022Cr25Ni7Mo4N · GB /T 20878-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic-ferritic duplex stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 20878—2007
Table / clause
Table 2, No. 76
PDF page references
10
Unit
Mass fraction (wt%)
Analysis type
Standard composition requirements

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Ni6 ~ 8
Cr24 ~ 26
Mo3 ~ 5
Cu≤ 0.5 (lower limit not stated)
N0.24 ~ 0.32

Applicability and limitations

Original GB/T 20878—2007 chemical composition, mass fraction wt%; parenthesized values are maximum permitted additions. This standard does not guarantee cold-heading suitability or actual supply. GB/T 20878—2007 is a historical edition; this record does not replace the current standard, contract, or verification of material suitability.

Verification notes

GB/T 20878—2007 historical original, Table 2, entry 76. The complete 45-page scan was checked. The standard is withdrawn; the historical edition’s application limits are retained.

022Cr25Ni7Mo4N · GB /T 12770-2012

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 20878-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 21833-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 24511-2017

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
Mo3 ~ 3.5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.03 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 31303-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 32569-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 3280-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 39033-2020

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

022Cr25Ni7Mo4N · GB /T 4237-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu≤ 0.5 (lower limit not stated)
Mn≤ 1.2 (lower limit not stated)
Mo3 ~ 5
N0.24 ~ 0.32
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 0.8 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →