| ID | 등급 | C | Si | Mn | P | S | Cr | Mo | B | 냉간압조 | 기타 |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 15 | SAE1019 | 0.15~0.20 | ≤0.10 | 0.60~0.90 | ≤0.020 | ≤0.020 | - | - | - | ≥0.020 | - |
MATERIAL DATA · COLD FORMING
SAE/AISI 1019(IFI-1019) 냉간압조용 강선
SAE/AISI 1019(IFI-1019) 냉간압조용 강선 기술 자료로, 적용 기준은 ISO 4954-부록A입니다. 해당 등급의 화학성분, 기계적 성질 및 관련 기술 요구사항을 확인하십시오.

01StandardSAE A510 / ASTM A510
02GradeSAE/AISI 1019(IFI-1019)
03Product formCold heading wire
04Delivery noteConfirmed by order specification
STANDARD & PROPERTIES
Material technical data
Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.
Enquire this gradeTECHNICAL NOTE
Application and ordering note
Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.
RFQ CHECKLIST
What to include in the enquiry
- Grade and applicable standard
- Diameter or section, delivery condition and quantity
- Drawing, forming route or failure photos when available
- Testing, certificate or report requirements