X153CrMoV12 material reference

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X153CRMOV12 →

Material demand assessment

Looking for X153CRMOV12 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X153CrMoV12 · ISO 4957-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 4957-2018
Table / clause
Table 4 · Notes a–g
PDF page references
15、16

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C1.45 ~ 1.6
Si0.1 ~ 0.6
Mn0.2 ~ 0.6
Cr11 ~ 13
Mo0.7 ~ 1
V0.7 ~ 1
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Table 4 heat composition for cold-work alloy tool steels, wt%; Default P/S are each ≤.030%. ; Product-analysis tolerances in Table 5 must not be applied to the default heat-analysis range. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; dashes are not entered as zero. ; Cold-work tool steel does not establish suitability for cold-heading wire; the words “cold work” alone do not justify listing a product in the product centre.

Verification notes

Official English Table 4 and footnotes visually checked.

X153CrMoV12 · BS EN ISO 4957:2018

Chemical-composition source verified. Properties and delivery conditions follow the sources and conditions stated here; actual supply and measured heat results are not verified by this reference.

Material category
Tool steel
Product form
Tool-steel standard reference; product form subject to the order
Standard edition
BS EN ISO 4957:2018
Table / clause
Table 4 and notes a–g
Source file
BS EN ISO 4957-2018-Tool steel.docx
Units
Mass fraction (wt%)
Analysis type
Cast analysis

Composition

ElementComposition requirement
C1.45 ~ 1.6
Si0.1 ~ 0.6
Mn0.2 ~ 0.6
Cr11 ~ 13
Mo0.7 ~ 1
V0.7 ~ 1
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)

Applicability and limitations

Cast analysis, mass fraction %. A dash means the standard gives no separate requirement; it does not mean zero. Unlisted elements shall not be intentionally added without purchaser consent, except additions needed to finish steelmaking. Permissible product-analysis deviations do not expand the default cast-analysis limits. Tool-steel classification and hardness depend on application, heat treatment and test conditions; they do not establish cold-heading suitability or guarantee properties in an arbitrary condition. Table 4: alloy cold-work tool steels; cast analysis, wt%; default P and S each ≤.030%. Product-analysis deviations in Table 5 must not be applied to the default cast-analysis limits. Unlisted elements shall not be intentionally added without purchaser consent, except to finish steelmaking. Dashes are not entered as zero. Annealed and cold-drawn (+A+C) hardness may be 20 HBW higher than annealed (+A) hardness. Hardness values for different conditions must not be interchanged.

Composition and ordering conditions

Mechanical properties and delivery condition

PropertyStandard requirements and applicable conditions
Annealed hardness HBW / maximum255
Hardening testAustenitizing 1020±10 °C ; air quenching ; tempering 180±10 °C ; hardness≥61 HRC

Mechanical-property provenance:BS EN ISO 4957:2018 · Table 4 and notes a–g · Standard tables embedded in the Word document supplied by the user

Verification notes

Checked against the standard text and table notes supplied by the user. Applicability to a specific order requires separate confirmation.

Related catalog and standard references

View standard reference information →

A reference link does not confirm supply or interchangeability. Specific requirements need technical confirmation.