← Back to the 11 process videos

Europe · EN / historical DIN: Cold heading wire: processes and delivery conditions

Read process sequences and delivery conditions by standard system. Confirm grade, product form, edition and acceptance requirements together.

Europe · EN / historical DIN

EN 10263-2/-3/-4/-5:2017 · DIN 1654:1989 (historical)

Keep +AC, +C and +LC distinct: spheroidizing, drawing and light drawing. +AC+C does not necessarily mean light drawing. Apply Parts 2, 3, 4 and 5 to their respective steel families and product forms; +FP is a bar condition. Stainless +AT solution treatment differs from +A soft annealing. +H, +HH, +HL and +CH concern hardenability or core hardening, not an annealing sequence.

+U
Hot rolling
EN 10263-2 Table 1: wire rod, bar
+U+PE
Hot rollingPeeling
EN 10263-2 Table 1: wire rod, bar
+U+C
Hot rollingCold drawing
EN 10263-2 Table 1: bar, wire
+U+C+AC
Hot rollingCold drawingSpheroidize annealing
EN 10263-2 Table 1: bar, wire
+U+C+AC+LC
Hot rollingCold drawingSpheroidize annealingLight drawing / skin passing
EN 10263-2 Table 1: bar, wire
+AC
Spheroidize annealing
EN 10263-2 Table 1: wire rod, bar
+AC+PE
Spheroidize annealingPeeling
EN 10263-2 Table 1: wire rod, bar
+AC+C
Spheroidize annealingCold drawing
EN 10263-2 Table 1: bar, wire
+U
Untreated
EN 10263-3 Table 1: wire rod, bar, wire
+AC
Spheroidize annealing
EN 10263-3 Table 1: wire rod, bar, wire
+FP
Controlled ferrite-pearlite structure and hardness
EN 10263-3 Table 1: bars only
+U
Untreated
EN 10263-4 Table 1: wire rod, bar
+AC
Spheroidize annealing
EN 10263-4 Table 1: wire rod, bar, wire
+A
Soft annealing
EN 10263-5 Table 1: ferritic and martensitic stainless steels; wire rod, bar, wire
+AT
Solution treatment
EN 10263-5 Table 1: austenitic and duplex stainless steels; wire rod, bar, wire
+C
Cold drawing
EN 10263-5 Table 2: wire rod, wire
+PE
Peeling
EN 10263-5Table2: Bars, Wire
+LC
Light drawing / skin passing
EN 10263-5Table2: Wire Only

Heat Treatment and Delivery Conditions

The following explains all 29 treatment-condition symbols in Table 18 of EN 10027-1:2016. Check the general meaning, the delivery conditions permitted by the relevant product standard and the actual processing sequence separately. These symbols do not all apply to cold-heading wire and do not define our supply capability.

EN 10027-1:2016 · Table 18

+A
Soft annealing to reduce hardness and improve subsequent processing.
+AC
Spheroidizing annealing: A process that transforms carbides in applicable steels into a spheroidal form.
+AR
As-rolled condition: No special rolling or heat treatment requirements are specified.
+AT
Solution treatment: Solid-solution annealing performed according to the applicable steel grade.
+C
Work-hardened condition: Achieved through cold working; the specific method depends on the product standard.
+Cnnn
Work hardened, with a minimum tensile strength specified as nnn MPa.
+CPnnn
Work hardened, with a minimum 0.2% proof strength specified as nnn MPa.
+CR
Cold-rolled condition.
+DC
The manufacturer selects the delivery condition, but the material must still meet the applicable standards and order requirements.
+FP
Treated to achieve the specified ferrite–pearlite microstructure and hardness range.
+HC
Hot rollingWork-hardened condition: Achieved through cold working; the specific method depends on the product standard.
+I
Isothermal treatment; microstructure and mechanical properties determined according to the relevant standard or technical agreement.
+LC
Skin-pass finishing by temper rolling or light drawing.
+M
Thermomechanical forming condition.
+N
Normalizing or normalized forming condition.
+NT
NormalizingTempering
+P
Precipitation-hardening condition, applicable to corresponding precipitation-hardening steel grades.
+Q
Quenched condition.
+QA
Air quenching.
+QO
Oil quenching.
+QT
QuenchingTempering
+QW
Water quenching.
+RA
Recrystallization annealing.
+S
Treatment to improve cold shearability.
+SR
Stress-relief treatment.
+T
Tempered condition.
+TH
Treated to achieve a specified hardness range.
+U
Not heat-treated; the specific original processing condition is confirmed according to the product standard.
+WW
Warm working condition.

