← BackMaterial grade directory

20MOCRS3

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for 20MOCRS3 →

20MoCrS3 · DIN EN 10084-2008

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10084-2008
Table / clause
Table 3, notes a–d

Carbon-equivalent reference

IIW / CEV:0.4100–0.6000Known-element contribution; incomplete value; missing V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2400–0.3500Known-element contribution; incomplete value; missing Cu, Ni, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Si≤ 0.4 (lower limit not stated)
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.04
Cr0.4 ~ 0.7
Mo0.3 ~ 0.4

Applicability and limitations

Ladle analysis, mass fraction wt%; the DIN EN 10084:2008-06 cover expressly identifies the German edition of EN 10084:2008; Table 3 follows that source text. Note b: minor composition deviations associated with hardenability requirements must be checked separately against Table 4 and the applicable conditions; they do not widen default ranges, and no such relaxation applies to P/S. Note c: higher S (approximately up to 0.10%) or Pb may be requested for improved machinability; in the higher-S case, the Mn upper limit may increase by 0.15 percentage points. Actual agreed values are not given; do not invent them or apply them automatically. Note d: B in this table improves toughness in the hardened case, not hardenability. Unlisted elements must not be intentionally added without purchaser approval (except as necessary during steelmaking); unspecified does not mean zero. A delivery standard for case-hardening steel does not mean all conditions are suitable for cold heading; verify mechanical properties, hardness and hardenability separately.

Verification notes

Original German Table 3 and its footnotes checked

Jominy end-quench hardenability (conditional requirements)

EN 10084:2008 · DIN EN 10084:2008-06, cover explicitly states German version of EN 10084:2008 · Table 5/Table 6/Table 8/Table 9; 7.1.2 and 8.2.2 · PDF pages 7, 10, 12, 18, 19, 22, 23

+H Normal hardenability band (7.1.2; applies to alloy steels in this standard unless otherwise agreed)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54149
33847
53445
72840
92235
112032
13Unspecified; do not treat as 031
15Unspecified; do not treat as 030
20Unspecified; do not treat as 028
25Unspecified; do not treat as 026
30Unspecified; do not treat as 025
35Unspecified; do not treat as 024
40Unspecified; do not treat as 023

+HH Restricted hardenability band (Table 6; agreement at enquiry and order required)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54449
34147
53845
73240
92635
112432
132331
152230
202028
25Unspecified; do not treat as 026
30Unspecified; do not treat as 025
35Unspecified; do not treat as 024
40Unspecified; do not treat as 023

+HL Restricted hardenability band (Table 6; agreement at enquiry and order required)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54146
33844
53441
72836
92231
112028
13Unspecified; do not treat as 027
15Unspecified; do not treat as 026
20Unspecified; do not treat as 024
25Unspecified; do not treat as 022
30Unspecified; do not treat as 021
35Unspecified; do not treat as 020
40Unspecified; do not treat as 0Unspecified; do not treat as 0

20MoCrS3 · EN 10084-2008

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10084-2008
Table / clause
Table 3, notes a–d

Carbon-equivalent reference

IIW / CEV:0.4100–0.6000Known-element contribution; incomplete value; missing V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2400–0.3500Known-element contribution; incomplete value; missing Cu, Ni, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Si≤ 0.4 (lower limit not stated)
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.04
Cr0.4 ~ 0.7
Mo0.3 ~ 0.4

Applicability and limitations

Ladle analysis, mass fraction wt%; the DIN EN 10084:2008-06 cover expressly identifies the German edition of EN 10084:2008; Table 3 follows that source text. Note b: minor composition deviations associated with hardenability requirements must be checked separately against Table 4 and the applicable conditions; they do not widen default ranges, and no such relaxation applies to P/S. Note c: higher S (approximately up to 0.10%) or Pb may be requested for improved machinability; in the higher-S case, the Mn upper limit may increase by 0.15 percentage points. Actual agreed values are not given; do not invent them or apply them automatically. Note d: B in this table improves toughness in the hardened case, not hardenability. Unlisted elements must not be intentionally added without purchaser approval (except as necessary during steelmaking); unspecified does not mean zero. A delivery standard for case-hardening steel does not mean all conditions are suitable for cold heading; verify mechanical properties, hardness and hardenability separately.

