2205 Grade 520 · ASTM A955/A955M-2020(c)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A955/A955M-2020(c)
Table / clause
Table 2 notes A–E; clauses 1.2,1.6,4.1.3/4.1.6,6.1
PDF page references
1、3、4

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr21.0 ~ 23.0
Ni4.5 ~ 6.5
Mo2.5 ~ 3.5
N0.08 ~ 0.2

Applicability and limitations

The composition alloy in this record is S31803

2205. Table 2 gives heat-analysis mass fractions wt%; values other than ranges are maxima. Ellipses indicate no requirement and are not entered as zero. Alloy type UNS and strength grade Grade are recorded separately; 60/75/80 uses the ksi system and 420/520/550 uses the MPa system. The alloy cannot be inferred from the strength grade. The name 2205 can correspond to S31803 or S32205; each must be used under its confirmed UNS, and the two composition ranges must not be combined. This standard concerns concrete reinforcement; applicability as a supplied cold-heading product is not established.

Verification notes

Official English 20c Table 2, footnotes and applicable clauses checked item by item.

2205 Grade 520 · ASTM A955/A955M-2020(c)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A955/A955M-2020(c)
Table / clause
Table 2 notes A–E; clauses 1.2,1.6,4.1.3/4.1.6,6.1
PDF page references
1、3、4

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr22.0 ~ 23.0
Ni4.5 ~ 6.5
Mo3.0 ~ 3.5
N0.14 ~ 0.2

Applicability and limitations

The composition alloy in this record is S32205

2205. Table 2 gives heat-analysis mass fractions wt%; values other than ranges are maxima. Ellipses indicate no requirement and are not entered as zero. Alloy type UNS and strength grade Grade are recorded separately; 60/75/80 uses the ksi system and 420/520/550 uses the MPa system. The alloy cannot be inferred from the strength grade. The name 2205 can correspond to S31803 or S32205; each must be used under its confirmed UNS, and the two composition ranges must not be combined. This standard concerns concrete reinforcement; applicability as a supplied cold-heading product is not established.