+QT denotes the quenched-and-tempered (QT) condition, +Q indicates quenching only, and +T indicates tempering only; +N refers to normalizing or normalized forming, while +NT denotes normalizing followed by tempering. Materials delivered in the quenched-and-tempered state should be ordered separately from spheroidizing annealed materials supplied for subsequent quenching and tempering.

The objectives of the treatments represented by +A, +AC, +AT, +RA, and +SR differ: they address softening, carbide spheroidization, solid solution treatment, recrystallization, and stress relief, respectively; +I indicates isothermal treatment and does not allow one to infer microstructure or spheroidization rate solely from this symbol.

In this general designation table, +C means cold-work hardened; in product standards such as EN 10263, it denotes cold drawing. +LC means skin-pass finishing by temper rolling or light drawing. Interpret +M, +HC and +WW under the relevant product standard as well.

+Cnnn specifies a minimum tensile strength of nnn MPa; +CPnnn specifies a minimum 0.2% proof strength of nnn MPa. +TH identifies treatment to an agreed hardness range. Specify the values, test method and sampling position; +TH does not mean spheroidizing annealing.

Symbols with identical codes may have different meanings depending on the standard in which they appear. For example, in the EN 10027-1 table 17, +A, +S, and +T denote corresponding coatings, whereas in the 18 table, the same symbols represent treatment conditions. When placing an order, the product standard, steel grade, condition, and acceptance criteria must be specified simultaneously.

Bright steel processing conditions and their sequence

ISO 683-7:2023 and EN ISO 683-7:2024 cover the relevant non-alloy and alloy bright steel products. Their delivery conditions are distinct from those in the cold-heading product standard EN 10263. Check each combination against the applicable steel grade, product form, dimensions and mechanical-property table.

ISO 683-7:2023 · EN ISO 683-7:2024

+C
Cold drawing
+SH
Peeling / turning
+G
Grinding
+PL
Polishing
+C+G
Cold drawingGrinding
+C+PL
Cold drawingPolishing
+QT+SH
QuenchingTemperingPeeling / turning
+C+QT
Cold drawingQuenchingTempering
+QT+C
QuenchingTemperingCold drawing
+A+SH
Soft annealingPeeling / turning
+A+C
Soft annealingCold drawing
+FP+SH
Controlled ferrite-pearlite structure and hardnessPeeling / turning
+FP+C
Controlled ferrite-pearlite structure and hardnessCold drawing
+C+N
Cold drawingNormalizing
+C+A
Cold drawingSoft annealing
+C+FP
Cold drawingControlled ferrite-pearlite structure and hardness
+N+SH
NormalizingPeeling / turning

Hardening requirements and treatment conditions

+H, +HH, +HL and +CH specify hardenability or core-hardening acceptance requirements. They do not mean that the material is delivered in the quenched-and-tempered condition +QT. Check the Jominy end-quench limits, restricted bands, core hardness and applicable diameters under EN 10263-3/-4, clause 6.4, and ISO 4954-1, clause 7.1.4.

+H
Specifies a standard hardenability band; acceptance is based on the corresponding end-quench test hardness requirement.
+HH
Restricted hardenability band with the same upper limit as the corresponding +H band.
+HL
Restricted hardenability band with the same lower limit as the corresponding +H band.
+CH
Specifies core hardening requirements and verifies the corresponding maximum diameter and core hardness.

DIN and EN process notation

Historical DIN uses K for drawing and GKZ for spheroidizing. These combinations describe sequence; they are not all fixed delivery conditions in current EN standards. Agree repeated +AC+C+AC routes and any final +LC separately. C means drawing; LC explicitly means light drawing.

K
+U+C
K+GKZ
+U+C+AC
GKZ+K
+AC+C
K+GKZ+K
+U+C+AC+LC
GKZ+K+GKZ
+AC+C+AC
GKZ+K+GKZ+K
+AC+C+AC+LC

Specify the steel grade and standard edition, finished dimensions and tolerances, surface or coating, mechanical properties, spheroidization and decarburization requirements, inspection documents and heat traceability. Similar codes do not establish material interchangeability. Creation Group processes and supplies cold-heading wire; subsequent part forming and heat treatment are qualified for the customer's process requirements.

Standards and editions

WhatsApp Technical enquiry →
Image and content use · Creation Group