← BackMaterial grade directory

06CR19NI10

24 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 06CR19NI10 →

06Cr19Ni10 · GB/T 1221-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Heat-resistant steels
Subcategory
Austenitic heat-resistant steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1221-2007
Table / clause
Table 4 · Notes; 7.1
PDF page references
6、7、8
Unit
Mass fraction (wt%)
Analysis type
Heat analysis, not product analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni8 ~ 11
Cr18 ~ 20

Applicability and limitations

GB/T1221—2007, Table 4, heat-analysis mass fractions wt%; The actual 2007 edition is retained separately. Standard for heat-resistant steel bars; A chemistry match does not guarantee supply of cold-heading wire, heat-treatment condition, mechanical properties or heat resistance. Under the table note, values other than explicit ranges and minima are maxima; A dash indicates unspecified content and is not entered as 0. 7.1.2 product chemical-analysis tolerances require separate verification under GB/T222 and do not directly widen heat-analysis limits. This record retains the heat-resistant-steel category in the original table; applicability of conventional welding carbon-equivalent formulas has not been independently verified, so no automatic calculation is provided.

Verification notes

The 2007 original images of Tables 4–7, footnotes and Clause 7.1 were checked; the melting analysis and scope for heat-resistant steel bars are retained.

06Cr19Ni10 · GB /T 20878-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless and heat-resistant steels
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 20878—2007
Table / clause
Table 1, No. 17
PDF page references
6
Unit
Mass fraction (wt%)
Analysis type
Standard composition requirements

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni8 ~ 11
Cr18 ~ 20

Applicability and limitations

Table 1 composition, mass fractions wt%; Parenthetical values are maximum permitted additions. This standard does not establish a guarantee of cold-heading suitability or actual supply. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.

Verification notes

GB/T 20878—2007 historical original, Table 1, entry 17. The complete 45-page scan was checked. The standard is withdrawn; the historical edition’s application limits are retained.

06Cr19Ni10 · GB /T 1220-2007

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 12770-2012

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 12771-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 14975-2012

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 14976-2012

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.035 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 20878-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 24511-2017

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 24588-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 3280-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Cr17.5 ~ 19.5
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 41157.3-2022

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr17 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 12
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 4237-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Cr17.5 ~ 19.5
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 4238-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Cr17.5 ~ 19.5
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 4240-2009

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 4240-2019

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 4356-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Cu≤ 1 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · GB /T 713.7-2023

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · JB /T 6908-2020

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · NB /T 20008.12-2010

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr17 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 12
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · YB /T 085-2007

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · YB /T 110-2011

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 10.5
P≤ 0.035 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · YB /T 5363-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Mn≤ 2 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

06Cr19Ni10 · Chinese national standard

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr18 ~ 20
Cu≤ 1 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
Mo≤ 0.6 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni8 ~ 11
P≤ 0.045 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →