← BackMaterial grade directory

X1NICRMOCU25-20-5

21 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X1NICRMOCU25-20-5 →

Material demand assessment

Looking for X1NICRMOCU25-20-5 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X1NiCrMoCu25-20-5 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 4 and continuation; notes a–e; all 50 austenitic corrosion-resistant steel grades
PDF page references
1、3、11、12

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
N≤ 0.15 (lower limit not stated)
Cr19.0 ~ 21.0
Cu1.2 ~ 2.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0

Applicability and limitations

EN 10088-1:2005 Table 4 and continuation: ladle analysis (wt%); the official SIST adoption preview PDF, pages 11/12, covers all 50 grades and notes. Note a: unlisted elements are not intentionally added without purchaser consent, except as needed to complete steelmaking; a blank is not zero. Note b: for grades marked b only, S is selected separately for long products and by property requirement. Note d: the increased Ni maximum for special reasons applies only to listed grades, not all grades. Note c: Cu up to 1.0% for cold heading/extrusion; this condition path is provided here only for grades with blank Cu in the original table. Existing Cu alloy ranges retain their original values; the exception has not automatically rewritten them. The linked Ti≥5C/Nb≥10C and Ti≥8(C+N) conditions are retained; an unlisted N maximum is not zero. Note e: the source warns of skin-contact regulatory issues for high-sulfur free-machining steel; this is retained as a historical warning only and is not a claim of current compliance based on the 2005 text. Listed chemistry and the cold-heading Cu exception alone do not establish overall cold-heading performance or company supply; mechanical and product standards must be checked separately, and national adoption does not mean automatic equivalence.

Original condition-branch records

Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
N≤ 0.15 (lower limit not stated)
Cr19.0 ~ 21.0
Cu1.2 ~ 2.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0

Verification notes

Official source Table 4, all 50 rows and footnotes visually checked; conditional route for Cu cells left blank in the original.

X1NiCrMoCu25-20-5 · NF EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Composition basis in the adopted standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 4 and continuation; notes a–e; all 50 austenitic corrosion-resistant steel grades
PDF page references
1、3、11、12

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
N≤ 0.15 (lower limit not stated)
Cr19.0 ~ 21.0
Cu1.2 ~ 2.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0

Applicability and limitations

NF EN 10088-1:2005 adopts EN 10088-1:2005 (EN 10088-1-2005); See the data basis for the actual composition source file and table number. EN10088-1:2005 Table 4 and its continuation; heat analysis wt%; all 50 grades and footnotes on PDF pages 11/12 of the official SIST adoption preview.. ; Note a: Elements not listed shall not be intentionally added without the consent of the purchaser (except additions needed to finish steelmaking).; Blanks are not entered as zero. ; Note b: For grades marked b, S shall be selected separately according to long products and properties.; The increased Ni upper limit based on special reasons in Note d applies only to the listed steel grades and cannot be generalized to all grades.. ; Note c: For cold-heading/cold-extrusion applications, Cu max 1.0%.; This conditional path is provided only for grades where Cu was blank in the original table; existing Cu alloying ranges shall retain their original values, and their Cu exceptions have not been automatically rewritten.. ; The linkages Ti≥5C/Nb≥10C and Ti≥8(C+N) are retained.; If no N upper limit is listed, do not fill as zero.. ; Note e retains the original historical caution about skin-contact regulations for high-sulfur free-cutting steel; the 2005 text is not used to claim present-day compliance.. ; The listed compositions and the cold-heading Cu exception do not independently prove the overall cold-heading properties of the material or company supply.; Mechanical properties and product standards require separate verification; national adoption does not automatically establish equivalence..

Original condition-branch records

Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
N≤ 0.15 (lower limit not stated)
Cr19.0 ~ 21.0
Cu1.2 ~ 2.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0

Verification notes

The formal adoption relationship and corresponding EN composition original have been checked; the complete national adoption text has not been verified page by page.

