Products/ISO 4954

MATERIAL DATA · COLD FORMING

X3CrNiCuMo17-11-3-2 CHQ wire

Reference technical data for X3CrNiCuMo17-11-3-2. Source edition: ISO 4954:2018 · Annex D. Read chemistry, delivery conditions and properties with their cited limits and notes. The applicable edition and acceptance requirements must be confirmed in the order technical agreement.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

X3CrNiCuMo17-11-3-2 CHQ wire product image
X3CrNiCuMo17-11-3-2 · Cold heading wire
01Applicable standardISO 4954:2018 · Annex D
02Material gradeX3CrNiCuMo17-11-3-2
03Product formCold heading wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

Composition source and applicability

Reference composition for the stated standard edition, not heat analysis. Confirm the order standard and the separate requirements for feedstock and finished product.

X3CrNiCuMo17-11-3-2 · ISO 4954:2018

X3CrNiCuMo17-11-3-2 · ISO 4954:2018 · Mass fraction / %
ElementMass fraction / %
C≤0.04
Si≤1
Mn≤2
P≤0.045
S≤0.015
Cr16.5–17.5
Ni10–11
Mo2–2.5
N≤0.1
Cu3–3.5
Source: ISO 4954:2018
Composition source and applicability · ISO 4954:2018 · PDF 29
ISO 4954:2018 · PDF 29
Composition source and applicability · ISO 4954:2018 · PDF 41
ISO 4954:2018 · PDF 41
Composition source and applicability · ISO 4954:2018 · PDF 42
ISO 4954:2018 · PDF 42
Composition source and applicability · ISO 4954:2018 · PDF 59
ISO 4954:2018 · PDF 59

1. Delivery conditions and applicable requirements

Table D.1 – Combinations of heat-treatment condition at delivery, product form and applicable requirements

Delivery conditionSymbolWire rodBarWireFerritic steelsMartensitic steelsAustenitic and austenitic-ferritic steels
Solution annealed or solution annealed and peeled+AT or AT+PEXXX——X
Solution annealed and cold drawn+AT+C—XX——X
Solution annealed, cold drawn and solution annealed again+AT+C+AT—XX——X
Solution annealed, cold drawn, solution annealed again and lightly cold drawn+AT+C+AT+LC—XX——X
Soft annealed or soft annealed and peeled+A or +A+PEXXXXX—
Soft annealed and lightly cold drawn+A+LC—XXXX—
Soft annealed, cold drawn and soft annealed again+A+C+A—XXXX—
Soft annealed, cold drawn, soft annealed again and lightly cold drawn+A+C+A+LC—XXXX—

X = applicable; — = not applicable.

Other delivery conditions may be agreed at the time of enquiry and order.

Applicable requirements according to the basis of order

Type of requirementRequirement
Chemical compositionAccording to Table D.2.
Mechanical propertiesTable D.1 refers to D.3, D.4 and D.6. D.5 contains requirements for ferritic steels but is omitted from this reference in the original table. Use the appropriate material group and table for assessment.

Supplementary or special requirements under Annex E apply if agreed at the time of enquiry and order.

Source: ISO 4954:2018, Table D.1, page 51 (PDF page 57). This table gives the standard relationship between product form, delivery condition and requirements; actual supply must be confirmed separately.

2. Chemical composition

Table D.2 – Chemical composition of stainless steels (cast analysis)

These are the standard’s reference requirements for cast analysis of X3CrNiCuMo17-11-3-2, not analysis results for a particular heat. The order standard and requirements for raw material and finished product must be confirmed separately.

ISO steel number: 4578-316-76-E.

Values are mass fractions in percent. Single values are maximum limits unless otherwise indicated. “—” means the table specifies no limit; it does not mean zero content.

Elements not listed must not be intentionally added without the purchaser’s agreement, except for finishing the heat. Precautions are required to prevent additions from scrap or other raw materials of elements that could impair mechanical properties or suitability.

Source: ISO 4954:2018, Table D.2, page 53 (PDF page 59). The table and notes do not replace the complete standard.

3. Mechanical properties

Table D.3 – Mechanical properties of austenitic stainless steels in the specified delivery condition

Steel nameISO steel numberDiameterDelivery condition
+AT or +AT+PE+AT+C+AT+C+AT+AT+C+AT+LC
over, mmup to and including, mmRm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %Rm max., MPaZ min., %
X3CrNiCuMo17-11-3-24578-316-76-E25————6306868063
X3CrNiCuMo17-11-3-24578-316-76-E51061068760—6106866063
X3CrNiCuMo17-11-3-24578-316-76-E102561068720—61068——
X3CrNiCuMo17-11-3-24578-316-76-E255061068——————

Source: ISO 4954:2018, Table D.3, page 57. Rm is tensile strength; Z is reduction of area at fracture. The values apply to the specified diameter intervals and delivery conditions. A dash does not mean zero or confirm availability.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — X3CrNiCuMo17-11-3-2

Basis: ISO 4954

Chemical composition source: ISO 4954:2018

Transcribed from the cited standard

Original source wording

Table D.2

These carbon and low-alloy steel formulas do not apply directly to this material; no carbon equivalent is calculated.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →