12 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
X2CrNiMo17-12-3 · EN 10263-5-2001
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10263-5-2001
Table / clause
Table 2 and notes a–e; Table 3 is cited only for deviations
PDF page references
1、8、9
Carbon-equivalent reference
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.11 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Applicability and limitations
Actual source: DIN EN 10263-5:2002-02; German adoption of EN 10263-5:2001, PDF p. 8 Table 2 and Notes a–e.
Default is ladle analysis, mass fraction wt%; product-analysis deviations are separately governed by Table 3 and are not added to default ladle ranges.
Unlisted elements must not be intentionally added without purchaser approval (except as necessary during steelmaking); residual elements must not impair performance or use.
This older edition does not use the 2017 edition’s conditional sulfur provisions; do not copy newer machining/welding/polishing options.
For Ti-stabilized grades, verify 5×C≤Ti≤0.70% using measured C; do not apply this condition to grades without Ti.
The standard covers cold heading/cold extrusion; actual supply, dimensions, delivery condition and properties still require confirmation.
Original condition-branch records
Default heat-analysis values in historical Table 2
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.11 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Verification notes
Visual check of the previous-edition cover, all 19 grades in Table 2, and footnotes
X2CrNiMo17-12-3 · ISO 4954
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
Cr
16.5 ~ 18.5
Ni
10.5 ~ 13
Mo
2.5 ~ 3
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1 (lower limit not stated)
Applicability and limitations
Composition based on ISO 4954:2018; the product edition is unspecified, so confirm the edition applicable to the contract.
Composition conditions
ISO 4954:2018, Table D.2 gives heat analysis; A single value is a maximum; a dash is not zero.
Product-analysis tolerances are listed separately under Table 2/3 of the standard and do not directly widen the heat-analysis composition ranges.
Unlisted elements must not be intentionally added without purchaser consent, except for additions needed to finish the heat.
Verification notes
Composition based on ISO 4954:2018; the product edition is unspecified, so confirm the edition applicable to the contract.View associated products →
X2CrNiMo17-12-3 · ISO 4954-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 4954:2018
Table / clause
Table D.2
Carbon-equivalent reference
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
Cr
16.5 ~ 18.5
Ni
10.5 ~ 13
Mo
2.5 ~ 3
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1 (lower limit not stated)
Applicability and limitations
ISO 4954:2018 Table D.2 gives cast analysis; single values are maxima and dashes are not zero.
Product-analysis deviations are listed separately under Tables 2/3, not used directly to relax cast-composition limits.
Elements not listed must not be intentionally added without the purchaser's consent, except for finishing the heat.
Verification notes
The original standard, Table D.2 and footnotes have been checked
X2CrNiMo17-12-3 · EN 10263-5-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10263-5-2017
Table / clause
Table 3 and footnotes a–e
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Default composition in Table 3
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Machinability condition S 0.015–0.030%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Weldability condition S 0.008–0.030%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Polishability recommendation S≤0.015%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Applicability and limitations
Heat-analysis mass fractions wt%; Product-analysis tolerances follow Table 4 separately. ; The sulfur conditions for machining, welding and polishing in Table 3, note b are retained separately; different requirements are not imposed simultaneously. ; Ti-stabilized grades require 5×C≤Ti≤0.70%, checked jointly with measured C/Ti. ; This standard covers stainless steel for cold heading and cold extrusion; delivery condition, dimensions, surface and mechanical properties still require independent confirmation. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; unspecified contents are not treated as zero.
Original condition-branch records
Default composition in Table 3
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Machinability condition S 0.015–0.030%
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.015 ~ 0.03
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Weldability condition S 0.008–0.030%
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.008 ~ 0.03
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Polishability recommendation S≤0.015%
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
A condition branch must be selected
Yes
Verification notes
The original English Table 3 and footnotes have been checked
X2CrNiMo17-12-3 · DIN EN 10263-5-2002
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10263-5-2002
Table / clause
Table 2 and notes a–e; Table 3 is cited only for deviations
PDF page references
1、8、9
Carbon-equivalent reference
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.11 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Applicability and limitations
Actual source: DIN EN 10263-5:2002-02; German adoption of EN 10263-5:2001, PDF p. 8 Table 2 and Notes a–e.
