOY G · 1 source record · Original-source verification pending
- HASTELLOY G-30 · 1 source record
- HASTELLOY X · 2 source records
- HAYNES 214 · 2 source records
- HAYNES 25 · 2 source records
- HAYNES 282 · 1 source record
- HB90-0.1 · 1 source record
- HBI59-1 · 1 source record
- HBI60-0.5-0.01 · 1 source record
- HBI60-0.8-0.01 · 1 source record
- HBI60-1.0-0.01 · 1 source record
- HBI60-1.0-0.05 · 1 source record
- HBI60-1.3 · 1 source record
- HBI60-2 · 1 source record
- HBI62-1 · 1 source record
- HBSC4C · 2 source records · Original-source verification pending
- HC180B · 4 source records · Original-source verification pending
- HC220B · 4 source records · Original-source verification pending
- HC260B · 4 source records · Original-source verification pending
- HC300B · 4 source records · Original-source verification pending
- HC440/780DHD+Z · 1 source record · Original-source verification pending
- HC550/980DHD+Z · 1 source record · Original-source verification pending
- HC570/780CPD+Z · 1 source record · Original-source verification pending
- HC700/980DHD+Z · 1 source record · Original-source verification pending
- HC780/980CPD+Z · 1 source record · Original-source verification pending
- HC820/1180DPD+Z · 1 source record · Original-source verification pending
- HFE58-1-1 · 2 source records
- HFE59-1-1 · 2 source records
- HGH3044 · 2 source records · Original-source verification pending
- HMG60-1 · 1 source record
- HMN55-3-1 · 2 source records
- HMN57-2-2-0.5 · 1 source record
- HMN57-3-1 · 2 source records
- HMN58-2 · 2 source records
- HMN59-2-1.5-0.5 · 1 source record
- HMN62-13 · 1 source record
- HMN62-3-3-0.7 · 2 source records
- HMN62-3-3-1 · 1 source record
- HMN64-8-5-1.5 · 1 source record
- HNI56-3 · 2 source records
- HNI65-5 · 2 source records
- HNS3306 · 1 source record · Original-source verification pending
- HP235 · 1 source record · Original-source verification pending
- HP265 · 1 source record · Original-source verification pending
- HP295 · 1 source record · Original-source verification pending
- HP325 · 1 source record · Original-source verification pending
- HPB57-4 · 1 source record
- HPB58-2 · 1 source record
- HPB58-3 · 1 source record
- HPB59-1 · 2 source records
- HPB59-2 · 1 source record
- HPB59-3 · 2 source records
- HPB60-2 · 2 source records
- HPB60-3 · 1 source record
- HPB61-1 · 2 source records
- HPB61-2-0.1 · 1 source record
- HPB61-2-1 · 1 source record
- HPB62-0.8 · 2 source records
- HPB62-2 · 2 source records
- HPB62-2-0.1 · 1 source record
- HPB62-3 · 2 source records
- HPB63-0.1 · 2 source records
- HPB63-3 · 2 source records
- HPB66-0.5 · 2 source records
- HPB89-2 · 2 source records
- HR2 · 2 source records · Original-source verification pending
- HRS6 · 1 source record
- HS0-4-1 · 2 source records
- HS1-4-2 · 2 source records
- HS1-8-1 · 2 source records
- HS10-4-3-10 · 2 source records
- HS18-0-1 · 2 source records
- HS2-9-1-8 · 2 source records
- HS2-9-2 · 2 source records
- HS3-3-2 · 2 source records
- HS6-5-2 · 2 source records
- HS6-5-2-5 · 2 source records
- HS6-5-2C · 2 source records
- HS6-5-3 · 2 source records
- HS6-5-3-8 · 2 source records
- HS6-5-3C · 2 source records
- HS6-5-4 · 2 source records
- HS6-6-2 · 2 source records
- HSB60-0.9 · 1 source record
- HSB61-0.8-0.5 · 1 source record
- HSI61-0.6 · 1 source record
- HSI62-0.6 · 4 source records
- HSI75-3 · 1 source record
- HSI80-3 · 2 source records
- HSLAS GRADE 55 [380] CLASS 1 · 3 source records · Original-source verification pending
- HSLAS GRADE 60 [410] CLASS 1 · 3 source records · Original-source verification pending
- HSLAS GRADE 60 [410] CLASS 2 · 3 source records · Original-source verification pending
- HSLAS GRADE 65 [450] CLASS 1 · 3 source records · Original-source verification pending
- HSLAS GRADE 65 [450] CLASS 2 · 3 source records · Original-source verification pending
- HSLAS GRADE 70 [480] CLASS 1 · 3 source records · Original-source verification pending
- HSN60-1 · 2 source records
- HSN62-1 · 2 source records
- HSN65-0.03 · 1 source record
- HSN70-1 · 2 source records
- HSN70-1-0.01 · 1 source record
- HSN70-1-0.01-0.04 · 1 source record
- HSN72-1 · 1 source record
- HSN90-1 · 2 source records
- HX180BD+Z · 1 source record · Original-source verification pending
- HX180YD+Z · 2 source records · Original-source verification pending
- HX220BD+Z · 1 source record · Original-source verification pending
- HX220YD+Z · 1 source record · Original-source verification pending
- HX260YD+Z · 1 source record · Original-source verification pending
- HX500LAD+Z · 1 source record · Original-source verification pending
- HⅡ · 1 source record
- IFI-1022/A · 1 source record
- IFI-1022/B · 1 source record
- IFI-1541/A · 2 source records
- IFI-1541/B · 2 source records
- INCOLOY 800 · 2 source records
- INCOLOY 800HT · 4 source records
- INCOLOY 825 · 2 source records
- INCOLOY A-286 · 2 source records
- INCOLOY ALLOY 020 · 1 source record · Original-source verification pending
- INCOLOY ALLOY 25-6MOHN · 1 source record · Original-source verification pending
- INCOLOY ALLOY 28 · 1 source record · Original-source verification pending
- INCOLOY ALLOY 800H · 1 source record · Original-source verification pending
- INCOLOY ALLOY A-286 · 1 source record · Original-source verification pending
- INCONEL 600 · 2 source records
- INCONEL 601 · 2 source records
- INCONEL 625 · 2 source records
- INCONEL 718 · 2 source records
- INCONEL ALLOY 22 · 1 source record · Original-source verification pending
- INCONEL ALLOY 686 · 1 source record · Original-source verification pending
- INCONEL X-750 · 2 source records
- J55 · 1 source record
- J93404 · 2 source records · Original-source verification pending
- JTS-SUYB1 · 1 source record
- K417G · 2 source records · Original-source verification pending
- K93600 · 1 source record · Original-source verification pending
- KA40 · 1 source record
- KA45 · 1 source record
- KA70 · 1 source record
- KBC50 · 1 source record
- KBC60 · 1 source record
- KBC60-A · 1 source record
- KCF10A · 1 source record
- KCF12A · 1 source record
- KCF15A · 1 source record
- KCF17A · 1 source record
- KCF20A · 1 source record
- KCF6A · 1 source record
- KCF8A · 1 source record
- KCH10AT · 1 source record
- KCH10KT · 1 source record
- KCH10R12 · 1 source record
- KCH10R12N · 1 source record
- KCH12AT · 1 source record
- KCH12KT · 1 source record
- KCH12R15 · 1 source record
- KCH12R15N · 1 source record
- KCH1330T · 1 source record
- KCH1335T · 1 source record
- KCH1340T · 1 source record
- KCH1345T · 1 source record
- KCH13AT · 1 source record
- KCH1524T · 1 source record
- KCH1527T · 1 source record
- KCH1536T · 1 source record
- KCH1541T · 1 source record
- KCH15AT · 1 source record
- KCH15KT · 1 source record
- KCH15R17 · 1 source record
- KCH15R17N · 1 source record
- KCH16AT · 1 source record
- KCH16KT · 1 source record
- KCH17KT · 1 source record
- KCH17R20 · 1 source record
- KCH17R20N · 1 source record
- KCH18AT · 1 source record
- KCH18KT · 1 source record
- KCH19AT · 1 source record
- KCH19KT · 1 source record
- KCH20AT · 1 source record
- KCH20KT · 1 source record
- KCH21AT · 1 source record
- KCH21KT · 1 source record
- KCH22AT · 1 source record
- KCH22KT · 1 source record
- KCH23AT · 1 source record
- KCH23KT · 1 source record
- KCH25AT · 1 source record
- KCH25KT · 1 source record
- KCH2R5 · 1 source record
- KCH30AT · 1 source record
- KCH30KT · 1 source record
- KCH33KT · 1 source record
- KCH35AT · 1 source record
- KCH35KT · 1 source record
- KCH38AT · 1 source record
- KCH38KT · 1 source record
- KCH40AT · 1 source record
- KCH40KT · 1 source record
- KCH43KT · 1 source record
- KCH45KT · 1 source record
- KCH48KT · 1 source record
- KCH4R6 · 1 source record
- KCH50KT · 1 source record
- KCH53KT · 1 source record
- KCH55KT · 1 source record
- KCH58KT · 1 source record
- KCH5AT · 1 source record
- KCH6AT · 1 source record
- KCH6R8 · 1 source record
- KCH6R8N · 1 source record
- KCH8AT · 1 source record
- KCH8KT · 1 source record
- KCH8R10 · 1 source record
- KCH8R10N · 1 source record
- KECH01KTM · 1 source record
- KGMS1215 · 1 source record
- KHV10N · 1 source record
- KHV6N · 1 source record
- KHV7 · 1 source record
- KKG3 · 1 source record
- KKG4 · 1 source record
- KKG8 · 1 source record
- KMN27-A · 1 source record
- KMN36-A · 1 source record
- KMN36-B · 1 source record
- KMN41 · 1 source record
- KMN41-A · 1 source record
- KMNC418H · 1 source record
- KMTBCR26 · 2 source records · Original-source verification pending
- KNCH10 · 1 source record
- KNCH7 · 1 source record
- KNCH7S · 1 source record
- KNCH8 · 1 source record
- KNCH8P · 1 source record
- KNCH8S · 1 source record
- KNDS2 · 1 source record
- KNDS4 · 1 source record
- KNF23M · 1 source record
- KNF40 · 1 source record
- KNF43 · 1 source record
- KNF45 · 1 source record
- KNF48 · 1 source record
- KNR65 · 1 source record
- KNR70S · 1 source record
- KNR75 · 1 source record
- KNR85 · 1 source record
- KNR90 · 1 source record
- KPR100A-E · 1 source record
- KPR110A · 1 source record
- KPR92A-C · 1 source record
- KRS62A · 1 source record
- KRS72A · 1 source record
- KRS82A · 1 source record
- KSC105-E · 1 source record
- KSC60 · 1 source record
- KSC72 · 1 source record
- KSC82 · 1 source record
- KSC90 · 1 source record
- KSC92-E · 1 source record
- KSCM418H · 1 source record
- KTCF10A · 1 source record
- KTCF15A · 1 source record
- KTCF20A · 1 source record
- KTCF25K · 1 source record
- KTCF35K · 1 source record
- KTCH10AT · 1 source record
- KTCH15AT · 1 source record
- KTCH20AT · 1 source record
- KTCH25KT · 1 source record
- KTCH35KT · 1 source record
- LDX 2101 · 1 source record · Original-source verification pending
- LF2 · 2 source records · Original-source verification pending
- LF6 · 2 source records · Original-source verification pending
- LH80 · 1 source record
- LY10 · 1 source record · Original-source verification pending
- M 1008 · 2 source records
- M 1010 · 2 source records
- M 1012 · 2 source records
- M 1015 · 2 source records
- M 1017 · 2 source records
- M 1020 · 2 source records
- M 1023 · 2 source records
- M 1025 · 2 source records
- M 1031 · 2 source records
- M 1044 · 2 source records
- M35 · 2 source records · Original-source verification pending
- MFT10 · 3 source records
- MFT10B · 1 source record
- MFT10DP · 1 source record
- MFT10LB · 1 source record
- MFT12LB · 1 source record
- MFT8 · 3 source records
- MFT8B · 1 source record
- MFT8DP · 1 source record
- MFT9 · 3 source records
- MFT9B · 1 source record
- MFT9DP · 1 source record
- ML022CR17NI12MO2 · 1 source record · Original-source verification pending
- ML022CR17NI13MO3 · 1 source record
- ML022CR18NI9CU3 · 1 source record
- ML022CR19NI10 · 1 source record · Original-source verification pending
- ML03CR16NI18 · 1 source record
- ML03CR18NI12 · 1 source record
- ML04AL · 6 source records
- ML04CR16MN8NI2CU3N · 1 source record
- ML04CR17 · 1 source record
- ML04CR17MN7NI5CUN · 1 source record
- ML06AL · 4 source records
- ML06CR12NB · 1 source record
- ML06CR12TI · 1 source record
- ML06CR17MO · 1 source record
- ML06CR17NI12MO2 · 2 source records
- ML06CR18NI11TI · 1 source record · Original-source verification pending
- ML06CR18NI9CU2 · 1 source record
- ML06CR19NI10 · 1 source record · Original-source verification pending
- ML06CR19NI9 · 1 source record
- ML08AL · 7 source records
- ML08AL-1 · 1 source record
- ML08AL-D · 3 source records
- ML10 · 6 source records
- ML10-D · 3 source records
- ML10AL · 5 source records
- ML10CR15 · 1 source record
- ML12 · 4 source records
- ML12AL · 4 source records
- ML12CR13 · 2 source records
- ML14CR17NI2 · 2 source records · Original-source verification pending
- ML15 · 6 source records
- ML15-D · 3 source records
- ML15AL · 7 source records
- ML15CR · 4 source records
- ML15CRMO · 1 source record
- ML15MN · 4 source records
- ML15MNB · 4 source records
- ML15MNVB · 6 source records
- ML16CR17NI2 · 1 source record
- ML18MN · 4 source records
- ML18MNAL · 1 source record
- ML20 · 5 source records
- ML20AL · 5 source records
- ML20B · 5 source records
- ML20CR · 5 source records
- ML20CR-D · 3 source records
- ML20CRB · 1 source record
- ML20CRMO · 3 source records
- ML20CRMOV · 1 source record
- ML20MN · 3 source records
- ML20MNAL · 1 source record
- ML20MNB · 5 source records
- ML20MNTIB · 8 source records
- ML20MNTIB-1 · 1 source record
- ML20MNTIB-D · 3 source records
- ML20MNVB · 6 source records
- ML22CR14NIMO · 1 source record
- ML22MN · 2 source records
- ML23B · 1 source record
- ML25 · 6 source records
- ML25B · 3 source records
- ML25CRB · 1 source record
- ML25CRMO · 3 source records
- ML25MN · 5 source records
- ML25MNB · 3 source records
- ML28B · 3 source records
- ML30 · 5 source records
- ML30B · 3 source records
- ML30CR · 3 source records
- ML30CR13 · 1 source record · Original-source verification pending
- ML30CRMNSI · 2 source records
- ML30CRMO · 5 source records
- ML30MN · 3 source records
- ML30MNB · 4 source records
- ML33B · 1 source record
- ML35 · 7 source records
- ML35-D · 1 source record
- ML35B · 5 source records
- ML35CR · 3 source records
- ML35CRMO · 6 source records
- ML35CRMO-D · 2 source records
- ML35CRMOV · 1 source record
- ML35CRMOZ · 1 source record
- ML35MN · 3 source records
- ML35MNB · 5 source records
- ML35VB · 1 source record
- ML37CR · 1 source record
- ML37CRB · 2 source records
- ML38 · 1 source record
- ML38B · 1 source record
- ML40 · 5 source records
- ML40CR · 9 source records
- ML40CR-1 · 1 source record
- ML40CR-D · 3 source records
- ML40CRMO · 4 source records
- ML40CR(FA) · 1 source record
