China · GB: Cold heading wire: processes and delivery conditions

Read process sequences and delivery conditions by standard system. Confirm grade, product form, edition and acceptance requirements together.

China · GB

GB/T 5953.1-2009 §3.2 · GB/T 5953.2-2009 §3 · GB/T 5953.3-2012 §3 · GB/T 5953-2026

HD is cold drawn; SA adds spheroidizing after drawing; SALD adds final light drawing; ASALD adds an earlier anneal. GB/T 5953.1-2009 covers four conditions, while Part 2 covers HD and SALD. GB/T 5953-2026 takes effect on 1 December 2026. Specify the edition in the order. GB/T 5953.3-2012: HD. GB/T 6478: Bar / Wire rod. GB/T 28906: Wire rod.

HD
Cold drawing
GB/T 5953.1; Part 2 covers HD and SALD
SA
Cold drawingSpheroidize annealing
GB/T 5953.1; Part 2 covers HD and SALD
SALD
Cold drawingSpheroidize annealingLight drawing / skin passing
GB/T 5953.1; Part 2 covers HD and SALD
ASALD
AnnealingCold drawingSpheroidize annealingLight drawing / skin passing
GB/T 5953.1; Part 2 covers HD and SALD

Specify the steel grade and standard edition, finished dimensions and tolerances, surface or coating, mechanical properties, spheroidization and decarburization requirements, inspection documents and heat traceability. Similar codes do not establish material interchangeability. Creation Group processes and supplies cold-heading wire; subsequent part forming and heat treatment are qualified for the customer's process requirements.