Products/GB/T 24242.2-2020

MATERIAL DATA · WIRE ROD

T700 · Wire rod for general-purpose wire drawing

GB/T 24242.2-2020 · Table C.1, C.2. Non-alloy steel wire rod for general-purpose wire drawing or cold rolling.

T700 Illustrative product image
T700 · Wire rod for general-purpose wire drawing · Illustrative product image
01Applicable standardGB/T 24242.2-2020
02Material gradeT700
03Product formWire rod for general-purpose wire drawing
04Delivery informationSubject to order specifications

Material technical data

Chemical composition

Cast analysis, mass fraction %. Unspecified values are not zero. This grade is designated by tensile strength; carbon and other unlisted elements are determined by the supplier and cannot be inferred from its name.

ElementMass fraction / %
Si0.1~0.3
Mn0.5~0.8
P≤0.03
S≤0.03

Properties and applicable conditions

PropertyStandard requirements and applicable conditions
Tensile strength Rm / MPa600~800

Standard reference and ordering limitations

  • Annex C designations are based on tensile strength. The supplier determines C, Cr, Ni, Cu, Mo and Al to meet strength requirements; the standard gives no numerical limits. Carbon content cannot be inferred from the grade designation.
  • Take specimens from 5 different coils per batch; tensile strength shall meet Table C.1. Intermediate grades require agreement between supplier and purchaser.
  • Cast analysis; composition is expressed as mass fraction, %. An unspecified lower limit is not zero.
  • Delivery condition, dimensions, surface, packaging and acceptance shall follow GB/T 24242.1—2020 and the order.

Reference: GB/T 24242.2-2020,Table C.1, C.2. Website information does not replace the official standard, order specifications or material certificates.

Illustrative packaging

Illustrative packaging
Sample shipment packaging · Illustration; packaging is subject to order confirmation.

Product and packaging images are illustrations; they do not identify a heat, stock availability, dimensions or a default delivery method. Confirm product form, delivery condition, packaging and acceptance requirements in the enquiry and order.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.