Material grade directory
5855 grades and 14528 source records with numerical compositions. Standards, editions and conditions are retained separately; these records do not establish interchangeability or a supply guarantee.
Material directory pages · 6 / 49
Filter this page; use the material query to search all grades.
0–9
- 20CRMNMO · 6 source records
- 20CRMNMOA · 1 source record
- 20CRMNMOAH · 1 source record
- 20CRMNMOE · 1 source record
- 20CRMNMOH · 4 source records
- 20CRMNSI · 5 source records
- 20CRMNSIA · 1 source record
- 20CRMNSIE · 1 source record
- 20CRMNTI · 5 source records
- 20CRMNTIA · 1 source record
- 20CRMNTIAH · 1 source record
- 20CRMNTIE · 1 source record
- 20CRMNTIH · 3 source records
- 20CRMO · 4 source records
- 20CRMO4 · 2 source records
- 20CRMO4+H · 1 source record
- 20CRMOA · 2 source records
- 20CRMOAH · 1 source record
- 20CRMOE · 1 source record
- 20CRMOH · 5 source records
- 20CRMOVTIB4-10 · 2 source records
- 20CRNI · 3 source records
- 20CRNI2MOAH · 1 source record
- 20CRNI2MOH · 2 source records
- 20CRNI3 · 3 source records
- 20CRNI3A · 1 source record
- 20CRNI3AH · 1 source record
- 20CRNI3E · 1 source record
- 20CRNI3H · 2 source records
- 20CRNIA · 1 source record
- 20CRNIE · 1 source record
- 20CRNIMO · 2 source records
- 20CRNIMOA · 1 source record
- 20CRNIMOAH · 1 source record
- 20CRNIMOE · 1 source record
- 20CRNIMOH · 4 source records
- 20CRS4 · 9 source records
- 20G · 5 source records · Original-source verification pending
- 20MN · 4 source records
- 20MN2 · 4 source records
- 20MN2A · 1 source record
- 20MN2E · 1 source record
- 20MN5 · 4 source records
- 20MNB4 · 11 source records
- 20MNB4-D · 3 source records
- 20MNB5 · 5 source records
- 20MNCR4-2 · 2 source records
- 20MNCR4-2+H · 1 source record
- 20MNCR5 · 5 source records
- 20MNCRMO4-2 · 2 source records
- 20MNCRMO4-2+H · 1 source record
- 20MNCRS5 · 9 source records
- 20MNG · 4 source records · Original-source verification pending
- 20MNMOB · 2 source records
- 20MNMOBA · 1 source record
- 20MNMOBE · 1 source record
- 20MNMONI4-5 · 1 source record
- 20MNNICRMO3-2 · 2 source records
- 20MNNICRMO3-2+H · 1 source record
- 20MNTIB · 2 source records
- 20MNTIBA · 1 source record
- 20MNTIBAH · 1 source record
- 20MNTIBE · 1 source record
- 20MNTIBH · 2 source records
- 20MNV · 3 source records
- 20MNVA · 1 source record
- 20MNVB · 2 source records
- 20MNVBA · 1 source record
- 20MNVBAH · 1 source record
- 20MNVBE · 1 source record
- 20MNVBH · 2 source records
- 20MNVE · 1 source record
- 20MNVS6 · 1 source record
- 20MOCR 4 · 1 source record · Original-source verification pending
- 20MOCR3 · 3 source records
- 20MOCR4 · 15 source records
- 20MOCRS3 · 3 source records
- 20MOCRS4 · 13 source records
- 20NICRMO13-4 · 1 source record
- 20NICRMO2 · 1 source record
- 20NICRMO2-2 · 16 source records
- 20NICRMO7 · 5 source records
- 20NICRMO7+H · 1 source record
- 20NICRMOS2 · 1 source record
- 20NICRMOS2-2 · 13 source records
- 20NICRMOS6-4 · 7 source records
- 20NIMO9-7 · 2 source records
- 20R · 1 source record · Original-source verification pending
- 20SIMN2MOV · 2 source records
- 20SIMN2MOVA · 1 source record
- 20SIMN2MOVE · 1 source record
- 2117 · 3 source records
- 2124 · 1 source record
- 21CR12MOV · 3 source records
- 21CRMOV5-7 · 2 source records
- 21MNCR5 · 2 source records
- 21NICRMO 2 · 1 source record · Original-source verification pending
- 21NICRMO2 · 1 source record · Original-source verification pending
- 21NICRMOS2 · 1 source record · Original-source verification pending
- 22 MNB4 · 1 source record
- 2205 · 14 source records · Original-source verification pending
- 2205 GRADE 420 · 2 source records
- 2205 GRADE 520 · 2 source records
- 2205 GRADE 550 · 2 source records
- 2205 GRADE 60 · 2 source records
- 2205 GRADE 75 · 2 source records
- 2205 GRADE 80 · 2 source records
- 220BH(CR220BH) · 1 source record · Original-source verification pending
- 2214 · 1 source record
- 2218 · 1 source record
- 2219 · 2 source records
- 22CR12NIWMOV · 2 source records
- 22CR20MN10NI2SI2N · 2 source records
- 22CR21NI12N · 2 source records
- 22CRMOAH · 1 source record
- 22CRMOH · 2 source records
- 22CRMOS 3-5 · 2 source records · Original-source verification pending
- 22CRMOS3-5 · 5 source records
- 22CRNIMOH · 1 source record
- 22MNB4 · 5 source records