PROFILE DEVELOPMENT / SUJ2
SUJ2 engine timing-chain trapezoidal pin
This case presents trapezoidal profile wire SUJ2 for trapezoidal pins used in engine timing chains. The page includes 4 photographs of samples and a 24-second conceptual assembly video showing the pin, timing chain assembly, and its position within the engine; cross-section geometry and subsequent processing requirements are to be confirmed per drawing.

Geometric Focus Points
Top and bottom widths, height, side angles, and fillets
Angle, parallelism of the base edge, and cross-sectional orientation
Confirm technical requirements based on the drawing
Conceptual illustration of trapezoidal pin, timing chain, and engine positioning.
Cross-sectional features and review points
Wire for trapezoidal pins must be specified with distinction between top and bottom bases, cross-sectional height, and two inclined sides; side angles and corner radii jointly define the profile contour. The product name indicates application orientation; specific chain type, part dimensions, and delivery form remain subject to confirmation per project drawings.
Drawings and measurement requirements
Recommend clarifying upper/lower base nomenclature, dimensional tolerances, height datum, sidewall angles, and fillet requirements—do not conflate base width with slanted side length.
Delivery and subsequent processing
SUJ2 is the raw material designation; standard revision level, heat treatment, hardness, and surface requirements must be confirmed separately per project and cannot be inferred from grade alone.
Documentation basis and scope of confirmation
Data originates from this case’s catalog and internal sample photographs; catalog dimensions are nominal values, and photographs do not substitute formal inspection reports. Material standards, mechanical properties, heat treatment, supply conditions, and acceptance criteria must be confirmed per project.
Photo recording
Development Q&A
For trapezoidal wire, must both top and bottom base widths be specified?
Specify upper base, lower base, height, and side relationships; the specific dimensions and angles used for definition must form a consistent, measurable datum in the drawing.
Has heat treatment or hardness been confirmed for the SUJ2 designation?
No. Material identification, heat treatment, hardness, mechanical properties, and delivery condition are distinct items and must be confirmed individually in technical specifications.
Related cross-sectional cases
Material data and technical communication
Technical requirements must include cross-sectional drawing and revision, critical tolerances, subsequent processing steps, delivery form, and inspection requirements.
View material selection documentation Submit technical requirements ↗