X1NiCrMoCu25-20-5 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 4 and continuation; notes a–e; all 50 austenitic corrosion-resistant steel grades
PDF page references
1、3、11、12

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
N≤ 0.15 (lower limit not stated)
Cr19.0 ~ 21.0
Cu1.2 ~ 2.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0

Applicability and limitations

EN 10088-1:2005 Table 4 and continuation: ladle analysis (wt%); the official SIST adoption preview PDF, pages 11/12, covers all 50 grades and notes. Note a: unlisted elements are not intentionally added without purchaser consent, except as needed to complete steelmaking; a blank is not zero. Note b: for grades marked b only, S is selected separately for long products and by property requirement. Note d: the increased Ni maximum for special reasons applies only to listed grades, not all grades. Note c: Cu up to 1.0% for cold heading/extrusion; this condition path is provided here only for grades with blank Cu in the original table. Existing Cu alloy ranges retain their original values; the exception has not automatically rewritten them. The linked Ti≥5C/Nb≥10C and Ti≥8(C+N) conditions are retained; an unlisted N maximum is not zero. Note e: the source warns of skin-contact regulatory issues for high-sulfur free-machining steel; this is retained as a historical warning only and is not a claim of current compliance based on the 2005 text. Listed chemistry and the cold-heading Cu exception alone do not establish overall cold-heading performance or company supply; mechanical and product standards must be checked separately, and national adoption does not mean automatic equivalence.

Original condition-branch records

Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
N≤ 0.15 (lower limit not stated)
Cr19.0 ~ 21.0
Cu1.2 ~ 2.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0

Verification notes

Official source Table 4, all 50 rows and footnotes visually checked; conditional route for Cu cells left blank in the original.

X1NiCrMoCu25-20-5 · EN 10270-3-2011

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless spring steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10270-3-2011
Table / clause
Table1, note a–e; 1.1–1.3; 4.4.1–4.4.2
PDF page references
6、7、8

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Cr19.0 ~ 21.0
Mo4.0 ~ 5.0
Ni24.0 ~ 26.0
N≤ 0.15 (lower limit not stated)
Cu1.2 ~ 2.0

Applicability and limitations

EN 10270-3:2011 Table 1 heat analysis, mass fraction wt%; The source is an official public SIST excerpt of 11 pages; all 6 rows of Table 1 and notes a–e are included in full.. The scope is stainless spring steel wire with a circular cross-section diameter ≤10mm, usually delivered in the cold-drawn condition.; Mechanical requirements must be agreed upon for 10–15mm and other steel types not listed separately in Table 1; cold-heading product applicability shall not be automatically confirmed based on this. Table 1 Note a allows other compositions to be agreed upon; the ranges listed in the table shall not be altered without such agreement.; Clause 4.4.2: Apply product-analysis tolerances separately under EN10088-3; for the same element in the same heat, deviations must not occur both above the upper limit and below the lower limit.. Note c allows the use of 1.4436 to improve corrosion resistance, subject to the provisions of this standard for 1.4401.; The chemical composition of 1.4436 is not listed separately in this table and shall not be duplicated as the same composition. Note d allows the Ni upper limit to be increased to 8.30% only when improving the cold forming performance of X7CrNiAl17-7, which is listed as a separate condition.; Unlisted elements are not entered as zero. Chemical clauses and footnotes have been verified; it is not declared that all mechanical properties, dimensional tolerances, tests, and annex contents have been verified..

Verification notes

All 6 rows in the officially published original SIST, Table 1, note a–e, scope and Clause 4.4 were visually checked; this is not verification of the complete DIN text

X1NiCrMoCu25-20-5 · DIN EN 10088-3-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · DIN EN 10296-2-2006

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10028-7-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10088-2-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10088-2-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10088-3-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10253-4-2003

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10272-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · EN 10296-2-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · NF EN 10028-7-2000

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · NF EN 10028-7-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · NF EN 10088-2-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · NF EN 10296-2-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · ISO 15510-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 22
Cu1 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni23.5 ~ 26
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · ISO 683-18

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 22
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni23.5 ~ 26
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · ISO 9328-7-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 21
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni24 ~ 26
P≤ 0.03 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X1NiCrMoCu25-20-5 · ISO TS 15510-2003

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Cr19 ~ 22
Cu1.2 ~ 2
Mn≤ 2 (lower limit not stated)
Mo4 ~ 5
N≤ 0.15 (lower limit not stated)
Ni23.5 ~ 26
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.