Products/Customer drawing / technical agreement

MATERIAL DATA · COLD FORMING

Custom shaped wire for knitting machine parts

Material selection for Custom shaped wire for knitting machine parts. The material grade, standard edition, delivery condition and acceptance requirements are confirmed in the order and technical agreement.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

Custom shaped wire for knitting machine parts product image
Custom shaped wire for knitting machine parts · Custom shaped wire
01Applicable standardCustomer drawing / technical agreement
02Application / sectionCustom shaped wire for knitting machine parts
03Product formCustom shaped wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this product

1. Available material list

ApplicationsMaterial No.DIN EN ISOASTM/AISIJIS
1.0304AISI 1008SWRM 8
1.031AISI 1010SWRM 10
1.0541AISI 1040SWRH 42A
1.0517AISI 1045SWRH 47A
1.0609SWRH 57A
1.0611SWRH 62A
1.0620SWRH 77B
1.0626SWRH 82A
1.0737AISI 12L14SUM24L
1.0762AISI 1144SUM43
1.7243SAE 4118SCM415
1.7220SAE 4135SCM435
1.722542CrMo4SAE 4140SCM440
1.652320CrNiMo2-2SAE 8620SNCM220
1.815951CrV4SAE 6150SUP10
1.7104SAE 9254SUP12
1.2067100Cr6SAE 52100SUJ2
Structural steel1.0038S235JR1015SS330
1.0577S355J2A738
1.0050E295S490
1.0060E335SM570
Free-cutting steel1.071511SMn301213、1215SUM22
1.071811SMnPb3012L13SUM22L
1.072635S201140
1.072746S201146
Heat-treatable steel1.0503C451043、1045S45CM,S45C
1.0601C601060S60CM,S60C
1.721825CrMo44130SCM430
1.722542CrMo44140SCM440
Roller bearing steel and tool steel1.779258CrMoV4
1.3505100Cr6E52100SUJ2
1.1213C53G1050、1055S50CM,S50C
1.284290MnCrV8A681
1.717760Cr3
1.815951CrV46145SUP10
Case-hardening steel and nitriding steel1.0401C151015、1017S15C
1.713116MnCr55115
1.591817CrNi6-6
1.592018CrNi8
1.652320CrNiMo2-28617\8620SNCM220
1.2764X19NiCrMo4
1.575215NiCr133310SNC815
1.851931CrMoV9

2. Surface quality

2.1 Hot-rolled profiles

Surface quality in accordance with standard EN 10163-3 or other national standards (ASTM, GB, JIS)
Surface roughness: Ra < 40 microns
Dimensional tolerance: max. 0.5 mm
Straightness: Standard s
1.0 mm/m; < 0.3 mm/m upon request
Twist: Standard 1/m; upon request ≤ 0.5/m
Cross-section: 10mm - 7000mm
Length: ≤ 12 m or cut to fixed lengths

2.2 Cold-rolled/cold-drawn profiles

Surface quality in accordance with EN 10277-1 or other national standards (ASTM, GB, JIS)
Surface roughness: Ra ≤
2.5 microns
Decarburization: ≤ 0.1mm
Straightness: ≤ 0.1mm/m
Twist: 0.25°/m
Dimensional tolerance: ≤ 0.05mm
Cross-section: 1mm - 3800mm
Length: ≤ 6 m or cut to fixed length

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →
Image and content use · Creation Group