60WCrV8 · ISO 4957-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 4957-2018
Table / clause
Table 4 · Notes a–g
PDF page references
15、16

Carbon-equivalent reference

IIW / CEV:0.7750–1.0050Known-element contribution; incomplete value; missing Mo, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.6358–0.7858Known-element contribution; incomplete value; missing Cu, Ni, Mo, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.6100–0.7550Known-element contribution; incomplete value; missing Mo, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.55 ~ 0.65
Si0.7 ~ 1
Mn0.15 ~ 0.45
Cr0.9 ~ 1.2
V0.1 ~ 0.2
W1.7 ~ 2.2
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Table 4 heat composition for cold-work alloy tool steels, wt%; Default P/S are each ≤.030%. ; Product-analysis tolerances in Table 5 must not be applied to the default heat-analysis range. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; dashes are not entered as zero. ; Cold-work tool steel does not establish suitability for cold-heading wire; the words “cold work” alone do not justify listing a product in the product centre.

Verification notes

Official English Table 4 and footnotes visually checked.

60WCrV8 · BS EN ISO 4957:2018

Chemical-composition source verified. Properties and delivery conditions follow the sources and conditions stated here; actual supply and measured heat results are not verified by this reference.

Material category
Tool steel
Product form
Tool-steel standard reference; product form subject to the order
Standard edition
BS EN ISO 4957:2018
Table / clause
Table 4 and notes a–g
Source file
BS EN ISO 4957-2018-Tool steel.docx
Units
Mass fraction (wt%)
Analysis type
Cast analysis

Composition

ElementComposition requirement
C0.55 ~ 0.65
Si0.7 ~ 1
Mn0.15 ~ 0.45
Cr0.9 ~ 1.2
V0.1 ~ 0.2
W1.7 ~ 2.2
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Cast analysis, mass fraction %. A dash means the standard gives no separate requirement; it does not mean zero. Unlisted elements shall not be intentionally added without purchaser consent, except additions needed to finish steelmaking. Permissible product-analysis deviations do not expand the default cast-analysis limits. Tool-steel classification and hardness depend on application, heat treatment and test conditions; they do not establish cold-heading suitability or guarantee properties in an arbitrary condition. Table 4: alloy cold-work tool steels; cast analysis, wt%; default P and S each ≤.030%. Product-analysis deviations in Table 5 must not be applied to the default cast-analysis limits. Unlisted elements shall not be intentionally added without purchaser consent, except to finish steelmaking. Dashes are not entered as zero. Annealed and cold-drawn (+A+C) hardness may be 20 HBW higher than annealed (+A) hardness. Hardness values for different conditions must not be interchanged.

Composition and ordering conditions

Mechanical properties and delivery condition

PropertyStandard requirements and applicable conditions
Annealed hardness HBW / maximum229
Hardening testAustenitizing 910±10 °C ; oil quenching ; tempering 180±10 °C ; hardness≥58 HRC

Mechanical-property provenance:BS EN ISO 4957:2018 · Table 4 and notes a–g · Standard tables embedded in the Word document supplied by the user

Verification notes

Checked against the standard text and table notes supplied by the user. Applicability to a specific order requires separate confirmation.

Linked products

View linked products for 60WCrV8 →

WhatsApp Technical enquiry →