- ML40MN · 1 source record
- ML40MN2 · 1 source record
- ML40MNB · 4 source records
- ML42CRMO · 5 source records
- ML42CRMOV · 1 source record
- ML42CRMOZ · 1 source record
- ML45 · 5 source records
- ML45B · 1 source record
- ML45CR · 3 source records
- ML45CRMO · 3 source records
- ML45MN · 1 source record
- ML45MN2 · 2 source records
- ML50 · 1 source record
- MNB120H · 2 source records
- MNB120H-D · 2 source records
- MNB123H · 4 source records
- MNB123H-D · 2 source records
- MO80CU20 · 2 source records · Original-source verification pending
- MONEL 400 · 2 source records
- MONEL K-500 · 2 source records
- MP35N · 2 source records
- MS 58 · 1 source record · Original-source verification pending
- MT 304 · 3 source records · Original-source verification pending
- MT 304L · 3 source records · Original-source verification pending
- MT 316 · 3 source records · Original-source verification pending
- MT 316L · 3 source records · Original-source verification pending
- MT 321 · 3 source records · Original-source verification pending
- MT 347 · 3 source records · Original-source verification pending
- MT 405 · 2 source records · Original-source verification pending
- MT 410 · 2 source records · Original-source verification pending
- MT 430 · 3 source records · Original-source verification pending
- N02200 · 1 source record
- N04400 · 1 source record
- N06022 · 6 source records · Original-source verification pending
- N06030 · 1 source record · Original-source verification pending
- N06200 · 4 source records · Original-source verification pending
- N06210 · 5 source records · Original-source verification pending
- N06600 · 1 source record
- N06617 · 1 source record
- N06625 · 1 source record
- N06650 · 2 source records · Original-source verification pending
- N06686 · 5 source records · Original-source verification pending
- N06690 · 1 source record
- N07718 · 6 source records · Original-source verification pending
- N08020 · 17 source records
- N08028 · 10 source records
- N08029 · 1 source record
- N08367 · 40 source records
- N08700 · 1 source record
- N08800 · 4 source records
- N08810 · 14 source records
- N08810/N08811 · 1 source record
- N08811 · 22 source records
- N08825 · 6 source records
- N08904 · 21 source records
- N08925 · 2 source records
- N08926 · 33 source records
- N10276 · 1 source record
- N10665 · 4 source records · Original-source verification pending
- NC21FEDU · 1 source record · Original-source verification pending
- NCF825 · 3 source records · Original-source verification pending
- NHB20 · 1 source record
- NHB30 · 1 source record
- NHF540 · 1 source record
- NHF540-S · 1 source record
- NHF590 · 1 source record
- NHF590-S · 1 source record
- NHF880 · 1 source record
- NI-SPAN-C ALLOY 902 · 2 source records
- NI53CR19MO3TINB · 1 source record · Original-source verification pending
- NICKEL 200 · 2 source records
- NICKEL 201 · 2 source records
- NICKEL 205 · 2 source records
- NICKEL 212 · 2 source records
- NICKEL 270 · 2 source records
- NICR15FE · 7 source records
- NICR15FE7TIAL · 2 source records
- NICR19FE19NB5MN3 · 1 source record · Original-source verification pending
- NICR19FE19NB5MO 3 · 2 source records
- NICR19FE19NB5MO3 · 8 source records
- NICR20TI · 2 source records
- NICR20TIAL · 2 source records
- NICR22MO9NB · 9 source records
- NICR23FE · 8 source records
- NICR23MO16AL · 4 source records · Original-source verification pending
- NICR28FESICE · 2 source records
- NICR29FE · 5 source records · Original-source verification pending
- NICU30FE · 4 source records · Original-source verification pending
- NILO 36 · 2 source records
- NILO 42 · 2 source records
- NILO 48 · 2 source records
- NILO 52 · 2 source records
- NILO ALLOY 36 · 2 source records · Original-source verification pending
- NILO K · 2 source records
- NIMO16CR16TI · 4 source records · Original-source verification pending
- NIMO28 · 6 source records · Original-source verification pending
- NIMONIC 75 · 2 source records
- NIMONIC 80A · 2 source records
- NIMONIC 90 · 2 source records
- NIMONIC C-263 · 1 source record
- NITRONIC 50 · 1 source record
- NITRONIC 60 · 1 source record
- NLP33K · 1 source record
- NLP77B · 1 source record
- NLP82B · 1 source record
- NS1401 · 3 source records · Original-source verification pending
- NS1403 · 4 source records · Original-source verification pending
- NS3102 · 4 source records · Original-source verification pending
- NS3103 · 3 source records · Original-source verification pending
- NS3303 · 5 source records · Original-source verification pending
- NS3306 · 5 source records · Original-source verification pending
- NS3312 · 1 source record · Original-source verification pending
- NS4102 · 1 source record · Original-source verification pending
- NS4301 · 1 source record · Original-source verification pending
- P20 · 1 source record · Original-source verification pending
- P215NL · 6 source records · Original-source verification pending
- P235 · 1 source record · Original-source verification pending
- P235GH · 12 source records · Original-source verification pending
- P245NB · 1 source record · Original-source verification pending
- P255QL · 2 source records · Original-source verification pending
- P265 · 1 source record · Original-source verification pending
- P265GH · 10 source records · Original-source verification pending
- P265NB · 1 source record · Original-source verification pending
- P265NL · 6 source records · Original-source verification pending
- P265TR1 · 3 source records · Original-source verification pending
- P265TR2 · 4 source records · Original-source verification pending
- P275NH · 3 source records · Original-source verification pending
- P275NL1 · 4 source records · Original-source verification pending
- P275NL2 · 5 source records · Original-source verification pending
- P295GH · 4 source records · Original-source verification pending
- P310NB · 1 source record · Original-source verification pending
- P345 · 1 source record · Original-source verification pending
- P355N · 5 source records · Original-source verification pending
- P355NH · 6 source records
- P355NL1 · 5 source records · Original-source verification pending
- P355NL2 · 4 source records · Original-source verification pending
- P420NL1 · 2 source records · Original-source verification pending
- P460NH · 5 source records · Original-source verification pending
- P460NL1 · 5 source records · Original-source verification pending
- P460NL2 · 4 source records · Original-source verification pending
- PCD18 · 1 source record
- PCD23 · 1 source record
- PCD40 · 1 source record
- PCD65 · 1 source record
- PHYNOX · 2 source records
- PL 21 · 3 source records · Original-source verification pending
- PL 23 · 3 source records · Original-source verification pending
- PL 25 · 3 source records · Original-source verification pending
- PM23 · 1 source record · Original-source verification pending
- POSCABLE82 · 1 source record
- POSCABLE86 · 1 source record
- POSCABLE90 · 1 source record
- POSCABLE92 · 1 source record
- POSCH6ASP · 1 source record
- POSCORD70S · 1 source record
- POSCORD80S · 1 source record
- POSCORD90 · 1 source record
- POSCORD92CR · 1 source record
- POSCUT1A · 1 source record
- POSCUT1S · 1 source record
- POSFIS5M1 · 1 source record
- POSFIS6B · 1 source record
- POSFIS6M1 · 1 source record
- POSHIS120D · 1 source record
- POSHIS120S · 1 source record
- POSHIS130D · 1 source record
- POSMA40 · 1 source record
- POSMA45R · 1 source record
- POSMICRO62 · 1 source record
- POSTEN20W · 1 source record
- POSWELD12K · 1 source record
- POSWELD1A · 1 source record
- POSWELD1B · 1 source record
- POSWELD1CM · 1 source record
- POSWELD23 · 1 source record
- POSWELD2A · 1 source record
- POSWELD2B · 1 source record
- POSWELD2J · 1 source record
- POSWELD2MO · 1 source record
- POSWELD2S · 1 source record
- POSWELD3CM · 1 source record
- POSWELD41 · 1 source record
- POSWELD4B · 1 source record
- POSWELD4D · 1 source record
- POSWELD50 · 1 source record
- POSWELD60 · 1 source record
- POT62C · 1 source record
- POT67C · 1 source record
- POT70C · 1 source record
- PSPC22 · 1 source record
- PSPC30B · 1 source record
- PSPC30SI · 1 source record
- PSPC32B · 1 source record
- PSPC32SI · 1 source record
- PSPC32SIB · 1 source record
- PSPC32SIBM · 1 source record
- PSPC35B · 1 source record
- PSPC35SI · 1 source record
- PSW10 · 1 source record
- Q10 · 1 source record
- Q10B18 · 1 source record
- Q10B21 · 3 source records
- Q10B21-C · 1 source record
- Q10B23M-C · 1 source record
- Q10B28 · 2 source records
- Q10B30 · 3 source records
- Q10B33 · 3 source records
- Q10B33-C · 1 source record
- Q10B35 · 2 source records
- Q10B38 · 2 source records
- Q17MNB4 · 1 source record
- Q195 · 3 source records
- Q195F · 1 source record
- Q20 · 1 source record
- Q20CR · 1 source record
- Q20CRMNTI · 1 source record
- Q20CRMO · 1 source record
- Q20MNB4 · 2 source records
- Q215A · 2 source records
- Q215AF · 1 source record
- Q215B · 2 source records
- Q215BF · 1 source record
- Q235 · 1 source record · Original-source verification pending
- Q235A · 3 source records
- Q235AF · 2 source records
- Q235B · 4 source records
- Q235BF · 1 source record
- Q235C · 4 source records
- Q235D · 4 source records
- Q23MNB3 · 1 source record
- Q23MNB4 · 1 source record
- Q255A · 2 source records
- Q255B · 2 source records
- Q275 · 1 source record
- Q275A · 1 source record
- Q275AF · 1 source record
- Q275B · 1 source record
- Q275C · 1 source record
- Q275D · 1 source record
- Q295A · 1 source record
- Q295B · 1 source record
- Q30MNB4 · 1 source record
- Q345A · 3 source records
- Q345B · 4 source records
- Q345C · 4 source records
- Q345D · 4 source records
- Q345E · 4 source records
- Q345GJ-B · 1 source record · Original-source verification pending
- Q345GJ-D · 2 source records · Original-source verification pending
- Q355B · 2 source records
- Q355C · 2 source records
- Q355D · 2 source records
- Q355MB · 1 source record
- Q355MC · 2 source records
- Q355MD · 1 source record
- Q355ME · 1 source record
- Q355MF · 1 source record
- Q355NB · 1 source record
- Q355NC · 1 source record
- Q355ND · 1 source record
- Q355NE · 1 source record
- Q355NF · 1 source record
- Q35CRMO · 1 source record
- Q390A · 3 source records
- Q390B · 5 source records
- Q390C · 5 source records
- Q390D · 4 source records
- Q390E · 5 source records
- Q390GJ-B · 2 source records · Original-source verification pending
- Q390GJ-C · 2 source records · Original-source verification pending
- Q390GJ-D · 2 source records · Original-source verification pending
- Q390GJ-E · 2 source records · Original-source verification pending
- Q390MB · 1 source record
- Q390MC · 1 source record
- Q390MD · 1 source record
- Q390ME · 1 source record
- Q390NB · 1 source record
- Q390NC · 1 source record
- Q390ND · 1 source record
- Q390NE · 1 source record
- Q40CR · 1 source record
- Q420A · 3 source records
- Q420B · 5 source records
- Q420C · 6 source records
- Q420D · 4 source records
- Q420E · 3 source records
- Q420GJ-B · 2 source records · Original-source verification pending
- Q420GJ-C · 2 source records · Original-source verification pending
- Q420GJ-D · 3 source records · Original-source verification pending
- Q420GJ-E · 2 source records · Original-source verification pending
- Q420MB · 1 source record
- Q420MC · 1 source record
- Q420MD · 1 source record
- Q420ME · 1 source record
- Q420NB · 1 source record
- Q420NC · 1 source record
- Q420ND · 1 source record
- Q420NE · 1 source record
- Q42CRMO · 1 source record
- Q460C · 5 source records
- Q460D · 4 source records
- Q460E · 3 source records
- Q460GJ-B · 2 source records · Original-source verification pending
- Q460GJ-C · 2 source records · Original-source verification pending
- Q460GJ-D · 2 source records · Original-source verification pending
- Q460GJ-E · 2 source records · Original-source verification pending
- Q460MC · 1 source record
- Q460MD · 1 source record
- Q460ME · 1 source record
- Q460NC · 1 source record
- Q460ND · 1 source record
- Q460NE · 1 source record
- Q500C · 1 source record
- Q500D · 1 source record
- Q500E · 1 source record
- Q500MC · 1 source record
- Q500MD · 1 source record
- Q500ME · 1 source record
- Q51B20 · 1 source record
- Q550C · 1 source record
- Q550D · 1 source record
- Q550E · 1 source record
- Q550MC · 1 source record
- Q550MD · 1 source record
- Q550ME · 1 source record
- Q620C · 1 source record
- Q620D · 1 source record
- Q620E · 1 source record
- Q620MC · 1 source record
- Q620MD · 1 source record
- Q620ME · 1 source record
- Q690C · 1 source record
- Q690D · 1 source record
- Q690E · 1 source record
- Q690MC · 1 source record
- Q690MD · 1 source record
- Q690ME · 1 source record
- QAL10-3-1.5 · 2 source records
- QAL10-4-4 · 2 source records
- QAL10-4-4-1 · 1 source record
- QAL10-5-5 · 2 source records
- QAL11-6-6 · 2 source records
- QAL5 · 2 source records
- QAL6 · 1 source record
- QAL7 · 2 source records
- QAL9-2 · 2 source records
- QAL9-4 · 2 source records
- QAL9-5-1-1 · 2 source records
- QB16 · 1 source record
- QBE0.3-1.5 · 1 source record
- QBE0.4-1.8 · 1 source record
- QBE0.6-2.5 · 1 source record
- QBE1.7 · 1 source record
- QBE1.9 · 1 source record
- QBE1.9-0.1 · 1 source record
- QBE2 · 1 source record
- QCD1 · 1 source record
- QCR0.5 · 1 source record
- QCR0.5-0.2-0.1 · 1 source record
- QCR0.6-0.4-0.05 · 1 source record
- QCR1 · 1 source record
- QCR4.5-2.5-0.6 · 1 source record
- QFE2.5 · 1 source record
- QMG0.8 · 1 source record
- QML06AL · 1 source record
- QML08AL · 2 source records
- QML10 · 1 source record