Default is ladle analysis, mass fraction wt%; product-analysis deviations are separately governed by Table 3 and are not added to default ladle ranges.
Unlisted elements must not be intentionally added without purchaser approval (except as necessary during steelmaking); residual elements must not impair performance or use.
This older edition does not use the 2017 edition’s conditional sulfur provisions; do not copy newer machining/welding/polishing options.
For Ti-stabilized grades, verify 5×C≤Ti≤0.70% using measured C; do not apply this condition to grades without Ti.
The standard covers cold heading/cold extrusion; actual supply, dimensions, delivery condition and properties still require confirmation.
Original condition-branch records
Default heat-analysis values in historical Table 2
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.11 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Verification notes
Visual check of the previous-edition cover, all 19 grades in Table 2, and footnotes
X2CrNiMo17-12-3 · DIN EN 10263-5-2002
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10263-5-2002
Table / clause
Table 2 and notes a–e; Table 3 is cited only for deviations
PDF page references
1、8、9
Carbon-equivalent reference
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.11 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Applicability and limitations
Actual source: DIN EN 10263-5:2002-02; German adoption of EN 10263-5:2001, PDF p. 8 Table 2 and Notes a–e.
Default is ladle analysis, mass fraction wt%; product-analysis deviations are separately governed by Table 3 and are not added to default ladle ranges.
Unlisted elements must not be intentionally added without purchaser approval (except as necessary during steelmaking); residual elements must not impair performance or use.
This older edition does not use the 2017 edition’s conditional sulfur provisions; do not copy newer machining/welding/polishing options.
For Ti-stabilized grades, verify 5×C≤Ti≤0.70% using measured C; do not apply this condition to grades without Ti.
The standard covers cold heading/cold extrusion; actual supply, dimensions, delivery condition and properties still require confirmation.
Original condition-branch records
Default heat-analysis values in historical Table 2
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.11 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Verification notes
Visual check of the previous-edition cover, all 19 grades in Table 2, and footnotes
X2CrNiMo17-12-3 · EN 10088-1-2005
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 4 and continuation; notes a–e; all 50 austenitic corrosion-resistant steel grades
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, S for long products/wire etc.: ≤0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, S for long products/wire etc.: ≤0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for machining: 0.015–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for machining: 0.015–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for welding: 0.008–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for welding: 0.008–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for polishing: ≤0.015%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for polishing: ≤0.015%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Applicability and limitations
EN 10088-1:2005 Table 4 and continuation: ladle analysis (wt%); the official SIST adoption preview PDF, pages 11/12, covers all 50 grades and notes. Note a: unlisted elements are not intentionally added without purchaser consent, except as needed to complete steelmaking; a blank is not zero. Note b: for grades marked b only, S is selected separately for long products and by property requirement. Note d: the increased Ni maximum for special reasons applies only to listed grades, not all grades. Note c: Cu up to 1.0% for cold heading/extrusion; this condition path is provided here only for grades with blank Cu in the original table. Existing Cu alloy ranges retain their original values; the exception has not automatically rewritten them. The linked Ti≥5C/Nb≥10C and Ti≥8(C+N) conditions are retained; an unlisted N maximum is not zero. Note e: the source warns of skin-contact regulatory issues for high-sulfur free-machining steel; this is retained as a historical warning only and is not a claim of current compliance based on the 2005 text. Listed chemistry and the cold-heading Cu exception alone do not establish overall cold-heading performance or company supply; mechanical and product standards must be checked separately, and national adoption does not mean automatic equivalence.
