440C
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for 440C →440C · ASTM A493-2009(2013)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ASTM A493-2009(2013)
- Table / clause
- Table 1 · Notes A–B
- PDF page references
- 1、2
Carbon-equivalent reference
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.95 ~ 1.2 |
| Mn | ≤ 1.0 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Cr | 16.0 ~ 18.0 |
| Mo | ≤ 0.75 (lower limit not stated) |
Applicability and limitations
Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1
note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.
Original condition-branch records
Default chemical requirements in Table 1
| Element | Composition requirement |
|---|---|
| C | 0.95 ~ 1.2 |
| Mn | ≤ 1.0 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Cr | 16.0 ~ 18.0 |
| Mo | ≤ 0.75 (lower limit not stated) |