- QML15 · 1 source record
- QML15AL · 1 source record
- QML15CR · 1 source record
- QML15MNVB · 1 source record
- QML20 · 1 source record
- QML20CR · 2 source records
- QML20CR-B · 1 source record
- QML20CR-C · 1 source record
- QML20CRMO · 1 source record
- QML20MNTIB · 2 source records
- QML20MNTIB-B · 1 source record
- QML20MNTIB-C · 1 source record
- QML20MNVB · 1 source record
- QML35CRMO · 2 source records
- QML40CR · 3 source records
- QML40CR-B · 1 source record
- QML40CR-C · 1 source record
- QML40CRMO · 2 source records
- QML42CRMO · 1 source record
- QMN1.5 · 2 source records
- QMN2 · 2 source records
- QMN5 · 2 source records
- QQ195 · 1 source record
- QQ215 · 1 source record
- QQ235 · 1 source record
- QS35C · 1 source record
- QS45C · 1 source record
- QSAE10B35-B · 1 source record
- QSAE4140 · 1 source record
- QSCM420 · 2 source records
- QSCM435 · 3 source records
- QSCM435-C · 1 source record
- QSCM440 · 3 source records
- QSCM440-C · 1 source record
- QSCR420 · 1 source record
- QSCR440 · 2 source records
- QSI0.6-2 · 1 source record
- QSI1-3 · 2 source records
- QSI3-1 · 2 source records
- QSI3.5-3-1.5 · 2 source records
- QSN0.4 · 1 source record
- QSN0.5-0.025 · 1 source record
- QSN0.6 · 1 source record
- QSN0.9 · 1 source record
- QSN1-0.5-0.5 · 1 source record
- QSN1.5-0.2 · 2 source records
- QSN1.8 · 1 source record
- QSN15-1-1 · 1 source record
- QSN4-0.3 · 2 source records
- QSN4-3 · 2 source records
- QSN4-4-2.5 · 2 source records
- QSN4-4-4 · 2 source records
- QSN5-0.2 · 1 source record
- QSN5-0.3 · 1 source record
- QSN6-0.05 · 1 source record
- QSN6.5-0.1 · 2 source records
- QSN6.5-0.4 · 2 source records
- QSN7-0.2 · 2 source records
- QSN8-0.3 · 2 source records
- QSTE340TM · 1 source record
- QSTE380TM · 1 source record
- QSTE420TM · 2 source records
- QSTE460TM · 1 source record
- QSTE500TM · 1 source record
- QSWRCH10A · 2 source records
- QSWRCH10A-B · 1 source record
- QSWRCH10A-C · 1 source record
- QSWRCH12A · 2 source records
- QSWRCH15A · 2 source records
- QSWRCH15A-B · 1 source record
- QSWRCH15A-C · 1 source record
- QSWRCH18A · 2 source records
- QSWRCH18A-B · 1 source record
- QSWRCH18A-C · 1 source record
- QSWRCH20K · 1 source record
- QSWRCH22A · 2 source records
- QSWRCH22A-B · 1 source record
- QSWRCH22A-C · 1 source record
- QSWRCH25K · 2 source records
- QSWRCH35K · 3 source records
- QSWRCH35K-B · 1 source record
- QSWRCH35K-C · 1 source record
- QSWRCH38K · 2 source records
- QSWRCH40K · 2 source records
- QSWRCH40K-B · 1 source record
- QSWRCH40K-C · 1 source record
- QSWRCH45K · 3 source records
- QSWRCH45K-B · 1 source record
- QSWRCH45K-C · 1 source record
- QSWRCH48K · 1 source record
- QSWRCH50K · 1 source record
- QSWRCH6A · 2 source records
- QSWRCH8A · 2 source records
- QTE0.5 · 1 source record
- QTRAL22 · 1 source record · Original-source verification pending
- QTRAL4SI4 · 1 source record · Original-source verification pending
- QTRAL5SI5 · 1 source record · Original-source verification pending
- QTRSI4 · 1 source record · Original-source verification pending
- QTRSI4MO1 · 1 source record · Original-source verification pending
- QTRSI5 · 1 source record · Original-source verification pending
- QZR0.2 · 1 source record
- QZR0.4 · 1 source record
- RENE 41 · 2 source records
- RST37-2 · 1 source record · Original-source verification pending
- S09CK · 10 source records
- S10C · 13 source records
- S10C-D · 3 source records
- S12C · 10 source records
- S15500 · 1 source record
- S15700 · 1 source record · Original-source verification pending
- S15C · 12 source records
- S15CK · 10 source records
- S17400 · 2 source records · Original-source verification pending
- S17700 · 1 source record · Original-source verification pending
- S17C · 9 source records
- S18A · 1 source record
- S20100 · 3 source records
- S20103 · 2 source records
- S20153 · 3 source records
- S20161 · 2 source records
- S20200 · 2 source records
- S20400 · 3 source records
- S20430 · 1 source record
- S20431 · 1 source record
- S20432 · 1 source record
- S20433 · 1 source record
- S20910 · 15 source records
- S20C · 15 source records
- S20C-D · 3 source records
- S20CK · 8 source records
- S21400 · 2 source records
- S21600 · 8 source records
- S21603 · 2 source records
- S21640 · 1 source record
- S21800 · 2 source records
- S21900 · 1 source record
- S21904 · 2 source records
- S22C · 9 source records
- S235J0 · 5 source records
- S235J0W · 1 source record
- S235J2 · 2 source records
- S235J2W · 1 source record
- S235JR · 8 source records
- S235JRC · 1 source record · Original-source verification pending
- S24000 · 4 source records
- S24100 · 1 source record
- S25C · 11 source records
- S25C-D · 3 source records
- S275J0 · 6 source records
- S275J2 · 1 source record
- S275J2G3 · 1 source record · Original-source verification pending
- S275JR · 6 source records
- S275N · 2 source records · Original-source verification pending
- S275NE · 2 source records · Original-source verification pending
- S275NL · 4 source records · Original-source verification pending
- S28C · 8 source records
- S2M · 1 source record
- S30100 · 2 source records
- S30103 · 1 source record
- S30153 · 1 source record
- S30200 · 2 source records
- S30400 · 16 source records
- S30403 · 16 source records
- S30409 · 8 source records
- S30415 · 17 source records
- S30430 · 1 source record
- S30432 · 1 source record
- S30435 · 1 source record
- S30441 · 1 source record
- S30451 · 12 source records
- S30452 · 2 source records
- S30453 · 12 source records
- S30500 · 2 source records
- S30530 · 1 source record
- S30600 · 3 source records
- S30601 · 3 source records
- S30615 · 3 source records
- S30815 · 4 source records
- S30908 · 12 source records
- S30909 · 3 source records
- S30940 · 3 source records
- S30941 · 3 source records
- S30C · 10 source records
- S31002 · 1 source record
- S31008 · 13 source records
- S31009 · 10 source records
- S31035 · 1 source record
- S31040 · 3 source records
- S31041 · 3 source records
- S31050 · 4 source records
- S31060 · 1 source record
- S31200 · 2 source records
- S31254 · 5 source records
- S31260 · 13 source records
- S31266 · 3 source records
- S31277 · 15 source records
- S31400 · 1 source record
- S31500 · 1 source record
- S31600 · 16 source records
- S31603 · 17 source records
- S31608 · 1 source record · Original-source verification pending
- S31609 · 3 source records
- S31635 · 12 source records
- S31640 · 2 source records
- S31651 · 3 source records
- S31653 · 12 source records
- S31655 · 1 source record
- S31700 · 3 source records
- S31703 · 7 source records
- S31725 · 24 source records
- S31726 · 23 source records
- S31727 · 3 source records
- S31730 · 1 source record
- S31753 · 2 source records
- S31803 · 34 source records
- S32001 · 1 source record
- S32003 · 1 source record
- S32050 · 1 source record
- S32053 · 3 source records
- S32100 · 13 source records
- S32101 · 22 source records
- S32109 · 3 source records
- S32202 · 20 source records
- S32205 · 22 source records
- S32304 · 15 source records
- S32506 · 16 source records
- S32520 · 11 source records
- S32550 · 2 source records
- S32615 · 17 source records
- S32654 · 3 source records
- S32750 · 23 source records
- S32760 · 31 source records
- S32803 · 2 source records
- S32808 · 1 source record
- S32900 · 3 source records
- S32906 · 16 source records
- S32950 · 25 source records
- S33228 · 3 source records
- S33400 · 1 source record
- S33425 · 1 source record
- S33550 · 1 source record
- S33C · 8 source records
- S34565 · 3 source records
- S34700 · 13 source records
- S34709 · 9 source records
- S34751 · 2 source records
- S34800 · 3 source records
- S34809 · 3 source records
- S35045 · 2 source records
- S35115 · 1 source record
- S35125 · 1 source record
- S35135 · 1 source record
- S35140 · 1 source record
- S35315 · 3 source records
- S355J0 · 3 source records
- S355J0W · 1 source record
- S355J0WP · 1 source record
- S355J2 · 5 source records
- S355J2C · 1 source record · Original-source verification pending
- S355J2W · 1 source record
- S355J2WP · 1 source record
- S355JR · 1 source record
- S355K2 · 1 source record
- S355K2W · 1 source record
- S355N · 2 source records · Original-source verification pending
- S355NE · 2 source records · Original-source verification pending
- S355NL · 3 source records · Original-source verification pending
- S35C · 15 source records
- S35C-D · 3 source records
- S38100 · 3 source records
- S38815 · 2 source records
- S38C · 12 source records
- S39274 · 14 source records
- S400 · 1 source record
- S40500 · 9 source records
- S40900 · 3 source records
- S40910 · 1 source record
- S40920 · 1 source record
- S40930 · 1 source record
- S40940 · 1 source record
- S40945 · 2 source records
- S40975 · 2 source records
- S40977 · 8 source records
- S40C · 11 source records
- S41000 · 11 source records
- S41003 · 2 source records
- S41008 · 7 source records
- S41045 · 2 source records
- S41050 · 6 source records
- S41500 · 23 source records
- S42010 · 1 source record
- S42030 · 4 source records
- S42035 · 1 source record
- S420N · 2 source records · Original-source verification pending
- S420NE · 2 source records · Original-source verification pending
- S420NL · 3 source records · Original-source verification pending
- S42900 · 2 source records
- S43000 · 13 source records
- S43035 · 4 source records
- S43036 · 2 source records · Original-source verification pending
- S43100 · 8 source records · Original-source verification pending
- S43400 · 2 source records
- S43600 · 2 source records
- S43932 · 8 source records
- S43940 · 8 source records
- S43C · 11 source records
- S44100 · 1 source record
- S44330 · 1 source record
- S44400 · 2 source records
- S44401 · 1 source record
- S44500 · 2 source records
- S44535 · 1 source record
- S44536 · 1 source record
- S44537 · 1 source record
- S44625 · 4 source records
- S44626 · 2 source records
- S44627 · 13 source records
- S44635 · 2 source records
- S44660 · 2 source records
- S44700 · 3 source records
- S44725 · 1 source record
- S44735 · 2 source records
- S44800 · 3 source records
- S45C · 14 source records
- S45C-D · 3 source records
- S460 · 1 source record
- S460J0 · 1 source record
- S460J2 · 1 source record
- S460JR · 1 source record
- S460K2 · 1 source record
- S460ME · 2 source records · Original-source verification pending
- S460ML · 4 source records · Original-source verification pending
- S460N · 2 source records · Original-source verification pending
- S460NE · 2 source records · Original-source verification pending
- S460NL · 3 source records · Original-source verification pending
- S460Q · 1 source record
- S460QL · 1 source record
- S460QL1 · 1 source record
- S46800 · 2 source records
- S48C · 9 source records
- S500J0 · 1 source record
- S500Q · 1 source record
- S500QL · 1 source record
- S500QL1 · 1 source record
- S50C · 12 source records
- S53C · 8 source records
- S550 · 1 source record
- S550GD+Z · 1 source record · Original-source verification pending
- S550Q · 1 source record
- S550QL · 1 source record
- S550QL1 · 1 source record
- S55C · 12 source records
- S58C · 8 source records
- S60C · 2 source records
- S620Q · 1 source record
- S620QL · 1 source record
- S620QL1 · 1 source record
- S65C · 2 source records
- S66286 · 1 source record · Original-source verification pending
- S690Q · 1 source record
- S690QL · 1 source record
- S690QL1 · 1 source record
- S70C · 2 source records
- S75C · 2 source records
- S81921 · 1 source record
- S82011 · 1 source record
- S82012 · 1 source record
- S82031 · 1 source record
- S82121 · 1 source record
- S82122 · 1 source record
- S82441 · 1 source record
- S890Q · 1 source record
- S890QL · 1 source record
- S890QL1 · 1 source record
- S960Q · 1 source record
- S960QL · 1 source record
- S960QL1 · 1 source record
- SA-106 GRADE B · 1 source record · Original-source verification pending
- SA-387 GRADE22 CLASS1 · 1 source record · Original-source verification pending
- SA-387 GRADE22 CLASS2 · 1 source record · Original-source verification pending
- SA-387 GRADE5 CLASS1 · 1 source record · Original-source verification pending
- SA-387 GRADE5 CLASS2 · 1 source record · Original-source verification pending
- SA135 GRADE B · 1 source record · Original-source verification pending
- SA178 GRADE C · 1 source record · Original-source verification pending
- SA194 GRADE 3 · 1 source record · Original-source verification pending
- SA194 GRADE 6 · 1 source record · Original-source verification pending
- SA194 GRADE 8 · 1 source record · Original-source verification pending
- SA194 GRADE 8A · 1 source record · Original-source verification pending
- SA194 GRADE 8C · 1 source record · Original-source verification pending
- SA194 GRADE 8CA · 1 source record · Original-source verification pending
- SA194 GRADE 8LN · 1 source record · Original-source verification pending
- SA194 GRADE 8LNA · 1 source record · Original-source verification pending
- SA194 GRADE 8M · 1 source record · Original-source verification pending
- SA194 GRADE 8MA · 1 source record · Original-source verification pending
- SA194 GRADE 8MLN · 1 source record · Original-source verification pending
- SA194 GRADE 8MLNA · 1 source record · Original-source verification pending
- SA194 GRADE 8N · 1 source record · Original-source verification pending
- SA194 GRADE 8NA · 1 source record · Original-source verification pending
- SA194 GRADE 8R · 1 source record · Original-source verification pending
- SA194 GRADE 8RA · 1 source record · Original-source verification pending
- SA194 GRADE 8T · 1 source record · Original-source verification pending
- SA194 GRADE 8TA · 1 source record · Original-source verification pending
- SA194 GRADE 9C · 1 source record · Original-source verification pending
- SA194 GRADE 9CA · 1 source record · Original-source verification pending
- SA203 GRADE D · 1 source record · Original-source verification pending
- SA203 GRADE E · 1 source record · Original-source verification pending
- SA203 GRADE F · 1 source record · Original-source verification pending
- SA210 GRADE A-1 · 1 source record · Original-source verification pending
- SA213 GRADE T2 · 1 source record · Original-source verification pending
- SA213 GRADE T22 · 1 source record · Original-source verification pending
- SA213 GRADE TP304H · 1 source record · Original-source verification pending
- SA213 TP317LM · 1 source record · Original-source verification pending
- SA213M GRADE TP347H · 1 source record · Original-source verification pending
- SA250 GRADE T2 · 1 source record · Original-source verification pending
- SA250 GRADE T22 · 1 source record · Original-source verification pending
- SA283 GRADE C · 1 source record · Original-source verification pending
- SA283 GRADE D · 1 source record · Original-source verification pending
- SA335 GRADE P2 · 1 source record · Original-source verification pending
- SA335 GRADE P22 · 1 source record · Original-source verification pending
- SA36 · 1 source record · Original-source verification pending
- SA414 GRADE C · 1 source record · Original-source verification pending
- SA414 GRADE D · 1 source record · Original-source verification pending
- SA414 GRADE E · 1 source record · Original-source verification pending
- SA414 GRADE F · 1 source record · Original-source verification pending
- SA453 GRADE 660 CLASS A · 1 source record · Original-source verification pending
- SA453 GRADE 660 CLASS B · 1 source record · Original-source verification pending
- SA515 GRADE 60 · 1 source record · Original-source verification pending
- SA515 GRADE 65 · 1 source record · Original-source verification pending
- SA515 GRADE 70 · 1 source record · Original-source verification pending
- SA516 GRADE 60 · 1 source record · Original-source verification pending
- SA516 GRADE 65 · 1 source record · Original-source verification pending
- SA516 GRADE 70 · 1 source record · Original-source verification pending
- SA537 CLASS 1 · 1 source record · Original-source verification pending
- SA556 GRADE B2 · 1 source record · Original-source verification pending
- SA572 GRADE 55[380] TYPE5 · 1 source record · Original-source verification pending
- SA572 GRADE 60[415] TYPE5 · 1 source record · Original-source verification pending
- SA572 GRADE 65[450] TYPE5 · 1 source record · Original-source verification pending
- SA662M GRADE A · 1 source record · Original-source verification pending
- SA662M GRADE B · 1 source record · Original-source verification pending
- SA662M GRADE C · 1 source record · Original-source verification pending
- SA737 GRADE B · 1 source record · Original-source verification pending
- SA841 GRADE A CLASS 1 · 1 source record · Original-source verification pending
- SA841 GRADE B CLASS 1 · 1 source record · Original-source verification pending
- SA841 GRADE C CLASS 1 · 1 source record · Original-source verification pending
- SACM645 · 3 source records
- SAE 1008 · 1 source record
- SAE 1019 · 1 source record
- SAE 4137 · 1 source record
- SAE 52100 · 1 source record · Original-source verification pending
- SAE/AISI 1006(IFI-1006) · 1 source record
- SAE/AISI 1008(IFI-1008) · 1 source record
- SAE/AISI 1010(IFI-1010) · 1 source record
- SAE/AISI 1018(IFI-1018) · 1 source record
- SAE/AISI 1033(IFI-1033) · 1 source record
- SAE/AISI 1035(IFI-1035) · 1 source record
- SAE/AISI 1038(IFI-1038) · 1 source record
- SAE/AISI 10B21(IFI-10B21) · 1 source record
- SAE/AISI 10B38(IFI-10B38) · 1 source record
- SAE/AISI 1335(IFI-1335) · 1 source record
- SAE/AISI 4037(IFI-4037) · 1 source record
- SAE/AISI 4042(IFI-4042) · 1 source record
- SAE/AISI 4118(IFI-4118) · 1 source record
- SAE/AISI 4140(IFI-4140) · 1 source record
- SAE/AISI 5140(IFI-5140) · 1 source record
- SAE/AISI 8637(IFI-8637) · 1 source record
- SAE1010 · 1 source record
- SAE1010-1 · 1 source record
- SAE1015 · 2 source records
- SAE1018 · 2 source records
- SAE1018-D · 1 source record
- SAE1019 · 1 source record
- SAE1020 · 1 source record
- SAE1022 · 1 source record
- SAE1035 · 1 source record
- SAE1045 · 2 source records
- SAE1050 · 2 source records
- SAE1080S · 1 source record
- SAE10B21-1 · 1 source record
- SAE10B35 · 1 source record
- SAE4037 · 1 source record
- SAE9254 · 2 source records
- SAPH310 · 1 source record
- SAPH370 · 1 source record
- SAPH400 · 1 source record
- SAPH440 · 1 source record
- SB-381 GRADE F-1 · 1 source record · Original-source verification pending
- SB-381 GRADE F-23 · 1 source record · Original-source verification pending
- SB-381 GRADE F-3 · 1 source record · Original-source verification pending
- SB-381 GRADE F-6 · 1 source record · Original-source verification pending
- SB-381 GRADE F-7 · 1 source record · Original-source verification pending
- SB-381 GRADE F-7H · 1 source record · Original-source verification pending
- SB25 · 2 source records
- SB338 GRADE 1 · 1 source record · Original-source verification pending
- SB338 GRADE 3 · 1 source record · Original-source verification pending
- SB338 GRADE 7 · 1 source record · Original-source verification pending
- SB338 GRADE 7H · 1 source record · Original-source verification pending
- SB410 · 2 source records
- SB450 · 1 source record · Original-source verification pending
- SB480 · 1 source record · Original-source verification pending
- SCH 12 · 1 source record · Original-source verification pending
- SCH 22 · 1 source record · Original-source verification pending
- SCH 34 · 2 source records · Original-source verification pending
- SCM27B · 1 source record
- SCM415 · 8 source records
- SCM415-1 · 2 source records
- SCM415-D · 2 source records
- SCM415H · 7 source records
- SCM415H-D · 2 source records
- SCM415H1RCH · 1 source record
- SCM415H2RCH · 1 source record
- SCM415HRCH · 3 source records
- SCM415RCH · 3 source records
- SCM415WCH · 2 source records
- SCM418 · 6 source records
- SCM418H · 4 source records
- SCM418H1RCH · 1 source record
- SCM418H2RCH · 1 source record
- SCM418HRCH · 3 source records
- SCM418RCH · 3 source records
- SCM418WCH · 2 source records
- SCM420 · 13 source records
- SCM420-1 · 1 source record
- SCM420-D · 2 source records
- SCM420H · 6 source records
- SCM420H-D · 2 source records
- SCM420H1RCH · 1 source record
- SCM420H2RCH · 1 source record
- SCM420HRCH · 3 source records
- SCM420RCH · 3 source records
- SCM420WCH · 2 source records
- SCM421 · 6 source records
- SCM425 · 4 source records
- SCM425H · 3 source records
- SCM425H1RCH · 1 source record
- SCM425H2RCH · 1 source record
- SCM425HRCH · 3 source records
- SCM425RCH · 3 source records
- SCM425WCH · 2 source records
- SCM430 · 6 source records
- SCM430RCH · 3 source records
- SCM430WCH · 2 source records
- SCM432 · 5 source records
- SCM435 · 15 source records
- SCM435-1 · 1 source record
- SCM435-2 · 2 source records
- SCM435-3 · 1 source record
- SCM435-D · 2 source records
- SCM435-N · 1 source record
- SCM435H · 5 source records
- SCM435H-D · 2 source records
- SCM435H1RCH · 1 source record
- SCM435H2RCH · 1 source record
- SCM435HRCH · 3 source records
- SCM435RCH · 3 source records
- SCM435TK · 1 source record · Original-source verification pending
- SCM435WCH · 2 source records
- SCM435(D) · 1 source record
- SCM440 · 14 source records
- SCM440-1 · 1 source record
- SCM440-2 · 1 source record
- SCM440-D · 2 source records
- SCM440H · 6 source records
- SCM440H-D · 2 source records
- SCM440H1RCH · 1 source record
- SCM440H2RCH · 1 source record
- SCM440HRCH · 3 source records
- SCM440RCH · 3 source records
- SCM440TK · 1 source record · Original-source verification pending
- SCM440WCH · 2 source records
- SCM440(42CRMO) · 1 source record
- SCM445 · 5 source records
- SCM445H · 4 source records
- SCM445H1RCH · 1 source record
- SCM445H2RCH · 1 source record
- SCM445HRCH · 3 source records
- SCM445RCH · 3 source records
- SCM445WCH · 2 source records
- SCM822 · 6 source records
- SCM822H · 4 source records
- SCM822H1RCH · 1 source record
- SCM822H2RCH · 1 source record
- SCM822HRCH · 3 source records
- SCM822RCH · 3 source records
- SCM822WCH · 1 source record
- SCMQ4E · 1 source record · Original-source verification pending
- SCMV4-1 · 1 source record · Original-source verification pending
- SCMV4-2 · 1 source record · Original-source verification pending
- SCMV6-1 · 1 source record · Original-source verification pending
- SCMV6-2 · 1 source record · Original-source verification pending
- SCR22B-A · 1 source record
- SCR415 · 6 source records
- SCR415H · 4 source records
- SCR415H1RCH · 1 source record
- SCR415H2RCH · 1 source record
- SCR415HRCH · 3 source records
- SCR415RCH · 3 source records
- SCR415WCH · 2 source records
- SCR420 · 6 source records
- SCR420-1 · 1 source record
- SCR420-D · 3 source records
- SCR420H · 6 source records
- SCR420H1RCH · 1 source record
- SCR420H2RCH · 1 source record
- SCR420HRCH · 3 source records
- SCR420RCH · 3 source records
- SCR420WCH · 2 source records
- SCR430 · 5 source records
- SCR430H · 4 source records
- SCR430H1RCH · 1 source record
- SCR430H2RCH · 1 source record
- SCR430HRCH · 3 source records
- SCR430RCH · 3 source records
- SCR430WCH · 2 source records
- SCR435 · 5 source records
- SCR435H · 4 source records
- SCR435H1RCH · 1 source record
- SCR435H2RCH · 1 source record
- SCR435HRCH · 3 source records
- SCR435RCH · 3 source records
- SCR435WCH · 2 source records
- SCR440 · 7 source records
- SCR440-1 · 1 source record
- SCR440-D · 2 source records
- SCR440H · 4 source records
- SCR440H1RCH · 1 source record
- SCR440H2RCH · 1 source record
- SCR440HRCH · 3 source records
- SCR440RCH · 3 source records
- SCR440WCH · 2 source records
- SCR445 · 4 source records
- SCU7061 · 1 source record · Original-source verification pending
- SD · 1 source record · Original-source verification pending
- SG255 · 1 source record · Original-source verification pending
- SG295 · 1 source record · Original-source verification pending
- SG325 · 1 source record · Original-source verification pending
- SGD1 · 1 source record
- SGD2 · 1 source record
- SGD3 · 1 source record
- SGD4 · 1 source record
- SGDA · 1 source record
- SGDB · 1 source record
- SGP · 1 source record · Original-source verification pending
- SGV410 · 1 source record · Original-source verification pending
- SGV450 · 1 source record · Original-source verification pending
- SGV480 · 1 source record · Original-source verification pending
- SK65 · 2 source records · Original-source verification pending
- SL3N255 · 1 source record · Original-source verification pending
- SL3N275 · 1 source record · Original-source verification pending
- SL3N440 · 1 source record · Original-source verification pending
- SLA235A · 1 source record · Original-source verification pending
- SLA235B · 1 source record · Original-source verification pending
- SLA325A · 1 source record · Original-source verification pending
- SLA325B · 1 source record · Original-source verification pending
- SLA365 · 1 source record · Original-source verification pending
- SM-27 · 1 source record
- SM3CR2MNNIMO · 1 source record · Original-source verification pending
- SM400A · 7 source records
- SM400B · 7 source records
- SM400C · 7 source records
- SM490A · 7 source records
- SM490B · 7 source records
- SM490BZ · 1 source record
- SM490C · 7 source records
- SM490YA · 6 source records
- SM490YB · 6 source records
- SM50B-1 · 1 source record
- SM520B · 2 source records
- SM520BZ · 1 source record
- SM520C · 2 source records
- SM570 · 1 source record
- SM570C · 2 source records · Original-source verification pending
- SMN420 · 4 source records
- SMN420H · 3 source records
- SMN420H1RCH · 1 source record
- SMN420H2RCH · 1 source record
- SMN420HRCH · 3 source records
- SMN420RCH · 3 source records
- SMN420WCH · 2 source records
- SMN433 · 5 source records
- SMN433H · 4 source records
- SMN433H1RCH · 1 source record
- SMN433H2RCH · 1 source record
- SMN433HRCH · 3 source records
- SMN433RCH · 3 source records
- SMN433WCH · 2 source records
- SMN438 · 5 source records
- SMN438H · 4 source records
- SMN438H1RCH · 1 source record
- SMN438H2RCH · 1 source record
- SMN438HRCH · 3 source records
- SMN438RCH · 3 source records
- SMN438WCH · 2 source records
- SMN443 · 5 source records
- SMN443H · 3 source records
- SMN443H1RCH · 1 source record
- SMN443H2RCH · 1 source record
- SMN443HRCH · 3 source records
- SMN443RCH · 3 source records
- SMN443WCH · 2 source records
- SMNC420 · 4 source records
- SMNC420H · 3 source records
- SMNC420RCH · 3 source records
- SMNC420WCH · 2 source records
- SMNC433 · 1 source record
- SMNC443 · 5 source records
- SMNC443H · 4 source records
- SMNC443RCH · 3 source records
- SMNC443WCH · 2 source records
- SN400A · 2 source records · Original-source verification pending
- SN400B · 2 source records · Original-source verification pending
- SN400C · 1 source record · Original-source verification pending
- SN490B · 2 source records · Original-source verification pending
- SN490C · 1 source record · Original-source verification pending
- SNB16 · 4 source records
- SNB16-D · 3 source records
- SNB5 · 2 source records
- SNB7 · 3 source records
- SNC22B-A · 1 source record
- SNC236 · 3 source records
- SNC415 · 3 source records
- SNC415H · 3 source records
