← Back to the 11 process videos

Japan · JIS: Cold heading wire: processes and delivery conditions

Read process sequences and delivery conditions by standard system. Confirm grade, product form, edition and acceptance requirements together.

Japan · JIS

JIS G 3507-2:2005 Table 1 (3), §5 · JIS G 3508-2:2005 · JIS G 3509-2:2003

DA includes cold working, annealing and final cold working, or annealing of rod followed by cold working. It does not by itself require spheroidizing. Confirm commercial AD/DAD notation operation by operation. R/A/K in SWCH grades describe deoxidation, separately from D/DA processing. Check the boron and low-alloy wire standards G 3508-2 and G 3509-2 separately.

D
Wire rodCold drawing
JIS G 3507-2 Table 1, note (3)
DA
Wire rodCold drawingAnnealingCold drawing
JIS G 3507-2 Table 1, note (3)
DA
Wire rodAnnealingCold drawing
JIS G 3507-2 Table 1, note (3)
D · G 3508-2
Wire rodCold drawing
JIS G 3508-2:2005 · Table 1 (2) · SWCHB223 / 320 / 420 / 526 / 620
DA · G 3508-2
Wire rodCold drawingAnnealingCold drawing
JIS G 3508-2:2005 · Table 1 (2)
DA · G 3508-2
Wire rodAnnealingCold drawing
JIS G 3508-2:2005 · Table 1 (2)
DA1 · G 3509-2
AnnealingCold drawing
JIS G 3509-2:2003 §3, Table 1 (3)
DA2 · G 3509-2
Cold drawingAnnealingCold drawing
JIS G 3509-2:2003 §3, Table 1 (3)
DA3 · G 3509-2
AnnealingCold drawingAnnealingCold drawing
JIS G 3509-2:2003 §3, Table 1 (3)

Specify the steel grade and standard edition, finished dimensions and tolerances, surface or coating, mechanical properties, spheroidization and decarburization requirements, inspection documents and heat traceability. Similar codes do not establish material interchangeability. Creation Group processes and supplies cold-heading wire; subsequent part forming and heat treatment are qualified for the customer's process requirements.

Standards and editions

WhatsApp Technical enquiry →
Image and content use · Creation Group