Products/EN 10263

MATERIAL DATA · COLD FORMING

X5CrNiMo17-12-2 Cold-drawn steel wire

Reference technical data for X5CrNiMo17-12-2. Source edition: EN 10263-5:2017. Read chemistry, delivery conditions and properties with their cited limits and notes. The applicable edition and acceptance requirements must be confirmed in the order technical agreement.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

X5CrNiMo17-12-2 Cold-drawn steel wire product image
X5CrNiMo17-12-2 · Cold-drawn steel wire
01Applicable standardEN 10263-5:2017
02Material gradeX5CrNiMo17-12-2
03Product formCold-drawn steel wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Delivery conditions and applicable requirements

Table 1 – Delivery conditions, product forms and applicable requirements

Heat-treatment conditionSymbolBarWire rodWireFerriticMartensiticAustenitic and austenitic-ferritic
Soft annealed+AXXXXX—
Solution annealed+ATXXX——X
Basis of orderApplicable requirements
Chemical compositionTable 3
Mechanical propertiesTable 5, 6, 7 or 8, depending on the steel grade
Supplementary or special requirementsEN 10263-1:2017, Annex A, if agreed at the time of enquiry and order.

Table 2 – Surface condition at delivery

Surface conditionSymbolBarWire rodWire
Cold drawn+C—XX
Peeled+PEX—X
Lightly drawn+LC——X

X = applicable; — = not applicable. Other delivery conditions may be agreed at the time of enquiry and order.

Heat-treatment condition, steel structure group and surface condition must be distinguished. This table is a standard reference and does not confirm actual supply.

Source: EN 10263-5:2017, Table 1 and 2, page 8–9 (PDF page 10–11).

2. Chemical composition

Table 3 – Chemical composition of stainless steels (cast analysis)

Reference requirements for X5CrNiMo17-12-2, steel number 1.4401. These are not analysis results for a particular heat. The order standard and requirements for raw material and finished product must be confirmed separately.

ElementMass fraction, %
C≤0.07
Si≤1.00
Mn≤2.00
P≤0.045
S≤0.030
Cr16.5–18.5
Mo2.00–2.50
Ni10.0–13.0
N≤0.10
Cu≤1.00
Other elements—

Elements not listed must not be intentionally added without the purchaser’s agreement, except for finishing the heat. Precautions are required to prevent additions from scrap and other production materials that could impair mechanical properties or the suitability of the steel.

Values are maximum limits unless a range or other qualification is given. A dash or blank source field supplies no numerical value and does not mean zero.

Note b: For machinability, controlled S of 0.015–0.030% is recommended and permitted. For weldability, controlled S of 0.008–0.030% is recommended and permitted. For polishability, S ≤0.015% is recommended.

Table 4 – Permissible deviations for product analysis

ElementLimiting values for cast analysis, %Permissible deviation for product analysis, %
C≤0.030+0.005
C>0.030 and ≤0.15±0.01
Si≤1.00+0.05
Si>1.00 and ≤2.00+0.10
Mn≤1.00+0.03
Mn>1.00 and ≤2.00±0.04
P≤0.045+0.005
S≤0.015+0.003
S>0.015 and ≤0.030+0.005
N≤0.22±0.01
Cr≥11.5 and <15.0±0.15
Cr≥15.0 and ≤20.0±0.20
Cr>20.0 and ≤23.0±0.25
Cu≤1.00+0.07
Cu>1.00 and ≤4.0±0.10
Mo<1.75±0.05
Mo≥1.75 and ≤3.5±0.10
Ni≤1.00+0.03
Ni>1.00 and ≤5.0±0.07
Ni>5.0 and ≤10.0±0.10
Ni>10.0 and ≤14.0±0.15
Ti≤0.70±0.05

± means that, within one heat, the product analysis for a given element may deviate above the upper limit or below the lower limit in Table 3, but not both at the same time.

Source: EN 10263-5:2017, Table 3 on page 10 (PDF page 12), and Table 4 on page 12 (PDF page 14). These tables do not replace the complete standard.

3. Mechanical properties

Table 5 – Mechanical properties of austenitic stainless steels in the specified delivery condition

Steel nameSteel numberDiameterDelivery condition
+AT or +AT+PE+AT+C+AT+C+AT+AT+C+AT+LC
over, mmup to and including, mmRm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %
X5CrNiMo17-12-21.440125————6906574060
X5CrNiMo17-12-21.440151066065830—6706572060
X5CrNiMo17-12-21.4401102566065790—66065——
X5CrNiMo17-12-21.4401255066065——————

Source: EN 10263-5:2017, Table 5, page 13. Rm is tensile strength; Z is reduction of area at fracture. The values apply to the specified diameter intervals and delivery conditions. A dash does not mean zero or confirm availability.

Table 9 – Permissible depth of surface defects

Diameter in the delivery condition, mmMaximum permissible defect depth, mm
≤100.10
>101% of the diameter

For diameters below 5 mm, the permissible depth of surface defects must be reduced in proportion to the diameter reduction during cold drawing.

For ferritic, martensitic and austenitic-ferritic steels, larger values may be agreed at the time of enquiry and order.

Source: EN 10263-5:2017, Table 9, page 15 (PDF page 17).

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — X5CrNiMo17-12-2

Basis: EN 10263

Chemical composition source: Original standard not yet verified

Original standard not yet verified

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group