Products/JIS G4805

MATERIAL DATA · COLD FORMING

SUJ4 Steel for cold forming

Technical data for SUJ4 Steel for cold forming, compliant with JIS G4805. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

SUJ4 Steel for cold forming
SUJ4 · Steel for cold forming
01Applicable standardJIS G4805
02Material gradeSUJ4
03Product formSteel for cold forming
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 -- Chemical Composition, %

GradeCSiMnPSCrMoNiCu a)
SUJ40.95~1.100.15~0.35≤0.50≤0.025≤0.0251.30~1.600.10~0.25≤0.25≤0.25
Elements not specified in this table shall not be intentionally added except for the purpose of finishing the molten steel, unless agreed upon between the parties involved. Note a) The Cu content in wire rod shall be 0.20% or less.
Elements not specified in this table shall not be intentionally added except for steelmaking purposes; any such addition shall be determined by agreement between the supplier and the purchaser.
Note a) The Cu content in wire rod shall be 0.20% or less.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

3. Dimensional Tolerances

4. Permissible Limits for Total Decarburized Layer Depth

Table 9 - Permissible Limits for Total Decarburized Layer Depth (Cold-Drawn Steel)

Cold-Drawn Round BarCold-Drawn Wire
DiameterTotal decarburized layer depth from the surfaceDiameterTotal decarburized layer depth from the surface
<15<0.20≤7<0.05
15<d≤25<0.257<d≤15<0.08
25<d≤35<0.3015<d≤20<0.10
Permissible tolerances for cold-drawn round steel with diameters exceeding 35 mm and cold-drawn steel wire with diameters exceeding 20 mm shall be subject to agreement between the supplier and the purchaser.

5. Hardness

Table 10 – Spheroidizing annealing hardness (rolled steel for machining)

GradeHardness
HBWHRBHV
SUJ2,SUJ4<201<94<218
For hot-rolled steel for machining that has undergone spheroidizing annealing, testing is performed in accordance with Clause 14.3, and hardness is expressed as Brinell hardness (HBW), Rockwell hardness (HRBW), or Vickers hardness (HV) as specified in Table 10. However, Vickers hardness (HV) applies only to diameters of 17 mm or less. The hardness of cold-drawn steel and the low-temperature annealing hardness of steel for forging shall be subject to agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — SUJ4

Basis: JIS G4805

Chemical composition source: JIS G 4805:2008

Transcribed from the cited standard

Original source wording

Table 1

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 1.2300–1.5833

Missing elements: V

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 1.0267–1.2475

Missing elements: V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Calculated range: 1.0250–1.2713

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group