← BackMaterial grade directory

1213

6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 1213 →

1213 · SAE J 403-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J403 NOV2001
Table / clause
Table3B and footnotes
PDF page references
1、4、5

Carbon-equivalent reference

IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1
P0.07 ~ 0.12
S0.24 ~ 0.33

Applicability and limitations

Table 3B SAE1213 corresponds to UNS G12130; Heat analysis wt%. ; Resulfurized

rephosphorized free-cutting steels; Machining performance characteristics do not prove suitability for cold heading forming, and cold heading products are not automatically added. ; The addition of Pb requires L identification and corresponding UNS; This record includes only the explicitly tabulated Pb .15–.35% for 12L14; do not merge this Pb addition into the data for other ordinary grades. ; Elements required to be reported do not equal uniform limits; Unspecified elements are not entered as zero; Product-analysis deviation under J409 requires separate verification. ; The 12xx series typically does not specify Si to avoid adverse effects on machinability; P/S is a bilateral range rather than only an upper limit.

Verification notes

All composition values and footnotes in PDF5, Table 3A/3B were visually checked

1213 · ASTM A29/A29M-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A29/A29M-2012
Table / clause
Table 1, footnotes A–G
PDF page references
1、3、4

Carbon-equivalent reference

IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33

Applicability and limitations

2012 original text Table 1 heat analysis mass fraction wt%; The applicability and deviations of product analysis must be separately confirmed according to 4.3 and Table 5. Grades and product forms are retained as listed in this standard; suitability for cold heading is not automatically guaranteed. Note D only specifies Pb 0.15–0.35% for lead-bearing 'L' grades; Standard grades without 'L' shall not automatically include Pb. Note F: Additions of Bi/Ca/Se/Te are subject to agreement between the supplier and purchaser; do not enter zero when no value is specified..

Verification notes

The 2012 Table 1 and footnotes have been checked; order-specific optional compositions and base-table limits remain separate.

1213 · POSCO wire rod catalogue (local archive 1203; original edition not stated)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Free-cutting steel
Subcategory
Free-cutting steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Local file 1203 (wire-rod pdf); the original does not state a publication edition; PDF metadata 2014-12-03 is only the file generation time
Document title
Wire rod
Table / clause
Printed page 19, composition table 4 (local table index)
PDF page references
10
Unit
Percentages as stated in the original table; refer to the source for the specific basis
Analysis type
The catalog does not consistently specify heat or product analysis
Manufacturer
POSCO

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.16 ~ 0.23

Applicability and limitations

Locally held POSCO wire rod catalogue, PDF page 10

printed page 19, table index 3, row 14. The original edition number is not stated. The PDF creation date 2014-12-03 is not a standard publication year. Manufacturer range data do not constitute our company’s supply guarantee.

Composition conditions

Verification notes

The original PDF tables and text coordinates were reconciled in both directions. Missing grade cells were restored; merged cells, footers and remarks were checked separately. Tables with identified disputes and rows without composition data are withheld.

1213 · Nippon Steel Wire Rods EXE203 2008.3 / SAE J403 NOV.2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Free-cutting steel
Subcategory
Free-cutting steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Cat. No. EXE203 2008.3 PDF; cover copyright 2008
Document title
Nippon Steel Wire Rods
Table / clause
Printed page 11, table index 3
PDF page references
7
Unit
Mass fraction (%)
Analysis type
The original catalogue does not explicitly identify the analysis type for this table
Manufacturer
NIPPON STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33

Applicability and limitations

Historical Nippon Steel wire-rod catalogue EXE203 2008.3, PDF page 7

printed page 11, SAE J403 NOV.2001. The original catalogue does not explicitly identify the analysis type for this table. Manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: the original note for the 12xx series generally does not specify Si; missing data remain missing. ; Pb 0.15–0.35 and B 0.0005–0.0030 are options requiring an additional L/B designation and are not automatically included in ordinary grades in the original table; Special-quality low P/S requires separate verification of the agreement.

Composition conditions

Verification notes

Grouped tables were expanded in full and checked against original images and notes. Ordinary, residual and conditional elements are kept separate; suffix tables lacking complete base-steel composition are excluded.