- SNC415H1RCH · 1 source record
- SNC415H2RCH · 1 source record
- SNC415HRCH · 3 source records
- SNC415RCH · 3 source records
- SNC415WCH · 2 source records
- SNC631 · 3 source records
- SNC631H · 3 source records
- SNC631H1RCH · 1 source record
- SNC631H2RCH · 1 source record
- SNC631HRCH · 3 source records
- SNC631RCH · 3 source records
- SNC631WCH · 2 source records
- SNC815 · 3 source records
- SNC815H · 3 source records
- SNC815H1RCH · 1 source record
- SNC815H2RCH · 1 source record
- SNC815HRCH · 3 source records
- SNC815RCH · 3 source records
- SNC815WCH · 2 source records
- SNC836 · 3 source records
- SNCM220 · 6 source records
- SNCM220H · 4 source records
- SNCM220H1RCH · 1 source record
- SNCM220H2RCH · 1 source record
- SNCM220HRCH · 3 source records
- SNCM220RCH · 3 source records
- SNCM220WCH · 2 source records
- SNCM240 · 4 source records
- SNCM240RCH · 3 source records
- SNCM240WCH · 2 source records
- SNCM415 · 4 source records
- SNCM420 · 4 source records
- SNCM420H · 4 source records
- SNCM420H1RCH · 1 source record
- SNCM420H2RCH · 1 source record
- SNCM420HRCH · 3 source records
- SNCM420RCH · 3 source records
- SNCM420WCH · 2 source records
- SNCM431 · 4 source records
- SNCM439 · 5 source records
- SNCM439RCH · 3 source records
- SNCM439WCH · 2 source records
- SNCM447 · 4 source records
- SNCM447RCH · 3 source records
- SNCM447WCH · 2 source records
- SNCM616 · 4 source records
- SNCM616RCH · 3 source records
- SNCM616WCH · 2 source records
- SNCM625 · 4 source records
- SNCM630 · 4 source records
- SNCM815 · 4 source records
- SNI1001 · 2 source records · Original-source verification pending
- SNI1066 · 1 source record · Original-source verification pending
- SNI4060 · 1 source record · Original-source verification pending
- SNI6625 · 1 source record · Original-source verification pending
- SNI7718 · 1 source record · Original-source verification pending
- SPCC · 1 source record
- SPCD · 3 source records
- SPCE · 1 source record
- SPHC · 1 source record
- SPHD · 1 source record
- SPHE · 1 source record
- SPHT1 · 1 source record
- SPHT2 · 1 source record
- SPHT2Z · 1 source record
- SPHT3 · 1 source record
- SPHT3Z · 1 source record
- SPV 24 · 1 source record · Original-source verification pending
- SPV 32 · 1 source record · Original-source verification pending
- SPV235 · 1 source record · Original-source verification pending
- SPV315 · 1 source record · Original-source verification pending
- SRS60 · 1 source record
- SS GRADE 33 [230] · 2 source records · Original-source verification pending
- SS GRADE 36 [250] TYPE 1 · 2 source records · Original-source verification pending
- SS GRADE 36 [250] TYPE 2 · 2 source records · Original-source verification pending
- SS GRADE 40 [275] · 2 source records · Original-source verification pending
- SS GRADE 45 [310] TYPE 1 · 2 source records · Original-source verification pending
- SS GRADE 45 [310] TYPE 2 · 2 source records · Original-source verification pending
- SS GRADE 50 [340] · 3 source records · Original-source verification pending
- SS GRADE 55 [380] · 2 source records · Original-source verification pending
- SS2324 · 2 source records · Original-source verification pending
- SS330 · 4 source records
- SS400 · 10 source records
- SS490 · 8 source records
- SS5114 · 1 source record · Original-source verification pending
- SS5122 · 1 source record · Original-source verification pending
- SS5150 · 1 source record · Original-source verification pending
- SS540 · 4 source records
- ST 37-2 · 1 source record
- ST 44-2 · 1 source record
- ST12 · 1 source record
- ST13 · 1 source record
- ST14 · 1 source record
- ST30AL · 1 source record · Original-source verification pending
- ST33 · 1 source record
- ST35 · 1 source record · Original-source verification pending
- ST37-2 · 3 source records · Original-source verification pending
- ST37-3 · 1 source record
- ST44-2 · 2 source records · Original-source verification pending
- ST44-3 · 1 source record · Original-source verification pending
- ST45 · 1 source record · Original-source verification pending
- ST50-2 · 1 source record
- ST52 · 1 source record · Original-source verification pending
- ST52-3 · 1 source record
- ST60-2 · 2 source records · Original-source verification pending
- ST70-2 · 2 source records · Original-source verification pending
- STAINLESS STEEL 1.4310 · 1 source record
- STAINLESS STEEL 302 · 2 source records
- STAINLESS STEEL 304 · 2 source records
- STAINLESS STEEL 316 · 2 source records
- STAINLESS STEEL 316 TI · 1 source record
- STAINLESS STEEL 316LVM · 2 source records
- STAINLESS STEEL 321 · 1 source record
- STAINLESS STEEL DTD 189A · 2 source records
- STAM290GA · 1 source record · Original-source verification pending
- STAM290GB · 1 source record · Original-source verification pending
- STAM340G · 1 source record · Original-source verification pending
- STAM390G · 1 source record · Original-source verification pending
- STAM440G · 1 source record · Original-source verification pending
- STAM440H · 1 source record · Original-source verification pending
- STAM470G · 1 source record · Original-source verification pending
- STAM470H · 1 source record · Original-source verification pending
- STAM500G · 1 source record · Original-source verification pending
- STAM500H · 1 source record · Original-source verification pending
- STAM540H · 1 source record · Original-source verification pending
- STB410 · 1 source record · Original-source verification pending
- STBA20 · 1 source record · Original-source verification pending
- STBA24 · 1 source record · Original-source verification pending
- STBL380 · 1 source record · Original-source verification pending
- STBL450 · 1 source record · Original-source verification pending
- STC370 · 1 source record · Original-source verification pending
- STC440 · 1 source record · Original-source verification pending
- STC510A · 1 source record · Original-source verification pending
- STC510B · 1 source record · Original-source verification pending
- STC540 · 1 source record · Original-source verification pending
- STC590A · 1 source record · Original-source verification pending
- STC590B · 1 source record · Original-source verification pending
- STELLITE 712 · 1 source record · Original-source verification pending
- STELLITE F · 1 source record · Original-source verification pending
- STELLITE FSX 414 · 2 source records · Original-source verification pending
- STELLITE NO.12 · 1 source record · Original-source verification pending
- STF410 · 1 source record · Original-source verification pending
- STFA24 · 1 source record · Original-source verification pending
- STI 6400 · 1 source record · Original-source verification pending
- STK290 · 1 source record · Original-source verification pending
- STK400 · 1 source record · Original-source verification pending
- STK490 · 1 source record · Original-source verification pending
- STK500 · 1 source record · Original-source verification pending
- STK540 · 1 source record · Original-source verification pending
- STKM 11A · 1 source record · Original-source verification pending
- STKM 12B · 1 source record · Original-source verification pending
- STKM 13A · 1 source record · Original-source verification pending
- STKM 17C · 1 source record · Original-source verification pending
- STKM11A · 1 source record · Original-source verification pending
- STKM12A · 1 source record · Original-source verification pending
- STKM12B · 1 source record · Original-source verification pending
- STKM12C · 1 source record · Original-source verification pending
- STKM13A · 1 source record · Original-source verification pending
- STKM13B · 1 source record · Original-source verification pending
- STKM13C · 1 source record · Original-source verification pending
- STKM14A · 1 source record · Original-source verification pending
- STKM14B · 1 source record · Original-source verification pending
- STKM14C · 1 source record · Original-source verification pending
- STKM15A · 1 source record · Original-source verification pending
- STKM15C · 1 source record · Original-source verification pending
- STKM16A · 1 source record · Original-source verification pending
- STKM16C · 1 source record · Original-source verification pending
- STKM17A · 1 source record · Original-source verification pending
- STKM17C · 1 source record · Original-source verification pending
- STKM18A · 1 source record · Original-source verification pending
- STKM18B · 1 source record · Original-source verification pending
- STKM18C · 1 source record · Original-source verification pending
- STKM19A · 1 source record · Original-source verification pending
- STKM19C · 1 source record · Original-source verification pending
- STKM20A · 1 source record · Original-source verification pending
- STKT590 · 2 source records · Original-source verification pending
- STPA20 · 1 source record · Original-source verification pending
- STPA24 · 1 source record · Original-source verification pending
- STPG410 · 1 source record · Original-source verification pending
- STPL380 · 1 source record · Original-source verification pending
- STPL450 · 1 source record · Original-source verification pending
- STPT 370 · 1 source record · Original-source verification pending
- STPT 410 · 1 source record · Original-source verification pending
- STPY400 · 1 source record · Original-source verification pending
- STS 370 · 2 source records · Original-source verification pending
- STS 410 · 3 source records · Original-source verification pending
- STW22 · 1 source record
- STW23 · 1 source record
- STW24 · 1 source record
- SUH 409L · 1 source record · Original-source verification pending
- SUH409L · 2 source records · Original-source verification pending
- SUH660-WSA · 1 source record · Original-source verification pending
- SUH660-WSB · 1 source record · Original-source verification pending
- SUJ2 · 4 source records
- SUJ3 · 2 source records
- SUJ4 · 2 source records
- SUJ5 · 2 source records
- SUM11 · 2 source records
- SUM12 · 2 source records
- SUM21 · 4 source records
- SUM22 · 5 source records
- SUM22L · 2 source records
- SUM23 · 4 source records
- SUM23L · 2 source records
- SUM24L · 3 source records
- SUM25 · 4 source records
- SUM31 · 5 source records
- SUM31L · 2 source records
- SUM32 · 4 source records
- SUM41 · 4 source records
- SUM42 · 4 source records
- SUM43 · 4 source records
- SUP10 · 2 source records
- SUP11A · 3 source records
- SUP12 · 3 source records
- SUP13 · 2 source records
- SUP6 · 3 source records
- SUP7 · 3 source records
- SUP9 · 3 source records
- SUP9A · 3 source records
- SUPER DUPLEX · 1 source record
- SUS 304 · 10 source records
- SUS 304L · 10 source records
- SUS 304L-W1 · 1 source record · Original-source verification pending
- SUS 304LN · 4 source records
- SUS 304N1 · 6 source records
- SUS 304N1-W1 · 1 source record · Original-source verification pending
- SUS 304N1-W1/2H · 1 source record · Original-source verification pending
- SUS 310S · 6 source records
- SUS 310S-W1 · 1 source record · Original-source verification pending
- SUS 316 · 10 source records
- SUS 316-W1 · 1 source record · Original-source verification pending
- SUS 316J1 · 4 source records
- SUS 316L · 10 source records
- SUS 316L-W1 · 1 source record · Original-source verification pending
- SUS 316LN · 4 source records
- SUS 316TI · 4 source records
- SUS 317L · 5 source records
- SUS 317L-W1 · 1 source record · Original-source verification pending
- SUS 321 · 8 source records
- SUS 321-W1 · 1 source record · Original-source verification pending
- SUS 329J1 · 5 source records
- SUS 329J3L · 5 source records
- SUS 329J4L · 7 source records
- SUS 347 · 7 source records
- SUS 347-W1 · 1 source record · Original-source verification pending
- SUS 405 · 3 source records
- SUS 405-W2 · 1 source record · Original-source verification pending
- SUS 410 · 7 source records
- SUS 410-W2 · 1 source record · Original-source verification pending
- SUS 410L · 6 source records
- SUS 410S · 2 source records
- SUS 430 · 10 source records
- SUS 430-W2 · 1 source record · Original-source verification pending
- SUS 430LX · 2 source records
- SUS 630 · 4 source records
- SUS 631 · 3 source records
- SUS 836L · 4 source records
- SUS 890L · 4 source records
- SUS XM27 · 3 source records
- SUS201 · 2 source records
- SUS301 · 1 source record
- SUS301-CSP-1/2H · 1 source record
- SUS301-CSP-3/4H · 1 source record
- SUS301-CSP-EH · 1 source record
- SUS301-CSP-H · 1 source record
- SUS301-CSP-SEH · 1 source record
- SUS301J1 · 1 source record
- SUS301L · 1 source record
- SUS302 · 2 source records
- SUS302B · 1 source record
- SUS303 · 2 source records
- SUS303CU · 2 source records
- SUS303SE · 2 source records
- SUS304 · 2 source records
- SUS304-CSP-1/2H · 1 source record
- SUS304-CSP-3/4H · 1 source record
- SUS304-CSP-H · 1 source record
- SUS304-WSA · 1 source record · Original-source verification pending
- SUS304-WSB · 1 source record · Original-source verification pending
- SUS304CU · 1 source record
- SUS304J1 · 1 source record
- SUS304J2 · 1 source record
- SUS304J3 · 2 source records
- SUS304J3-WSA · 1 source record · Original-source verification pending
- SUS304J3-WSB · 1 source record · Original-source verification pending
- SUS304L · 2 source records
- SUS304L-WSA · 1 source record · Original-source verification pending
- SUS304L-WSB · 1 source record · Original-source verification pending
- SUS304N1 · 1 source record
- SUS304N2 · 1 source record
- SUS304TKA · 1 source record · Original-source verification pending
- SUS304TKC · 1 source record · Original-source verification pending
