| ID | 鋼種 | C | Si | Mn | P | S | Cr | Mo | B | Alt | その他 |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 15 | SAE1019 | 0.15~0.20 | ≤0.10 | 0.60~0.90 | ≤0.020 | ≤0.020 | - | - | - | ≥0.020 | - |
MATERIAL DATA · COLD FORMING
SAE/AISI 1019(IFI-1019) 冷間圧造用鋼線
SAE/AISI 1019(IFI-1019) 冷間圧造用鋼線技術資料、適用規格は ISO 4954-附属書A。当該鋼種の化学成分、機械的性質及び関連技術要求を参照。

01StandardSAE A510 / ASTM A510
02GradeSAE/AISI 1019(IFI-1019)
03Product formCold heading wire
04Delivery noteConfirmed by order specification
STANDARD & PROPERTIES
Material technical data
Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.
Enquire this gradeTECHNICAL NOTE
Application and ordering note
Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.
RFQ CHECKLIST
What to include in the enquiry
- Grade and applicable standard
- Diameter or section, delivery condition and quantity
- Drawing, forming route or failure photos when available
- Testing, certificate or report requirements
RELATED CAPABILITIES