1213 · ASTM A29/A29M-2023

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A29/A29M-2023
Table / clause
Table 1, footnotes A–G
PDF page references
5
Unit
Mass fraction (wt%)
Analysis type
Heat analysis (composition ranges and limits in the original table)

Carbon-equivalent reference

IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33

Applicability and limitations

Original ASTM A29/A29M-2023, Table 1: the basic table gives heat-analysis mass fractions wt%; Product-analysis tolerances require separate confirmation under 4.3 and Table 5 and are not added to heat-analysis limits. When 4.1.1 is ordered by a grade in this table, the corresponding heat-analysis limits must be met; Other ordered compositions require separate agreement under 4.1.2 and Table 3/4 and are not merged into this table. General requirements for hot-worked bars; chemistry alone does not establish cold-heading suitability, supply or mechanical properties. Note D: Pb for leaded steel is 0.15–0.35%; L must remain part of the grade identity and is not included in ordinary grades; If lead is added in the ladle stream, its cast or heat-analysis content cannot be determined. Note F: Bi/Ca/Se/Te is specified by purchaser-supplier agreement; Unspecified numerical values are not entered as zero. The 4.3.2 product-analysis tolerance restrictions for P and S do not apply to resulfurized or rephosphorized/resulfurized steels; Product-analysis tolerances are not added to heat-analysis limits.

Verification notes

Existing OCR of the four-page, 190-row original 2023 table was parsed cell by cell. All values were screened for differences against independent 2012 data and checked against the original 2023 images and footnotes; no values were filled from the older edition.

1213 · SAE J403-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Free-cutting carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J403-2014
Table / clause
Table 3B
PDF page references
7
Unit
Mass fraction (wt%)
Analysis type
Cast or heat analysis

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Semi-finished forgings / bars / wire rod / seamless tube; Residual B (default unless separately agreed)
IIW / CEV:0.1167–0.3887Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.2157Known-element contribution; incomplete value; missing Si, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2697 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Semi-finished forgings / bars / wire rod / seamless tube; Residual A
IIW / CEV:0.1167–0.3653Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.2048Known-element contribution; incomplete value; missing Si, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2585 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Semi-finished forgings / bars / wire rod / seamless tube; Residual C
IIW / CEV:0.1167–0.4340Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.2297Known-element contribution; incomplete value; missing Si, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2870 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Semi-finished forgings / bars / wire rod / seamless tube; Residual D (no limit, but reporting is required)
IIW / CEV:0.1167–0.2967 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0350–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0700–0.2300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Applicability and limitations

SAE J403 Revised JUN2014 Table 3B: original cast or heat analysis, mass fraction wt%. Product-analysis deviations are addressed separately under SAE J409; J409 is not used to widen this table's limits. UNS G12130 and SAE 1213 are names directly listed in the same row of this table; other standards or editions are not treated as this edition. Unless residual elements are otherwise specified, the default is B. A/B/C is selected for the applicable product form/agreement. No limit is listed for D, but the amount of Cu/Ni/Cr/Mo must still be reported; it is not treated as zero. To demonstrate table compliance, Cu/Cr/Ni/Mo/Si must be reported in addition to C/Mn/P/S. A value below 0.02% may be reported as <0.02% as specified in the source; this is neither a universal upper limit nor zero. Table 3A/3B covers forged semi-finished products, bars, wire rod and seamless tubes of free-cutting carbon steels; it is not presented as universal composition requirements for flat products. Retain the two-sided P/S range in this row. V0.04–0.08% for 11V41 is an explicit row requirement; ordinary 11xx does not include V. Si is normally not specified for 12xx to avoid impairing machinability. Unspecified Si remains unknown and must be reported under 3.1, not treated as zero. Pb is included only in the row for 12L14; ordinary 1212/1213/1215 does not include Pb. The identities L and UNS G12144 are retained. A free-cutting application does not establish cold-heading suitability; delivery, project-specific processing and supply require separate confirmation. 3.1 and Table 6 require reporting C/Mn/P/S/Si/Al/Cu/Ni/Cr/Mo/Nb(Cb)/Ti/V/B/N; As/Sb is also reported when requested by the purchaser. Si/Cu/Ni/Cr/Mo below 0.02% may be reported as <0.02%, and Nb/Ti/V below 0.008% as <0.008%. These are reporting thresholds, not universal composition maxima; they do not justify filling in zero or an unspecified limit.

Original condition-branch records

Semi-finished forgings / bars / wire rod / seamless tube; Residual B (default unless separately agreed)

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Semi-finished forgings / bars / wire rod / seamless tube; Residual A

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cr≤ 0.15 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Semi-finished forgings / bars / wire rod / seamless tube; Residual C

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33
Cu≤ 0.4 (lower limit not stated)
Ni≤ 0.4 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Mo≤ 0.12 (lower limit not stated)

Semi-finished forgings / bars / wire rod / seamless tube; Residual D (no limit, but reporting is required)

ElementComposition requirement
C≤ 0.13 (lower limit not stated)
Mn0.7 ~ 1.0
P0.07 ~ 0.12
S0.24 ~ 0.33

A condition branch must be selected

Yes

Verification notes

The original 2014 text was checked across four tables and 79 rows, including composition cells, product-form columns, UNS designations and notes; sources and distinct order conditions are retained separately.
WhatsApp Technical enquiry →