- SUS305 · 3 source records
- SUS305-WSA · 1 source record · Original-source verification pending
- SUS305-WSB · 1 source record · Original-source verification pending
- SUS305J1 · 2 source records
- SUS305J1-WSA · 1 source record · Original-source verification pending
- SUS305J1-WSB · 1 source record · Original-source verification pending
- SUS309S · 3 source records
- SUS310S · 2 source records
- SUS312L · 1 source record
- SUS315J1 · 1 source record
- SUS315J2 · 1 source record
- SUS316 · 2 source records
- SUS316-WSA · 1 source record · Original-source verification pending
- SUS316-WSB · 1 source record · Original-source verification pending
- SUS316F · 2 source records
- SUS316J1L · 1 source record
- SUS316L · 2 source records
- SUS316L-WSA · 1 source record · Original-source verification pending
- SUS316L-WSB · 1 source record · Original-source verification pending
- SUS316N · 1 source record
- SUS316TKA · 1 source record · Original-source verification pending
- SUS316TKC · 1 source record · Original-source verification pending
- SUS317 · 3 source records
- SUS317J1 · 1 source record
- SUS317J2 · 1 source record
- SUS317L · 1 source record
- SUS317LN · 1 source record
- SUS321 · 1 source record
- SUS321TKA · 1 source record · Original-source verification pending
- SUS323L · 1 source record
- SUS327L1 · 1 source record
- SUS347 · 1 source record
- SUS347TKA · 1 source record · Original-source verification pending
- SUS384 · 2 source records
- SUS384-WSA · 1 source record · Original-source verification pending
- SUS384-WSB · 1 source record · Original-source verification pending
- SUS403 · 3 source records
- SUS403-WSB · 1 source record · Original-source verification pending
- SUS405 · 1 source record · Original-source verification pending
- SUS410 · 2 source records
- SUS410-WSB · 1 source record · Original-source verification pending
- SUS410F2 · 2 source records
- SUS410TKA · 1 source record · Original-source verification pending
- SUS410TKC · 1 source record · Original-source verification pending
- SUS416 · 2 source records
- SUS420F · 2 source records
- SUS420F2 · 2 source records
- SUS420J1 · 3 source records
- SUS420J2 · 3 source records
- SUS420J2-CSP-O · 1 source record
- SUS429 · 1 source record
- SUS430 · 2 source records
- SUS430-WSB · 1 source record · Original-source verification pending
- SUS430F · 2 source records
- SUS430J1L · 1 source record
- SUS430TKA · 1 source record · Original-source verification pending
- SUS430TKC · 1 source record · Original-source verification pending
- SUS431 · 2 source records
- SUS434 · 3 source records
- SUS434-WSB · 1 source record · Original-source verification pending
- SUS436J1L · 1 source record
- SUS436L · 1 source record
- SUS440A · 1 source record
- SUS440C · 2 source records
- SUS443J1 · 1 source record
- SUS444 · 1 source record
- SUS445J1 · 1 source record
- SUS445J2 · 1 source record
- SUS447J1 · 1 source record
- SUS631-CSP-1/2H · 1 source record
- SUS631-CSP-3/4H · 1 source record
- SUS631-CSP-H · 1 source record
- SUS631-CSP-O · 1 source record
- SUS631J1 · 2 source records
- SUS632J1-CSP-1/2H · 1 source record
- SUS632J1-CSP-3/4H · 1 source record
- SUS821L1 · 1 source record
- SUSXM15J1 · 2 source records
- SUSXM7 · 3 source records
- SUSXM7-WSA · 1 source record · Original-source verification pending
- SUSXM7-WSB · 1 source record · Original-source verification pending
- SWCH10A · 2 source records
- SWCH10K · 2 source records
- SWCH10R · 2 source records
- SWCH12A · 2 source records
- SWCH12K · 2 source records
- SWCH12R · 2 source records
- SWCH15A · 2 source records
- SWCH15K · 2 source records
- SWCH15R · 2 source records
- SWCH16A · 2 source records
- SWCH16K · 2 source records
- SWCH17K · 2 source records
- SWCH17R · 2 source records
- SWCH18A · 2 source records
- SWCH18K · 2 source records
- SWCH19A · 2 source records
- SWCH20A · 2 source records
- SWCH20K · 2 source records
- SWCH22A · 2 source records
- SWCH22K · 2 source records
- SWCH24K · 2 source records
- SWCH25A · 2 source records
- SWCH25K · 2 source records
- SWCH27K · 2 source records
- SWCH30K · 2 source records
- SWCH33K · 2 source records
- SWCH35K · 2 source records
- SWCH38K · 2 source records
- SWCH40K · 2 source records
- SWCH41K · 2 source records
- SWCH43K · 2 source records
- SWCH45K · 2 source records
- SWCH48K · 2 source records
- SWCH50K · 2 source records
- SWCH6A · 2 source records
- SWCH6R · 2 source records
- SWCH8A · 2 source records
- SWCH8R · 2 source records
- SWCHB223 · 2 source records
- SWCHB237 · 2 source records
- SWCHB320 · 2 source records
- SWCHB323 · 2 source records
- SWCHB331 · 2 source records
- SWCHB334 · 2 source records
- SWCHB420 · 2 source records
- SWCHB526 · 2 source records
- SWCHB620 · 2 source records
- SWCHB623 · 2 source records
- SWCHB726 · 2 source records
- SWCHB734 · 2 source records
- SWG-2311 · 1 source record · Original-source verification pending
- SWG-2344 · 1 source record · Original-source verification pending
- SWRCH10A · 9 source records
- SWRCH10A-1 · 1 source record
- SWRCH10A-D · 3 source records
- SWRCH10K · 9 source records
- SWRCH10K-D · 3 source records
- SWRCH10R · 4 source records
- SWRCH12A · 9 source records
- SWRCH12A-1 · 1 source record
- SWRCH12A-D · 3 source records
- SWRCH12K · 7 source records
- SWRCH12R · 4 source records
- SWRCH15A · 9 source records
- SWRCH15A-1 · 1 source record
- SWRCH15A-D · 3 source records
- SWRCH15K · 8 source records
- SWRCH15K-D · 3 source records
- SWRCH15R · 4 source records
- SWRCH16A · 8 source records
- SWRCH16A-1 · 1 source record
- SWRCH16K · 7 source records
- SWRCH17K · 9 source records
- SWRCH17R · 4 source records
- SWRCH18A · 9 source records
- SWRCH18A-1 · 1 source record
- SWRCH18A-2 · 1 source record
- SWRCH18A-3 · 1 source record
- SWRCH18A-D · 3 source records
- SWRCH18AB-D · 3 source records
- SWRCH18K · 7 source records
- SWRCH19A · 8 source records
- SWRCH20A · 8 source records
- SWRCH20K · 8 source records
- SWRCH20K-1 · 1 source record
- SWRCH22A · 10 source records
- SWRCH22A-1 · 1 source record
- SWRCH22A-B · 1 source record
- SWRCH22A-D · 3 source records
- SWRCH22AB-D · 3 source records
- SWRCH22K · 8 source records
- SWRCH24K · 6 source records
- SWRCH25A · 6 source records
- SWRCH25K · 8 source records
- SWRCH25K-D · 3 source records
- SWRCH27K · 6 source records
- SWRCH30K · 7 source records
- SWRCH33K · 6 source records
- SWRCH35K · 8 source records
- SWRCH35K-1 · 1 source record
- SWRCH35K-B · 1 source record
- SWRCH35K-D · 3 source records
- SWRCH38K · 7 source records
- SWRCH38K-D · 3 source records
- SWRCH40K · 7 source records
- SWRCH40K-1 · 1 source record
- SWRCH41K · 6 source records
- SWRCH43K · 6 source records
- SWRCH45K · 9 source records
- SWRCH45K-1 · 1 source record
- SWRCH45K-D · 3 source records
- SWRCH48K · 6 source records
- SWRCH50K · 7 source records
- SWRCH50K-1 · 1 source record
- SWRCH6A · 9 source records
- SWRCH6A-1 · 1 source record
- SWRCH6A-D · 3 source records
- SWRCH6A-H · 1 source record
- SWRCH6R · 5 source records
- SWRCH8A · 9 source records
- SWRCH8A-1 · 1 source record
- SWRCH8A-D · 3 source records
- SWRCH8R · 4 source records
- SWRCHB220 · 2 source records
- SWRCHB223 · 2 source records
- SWRCHB226 · 2 source records
- SWRCHB231 · 2 source records
- SWRCHB234 · 2 source records
- SWRCHB237 · 2 source records
- SWRCHB320 · 2 source records
- SWRCHB323 · 2 source records
- SWRCHB331 · 2 source records
- SWRCHB334 · 2 source records
- SWRCHB420 · 2 source records
- SWRCHB423 · 2 source records
- SWRCHB437 · 2 source records
- SWRCHB526 · 2 source records
- SWRCHB531 · 2 source records
- SWRCHB620 · 2 source records
- SWRCHB623 · 2 source records
- SWRCHB634 · 2 source records
- SWRCHB637 · 2 source records
- SWRCHB726 · 2 source records
- SWRCHB731 · 2 source records
- SWRCHB734 · 2 source records
- SWRCHB737 · 2 source records
- SWRCHB823 · 2 source records
- SWRH27 · 6 source records
- SWRH32 · 5 source records
- SWRH37 · 6 source records
- SWRH42A · 6 source records
- SWRH42B · 6 source records
- SWRH47A · 6 source records
- SWRH47B · 6 source records
- SWRH52A · 6 source records
- SWRH52B · 6 source records
- SWRH57A · 6 source records
- SWRH57B · 6 source records
- SWRH62A · 6 source records
- SWRH62B · 6 source records
- SWRH67A · 6 source records
- SWRH67B · 6 source records
- SWRH72A · 6 source records
- SWRH72B · 6 source records
- SWRH77A · 6 source records
- SWRH77B · 6 source records
- SWRH82A · 6 source records
- SWRH82B · 6 source records
- SWRM10 · 6 source records
- SWRM10K · 1 source record
- SWRM12 · 6 source records
- SWRM12K · 1 source record
- SWRM15 · 6 source records
- SWRM15K · 1 source record
- SWRM17 · 6 source records
- SWRM17K · 1 source record
- SWRM17M · 1 source record
- SWRM2 · 1 source record
- SWRM20 · 6 source records
- SWRM20K · 1 source record
- SWRM20M · 1 source record
- SWRM22 · 6 source records
- SWRM22K · 1 source record
- SWRM2K · 1 source record
- SWRM4 · 1 source record
- SWRM4K · 1 source record
- SWRM6 · 6 source records
- SWRM6K · 1 source record
- SWRM8 · 6 source records
- SWRM8K · 1 source record
- SWRS62A · 2 source records
- SWRS62B · 2 source records
- SWRS67A · 2 source records
- SWRS67B · 2 source records
- SWRS72A · 2 source records
- SWRS72B · 2 source records
- SWRS75A · 1 source record
- SWRS75B · 1 source record
- SWRS77A · 2 source records
- SWRS77B · 2 source records
- SWRS80A · 1 source record
- SWRS80B · 2 source records
- SWRS82A · 2 source records
- SWRS82B · 2 source records
- SWRS87A · 1 source record
- SWRS87B · 1 source record
- SWRS92A · 2 source records
- SWRS92B · 1 source record
- SWRY11 · 3 source records
- SWRY11L · 1 source record
- SWRY21 · 2 source records
- T1 · 2 source records
- T10 · 1 source record
- T11 · 1 source record
- T12 · 1 source record
- T13 · 1 source record
- T2 · 2 source records
- T3 · 2 source records
- T7 · 1 source record
- T8 · 1 source record
- T8MN · 1 source record
- T9 · 1 source record
- T91 · 1 source record
- TA15 · 2 source records · Original-source verification pending
- TA23 · 1 source record · Original-source verification pending
- TA24 · 1 source record · Original-source verification pending
- TA2 (titanium) · 4 source records · Original-source verification pending
- TA2 (tantalum) · 7 source records · Original-source verification pending
- TA5 · 2 source records · Original-source verification pending
- TA7ELI · 1 source record · Original-source verification pending
- TA9-1 · 2 source records · Original-source verification pending
- TAG0.1 · 2 source records
- TAG0.1-0.01 · 1 source record
- TAG0.15 · 1 source record
- TB3 · 3 source records · Original-source verification pending
- TB6 · 2 source records · Original-source verification pending
- TBE0.3-1.5 · 1 source record
- TBE0.4-1.8 · 1 source record
- TBE0.6-2.5 · 1 source record
- TBE1.7 · 1 source record
- TBE1.9 · 1 source record
- TBE1.9-0.1 · 1 source record
- TBE1.9-0.4 · 1 source record
- TBE2 · 1 source record
- TC10 · 1 source record · Original-source verification pending
- TC15 · 1 source record · Original-source verification pending
- TC20 · 1 source record · Original-source verification pending
- TC4 · 6 source records · Original-source verification pending
- TCD1 · 1 source record
- TCR0.3-0.3 · 1 source record
- TCR0.5 · 1 source record
- TCR0.5-0.1 · 1 source record
- TCR0.5-0.2-0.1 · 1 source record
- TCR0.6-0.4-0.05 · 1 source record
- TCR0.7 · 1 source record
- TCR0.8 · 1 source record
- TCR1 · 1 source record
- TCR1-0.15 · 3 source records
- TCR1-0.18 · 1 source record
- TFE0.1 · 1 source record
- TFE1.0 · 1 source record
- TFE2.5 · 1 source record
- TI-6AL-4V · 3 source records · Original-source verification pending
- TI2 · 3 source records · Original-source verification pending
- TIAL6V4 · 4 source records · Original-source verification pending
- TITANIUM GR. 1 · 1 source record
- TITANIUM GR. 2 · 1 source record
- TITANIUM GRADE 5 · 2 source records
- TMG0.2 · 1 source record
- TMG0.4 · 1 source record
- TMG0.5 · 1 source record
- TMG0.8 · 1 source record
- TNI2.4-0.6-0.5 · 1 source record
- TP 304 · 5 source records · Original-source verification pending
- TP 304H · 1 source record · Original-source verification pending
- TP 304L · 4 source records · Original-source verification pending
- TP 304LN · 3 source records · Original-source verification pending
- TP 304N · 3 source records · Original-source verification pending
- TP 309S · 1 source record · Original-source verification pending
- TP 310S · 1 source record · Original-source verification pending
- TP 316 · 6 source records · Original-source verification pending
- TP 316L · 4 source records · Original-source verification pending
- TP 316LN · 3 source records · Original-source verification pending
- TP 321 · 3 source records · Original-source verification pending
- TP 347 · 3 source records · Original-source verification pending
- TP 347H · 1 source record · Original-source verification pending
- TP1 · 2 source records
- TP2 · 2 source records
- TP201 · 1 source record
- TP201LN · 1 source record
- TP3 · 1 source record
- TP304 · 7 source records
- TP304H · 3 source records
- TP304L · 3 source records
- TP304LN · 3 source records
- TP304N · 4 source records
- TP309CB · 1 source record
- TP309S · 2 source records
- TP310CB · 1 source record
- TP310H · 1 source record · Original-source verification pending
- TP310S · 2 source records
- TP316 · 4 source records
- TP316H · 1 source record
- TP316L · 3 source records
- TP316LN · 4 source records
- TP316N · 1 source record
- TP317 · 1 source record
- TP317L · 2 source records
