| ID | Grade | C | Si | Mn | P | S | Cr | Mo | B | Alt | Diğerleri |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 15 | SAE1019 | 0.15~0.20 | ≤0.10 | 0.60~0.90 | ≤0.020 | ≤0.020 | - | - | - | ≥0.020 | - |
MATERIAL DATA · COLD FORMING
SAE/AISI 1019(IFI-1019) Soğuk şekillendirme çelik teli
SAE/AISI 1019 (IFI-1019) soğuk başlık çelik teli teknik bilgileri, uygulanan standart ISO 4954-Ek A’dır. Mevcut sınıfın kimyasal bileşimi, mekanik özellikleri ve ilgili teknik gereklilikleri inceleyin.

01StandardSAE A510 / ASTM A510
02GradeSAE/AISI 1019(IFI-1019)
03Product formCold heading wire
04Delivery noteConfirmed by order specification
STANDARD & PROPERTIES
Material technical data
Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.
Enquire this gradeTECHNICAL NOTE
Application and ordering note
Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.
RFQ CHECKLIST
What to include in the enquiry
- Grade and applicable standard
- Diameter or section, delivery condition and quantity
- Drawing, forming route or failure photos when available
- Testing, certificate or report requirements
RELATED CAPABILITIES