Products/JIS G 3505-2017

MATERIAL DATA · WIRE ROD

SWRM17K · Low-carbon steel wire rod

JIS G 3505:2017. Dimensions, delivery condition, quantity and acceptance requirements are confirmed in the order technical agreement.

SWRM17K Illustrative product image
SWRM17K · Low-carbon steel wire rod · Illustrative product image
01Applicable standardJIS G 3505-2017
02Material gradeSWRM17K
03Product formLow-carbon steel wire rod
04Delivery informationSubject to order specifications

Material technical data

SWRM17K · JIS G 3505-2017

Mild-steel wire rod; specified killed-steel designation K · Clause5/Table1 and AnnexJA.1-JA.3 · PDF page 5、6、8 · Mass fraction %

ElementHeat analysis / guide composition
C0.15~0.2
Mn0.3~0.6
P≤0.04
S≤0.04

Verify against the actual Japanese original Table 1 and normative Annex JA of JIS G3505:2017; heat analysis mass fraction wt%. The standard applies to mild steel wire rod for further processing into products such as iron wire and galvanized iron wire; electrode core wire rod is excluded.; Not automatically equivalent to special cold-heading steel. C and Mn for SWRM6/8 have only upper limits; unspecified lower limits shall not be added; Si and elements not listed in the table shall not be entered as 0; they shall not be intentionally added except for the purpose of finishing steelmaking; B addition by agreement shall follow JA.3. Add K to the end of the grade when killed steel is specified; K denotes deoxidation conditions; do not independently prescribe Al or Si content.. SWRM2/4 shall be adopted only per JA.1 agreement; SWRM17M/20M shall only have Mn changed to 0.60—0.90% per JA.2 agreement; the Mn range for ordinary 17/20 shall not be automatically expanded. When B is added per JA.3 agreement, B ≤ 70ppm, i.e., 0.007wt%; B content and B/N must be reported simultaneously. B/N for 2/4/6/8/10/12 is 0.4—1.8, and for 15/17/20/22 is 0.4—0.9. Compliance with the agreed conditions shall not be determined solely by satisfying the B upper limit; this upper limit shall not be applied if B is not agreed. The current composition table shows the default range without B addition; Agreed B/N must be verified separately in conjunction with the actual measured values of B and N for the heat; unspecified values for N shall not be entered as 0, nor shall B-suffix grades without original text basis be generated. Standard nominal diameters include 6.4mm; do not erroneously enter 6.5mm; Tolerances and diameter deviations for diameters > 25mm shall be per agreement; stricter precision per JA.4 must be separately agreed.

Original source: JIS G 3505:2017

Illustrative packaging

Illustrative packaging
Illustrative packaging; details are confirmed in the order.

Illustrative company wire products and packaging; the images do not identify the listed grade’s heat or batch, current stock, or default delivery conditions.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.