1.4104 · Walsin Lihwa official website catalog (steel billets and bars; file named 2024, original edition not indicated)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Bars
Original record status
Manufacturer source verified
Document edition
Official website document 2024_Walsin_Catalog_YT-JY-1.pdf; Publication date and edition number not specified on inner pages
Document title
Available Stainless Steel Grades & Chemical Composition — For Stainless Steel Billet & Bar
Table / clause
Steel grades and chemical composition table
PDF page references
7
Unit
Percentages as stated in the original table; refer to the source for the specific basis
Analysis type
Analysis type not stated
Manufacturer
Walsin Lihwa

Source document

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.1 ~ 0.17
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.5 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S0.15 ~ 0.35
Ni≤ 0.6 (lower limit not stated)
Cr15.5 ~ 17.5
Mo0.2 ~ 0.6

Applicability and limitations

Walsin Lihwa official website catalogue, PDF page 7

printed page 11, row 15; manufacturer composition table %, covering billets and bars, analysis type not stated. The website filename includes 2024, but no edition number was found inside; not a verified edition of the compared standard or our company’s supply guarantee.

Composition conditions

Verification notes

Composition, conditional rows and linked requirements checked cell by cell against the original image; anomalous row 303 on page 10 excluded.