Original condition-branch records
Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, S for long products/wire etc.: ≤0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, S for long products/wire etc.: ≤0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for machining: 0.015–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for machining: 0.015–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for welding: 0.008–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for welding: 0.008–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for polishing: ≤0.015%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for polishing: ≤0.015%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Applicability and limitations
EN 10088-1:2005 Table 4 and continuation: ladle analysis (wt%); the official SIST adoption preview PDF, pages 11/12, covers all 50 grades and notes. Note a: unlisted elements are not intentionally added without purchaser consent, except as needed to complete steelmaking; a blank is not zero. Note b: for grades marked b only, S is selected separately for long products and by property requirement. Note d: the increased Ni maximum for special reasons applies only to listed grades, not all grades. Note c: Cu up to 1.0% for cold heading/extrusion; this condition path is provided here only for grades with blank Cu in the original table. Existing Cu alloy ranges retain their original values; the exception has not automatically rewritten them. The linked Ti≥5C/Nb≥10C and Ti≥8(C+N) conditions are retained; an unlisted N maximum is not zero. Note e: the source warns of skin-contact regulatory issues for high-sulfur free-machining steel; this is retained as a historical warning only and is not a claim of current compliance based on the 2005 text. Listed chemistry and the cold-heading Cu exception alone do not establish overall cold-heading performance or company supply; mechanical and product standards must be checked separately, and national adoption does not mean automatic equivalence.
Original condition-branch records
Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, S for long products/wire etc.: ≤0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, S for long products/wire etc.: ≤0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for machining: 0.015–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for machining: 0.015–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for welding: 0.008–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for welding: 0.008–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for polishing: ≤0.015%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note b, recommended S for polishing: ≤0.015%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Applicability and limitations
NF EN 10088-1:2005 adopts EN 10088-1:2005 (EN 10088-1-2005); See the data basis for the actual composition source file and table number. EN10088-1:2005 Table 4 and its continuation; heat analysis wt%; all 50 grades and footnotes on PDF pages 11/12 of the official SIST adoption preview.. ; Note a: Elements not listed shall not be intentionally added without the consent of the purchaser (except additions needed to finish steelmaking).; Blanks are not entered as zero. ; Note b: For grades marked b, S shall be selected separately according to long products and properties.; The increased Ni upper limit based on special reasons in Note d applies only to the listed steel grades and cannot be generalized to all grades.. ; Note c: For cold-heading/cold-extrusion applications, Cu max 1.0%.; This conditional path is provided only for grades where Cu was blank in the original table; existing Cu alloying ranges shall retain their original values, and their Cu exceptions have not been automatically rewritten.. ; The linkages Ti≥5C/Nb≥10C and Ti≥8(C+N) are retained.; If no N upper limit is listed, do not fill as zero.. ; Note e retains the original historical caution about skin-contact regulations for high-sulfur free-cutting steel; the 2005 text is not used to claim present-day compliance.. ; The listed compositions and the cold-heading Cu exception do not independently prove the overall cold-heading properties of the material or company supply.; Mechanical properties and product standards require separate verification; national adoption does not automatically establish equivalence..
Original condition-branch records
Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.
Note b, S for long products/wire etc.: ≤0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Note b, S for long products/wire etc.: ≤0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Cu
≤ 1.0 (lower limit not stated)
Note b, recommended S for machining: 0.015–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.015 ~ 0.03
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Note b, recommended S for machining: 0.015–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.015 ~ 0.03
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Cu
≤ 1.0 (lower limit not stated)
Note b, recommended S for welding: 0.008–0.030%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.008 ~ 0.03
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Note b, recommended S for welding: 0.008–0.030%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.008 ~ 0.03
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Cu
≤ 1.0 (lower limit not stated)
Note b, recommended S for polishing: ≤0.015%Default Ni; cold-heading Cu exception not selected, so the original-table Cu requirement applies.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Note b, recommended S for polishing: ≤0.015%Default Ni; note c allows Cu≤1.0% for cold heading/cold extrusion.
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
N
≤ 0.11 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
Cu
≤ 1.0 (lower limit not stated)
A condition branch must be selected
Yes
Verification notes
The formal adoption relationship and corresponding EN composition original have been checked; the complete national adoption text has not been verified page by page.
