PROFILE DEVELOPMENT / DT4C
Soft magnetic pure iron profile wire for solenoid valve cores
DT4C 0.9 × 4.55 Soft Magnetic Pure Iron Profile Wire for Solenoid Valve Cores: Thin flat-shaped sample record. This case retains DT4C material designation and catalogued dimensions 0.9 × 4.55 mm, classified as thin flat. Thickness, width, and edge transition are key cross-sectional communication points.

Geometric Focus Points
Thin-edge thickness, width, and edge transitions
Thickness uniformity, edge shape, and surface condition
Confirm technical requirements based on the drawing
Cross-sectional features and review points
This case retains material identification DT4C and catalog dimensions 0.9 × 4.55 mm, classified as thin flat. Thickness, width, and edge transitions are key aspects for cross-sectional communication.
Drawings and measurement requirements
Recommend specifying measurement location for thin-edge thickness, width datum, edge geometry, and surface inspection requirements; measurements shown in photographs do not equate to formal tolerance acceptance.
Delivery and subsequent processing
If the project involves electromagnetic or other functional performance, provide corresponding specifications, states, and test bases separately—performance compliance cannot be inferred from DT4C designation or cross-sectional photographs.
Documentation basis and scope of confirmation
Data originates from this case’s catalog and internal sample photographs; catalog dimensions are nominal values, and photographs do not substitute formal inspection reports. Material standards, mechanical properties, heat treatment, supply conditions, and acceptance criteria must be confirmed per project.
Photo recording
Development Q&A
Is 0.9 × 4.55 a verified, conforming measurement result?
Nominal dimensions on this page follow the catalog; compliance with tolerances requires formal inspection records and agreed-upon acceptance criteria.
Can DT4C sample photographs demonstrate functional performance?
No. Material designation and external geometry cannot substitute functional performance testing; relevant parameters and test conditions must be confirmed separately.
Related cross-sectional cases
Material data and technical communication
Technical requirements must include cross-sectional drawing and revision, critical tolerances, subsequent processing steps, delivery form, and inspection requirements.
View material selection documentation Submit technical requirements ↗