- Material form
- Wire rod
- Original record status
- Reference transcription of standard
- Standard edition
- JIS G 4805:2008
- Table / clause
- Table 1
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.95 ~ 1.1 |
| Si | 0.15 ~ 0.35 |
| Mn | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 1.3 ~ 1.6 |
| Mo | 0.1 ~ 0.25 |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
JIS G 4805:2008; Heat analysis, mass percent; See the original page for table notes and applicability conditions. This record concerns wire rod, under note a, Cu≤0.20%; Non-wire-rod maximum 0.25%. No edition is stated on the website; Displayed under this source edition; contract applicability is not established
Verification notes
Standard source: JIS G 4805:2008 · Table 1View associated products →SUJ4 · JIS G 4805:2008
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- High-carbon chromium bearing steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- JIS G 4805:2008
- Table / clause
- Table 1 and notes a–d; 4c
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
Wire rod, heat analysis, Table 1, note a Cu≤0.20%
Steel products other than wire rod, heat analysis, Table 1, note a Cu≤0.25%
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.95 ~ 1.1 |
| Si | 0.15 ~ 0.35 |
| Mn | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 1.3 ~ 1.6 |
| Mo | 0.1 ~ 0.25 |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
Applicability and limitations
Table 1 Heat analysis, unit mass fraction %. ; Note a: Ni/Cu each ≤0.25%, with Cu≤0.20% for wire rod.. ; Note b: except for the purpose of deoxidation, elements not specified shall not be intentionally added without agreement between both parties; Agreement may allow addition of elements outside the table up to 0.25%, which cannot be presumed as a general guaranteed upper limit for all residual elements. ; Note c: When product analysis is required by the purchaser, it shall be tested according to 14.1; permissible deviations shall be per JIS G0321 Table 4; Heat analysis limits cannot be directly used as product analysis tolerances. ; Note d: Mo impurity for SUJ2/3 ≤0.08%. ; Under 4c, spheroidizing annealing is normally performed but may be omitted when specified by the purchaser.; This manufacturing condition clause itself is not proof that all parts are suitable for cold heading.
Original condition-branch records
Wire rod, heat analysis, Table 1, note a Cu≤0.20%
| Element | Composition requirement |
|---|---|
| C | 0.95 ~ 1.1 |
| Si | 0.15 ~ 0.35 |
| Mn | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 1.3 ~ 1.6 |
| Mo | 0.1 ~ 0.25 |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Steel products other than wire rod, heat analysis, Table 1, note a Cu≤0.25%
| Element | Composition requirement |
|---|---|
| C | 0.95 ~ 1.1 |
| Si | 0.15 ~ 0.35 |
| Mn | ≤ 0.5 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 1.3 ~ 1.6 |
| Mo | 0.1 ~ 0.25 |
| Ni | ≤ 0.25 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |