ENGINEERING MATERIAL DATABASE
Material selector and grade comparison Filter cold-forming materials by standard, grade, material family, alloying elements, available technical data and application, then compare candidate grades.
Reference data
Find grades from measured chemistry Enter a heat-analysis result in mass percent. The system ranks records with stated composition limits, calculates CE(IIW), and identifies the information still needed for a cold-heading quotation.
Method reference
Carbon equivalent — CE(IIW) — CE(IIW) = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. It is a weldability screening indicator, not a cold-heading approval or a bolt strength-class calculation.
Filter & Compare
Find a suitable starting point The selector narrows the published material catalogue. Final grade, standard edition, delivery condition and acceptance criteria must still be confirmed by the technical team.
Grade, standard or alloying element
Standard family Alle Optionen GB JIS ISO ASTM / SAE / IFI EN / DIN Kundenzeichnung / technische Vereinbarung
Produktform Alle Optionen Wire rod Cold-drawn wire CHQ wire Shaped wire Shaped tube Cold-forming material Reference material data
Material family Alle Optionen Carbon steel Boron steel Alloy steel Shaped wire Shaped tube
Kennzeichnende Elemente der Werkstoffbezeichnung Alle Optionen Si Mn Cr Ni Mo B S Al Ti V Cu Nb W
Applications Alle Optionen Industrial cold forming Automobilindustrie Bauwesen Precision electronics Aerospace Maschinenbau Custom development Fasteners
Available technical data Alle Optionen Chemical composition Mechanical properties Hardenability Microstructure Decarburization Surface quality Dimensions and tolerances Delivery condition
Clear filters
Creation Group published material data takes priority. Supplementary reference data is clearly marked and supports screening only; it is not an approved engineering recommendation.
Materialdaten werden geladen…
Load more Compare
Grade comparison Selected materials
You can compare up to three materials at one time.
Start comparison Clear all