T700 material reference
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for T700 →Material demand assessment
Looking for T700 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
T700 · GB/T 24242.2-2020
Chemical-composition source verified. Properties and delivery conditions follow the sources and conditions stated here; actual supply and measured heat results are not verified by this reference.
- Material category
- Carbon steels
- Product form
- Wire rod
- Standard edition
- GB/T 24242.2-2020
- Table / clause
- Table C.1, C.2
- Source file
- GB_T 24242.2-2020.pdf
- PDF page
- 10
- Units
- Mass fraction (wt%)
- Analysis type
- Cast analysis
Composition
| Element | Composition requirement |
|---|---|
| Si | 0.1 ~ 0.3 |
| Mn | 0.5 ~ 0.8 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
Applicability and limitations
Annex C designations are based on tensile strength. The supplier determines C, Cr, Ni, Cu, Mo and Al to meet strength requirements; the standard gives no numerical limits. Carbon content cannot be inferred from the grade designation. Take specimens from 5 different coils per batch; tensile strength shall meet Table C.1. Intermediate grades require agreement between supplier and purchaser. Cast analysis; composition is expressed as mass fraction, %. An unspecified lower limit is not zero. Delivery condition, dimensions, surface, packaging and acceptance shall follow GB/T 24242.1—2020 and the order.
Composition and ordering conditions
- Annex C designations are based on tensile strength. The supplier determines C, Cr, Ni, Cu, Mo and Al to meet strength requirements; the standard gives no numerical limits. Carbon content cannot be inferred from the grade designation.
- Take specimens from 5 different coils per batch; tensile strength shall meet Table C.1. Intermediate grades require agreement between supplier and purchaser.
- Cast analysis; composition is expressed as mass fraction, %. An unspecified lower limit is not zero.
- Delivery condition, dimensions, surface, packaging and acceptance shall follow GB/T 24242.1—2020 and the order.
Mechanical properties and delivery condition
| Property | Standard requirements and applicable conditions |
|---|---|
| Tensile strength Rm / MPa | 600~800 |
Mechanical-property provenance:GB/T 24242.2-2020 · Table C.1, C.2 · PDF page 10, Annex C
Verification notes
Checked against the standard text and table notes supplied by the user. Applicability to a specific order requires separate confirmation.
Related catalog and standard references
View standard reference information →
A reference link does not confirm supply or interchangeability. Specific requirements need technical confirmation.