- TP321 · 7 source records
- TP321H · 1 source record
- TP347 · 4 source records
- TP347H · 3 source records
- TP348 · 1 source record
- TP348H · 1 source record
- TP4 · 1 source record
- TP405 · 1 source record · Original-source verification pending
- TP409 · 1 source record · Original-source verification pending
- TP410 · 1 source record · Original-source verification pending
- TP430 · 2 source records · Original-source verification pending
- TP439 · 1 source record · Original-source verification pending
- TPB1 · 1 source record
- TPXM-10 · 1 source record
- TPXM-11 · 1 source record
- TPXM-15 · 1 source record
- TPXM-19 · 2 source records
- TPXM-29 · 1 source record
- TRIBALOY T-800 · 1 source record · Original-source verification pending
- TS 1 · 1 source record · Original-source verification pending
- TS 18 · 1 source record · Original-source verification pending
- TS 4 · 1 source record · Original-source verification pending
- TS 9 · 1 source record · Original-source verification pending
- TS0.4 · 1 source record
- TTE0.3 · 1 source record
- TTE0.5 · 1 source record
- TTE0.5-0.008 · 1 source record
- TTE0.5-0.02 · 1 source record
- TTI3.0-0.2 · 1 source record
- TU 10 CD9-10 · 1 source record · Original-source verification pending
- TU 15 CD2-05 · 1 source record · Original-source verification pending
- TU 37 C · 1 source record · Original-source verification pending
- TU 42 C · 1 source record · Original-source verification pending
- TU0 · 2 source records
- TU00 · 1 source record
- TU00AG0.06 · 1 source record
- TU1 · 2 source records
- TU2 · 2 source records
- TU3 · 1 source record
- TUAG0.03 · 1 source record
- TUAG0.05 · 1 source record
- TUAG0.1 · 1 source record
- TUAG0.2 · 1 source record
- TUAG0.3 · 1 source record
- TUAL0.12 · 1 source record
- TUAL0.25 · 1 source record · Original-source verification pending
- TUZR0.15 · 1 source record
- TYPE 304 · 4 source records · Original-source verification pending
- TYPE 304L · 2 source records · Original-source verification pending
- TYPE 309S · 2 source records · Original-source verification pending
- TYPE 310S · 2 source records · Original-source verification pending
- TYPE 316 · 4 source records · Original-source verification pending
- TYPE 316L · 2 source records · Original-source verification pending
- TYPE 316TI · 1 source record · Original-source verification pending
- TYPE 321 · 2 source records · Original-source verification pending
- TYPE 347 · 2 source records · Original-source verification pending
- TYPE 405 · 2 source records · Original-source verification pending
- TYPE 410 · 2 source records · Original-source verification pending
- TYPE 430 · 2 source records · Original-source verification pending
- TYPE 431 · 3 source records · Original-source verification pending
- TYPE 630 · 1 source record · Original-source verification pending
- TYPE 631 · 1 source record · Original-source verification pending
- TYPE 632 · 1 source record · Original-source verification pending
- TYPE 634 · 1 source record · Original-source verification pending
- TYPE 635 · 1 source record · Original-source verification pending
- TZR0.15 · 1 source record
- TZR0.2 · 1 source record
- TZR0.4 · 1 source record
- UHS1900 · 1 source record
- UHS1900M · 1 source record
- UHS1970 · 1 source record
- VDM ALLOY 33 · 2 source records · Original-source verification pending
- VDM ALLOY 602 CA · 1 source record · Original-source verification pending
- VDM NICKEL 201 · 1 source record · Original-source verification pending
- W10MO2CR4V5CO8 · 1 source record
- W10MO4CR4V3CO10 · 1 source record
- W12CR4V5CO5 · 1 source record
- W18CR4V · 1 source record
- W2MO8CR4V · 1 source record
- W2MO9CR4V2 · 3 source records
- W2MO9CR4VCO8 · 1 source record
- W3MO3CR4V2 · 1 source record
- W4MO3CR4VSI · 1 source record
- W6MO5CR4V2 · 1 source record
- W6MO5CR4V2AL · 5 source records
- W6MO5CR4V2CO2 · 1 source record
- W6MO5CR4V2CO5 · 1 source record
- W6MO5CR4V3 · 1 source record
- W6MO5CR4V3CO8 · 1 source record
- W6MO5CR4V4 · 1 source record
- W7MO4CR4V2CO5 · 2 source records · Original-source verification pending
- W7MO7CR4V7CO11 · 1 source record
- W9MO3CR4V · 1 source record
- WASPALOY · 2 source records
- WP1925N · 1 source record · Original-source verification pending
- WP20CB · 1 source record · Original-source verification pending
- WP304 · 1 source record · Original-source verification pending
- WP304H · 1 source record · Original-source verification pending
- WP304L · 1 source record · Original-source verification pending
- WP304LN · 1 source record · Original-source verification pending
- WP304N · 1 source record · Original-source verification pending
- WP310H · 1 source record · Original-source verification pending
- WP310S · 1 source record · Original-source verification pending
- WP316 · 1 source record · Original-source verification pending
- WP316L · 1 source record · Original-source verification pending
- WP316LN · 1 source record · Original-source verification pending
- WP317L · 1 source record · Original-source verification pending
- WP321 · 1 source record · Original-source verification pending
- WP347 · 1 source record · Original-source verification pending
- WP347H · 1 source record · Original-source verification pending
- WP6XN · 1 source record · Original-source verification pending
- WP904L · 1 source record · Original-source verification pending
- WPNIC10 · 1 source record · Original-source verification pending
- WPNIC11 · 1 source record · Original-source verification pending
- WPS31725 · 1 source record · Original-source verification pending
- WPS31726 · 1 source record · Original-source verification pending
- WPXM-19 · 1 source record · Original-source verification pending
- X 2 CRNIN 18 10 · 2 source records · Original-source verification pending
- X100CRMOV5 · 2 source records
- X105CRMO17 · 1 source record
- X108CRMO17 · 2 source records
- X10CR 13 · 3 source records · Original-source verification pending
- X10CRALSI13 · 2 source records
- X10CRALSI18 · 2 source records
- X10CRALSI25 · 2 source records
- X10CRALSI7 · 2 source records
- X10CRNI18-8 · 10 source records
- X10CRNIMOMNNBVB15-10-1 · 2 source records
- X10CRNIMOTI 18-10 · 1 source record · Original-source verification pending
- X10CRNINB 18-9 · 1 source record · Original-source verification pending
- X10CRNITI 18-9 · 1 source record · Original-source verification pending
- X10NICRAITI32-21 · 1 source record · Original-source verification pending
- X10NICRALTI 32-20 · 2 source records · Original-source verification pending
- X10NICRALTI 32-21 · 1 source record
- X10NICRALTI32-21 · 3 source records
- X10NICRSI35-19 · 2 source records
- X10NICRSINB35-22 · 2 source records
- X11CRMO5 · 1 source record · Original-source verification pending
- X11CRNIMNN19-8-6 · 1 source record
- X12CR13 · 13 source records
- X12CRCONI 21-20 · 2 source records · Original-source verification pending
- X12CRCONI21-22 · 1 source record · Original-source verification pending
- X12CRMNNIN17-7-5 · 1 source record
- X12CRMNNIN18-9-5 · 1 source record
- X12CRMO5 · 3 source records · Original-source verification pending
- X12CRNI 23-13 · 1 source record
- X12CRNI23-13 · 8 source records
- X12CRNI25-21 · 2 source records · Original-source verification pending
- X12CRNIMOV12-3 · 2 source records
- X12CRNIS 18-8 · 1 source record · Original-source verification pending
- X12CRNIS18-8 · 1 source record · Original-source verification pending
- X12CRNITI18-9 · 1 source record · Original-source verification pending
- X12CRS13 · 1 source record
- X12NI5 · 2 source records
- X12NICRSI 35-16 · 1 source record
- X12NICRSI35-16 · 6 source records
- X12NICRSI36-16 · 1 source record · Original-source verification pending
- X14CRMOS17 · 1 source record
- X153CRMOV 12 · 1 source record · Original-source verification pending
- X153CRMOV12 · 2 source records
- X155CRMOV 12-1 · 2 source records · Original-source verification pending
- X15CR13 · 1 source record
- X15CRMO5-1 · 2 source records
- X15CRNISI 20-12 · 1 source record · Original-source verification pending
- X15CRNISI 25-20 · 1 source record · Original-source verification pending
- X15CRNISI20-12 · 15 source records
- X15CRNISI25-20 · 2 source records · Original-source verification pending
- X15CRNISI25-21 · 9 source records
- X15CRNISI25-4 · 2 source records
- X17CRNI16-2 · 1 source record
- X18CRN28 · 2 source records
- X19CRMONBVN11-1 · 2 source records
- X1CRMO26-1 · 1 source record · Original-source verification pending
- X1CRNB15 · 1 source record
- X1CRNI25-21 · 1 source record
- X1CRNIMOALTI12-10-2 · 1 source record
- X1CRNIMOALTI12-9-2 · 1 source record
- X1CRNIMOCU12-5-2 · 1 source record
- X1CRNIMOCU12-7-3 · 1 source record
- X1CRNIMOCUN 20-18-7 · 5 source records · Original-source verification pending
- X1CRNIMOCUN20-18-7 · 14 source records
- X1CRNIMOCUN24-22-8 · 1 source record
- X1CRNIMOCUN25-25-5 · 1 source record
- X1CRNIMOCUNW24-22-6 · 1 source record
- X1CRNIMON25-22-2 · 1 source record
- X1CRNISI18-15-4 · 1 source record
- X1NICRMOCU 25-20-5 · 3 source records · Original-source verification pending
- X1NICRMOCU25- 20-5 · 1 source record
- X1NICRMOCU25-20-5 · 21 source records
- X1NICRMOCU31-27-4 · 1 source record
- X1NICRMOCUN 25-20-7 · 2 source records · Original-source verification pending
- X1NICRMOCUN25-20-7 · 15 source records
- X1NIMOCUN 25-20-7 · 1 source record · Original-source verification pending
- X20CR 13 · 4 source records · Original-source verification pending
- X20CR13 · 13 source records
- X20CRMOWV 12-1 · 2 source records · Original-source verification pending
- X20CRMOWV12-1 · 1 source record · Original-source verification pending
- X20NICRALMOV6-5-2-1 · 9 source records
- X210CR12 · 2 source records
- X210CRW12 · 2 source records
- X22CRMOV12-1 · 2 source records
- X25CRMNNIN25-9-7 · 2 source records
- X29CRS13 · 1 source record
- X2CRMNNIN17-7-5 · 1 source record
- X2CRMOTI17-1 · 1 source record
- X2CRMOTI18-2 · 1 source record
- X2CRMOTI29-4 · 1 source record
- X2CRMOTIS18-2 · 1 source record
- X2CRNBZR17 · 1 source record
- X2CRNI 12 · 3 source records · Original-source verification pending
- X2CRNI 18-9 · 2 source records
- X2CRNI 19 11 · 1 source record · Original-source verification pending
- X2CRNI12 · 15 source records
- X2CRNI18-9 · 17 source records
- X2CRNI19-11 · 13 source records
- X2CRNICU19-10 · 1 source record
- X2CRNICUN23-4 · 1 source record
- X2CRNIMNMON25-18-6-5 · 1 source record
- X2CRNIMO 17-12-2 · 2 source records
- X2CRNIMO 17-12-3 · 1 source record
- X2CRNIMO 18-10 · 1 source record · Original-source verification pending
- X2CRNIMO 18-12 · 1 source record · Original-source verification pending
- X2CRNIMO 18-14-3 · 3 source records · Original-source verification pending
- X2CRNIMO 18-15-4 · 4 source records · Original-source verification pending
- X2CRNIMO 18-16 · 1 source record · Original-source verification pending
- X2CRNIMO17-12-2 · 16 source records
- X2CRNIMO17-12-3 · 12 source records
- X2CRNIMO18-14-3 · 20 source records
- X2CRNIMO18-15-4 · 10 source records
- X2CRNIMOCON28-8-5-1 · 1 source record · Original-source verification pending
- X2CRNIMOCON28–8-5– 1 · 2 source records · Original-source verification pending
- X2CRNIMOCUN 25-6-3 · 2 source records
- X2CRNIMOCUN25-6-3 · 14 source records
- X2CRNIMOCUS17-10-2 · 1 source record
- X2CRNIMOCUWN 25-7-4 · 3 source records
- X2CRNIMOCUWN25-7-4 · 15 source records
- X2CRNIMON 17 13 3 · 1 source record · Original-source verification pending
- X2CRNIMON 17-11-2 · 4 source records · Original-source verification pending
- X2CRNIMON 17-13-3 · 2 source records
- X2CRNIMON 17-13-5 · 2 source records
- X2CRNIMON 18-12 · 1 source record · Original-source verification pending
- X2CRNIMON 18-13 · 1 source record · Original-source verification pending
- X2CRNIMON 25-7-4 · 3 source records
- X2CRNIMON 29-7-2 · 3 source records
- X2CRNIMON17-11-2 · 13 source records
- X2CRNIMON17-12-3 · 2 source records
- X2CRNIMON17-13-3 · 15 source records
- X2CRNIMON17-13-3E · 1 source record · Original-source verification pending
- X2CRNIMON17-13-5 · 18 source records
- X2CRNIMON18-12-4 · 1 source record
- X2CRNIMON22-5-3 · 15 source records
- X2CRNIMON25-7-4 · 19 source records
- X2CRNIMON29-7-2 · 5 source records
- X2CRNIMOSI18-5-3 · 1 source record
- X2CRNIMOSIMNN19-5-3-2-2 · 1 source record · Original-source verification pending
- X2CRNIMOV 13-5-2 · 2 source records · Original-source verification pending
- X2CRNIMOV13-5-2 · 4 source records
- X2CRNIN 18 10 · 1 source record · Original-source verification pending
- X2CRNIN 18-10 · 6 source records
- X2CRNIN 23-4 · 3 source records
- X2CRNIN18-10 · 18 source records
- X2CRNIN18-7 · 1 source record
- X2CRNIN19-11 · 1 source record · Original-source verification pending
- X2CRNIN23-4 · 19 source records
- X2CRTI 12 · 1 source record
- X2CRTI 17 · 3 source records
- X2CRTI12 · 11 source records
- X2CRTI17 · 9 source records
- X2CRTINB 18 · 1 source record
- X2CRTINB18 · 17 source records
- X2NICRAITI32-20 · 1 source record · Original-source verification pending
- X2NICRALTI 32-20 · 2 source records
- X2NICRALTI32-20 · 2 source records
- X30CR13 · 1 source record
- X30WCRV9-3 · 2 source records
- X35CRWMOV5 · 2 source records
- X37CRMOV5-1 · 2 source records
- X38CRMO14 · 1 source record
- X38CRMO16 · 2 source records
- X38CRMOV5-3 · 2 source records
- X39CR13 · 1 source record
- X39CRMO17-1 · 1 source record
- X3CRALTI18-2 · 2 source records
- X3CRNB 17 · 2 source records · Original-source verification pending
- X3CRNB17 · 8 source records
- X3CRNICU18-9-4 · 9 source records
- X3CRNICU19-9-2 · 7 source records
