008CR30MO2
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 008CR30MO2 →008Cr30Mo2 · GB /T 20878-2007
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Ferritic stainless and heat-resistant steels
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 20878—2007
- Table / clause
- Table 3, No. 95
- PDF page references
- 12
- Unit
- Mass fraction (wt%)
- Analysis type
- Standard composition requirements
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Mn | ≤ 0.4 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Cr | 28.5 ~ 32 |
| Mo | 1.5 ~ 2.5 |
| N | ≤ 0.015 (lower limit not stated) |
| Ni | ≤ 0.5 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Original GB/T 20878—2007 composition, mass fractions wt%; Values in parentheses are maximum permitted additions. Footnote b permits Ni ≤0.50 and Cu ≤0.20, with Ni+Cu ≤0.50 also required. This standard does not guarantee cold-heading suitability or actual supply. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.
Combined limits
- Combined-element limits
- Element coefficient
- Ni
- 1
- Cu
- 1
- Requirement
- Ni+Cu≤0.50
- Upper limit
- 0.5