S44535 · ASTM A240/A240M-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Ferritic and martensitic stainless steels
Material form
Reference record
Original record status
Original-standard record
Standard edition
ASTM A240/A240M-2014
Table / clause
Table 1 and footnotes A–O
PDF page references
1、5、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn0.3 ~ 0.8
P≤ 0.05 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Cr20.0 ~ 24.0
Cu≤ 0.5 (lower limit not stated)
La0.04 ~ 0.2
Ti0.03 ~ 0.2
Al≤ 0.5 (lower limit not stated)

Applicability and limitations

Table 1 gives heat-analysis mass percentages; A single value without a stated range or minimum is a maximum; unspecified elements are not entered as zero. ; Cb and Nb are the same element; Where both a formula and a fixed limit apply, the stricter limit is used. ; This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. ; Clause 4.1 also requires compliance with the applicable provisions of ASTM A480/A480M; This record displays the heat composition in Table 1; it does not establish verification of A480 or all product acceptance requirements. ; Other elements in the original table: La 0.04–0.20 Ti 0.03–0.20 Al 0.50; See the limits below for the specific coupled requirements.