X6NICRTIMOVB25-15-2
4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for X6NICRTIMOVB25-15-2 →Material demand assessment
Looking for X6NICRTIMOVB25-15-2 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
X6NiCrTiMoVB25-15-2 · ISO 4954
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Stainless steel
- Material form
- Cold-heading wire
- Original record status
- Reference transcription of standard
- Standard edition
- ISO 4954:2018
- Table / clause
- Table D.2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 13.5 ~ 16.0 |
| Ni | 24.0 ~ 27.0 |
| Mo | 1.0 ~ 1.5 |
| Ti | 1.9 ~ 2.35 |
| Al | ≤ 0.35 (lower limit not stated) |
| V | 0.1 ~ 0.5 |
| B | 0.001 ~ 0.01 |
Applicability and limitations
ISO 4954:2018; Heat analysis, mass percent; Values without stated ranges are maxima; See the original page for the complete table notes. Other element requirements: Ti: 1,90 to 2,35 Al: 0,35 V: 0,10 to 0,50 B: 0,001 to 0,010; no edition is identified on the website; Displayed under this source edition; contract applicability is not established
Verification notes
Standard source: ISO 4954:2018 · Table D.2View associated products →X6NiCrTiMoVB25-15-2 · ISO 4954-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- ISO 4954:2018
- Table / clause
- Table D.2
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 13.5 ~ 16.0 |
| Ni | 24.0 ~ 27.0 |
| Mo | 1.0 ~ 1.5 |
| Ti | 1.9 ~ 2.35 |
| Al | ≤ 0.35 (lower limit not stated) |
| V | 0.1 ~ 0.5 |
| B | 0.001 ~ 0.01 |
Applicability and limitations
ISO 4954:2018 Table D.2 gives cast analysis; single values are maxima and dashes are not zero.
Product-analysis deviations are listed separately under Tables 2/3, not used directly to relax cast-composition limits.
Elements not listed must not be intentionally added without the purchaser's consent, except for finishing the heat.
Verification notes
The original standard, Table D.2 and footnotes have been checkedX6NiCrTiMoVB25-15-2 · EN 10269-2013
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10269-2013
- Table / clause
- Table1 high-temperature steels and note a/b
- PDF page references
- 18、19
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.03 ~ 0.08 |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | 1.0 ~ 2.0 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Al | ≤ 0.35 (lower limit not stated) |
| B | 0.003 ~ 0.01 |
| Cr | 13.5 ~ 16.0 |
| Mo | 1.0 ~ 1.5 |
| Ni | 24.0 ~ 27.0 |
| V | 0.1 ~ 0.5 |
| Ti | 1.9 ~ 2.3 |
Applicability and limitations
Table 1 and Note a/b in the official BS English adoption of EN10269:2013; heat analysis, wt%. ; The Al column is total aluminum; Elements not listed shall not be filled as zero and shall not be intentionally added without the consent of the purchaser (except those required to complete the smelting process). ; Note b: Sulfur levels by agreement are available only for marked grades; ordinary, machining and welding conditions are retained separately.. ; Titanium-stabilized grade X6CrNiTiB18-10 shall simultaneously satisfy Ti≥5C and Ti≤.80; a single-item upper limit shall not replace a linked lower limit. ; Product-analysis deviations, mechanical properties, delivery heat treatment and suitability for cold heading require separate verification; this record is not automatically included in the supply offering..
Verification notes
Official English Table 1 and applicable footnotes were visually checkedX6NiCrTiMoVB25-15-2 · NF EN 10269:1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- NF EN 10269:1999
- Table / clause
- EN 10269:1999 Table 1 and footnotes 1 and 2
- PDF page references
- 2、23
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.03 ~ 0.08 |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | 1.0 ~ 2.0 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Al | ≤ 0.35 (lower limit not stated) |
| B | 0.003 ~ 0.01 |
| Cr | 13.5 ~ 16.0 |
| Mo | 1.0 ~ 1.5 |
| Ni | 24.0 ~ 27.0 |
| V | 0.1 ~ 0.5 |
| Ti | 1.9 ~ 2.3 |
Applicability and limitations
The cover of NF EN 10269:1999 explicitly adopts EN 10269:1999; Preserve the correspondence between the French adoption version and the European version; do not label as other countries or new editions. ; Table 1 gives heat-analysis mass percentages; Single values in P and S columns are upper limits; other single values are parsed according to the inequality signs in the original table; Unspecified elements shall not be filled as zero. ; Applies to billets, bars and wire rod of steels and nickel alloys for fasteners with specified high- or low-temperature properties.; Cold heading and actual supply must be verified in conjunction with delivery condition, dimensions, and process. ; Table 1 Footnote 1: Elements not listed in the table shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking); Elements that affect properties must be prevented from being introduced via scrap steel, etc.. ; This record only verifies the heat analysis composition in Table 1; product analysis tolerances in Table 2 shall not be automatically added to the heat limits.
Combined limits
- Combined-element limits