Verification notes

The official German edition of DIN expressly adopts EN10084:2008; Table 3 and footnotes have been checked

Jominy end-quench hardenability (conditional requirements)

EN 10084:2008 · DIN EN 10084:2008-06, cover explicitly states German version of EN 10084:2008 · Table 5/Table 6/Table 8/Table 9; 7.1.2 and 8.2.2 · PDF pages 7, 10, 12, 18, 19, 22, 23

+H Normal hardenability band (7.1.2; applies to alloy steels in this standard unless otherwise agreed)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54149
33847
53445
72840
92235
112032
13Unspecified; do not treat as 031
15Unspecified; do not treat as 030
20Unspecified; do not treat as 028
25Unspecified; do not treat as 026
30Unspecified; do not treat as 025
35Unspecified; do not treat as 024
40Unspecified; do not treat as 023

+HH Restricted hardenability band (Table 6; agreement at enquiry and order required)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54449
34147
53845
73240
92635
112432
132331
152230
202028
25Unspecified; do not treat as 026
30Unspecified; do not treat as 025
35Unspecified; do not treat as 024
40Unspecified; do not treat as 023

+HL Restricted hardenability band (Table 6; agreement at enquiry and order required)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54146
33844
53441
72836
92231
112028
13Unspecified; do not treat as 027
15Unspecified; do not treat as 026
20Unspecified; do not treat as 024
25Unspecified; do not treat as 022
30Unspecified; do not treat as 021
35Unspecified; do not treat as 020
40Unspecified; do not treat as 0Unspecified; do not treat as 0

20MoCrS3 · NF EN 10084-2008

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Adopted-standard basis verified
Standard edition
EN 10084-2008
Table / clause
Table 3, notes a–d

Carbon-equivalent reference

IIW / CEV:0.4100–0.6000Known-element contribution; incomplete value; missing V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2400–0.3500Known-element contribution; incomplete value; missing Cu, Ni, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2800–0.3950Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Si≤ 0.4 (lower limit not stated)
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S0.02 ~ 0.04
Cr0.4 ~ 0.7
Mo0.3 ~ 0.4

Applicability and limitations

Ladle analysis, mass fraction wt%; the DIN EN 10084:2008-06 cover expressly identifies the German edition of EN 10084:2008; Table 3 follows that source text. Note b: minor composition deviations associated with hardenability requirements must be checked separately against Table 4 and the applicable conditions; they do not widen default ranges, and no such relaxation applies to P/S. Note c: higher S (approximately up to 0.10%) or Pb may be requested for improved machinability; in the higher-S case, the Mn upper limit may increase by 0.15 percentage points. Actual agreed values are not given; do not invent them or apply them automatically. Note d: B in this table improves toughness in the hardened case, not hardenability. Unlisted elements must not be intentionally added without purchaser approval (except as necessary during steelmaking); unspecified does not mean zero. A delivery standard for case-hardening steel does not mean all conditions are suitable for cold heading; verify mechanical properties, hardness and hardenability separately.

Verification notes

The official adoption relationship for NF and original EN10084:2008, Table 3 have been checked; The complete main text of NF has not been checked page by page

Jominy end-quench hardenability (conditional requirements)

EN 10084:2008 · DIN EN 10084:2008-06, cover explicitly states German version of EN 10084:2008 · Table 5/Table 6/Table 8/Table 9; 7.1.2 and 8.2.2 · PDF pages 7, 10, 12, 18, 19, 22, 23

+H Normal hardenability band (7.1.2; applies to alloy steels in this standard unless otherwise agreed)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54149
33847
53445
72840
92235
112032
13Unspecified; do not treat as 031
15Unspecified; do not treat as 030
20Unspecified; do not treat as 028
25Unspecified; do not treat as 026
30Unspecified; do not treat as 025
35Unspecified; do not treat as 024
40Unspecified; do not treat as 023

+HH Restricted hardenability band (Table 6; agreement at enquiry and order required)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54449
34147
53845
73240
92635
112432
132331
152230
202028
25Unspecified; do not treat as 026
30Unspecified; do not treat as 025
35Unspecified; do not treat as 024
40Unspecified; do not treat as 023

+HL Restricted hardenability band (Table 6; agreement at enquiry and order required)

End-quench test temperature 880 °C (tolerance not stated in the source); this is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.54146
33844
53441
72836
92231
112028
13Unspecified; do not treat as 027
15Unspecified; do not treat as 026
20Unspecified; do not treat as 024
25Unspecified; do not treat as 022
30Unspecified; do not treat as 021
35Unspecified; do not treat as 020
40Unspecified; do not treat as 0Unspecified; do not treat as 0