← BackMaterial grade directory

22 MNB4

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 22 MNB4 →

22 MnB4 · EN 10263

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Drawn wire
Original record status
Reference transcription of standard
Standard edition
BS EN 10263-3:2017
Table / clause
Table 3

Carbon-equivalent reference

IIW / CEV:0.3500–0.4567Known-element contribution; incomplete value; missing Cr, Mo, V, Ni CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2490–0.3475Known-element contribution; incomplete value; missing Cr, Ni, Mo, V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2900–0.3725Known-element contribution; incomplete value; missing Mo, Cr, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.2 ~ 0.24
Si≤ 0.3 (lower limit not stated)
Mn0.9 ~ 1.2
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
B0.0008 ~ 0.005
Cu≤ 0.25 (lower limit not stated)

Applicability and limitations

BS EN 10263-3:2017; Heat analysis, mass percent; Values without a stated range are maxima; Notes below the table are retained. No edition is stated on the website; Displayed under this source edition; contract applicability is not established

Verification notes

Standard source: BS EN 10263-3:2017 · Table 3View associated products →