01Applicable standardISO 4954:2018 · Annex A
02Material gradeC25GC
03Product formCold heading wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Delivery conditions and applicable requirements

Table A.1 – Heat-treatment conditions, product forms and applicable requirements

Delivery conditionSymbolWire rodBarWire
Untreated, as hot rolled+ARXX—
Untreated and peeled+AR+PEXX—
Untreated and cold drawn+AR+C—XX
Untreated, cold drawn and spheroidize annealed+AR+C+AC—XX
Untreated, cold drawn, spheroidize annealed and skin passed+AR+C+AC+LC—XX
Annealed to achieve spheroidal carbides, as treated or peeled+AC or AC+PEXX—
Annealed to achieve spheroidal carbides, then cold drawn+AC+C—XX

X = applicable; — = not applicable. Chemical composition is specified in Table A.2 and mechanical properties in Table A.3. Supplementary or special requirements under Annex E apply if agreed at enquiry and order. Other delivery conditions may be agreed at the time of order.

Source: ISO 4954:2018, Table A.1, page 17 (PDF page 23). The original prints “+AC or AC+PE”; the notation is retained as printed. Confirm the exact delivery condition in the order.

2. Chemical composition

Table A.2 – Cast analysis of steels not intended for heat treatment after cold working, mass fraction %

Reference requirements for C25GC under ISO 4954:2018. These are not measured heat results; the order standard and requirements for feedstock and finished product must be confirmed separately.

Steel nameCSiMnPSCrNiMoAlbCuCr + Ni + Mo
C25GC0.23 to 0.270.15 to 0.25c0.80 to 1.00d0.0250.0250.300.300.10—c0.300.50

Elements not listed must not be intentionally added to the steel without the purchaser’s agreement, except for finishing the heat. Appropriate precautions are required to prevent additions of elements from scrap or other production materials. Residual elements may nevertheless be present if they do not impair mechanical properties or suitability.

a: Values are maximum limits unless otherwise indicated.

b: Aluminium may be replaced by one or more elements with a similar effect.

c: C10GC, C15GC, C17GC and C20GC may be supplied in two qualities: a) with a maximum aluminium content of 0.015%, or b) without aluminium and with silicon of 0.15 to 0.25% for hot-dip galvanizing.

d: For C2C, C20C, C20GC and C25C, a lower manganese content may be specified with a range of 0.20%.

Source note: The C25GC row carries footnote markers c and d in ISO 4954:2018, but C25GC is not named in the wording of these footnotes. The markers and notes are reproduced as in the source; the conditions require clarification before application to C25GC.

Source: ISO 4954:2018, Table A.2, page 18 (PDF page 24). Footnote conditions do not transfer automatically to grades absent from their wording. Unspecified limits and blank fields do not mean zero content.

3. Mechanical properties

Table A.3 – Wire rod, bars and wire not intended for heat treatment after cold working

Steel nameDiameter over, mmDiameter up to and including, mm+AR or +AR+PE+AC or +AC+PE+AR+C+AR+C+AC+AR+C+AC+LC+AC+C
Rm max., MPaZa min., %Rm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %
C25GC25————57045——44055——
C25GC51059050——47045——4405544055
C25GC104059050——47045——4405544055
C25GC4010059050——————————

a: Z values in the first delivery condition (+AR or +AR+PE) are given for information only. Rm is tensile strength and Z is reduction of area at fracture. Blank cells and dashes are retained from the source and do not indicate zero or a supply commitment.

Source: ISO 4954:2018, Table A.3, pages 19–20 (PDF pages 25–26). Values apply only to the specified diameter intervals and delivery conditions.

These excerpts do not replace the complete standard. Annex A concerns steels not intended for heat treatment after cold working; it supplies no hardenability table for this grade.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — C25GC

Basis: ISO 4954

Chemical composition source: ISO 4954:2018

Transcribed from the cited standard

The bounds below use the main-row limits in ISO 4954:2018, Table A.2, including Cr + Ni + Mo ≤0.50% as a combined limit. The individual Cr, Ni and Mo maxima cannot all occur together. Agreed alternative ordering conditions require separate recalculation. Missing elements remain unknown; partial contributions are not complete carbon-equivalent values. These are theoretical source-limit bounds, not measured heat results.

Original source wording

Table A.2

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.3633–0.5433

Missing elements: V

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.2750–0.3667

Missing elements: V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Calculated range: 0.3100–0.4125

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group