HS6-5-2-5 · ISO 4957-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 4957-2018
Table / clause
Table 8 · Notes a–f
PDF page references
19

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default S≤.030%, Mn≤.40%
IIW / CEV:2.9100–3.3767Known-element contribution; incomplete value; missing Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):1.5433–1.7667Known-element contribution; incomplete value; missing Cu, Ni, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:1.5300–1.7350Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Agreed S .060–.150%, Mn≤.80%
IIW / CEV:2.9100–3.4433Known-element contribution; incomplete value; missing Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):1.5433–1.7867Known-element contribution; incomplete value; missing Cu, Ni, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:1.5300–1.7750Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.87 ~ 0.95
Si≤ 0.45 (lower limit not stated)
Cr3.8 ~ 4.5
V1.7 ~ 2.1
Mn≤ 0.4 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Mo4.7 ~ 5.2
W5.9 ~ 6.7
Co4.5 ~ 5

Applicability and limitations

Table 8 high-speed tool steel heat analysis wt%; Default Mn≤.40%, P/S each ≤.030%. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; dashes are not entered as zero. ; Product-analysis tolerances in Table 9 must not expand the default heat-analysis range; Hardness and test temperature in the table depend on specific conditions; only composition is recorded in this round. ; High-speed tool steel is not automatically classified as a cold-heading wire product. ; Note f: For HS6-5-2-5, when S is agreed as .060–.150%, Mn ≤ .80%; both limits shall be switched together.

Original condition-branch records

Default S≤.030%, Mn≤.40%

ElementComposition requirement
C0.87 ~ 0.95
Si≤ 0.45 (lower limit not stated)
Cr3.8 ~ 4.5
V1.7 ~ 2.1
Mn≤ 0.4 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Mo4.7 ~ 5.2
W5.9 ~ 6.7
Co4.5 ~ 5

Agreed S .060–.150%, Mn≤.80%

ElementComposition requirement
C0.87 ~ 0.95
Si≤ 0.45 (lower limit not stated)
Cr3.8 ~ 4.5
V1.7 ~ 2.1
Mn≤ 0.8 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S0.06 ~ 0.15
Mo4.7 ~ 5.2
W5.9 ~ 6.7
Co4.5 ~ 5

A condition branch must be selected

Yes

Verification notes

All ranges and footnotes in original Table 8 were visually checked

HS6-5-2-5 · BS EN ISO 4957:2018

Chemical-composition source verified. Properties and delivery conditions follow the sources and conditions stated here; actual supply and measured heat results are not verified by this reference.

Material category
Tool steel
Product form
Tool-steel standard reference; product form subject to the order
Standard edition
BS EN ISO 4957:2018
Table / clause
Table 8 and notes a–f
Source file
BS EN ISO 4957-2018-Tool steel.docx
Units
Mass fraction (wt%)
Analysis type
Cast analysis

Composition (agreed alternatives apply)

ElementComposition requirement
C0.87 ~ 0.95
Si≤ 0.45 (lower limit not stated)
Cr3.8 ~ 4.5
V1.7 ~ 2.1
Mn≤ 0.4 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Mo4.7 ~ 5.2
W5.9 ~ 6.7
Co4.5 ~ 5

Default S≤.030%, Mn≤.40%

ElementComposition requirement
C0.87 ~ 0.95
Si≤ 0.45 (lower limit not stated)
Cr3.8 ~ 4.5
V1.7 ~ 2.1
Mn≤ 0.4 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Mo4.7 ~ 5.2
W5.9 ~ 6.7
Co4.5 ~ 5

Agreed S .060–.150%, Mn≤.80%

ElementComposition requirement
C0.87 ~ 0.95
Si≤ 0.45 (lower limit not stated)
Cr3.8 ~ 4.5
V1.7 ~ 2.1
Mn≤ 0.8 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S0.06 ~ 0.15
Mo4.7 ~ 5.2
W5.9 ~ 6.7
Co4.5 ~ 5

Applicability and limitations

Cast analysis, mass fraction %. A dash means the standard gives no separate requirement; it does not mean zero. Unlisted elements shall not be intentionally added without purchaser consent, except additions needed to finish steelmaking. Permissible product-analysis deviations do not expand the default cast-analysis limits. Tool-steel classification and hardness depend on application, heat treatment and test conditions; they do not establish cold-heading suitability or guarantee properties in an arbitrary condition. Table 8: high-speed tool steels; cast analysis, wt%; default Mn≤.40%, P and S each ≤.030%. Unlisted elements shall not be intentionally added without purchaser consent, except to finish steelmaking. Dashes are not entered as zero. Note f: When S .060–.150% is agreed for HS6-5-2-5, Mn≤.80%. Both limits must change together. Annealed and cold-drawn (+A+C) hardness may be 50 HBW higher than annealed (+A); annealed and cold-rolled (+A+CR) may be 70 HBW higher. Only HS6-5-2C and HS6-5-2-5 may use S 0.060%–0.150% with Mn≤0.80% by agreement under Table 8 note f. This exception does not apply to other grades.

Composition and ordering conditions

Mechanical properties and delivery condition

PropertyStandard requirements and applicable conditions
Annealed hardness HBW / maximum269
Hardening testAustenitizing 1210±10 °C ; oil or salt bath; oil quenching in case of dispute ; minimum tempering temperature 560±10 °C ; hardness≥64 HRC; testing in accordance with B.3.

Mechanical-property provenance:BS EN ISO 4957:2018 · Table 8 and notes a–f · Standard tables embedded in the Word document supplied by the user

Verification notes

Checked against the standard text and table notes supplied by the user. Applicability to a specific order requires separate confirmation.