← BackMaterial grade directory

1033

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 1033 →

1033 · SAE J 403-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J403 NOV2001
Table / clause
Table 1 and Notes 1, 2 and *
PDF page references
1、3、4

Carbon-equivalent reference

IIW / CEV:0.4167–0.5267 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4100Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4600 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

Table 1: UNS G10330 corresponds to SAE 1033; heat analysis, wt%. Si is not a universally mandatory constituent. When specified, common limits for bars/semi-finished products are ≤.10, .10–.20, .15–.35, .20–.40 and .30–.60%; wire rod also has the .07–.15% option. This record does not select a range without agreement. When Cu is required, ≥.20% is generally specified; this is neither a universal upper limit for Cu nor a default requirement. Addition of Pb at .15–.35% requires the L designation and a change to UNS; addition of B at .0005–.003% requires the B designation. These treatments are not included in ordinary grades. Lower P/S limits for certain qualities/products require separate verification against J411; agreement values from later editions are not imported. A requirement to report additional elements does not establish universal limits in this table. Unspecified Si/Cr/Ni/Mo and other elements are not assigned zero. Product-analysis deviations under J409 require separate verification.

Verification notes

Official English Table 1 and footnotes visually checked.

1033 · SAE J403-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J403-2014
Table / clause
Table 1
PDF page references
3
Unit
Mass fraction (wt%)
Analysis type
Cast or heat analysis

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group B (default unless otherwise agreed)
IIW / CEV:0.4167–0.6187Known-element contribution; incomplete value; missing V; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4457Known-element contribution; incomplete value; missing Si, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4997 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group A
IIW / CEV:0.4167–0.5953Known-element contribution; incomplete value; missing V; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4348Known-element contribution; incomplete value; missing Si, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4885 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group C
IIW / CEV:0.4167–0.6640Known-element contribution; incomplete value; missing V; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4597Known-element contribution; incomplete value; missing Si, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.5170 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group D (no limit specified, but reporting is required)
IIW / CEV:0.4167–0.5267Known-element contribution; incomplete value; missing Cr, Mo, V, Ni, Cu; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4100Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4600Known-element contribution; incomplete value; missing Mo, Cr, Cu, Ni; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Flat products: structural shapes, plate, strip, sheet and welded pipe (as defined in note 1); residual-element group B (default unless otherwise agreed)
IIW / CEV:0.4167–0.6187Known-element contribution; incomplete value; missing V; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4457Known-element contribution; incomplete value; missing Si, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4997 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Flat products: sections, plate, strip, sheet and welded tube (as defined in Note 1); residual category A
IIW / CEV:0.4167–0.5953Known-element contribution; incomplete value; missing V; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4348Known-element contribution; incomplete value; missing Si, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4885 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Flat products: structural shapes, plate, strip, sheet and welded pipe (as defined in note 1); residual-element group C
IIW / CEV:0.4167–0.6640Known-element contribution; incomplete value; missing V; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4597Known-element contribution; incomplete value; missing Si, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.5170 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Flat products: structural shapes, plate, strip, sheet and welded pipe (as defined in note 1); residual-element group D (no limit specified, but reporting is required)
IIW / CEV:0.4167–0.5267Known-element contribution; incomplete value; missing Cr, Mo, V, Ni, Cu; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3350–0.4100Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3700–0.4600Known-element contribution; incomplete value; missing Mo, Cr, Cu, Ni; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Applicability and limitations

SAE J403 Revised JUN2014 Table 1: original cast or heat analysis, mass fraction wt%. Product-analysis deviations are addressed separately under SAE J409; J409 is not used to widen this table's limits. UNS G10330 and SAE 1033 are names directly listed in the same row of this table; other standards or editions are not treated as this edition. Unless residual elements are otherwise specified, the default is B. A/B/C is selected for the applicable product form/agreement. No limit is listed for D, but the amount of Cu/Ni/Cr/Mo must still be reported; it is not treated as zero. To demonstrate table compliance, Cu/Cr/Ni/Mo/Si must be reported in addition to C/Mn/P/S. A value below 0.02% may be reported as <0.02% as specified in the source; this is neither a universal upper limit nor zero. Select P/S separately for flat and long products; do not combine them using the wider upper limit. Select 1006/1008 Mn by product form under note 6/7 to Table 1. Si is specified only by order agreement. Common wire-rod options are ≤0.10, 0.07–0.15, 0.10–0.20, 0.15–0.35, 0.20–0.40 and 0.30–0.60%; the common option 0.07–0.15 is not listed for other products. Verify the contractual value against product form; no fixed Si is assigned without agreement. Ordinary grades in this table do not automatically include Pb or B. Separately lead- or boron-treated grades require the L/B designation and the corresponding UNS. The source values Pb0.15–0.35% and B0.0005–0.003% apply to those treatments and are not included in ordinary steels. Note 3 to Table 1: when Cu is specifically required, Cu≥0.20% is normally specified. Residual options in this batch serve residual control only; the deliberate-addition condition for Cu is not unconditionally combined with residual maxima. The order range requires separate agreement, and this specific Cu condition is not evaluated automatically. 3.1 and Table 6 require reporting C/Mn/P/S/Si/Al/Cu/Ni/Cr/Mo/Nb(Cb)/Ti/V/B/N; As/Sb is also reported when requested by the purchaser. Si/Cu/Ni/Cr/Mo below 0.02% may be reported as <0.02%, and Nb/Ti/V below 0.008% as <0.008%. These are reporting thresholds, not universal composition maxima; they do not justify filling in zero or an unspecified limit.

Original condition-branch records

Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group B (default unless otherwise agreed)

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group A

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cr≤ 0.15 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group C

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)
Cu≤ 0.4 (lower limit not stated)
Ni≤ 0.4 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Mo≤ 0.12 (lower limit not stated)

Long products: forged semifinished products, hot-rolled/cold-finished bars, wire rod and seamless tubes; residual-element group D (no limit specified, but reporting is required)

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.04 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Flat products: structural shapes, plate, strip, sheet and welded pipe (as defined in note 1); residual-element group B (default unless otherwise agreed)

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.35 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Flat products: sections, plate, strip, sheet and welded tube (as defined in Note 1); residual category A

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cr≤ 0.15 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Flat products: structural shapes, plate, strip, sheet and welded pipe (as defined in note 1); residual-element group C

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Cu≤ 0.4 (lower limit not stated)
Ni≤ 0.4 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Mo≤ 0.12 (lower limit not stated)

Flat products: structural shapes, plate, strip, sheet and welded pipe (as defined in note 1); residual-element group D (no limit specified, but reporting is required)

ElementComposition requirement
C0.3 ~ 0.36
Mn0.7 ~ 1.0
P≤ 0.03 (lower limit not stated)
S≤ 0.035 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

The original 2014 text was checked across four tables and 79 rows, including composition cells, product-form columns, UNS designations and notes; sources and distinct order conditions are retained separately.
WhatsApp Technical enquiry →