- X3CRNICUMO17-11-3-2 · 7 source records
- X3CRNIMO 13-4 · 1 source record · Original-source verification pending
- X3CRNIMO 17-13-3 · 1 source record
- X3CRNIMO13-4 · 15 source records
- X3CRNIMO17-12-3 · 6 source records
- X3CRNIMO17-13-3 · 11 source records
- X3CRNIMO18-12-3 · 1 source record
- X3CRNIMOBN17-13-3 · 2 source records
- X3CRNIMON27-5-2 · 1 source record
- X3CRTI17 · 17 source records
- X3NICR18-16 · 2 source records
- X40CR 13 · 1 source record · Original-source verification pending
- X40CR13 · 2 source records · Original-source verification pending
- X40CR14 · 2 source records
- X40CRMOV5-1 · 2 source records
- X40CRMOVN16-2 · 3 source records
- X45CR13 · 1 source record · Original-source verification pending
- X46CR 13 · 2 source records · Original-source verification pending
- X46CR13 · 8 source records
- X46CRS13 · 1 source record
- X47CR14 · 3 source records
- X4CRNI18-12 · 7 source records
- X4CRNIMO16-5-1 · 1 source record
- X4NICRCUMO35-20-4-3 · 1 source record · Original-source verification pending
- X50CRMOV15 · 1 source record
- X53CRMNNIN 21-9-4 · 2 source records · Original-source verification pending
- X53CRMNNIN21-9-4 · 1 source record · Original-source verification pending
- X55CRMO14 · 1 source record
- X5CRNI 18-10 · 1 source record
- X5CRNI 18-9 · 1 source record · Original-source verification pending
- X5CRNI17-7 · 1 source record
- X5CRNI18-10 · 19 source records
- X5CRNI18-9 · 3 source records · Original-source verification pending
- X5CRNICUNB 16-4 · 4 source records · Original-source verification pending
- X5CRNICUNB16-4 · 7 source records
- X5CRNIMO 17 12 2 · 1 source record · Original-source verification pending
- X5CRNIMO 17-12-2 · 2 source records
- X5CRNIMO 18-10 · 2 source records · Original-source verification pending
- X5CRNIMO 18-12 · 1 source record · Original-source verification pending
- X5CRNIMO17-12-2 · 19 source records
- X5CRNIMO17-12-2E · 1 source record · Original-source verification pending
- X5CRNIMO18-10 · 1 source record · Original-source verification pending
- X5CRNIMOCUNB14-5 · 1 source record
- X5CRNIMOTI15-2 · 1 source record
- X5CRNIN 19-9 · 3 source records
- X5CRNIN19-9 · 9 source records
- X5NICRTIMOVB25-15-2 · 1 source record
- X65CR14 · 2 source records
- X6CR 17 · 1 source record · Original-source verification pending
- X6CR13 · 11 source records
- X6CR17 · 13 source records
- X6CRAI13 · 2 source records · Original-source verification pending
- X6CRAL 13 · 1 source record · Original-source verification pending
- X6CRAL13 · 6 source records
- X6CRMO17-1 · 7 source records
- X6CRMO17-1E · 2 source records · Original-source verification pending
- X6CRMONB17-1 · 1 source record
- X6CRMOS17 · 1 source record
- X6CRNI 18-10 · 3 source records
- X6CRNI 25-20 · 4 source records
- X6CRNI17-1 · 1 source record
- X6CRNI18-10 · 9 source records
- X6CRNI18-12 · 2 source records
- X6CRNI23-14 · 1 source record · Original-source verification pending
- X6CRNI25-20 · 7 source records · Original-source verification pending
- X6CRNICU18-9-2 · 2 source records
- X6CRNICUS18-9-2 · 1 source record
- X6CRNIMOB17-12-2 · 2 source records
- X6CRNIMON17-12-3 · 1 source record · Original-source verification pending
- X6CRNIMONB17-12-2 · 1 source record
- X6CRNIMOTI 17 12 2 · 1 source record · Original-source verification pending
- X6CRNIMOTI 17-12-2 · 1 source record
- X6CRNIMOTI17-12-2 · 12 source records
- X6CRNIMOTI17-12-2E · 1 source record · Original-source verification pending
- X6CRNINB 18-10 · 5 source records · Original-source verification pending
- X6CRNINB18-10 · 18 source records
- X6CRNISINCE 19-10 · 1 source record
- X6CRNISINCE19-10 · 10 source records
- X6CRNITI 18 10 · 1 source record · Original-source verification pending
- X6CRNITI12 · 1 source record
- X6CRNITI18-10 · 13 source records
- X6CRNITI18-10E · 1 source record · Original-source verification pending
- X6CRNITIB 18-10 · 3 source records
- X6CRNITIB18-10 · 10 source records
- X6CRTI12 · 2 source records · Original-source verification pending
- X6NICRNBCE 32-27 · 1 source record
- X6NICRNBCE32-27 · 5 source records
- X6NICRSINCE 35-25 · 1 source record
- X6NICRSINCE35-25 · 10 source records
- X6NICRTIMOVB25-15-2 · 4 source records
- X70CRMO15 · 1 source record
- X75WCRV18-4-1 · 2 source records
- X7CR 13 · 1 source record · Original-source verification pending
- X7CRAL 13 · 1 source record · Original-source verification pending
- X7CRNI 23-14 · 1 source record · Original-source verification pending
- X7CRNIAI17-7 · 1 source record · Original-source verification pending
- X7CRNIAL 17-7 · 3 source records · Original-source verification pending
- X7CRNIAL17-7 · 9 source records
- X7CRNIMOBNB16-16 · 2 source records
- X7NICRALTI33-21 · 1 source record · Original-source verification pending
- X82WMOCRV6-5-4 · 2 source records
- X89CRMOV18-1 · 2 source records
- X8CR 17 · 1 source record · Original-source verification pending
- X8CRMNCUNB17-8-3 · 1 source record
- X8CRMNNIN18-9-5 · 1 source record
- X8CRNB 17 · 1 source record · Original-source verification pending
- X8CRNI25-21 · 11 source records
- X8CRNIMOAL 15-7-2 · 1 source record · Original-source verification pending
- X8CRNIMOAL15-7-2 · 3 source records · Original-source verification pending
- X8CRNIS 18-9 · 1 source record
- X8CRNIS18-9 · 7 source records
- X8CRNITI 18-10 · 1 source record
- X8CRNITI18-10 · 4 source records
- X8CRTI 17 · 1 source record · Original-source verification pending
- X8NI9 · 2 source records
- X8NICRAITI32-21 · 3 source records · Original-source verification pending
- X8NICRALTI 32-21 · 2 source records · Original-source verification pending
- X8NICRALTI32-21 · 6 source records · Original-source verification pending
- X8NICRALTI33-21 · 1 source record · Original-source verification pending
- X90CRMOV18 · 1 source record
- X9CRNI 18-9 · 1 source record
- X9CRNI18-9 · 6 source records
- X9CRNISINCE 21-11-2 · 1 source record
- X9CRNISINCE21-11-2 · 7 source records
- XG10B18 · 1 source record
- XG10B19 · 1 source record
- XG10B20 · 1 source record
- XG10B21 · 1 source record
- XG10B22 · 1 source record
- XG10B23 · 1 source record
- XG10B25 · 1 source record
- XG10B26 · 1 source record
- XG10B28 · 1 source record
- XG10B30 · 1 source record
- XG10B33 · 1 source record
- XG10B35 · 1 source record
- XG10B37 · 1 source record
- XG10B38 · 1 source record
- XG10B39 · 1 source record
- XG10B40 · 1 source record
- XG10B42 · 1 source record
- XGSWRCH10A · 1 source record
- XGSWRCH10AB · 1 source record
- XGSWRCH10K · 1 source record
- XGSWRCH10KB · 1 source record
- XGSWRCH12A · 1 source record
- XGSWRCH12AB · 1 source record
- XGSWRCH12K · 1 source record
- XGSWRCH12KB · 1 source record
- XGSWRCH15A · 1 source record
- XGSWRCH15AB · 1 source record
- XGSWRCH15K · 1 source record
- XGSWRCH15KB · 1 source record
- XGSWRCH16A · 1 source record
- XGSWRCH16AB · 1 source record
- XGSWRCH16K · 1 source record
- XGSWRCH16KB · 1 source record
- XGSWRCH17K · 1 source record
- XGSWRCH17KB · 1 source record
- XGSWRCH18A · 1 source record
- XGSWRCH18AB · 1 source record
- XGSWRCH18K · 1 source record
- XGSWRCH18KB · 1 source record
- XGSWRCH19A · 1 source record
- XGSWRCH19AB · 1 source record
- XGSWRCH20A · 1 source record
- XGSWRCH20AB · 1 source record
- XGSWRCH20K · 1 source record
- XGSWRCH20KB · 1 source record
- XGSWRCH22A · 1 source record
- XGSWRCH22AB · 1 source record
- XGSWRCH22K · 1 source record
- XGSWRCH22KB · 1 source record
- XGSWRCH24K · 1 source record
- XGSWRCH24KB · 1 source record
- XGSWRCH25K · 1 source record
- XGSWRCH25KB · 1 source record
- XGSWRCH27K · 1 source record
- XGSWRCH27KB · 1 source record
- XGSWRCH30K · 1 source record
- XGSWRCH30KB · 1 source record
- XGSWRCH33K · 1 source record
- XGSWRCH33KB · 1 source record
- XGSWRCH35K · 1 source record
- XGSWRCH35KB · 1 source record
- XGSWRCH38K · 1 source record
- XGSWRCH38KB · 1 source record
- XGSWRCH40K · 1 source record
- XGSWRCH40KB · 1 source record
- XGSWRCH41K · 1 source record
- XGSWRCH41KB · 1 source record
- XGSWRCH43K · 1 source record
- XGSWRCH43KB · 1 source record
- XGSWRCH45K · 1 source record
- XGSWRCH45KB · 1 source record
- XGSWRCH48K · 1 source record
- XGSWRCH48KB · 1 source record
- XGSWRCH50K · 1 source record
- XGSWRCH50KB · 1 source record
- XGSWRCH6A · 1 source record
- XGSWRCH6AB · 1 source record
- XGSWRCH8A · 1 source record
- XGSWRCH8AB · 1 source record
- XLH 01 · 1 source record · Original-source verification pending
- XM-16 · 1 source record
- XM-19 · 5 source records
- XM-27 · 2 source records · Original-source verification pending
- XM-28 · 1 source record
- Y08 · 1 source record
- Y08MNS · 1 source record
- Y08PB · 1 source record
- Y08SN · 1 source record
- Y108CR17 · 1 source record
- Y10CR17 · 1 source record
- Y12 · 1 source record
- Y12CR13 · 1 source record
- Y12CR18NI9 · 1 source record
- Y12CR18NI9SE · 1 source record
- Y12PB · 1 source record
- Y15 · 1 source record
- Y15MN · 1 source record
- Y15PB · 1 source record
- Y15SN · 1 source record
- Y20 · 1 source record
- Y25CR13NI2 · 4 source records
- Y2CR13NI2 · 1 source record · Original-source verification pending
- Y30 · 1 source record
- Y30CR13 · 1 source record
- Y35 · 1 source record
- Y35MN · 1 source record
- Y40MN · 2 source records
- Y45 · 1 source record
- Y45CA · 1 source record
- Y45MN · 1 source record
- Y45MNS · 1 source record
- Y45MNSN · 1 source record
- Y45MNSPB · 1 source record
- Y45SN · 1 source record
- YGW11 · 1 source record
- YGW12 · 1 source record
- YGW13 · 1 source record
- YGW14 · 1 source record
- YGW15 · 1 source record
- YGW16 · 1 source record
- YGW17 · 1 source record
- YGW18 · 1 source record
- YGW19 · 1 source record
- Z2CN18.10 · 1 source record
- Z2CND17.12 · 1 source record
- Z2CND18.12 · 1 source record
- ZA-27 · 1 source record · Original-source verification pending
- ZA-8 · 1 source record · Original-source verification pending
- ZCUAL10FE3 · 4 source records · Original-source verification pending
- ZG0CR17NI4CU4NB · 1 source record · Original-source verification pending
- ZG0CR18NI9TI · 1 source record · Original-source verification pending
- ZG30CR21NI10 · 1 source record · Original-source verification pending
- ZG30CR26NI20 · 1 source record · Original-source verification pending
- ZG35CR24NI8SI2N · 1 source record · Original-source verification pending
- ZG40CR23NI4N · 1 source record · Original-source verification pending
- ZG40CR25NI20SI2 · 1 source record · Original-source verification pending
- ZG40CR9SI3 · 1 source record · Original-source verification pending
- ZG8CR26NI4MN3NRE · 1 source record · Original-source verification pending
- ZGMN13-1 · 3 source records · Original-source verification pending
- ZGMN13-2 · 3 source records · Original-source verification pending
- ZGMN13-3 · 2 source records · Original-source verification pending
- ZGMN13-4 · 2 source records · Original-source verification pending
- ZHPBD65-2 · 2 source records · Original-source verification pending
- ZNAL4CU1 · 1 source record · Original-source verification pending
- ZT10B21 · 1 source record
- ZT10B30 · 1 source record
- ZT10B33 · 1 source record
- ZTML35CRMO · 1 source record
- ZTML40CR · 1 source record
- ZTML40CRMO · 1 source record
- ZTML42CRMO · 1 source record
- ZTSCM435 · 1 source record
- ZTSCM440 · 1 source record
- ZTSWRCH35K · 1 source record
- ZTSWRCH45K · 1 source record
- АД00 · 1 source record · Original-source verification pending
- Ц1 · 1 source record · Original-source verification pending
- C4D · 1 source records
- C7D · 1 source records
- C9D · 1 source records
- C10D · 1 source records
- C12D · 1 source records
- C15D · 1 source records
- C18D · 1 source records
- C20D · 1 source records
- C26D · 1 source records
- C32D · 1 source records
- C38D · 1 source records
- C42D · 1 source records
- C48D · 1 source records
- C50D · 1 source records
- C52D · 1 source records
- C56D · 1 source records
- C58D · 1 source records
- C60D · 1 source records
- C62D · 1 source records
- C66D · 1 source records
- C68D · 1 source records
- C70D · 1 source records
- C72D · 1 source records
- C76D · 1 source records
- C78D · 1 source records
- C80D · 1 source records
- C82D · 1 source records
- C86D · 1 source records
- C88D · 1 source records
- C92D · 1 source records
- C26DA · 1 source records
- C26DB · 1 source records
- C32DA · 1 source records
- C32DB · 1 source records
- C38DA · 1 source records
- C38DB · 1 source records
- C42DA · 1 source records
- C42DB · 1 source records
- C48DA · 1 source records
- C48DB · 1 source records
- C50DA · 1 source records
- C50DB · 1 source records
- C52DA · 1 source records
- C52DB · 1 source records
- C56DA · 1 source records
- C56DB · 1 source records
- C58DA · 1 source records
- C58DB · 1 source records
- C60DA · 1 source records
- C60DB · 1 source records
- C62DA · 1 source records
- C62DB · 1 source records
- C66DA · 1 source records
- C66DB · 1 source records
- C68DA · 1 source records
- C68DB · 1 source records
- C70DA · 1 source records
- C70DB · 1 source records
- C72DA · 1 source records
- C72DB · 1 source records
- C76DA · 1 source records
- C76DB · 1 source records
- C78DA · 1 source records
- C78DB · 1 source records
- C80DA · 1 source records
- C80DB · 1 source records
- C82DA · 1 source records
- C82DB · 1 source records
- C86DA · 1 source records
- C86DB · 1 source records
- C88DA · 1 source records
- C88DB · 1 source records
- C92DA · 1 source records
- C92DB · 1 source records
- T700 · 1 source records
- T800 · 1 source records
- T900 · 1 source records
- T1000 · 1 source records
- T1100 · 1 source records
- T1200 · 1 source records