X3NICR18-16
2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for X3NICR18-16 →Material demand assessment
Looking for X3NICR18-16 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
X3NiCr18-16 · ISO 4954
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Stainless steel
- Material form
- Cold-heading wire
- Original record status
- Reference transcription of standard
- Standard edition
- ISO 4954:2018
- Table / clause
- Table D.2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.04 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 15.0 ~ 17.0 |
| Ni | 17.0 ~ 19.0 |
Applicability and limitations
ISO 4954:2018; heat analysis, mass fraction %; values without a stated range are upper limits; see the source page for complete table footnotes. The website does not specify the edition; the source edition is shown here and does not establish contractual applicability.
Verification notes
Standard source: ISO 4954:2018 · Table D.2View associated products →X3NiCr18-16 · ISO 4954-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ISO 4954:2018
- Table / clause
- Table D.2
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Tabulated C≤0.04%
Note d: this standard permits C≤0.08%
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | ≤ 0.04 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 15.0 ~ 17.0 |
| Ni | 17.0 ~ 19.0 |
Applicability and limitations
ISO 4954:2018 Table D.2 gives cast analysis; single values are maxima and dashes are not zero.
Product-analysis deviations are listed separately under Tables 2/3, not used directly to relax cast-composition limits.
Elements not listed must not be intentionally added without the purchaser's consent, except for finishing the heat.
Original condition-branch records
Tabulated C≤0.04%
| Element | Composition requirement |
|---|---|
| C | ≤ 0.04 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 15.0 ~ 17.0 |
| Ni | 17.0 ~ 19.0 |
Note d: this standard permits C≤0.08%
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 15.0 ~ 17.0 |
| Ni | 17.0 ~ 19.0 |