X2CrNiMo17-12-3 · ISO 15510-2014
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 15510-2014
Table / clause
The current grade row in Table1; Note a and corresponding footnotes (original text on the publishing platform)
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Base range in Table 1
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note c: only where ferrite content must be reduced for a special reason, the Ni maximum may be increased by 1.50 percentage points; This condition must be confirmed
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Applicability and limitations
ISO 15510:2014, Table 1 gives heat analysis, mass fractions wt%; Under note a, values without a stated range or minimum are maxima; a dash is not treated as zero. Composition rows follow an excerpt of the official PDF edition; relevant footnotes follow the original Table 1 in the Sample text section of the standards publishing platform; Verification of the complete standard text or mechanical properties is not claimed. The standard covers material for wrought products, including ingots and semi-finished products; Similar composition does not establish direct substitution; cold-heading suitability and supply condition require separate confirmation. The S 0.015–0.030% machinability recommendations, 0.008–0.020% weldability recommendation and S≤0.015% polishability recommendation in note b concern specific properties and do not directly replace this row’s sulfur limits. Note c applies only where ferrite content must be reduced for special reasons such as hot workability or low magnetic permeability; The increased Ni maximum is not treated as an unconditional range.
Original condition-branch records
Base range in Table 1
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Note c: only where ferrite content must be reduced for a special reason, the Ni maximum may be increased by 1.50 percentage points; This condition must be confirmed
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 14.5
N
≤ 0.1 (lower limit not stated)
A condition branch must be selected
Yes
Verification notes
The row for this grade in Table 1 has been checked against the official PDF; Relevant original footnotes are retained in the supporting verification record; Full standard text and mechanical properties to be verified separately
X2CrNiMo17-12-3 · DIN EN 10263-5-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10263-5:2018-02
Table / clause
Tabelle 3 and footnote a–e; Tabelle 4 product-analysis tolerances require separate verification
PDF page references
1、10、11
Unit
Mass fraction (wt%)
Analysis type
Heat analysis
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Default composition in Table 3
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Machinability condition S 0.015–0.030%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Weldability condition S 0.008–0.030%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Polishability recommendation S≤0.015%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition record (conditional branches apply; this is not an unconditional requirement)
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Applicability and limitations
DIN EN 10263-5:2018-02 is the German-language edition of EN 10263-5:2017; This record was verified against heat analysis and footnotes in Table 3 of the official German edition. ; Heat-analysis mass fractions wt%; Product-analysis tolerances follow Table 4 separately. ; The sulfur conditions for machining, welding and polishing in Table 3, note b are retained separately; different requirements are not imposed simultaneously. ; Ti-stabilized grades require 5×C≤Ti≤0.70%, checked jointly with measured C/Ti. ; This standard covers stainless steel for cold heading and cold extrusion; delivery condition, dimensions, surface and mechanical properties still require independent confirmation. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; unspecified contents are not treated as zero.
Original condition-branch records
Default composition in Table 3
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Machinability condition S 0.015–0.030%
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.015 ~ 0.03
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Weldability condition S 0.008–0.030%
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
0.008 ~ 0.03
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
Polishability recommendation S≤0.015%
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Si
≤ 1.0 (lower limit not stated)
Mn
≤ 2.0 (lower limit not stated)
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
Cr
16.5 ~ 18.5
Mo
2.5 ~ 3.0
Ni
10.5 ~ 13.0
N
≤ 0.1 (lower limit not stated)
Cu
≤ 1.0 (lower limit not stated)
A condition branch must be selected
Yes
Verification notes
DIN EN 10263-5:2018-02 official German edition, Table 3, row 8 and notes a–e checked; adopts EN 10263-5:2017.
X2CrNiMo17-12-3 · EN 10263
Original-source verification is incomplete; this is not a formal standard reference
Material category
Stainless steel
Subcategory
Stainless steel
Material form
Drawn wire
Verification status
Published on the website; original-source verification pending
Carbon-equivalent reference
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Composition
Element
Composition requirement
C
≤ 0.03 (lower limit not stated)
Cr
16.5 ~ 18.5
Cu
≤ 1 (lower limit not stated)
Mn
≤ 2 (lower limit not stated)
Mo
2.5 ~ 3
N
≤ 0.11 (lower limit not stated)
Ni
10.5 ~ 13
P
≤ 0.045 (lower limit not stated)
S
≤ 0.015 (lower limit not stated)
Si
≤ 1 (lower limit not stated)
Applicability and limitations