← BackMaterial grade directory

316

24 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 316 →

316 · ASTM A 493-2025

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A 493-2025; that original edition remains unavailable, and differences between editions have not been confirmed. Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Verification notes

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A 493-2025; that original edition remains unavailable, and differences between editions have not been confirmed.

316 · ASTM A313/A313M-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A313/A313M-2003
Table / clause
Table 1, footnotes A–B; clauses 1.1, 5, 6
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Cr16.5 ~ 18
Ni10.5 ~ 13.5
Mo2 ~ 2.5
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Edition 2003, round stainless spring wire, mass fraction wt%. Footnote B to Table 1: values without ranges are maxima; blanks mean unspecified and are not replaced with zero. Table 1UNS, S31600. Mechanical properties for categories such as A/B, or for cold-drawing and subsequent ageing conditions, cannot be inferred from the composition table. This edition does not list 2205; similar grades are not used to fill the gap. The original 2018 and 2025 reaffirmed editions have not been verified. Spring-wire use does not automatically establish cold-heading suitability; no supply product is added automatically.

Verification notes

The current chemical composition is based on original 2003; Original 2018 and reaffirmed 2025 have not been verified; equivalence between editions is not assumed.

316 · ASTM A313/A313M-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A313/A313M-2003
Table / clause
Table 1, footnotes A–B; clauses 1.1, 5, 6
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Cr16.5 ~ 18
Ni10.5 ~ 13.5
Mo2 ~ 2.5
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Edition 2003, round stainless spring wire, mass fraction wt%. Footnote B to Table 1: values without ranges are maxima; blanks mean unspecified and are not replaced with zero. Table 1UNS, S31600. Mechanical properties for categories such as A/B, or for cold-drawing and subsequent ageing conditions, cannot be inferred from the composition table. This edition does not list 2205; similar grades are not used to fill the gap. The original 2018 and 2025 reaffirmed editions have not been verified. Spring-wire use does not automatically establish cold-heading suitability; no supply product is added automatically.

Verification notes

The current chemical composition is based on original 2003; Original 2018 and reaffirmed 2025 have not been verified; equivalence between editions is not assumed.

316 · ASTM A493-2009(2013)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Verification notes

The title page of the official English text and the corresponding row and footnotes in Table 1 were visually checked.

316 · ASTM A493-2016

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A493-2016; that original edition remains unavailable, and differences between editions have not been confirmed. Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Verification notes

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A493-2016; that original edition remains unavailable, and differences between editions have not been confirmed.

316 · SAE J405-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
SAE J405 JUN1998
Table / clause
Table 1, page 2 / page 5, notes 1–7
PDF page references
1、3、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Based on SAE J405 JUN1998 original Table 1; mass fraction wt%. Note 1: a value without a range or lower limit is a maximum; a dash means unspecified, not zero. Note 5: Cb and Nb denote the same element; verify alloying elements against the corresponding UNS row and additional conditions. Note 4: carbon is generally reported to 0.01%, and low-carbon types to 0.001%; this is reporting precision and does not relax composition limits. Original Table 1 type names may include common names or ASTM-naming footnotes; create search aliases only for explicit same-row correspondences, without implying cross-standard equivalence. 1998 is the actual composition basis; the specified newer edition has not been checked, so consistency between editions is not assumed.

Verification notes

The current composition is based on the 1998 original. The specified newer edition has not been checked; equivalence between editions is not assumed.

316 · ASTM A493-2009(2013)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Verification notes

The title page of the official English text and the corresponding row and footnotes in Table 1 were visually checked.

316 · ASTM A313/A313M-2003

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A313/A313M-2003
Table / clause
Table 1, footnotes A–B; clauses 1.1, 5, 6
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Cr16.5 ~ 18
Ni10.5 ~ 13.5
Mo2 ~ 2.5
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Edition 2003, round stainless spring wire, mass fraction wt%. Footnote B to Table 1: values without ranges are maxima; blanks mean unspecified and are not replaced with zero. Table 1UNS, S31600. Mechanical properties for categories such as A/B, or for cold-drawing and subsequent ageing conditions, cannot be inferred from the composition table. This edition does not list 2205; similar grades are not used to fill the gap. The original 2018 and 2025 reaffirmed editions have not been verified. Spring-wire use does not automatically establish cold-heading suitability; no supply product is added automatically.

Verification notes

Original 2003, Table 1 and footnotes have been checked; Original 2018/2025 remains unavailable.

