← BackMaterial grade directory

T900 material reference

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for T900 →

Material demand assessment

Looking for T900 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

T900 · GB/T 24242.2-2020

Chemical-composition source verified. Properties and delivery conditions follow the sources and conditions stated here; actual supply and measured heat results are not verified by this reference.

Material category
Carbon steels
Product form
Wire rod
Standard edition
GB/T 24242.2-2020
Table / clause
Table C.1, C.2
Source file
GB_T 24242.2-2020.pdf
PDF page
10
Units
Mass fraction (wt%)
Analysis type
Cast analysis

Composition

ElementComposition requirement
Si0.1 ~ 0.3
Mn0.5 ~ 0.8
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Annex C designations are based on tensile strength. The supplier determines C, Cr, Ni, Cu, Mo and Al to meet strength requirements; the standard gives no numerical limits. Carbon content cannot be inferred from the grade designation. Take specimens from 5 different coils per batch; tensile strength shall meet Table C.1. Intermediate grades require agreement between supplier and purchaser. Cast analysis; composition is expressed as mass fraction, %. An unspecified lower limit is not zero. Delivery condition, dimensions, surface, packaging and acceptance shall follow GB/T 24242.1—2020 and the order.

Composition and ordering conditions

Mechanical properties and delivery condition

PropertyStandard requirements and applicable conditions
Tensile strength Rm / MPa800~1000

Mechanical-property provenance:GB/T 24242.2-2020 · Table C.1, C.2 · PDF page 10, Annex C

Verification notes

Checked against the standard text and table notes supplied by the user. Applicability to a specific order requires separate confirmation.