← BackMaterial grade directory

C88DA material reference

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for C88DA →

C88DA · GB/T 24242.2-2020

Chemical-composition source verified. Properties and delivery conditions follow the sources and conditions stated here; actual supply and measured heat results are not verified by this reference.

Material category
Carbon steels
Product form
Wire rod
Standard edition
GB/T 24242.2-2020
Table / clause
Table 1 and clauses 3.2, 4.2.7
Source file
GB_T 24242.2-2020.pdf
PDF page
5
Units
Mass fraction (wt%)
Analysis type
Cast analysis

Composition

ElementComposition requirement
C0.85 ~ 0.9
Si0.1 ~ 0.3
Mn0.3 ~ 0.6
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cr≤ 0.15 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Mo≤ 0.05 (lower limit not stated)
Cu≤ 0.25 (lower limit not stated)
Al≤ 0.01 (lower limit not stated)

Applicability and limitations

Cast analysis; composition is expressed as mass fraction, %. An unspecified lower limit is not zero. Class A: Mn 0.30%–0.60%; class B: Mn 0.60%–0.90%. These classes apply only to C26D–C92D and are agreed at ordering. 4.2.4: Unlisted elements shall not be intentionally added without purchaser consent. Cr and V may be added by agreement at ordering: Cr≤0.30%, V≤0.10%. 4.2.5: For C26D–C92D, agreement may raise the C upper limit by 0.01% or lower the lower limit by 0.01%. This does not expand the default table limits. 4.2.6: The Si lower limit for galvanizing, or the Si upper limit for C4D–C20D, may be separately agreed at ordering. 4.2.8–4.2.10: By agreement, Cu≤0.20%; for C48D–C92D, Cu+Sn≤0.25% may be specified; Al of 0.01%–0.06% with Si≤0.10% may be agreed. 4.3: Mechanical properties of composition-designated grades are agreed between supplier and purchaser. Table 2 gives recommended within-batch tensile-strength variation, not guaranteed tensile-strength limits. Delivery condition, dimensions, surface, packaging and acceptance shall follow GB/T 24242.1—2020 and the order.

Composition and ordering conditions

Mechanical properties and delivery condition

Mechanical properties for this grade are agreed between supplier and purchaser and stated in the contract. Recommended variation in Table 2 is not a tensile-strength guarantee.

Verification notes

Checked against the standard text and table notes supplied by the user. Applicability to a specific order requires separate confirmation.

Linked products

View linked products for C88DA →

WhatsApp Technical enquiry →