316 · ASTM A358/A358M-2024

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Welded-pipe reference
Original record status
Historically referenced table verified
Standard edition
ASTM A240/A240M-2014
Table / clause
Table 1 and footnotes A–O
PDF page references
1、3、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)
Cr16.0 ~ 18.0
Ni10.0 ~ 14.0
Mo2.0 ~ 3.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

The chemical composition currently uses only the verified base-material ranges in the original ASTM A240/A240M—2014; The applicable composition-standard edition and full requirements for A358—2024 have not been verified; compliance with a newer edition cannot be confirmed on this basis. Clause 6.1.1 of A358—2024 references A240/A240M base material; Clause 7.2 specifies separate requirements for welding filler metal; No weld-metal or mixed whole-tube composition is currently provided. Class 1 are welding and radiographic examination classes, not separate chemical-composition grades; This record does not establish capability to supply welded tube; a linked wire-rod product does not establish direct supply of A358 welded tube. Table 1 gives heat-analysis mass percentages; A single value without a stated range or minimum is a maximum; unspecified elements are not entered as zero. Cb and Nb are the same element; Where both a formula and a fixed limit apply, the stricter limit is used. This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. Clause 4.1 also requires compliance with the applicable provisions of ASTM A480/A480M; This record displays the heat composition in Table 1; it does not establish verification of A480 or all product acceptance requirements.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Historical base-material reference: ASTM A240/A240M—2014; Weld metal and the applicable A358—2024 edition have not been verified

      316 · Walsin Lihwa official website catalog (steel billets and bars; file named 2024, original edition not indicated)

      Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

      Material category
      Stainless steel
      Subcategory
      Stainless steel
      Material form
      Bars
      Original record status
      Manufacturer source verified
      Document edition
      Official website document 2024_Walsin_Catalog_YT-JY-1.pdf; Publication date and edition number not specified on inner pages
      Document title
      Available Stainless Steel Grades & Chemical Composition — For Stainless Steel Billet & Bar
      Table / clause
      Steel grades and chemical composition table
      PDF page references
      7
      Unit
      Percentages as stated in the original table; refer to the source for the specific basis
      Analysis type
      Analysis type not stated
      Manufacturer
      Walsin Lihwa

      Source document

      Carbon-equivalent reference

      Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.07 (lower limit not stated)
      Si≤ 1.0 (lower limit not stated)
      Mn≤ 2.0 (lower limit not stated)
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Ni10.0 ~ 13.0
      Cr16.5 ~ 18.0
      Mo2.0 ~ 2.5

      Applicability and limitations

      Walsin Lihwa official website catalogue, PDF page 7

      printed page 10, row 16; manufacturer composition table %, covering billets and bars, analysis type not stated. The website filename includes 2024, but no edition number was found inside; not a verified edition of the compared standard or our company’s supply guarantee.

      Composition conditions

      Verification notes

      Composition, conditional rows and linked requirements checked cell by cell against the original image; anomalous row 303 on page 10 excluded.

      316 · Walsin Lihwa official website catalog (steel billets and bars; file named 2024, original edition not indicated)

      Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

      Material category
      Stainless steel
      Subcategory
      Stainless steel
      Material form
      Bars
      Original record status
      Manufacturer source verified
      Document edition
      Official website document 2024_Walsin_Catalog_YT-JY-1.pdf; Publication date and edition number not specified on inner pages
      Document title
      Available Stainless Steel Grades & Chemical Composition — For Stainless Steel Billet & Bar
      Table / clause
      Steel grades and chemical composition table
      PDF page references
      7
      Unit
      Percentages as stated in the original table; refer to the source for the specific basis
      Analysis type
      Analysis type not stated
      Manufacturer
      Walsin Lihwa

      Source document

      Carbon-equivalent reference

      Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.07 (lower limit not stated)
      Si≤ 1.0 (lower limit not stated)
      Mn≤ 2.0 (lower limit not stated)
      P≤ 0.045 (lower limit not stated)
      S0.02 ~ 0.03
      Ni10.0 ~ 13.0
      Cr16.5 ~ 18.0
      Mo2.0 ~ 2.5

      Applicability and limitations

      Walsin Lihwa official website catalogue, PDF page 7

      printed page 10, row 17; manufacturer composition table %, covering billets and bars, analysis type not stated. The website filename includes 2024, but no edition number was found inside; not a verified edition of the compared standard or our company’s supply guarantee.

      Composition conditions

      Verification notes

      Composition, conditional rows and linked requirements checked cell by cell against the original image; anomalous row 303 on page 10 excluded.

      316 · ASME SA-240

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASME SA-666

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM A 314-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM A240/240M-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM A240/A240M-2020

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM A554-2026

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM A666/A666M-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM A959-2019

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · ASTM F899-2020

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      Mn≤ 2 (lower limit not stated)
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · SAE J467b-1956

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Special alloy steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C0.05 ~ 0.05
      Cr17 ~ 17
      Mn1 ~ 1
      Mo2.5 ~ 2.5
      Ni12.5 ~ 12.5
      Si0.4 ~ 0.4

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · CNS 3477-2016

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · Q/RP 006-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Cu≤ 1 (lower limit not stated)
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      316 · Q/RP 007-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.08 (lower limit not stated)
      Cr16 ~ 18
      Cu≤ 1 (lower limit not stated)
      Mn≤ 2 (lower limit not stated)
      Mo2 ~ 3
      N≤ 0.1 (lower limit not stated)
      Ni10 ~ 14
      P≤ 0.045 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      WhatsApp Technical enquiry →