← BackMaterial grade directory

022CR18NBTI

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 022CR18NBTI →

022Cr18NbTi · GB /T 20878-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Ferritic stainless and heat-resistant steels
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 20878—2007
Table / clause
Table 3, No. 91
PDF page references
12
Unit
Mass fraction (wt%)
Analysis type
Standard composition requirements

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr17.5 ~ 18.5
Ti0.1 ~ 0.6
NbNot listed; must not be treated as 0

Applicability and limitations

Original GB/T 20878—2007 composition, mass fractions wt%; Values in parentheses are maximum permitted additions. Nb ≥0.30+3C,Ti 0.10~0.60; The Nb minimum is coupled with measured C. This standard does not guarantee cold-heading suitability or actual supply. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.

Combined limits

Combined-element limits
  • Element coefficient
    Nb
    1
    C
    -3
    Requirement
    Nb≥0.30+3C
    Lower limit
    0.3
Elements requiring measured values from the same heat
  • Nb

Verification notes

Original historical edition GB/T 20878—2007, Table 3, item 91; The complete 45-page scan was checked; the standard has been withdrawn, and the historical edition’s applicability boundaries are retained. This row includes coupled requirements across elements; without measured composition, manual review is required, and independent intervals must not be treated as a complete assessment.