Products/GB/T 3077-2015 / Q/BQB 517-2023 / BEXG 021-2020

MATERIAL DATA · COLD FORMING

20CrMnTi Steel Material for Cold Forming (Wire Rod)

20CrMnTi · GB/T 3077 / Q/BQB 517-2023 / BEXG 021-2020. Delivery condition, dimensions, mechanical properties, hardenability and acceptance must be confirmed against the applicable standard and order agreement. Similar grades are not interchangeable; this page does not guarantee supply or forming performance.

20CrMnTi Steel Material for Cold Forming (Wire Rod) product image
20CrMnTi · Cold forming wire rod
01Applicable standardGB/T 3077-2015 / Q/BQB 517-2023 / BEXG 021-2020
02Material grade20CrMnTi
03Product formCold forming wire rod
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

Standard and grade references

Standard grade reference: GB/T 3077-2015

Baosteel delivery specification: Q/BQB 517-2023 / BEXG 021-2020

The values below come from the identified Baosteel standard or agreement, not from a general national-standard chemistry table. Different sources are shown separately and their limits are not combined.

Chemical composition (mass fraction, %)

Q/BQB 517-2023 · PDF 12 · Table 1 · Row 99

CSiMnPSCrMoBAltOther
0.17-0.230.17-0.370.80-1.10≤0.020≤0.0201.00-1.30≤0.10——Ti:0.04-0.10;Ni:≤0.20;Cu:≤0.20

Chemical composition (mass fraction, %)

BEXG 021-2020 · PDF 3 · Table 1 · Row 2

CSiMnPSCrOther
0.17-0.230.17-0.370.80-1.10≤0.025≤0.0251.00-1.30Ti:0.04-0.10,Ni≤0.20,Cu≤0.20,Mo≤0.10

Delivery condition, dimensions, mechanical properties, hardenability and acceptance must be confirmed against the applicable standard and order agreement. Similar grades are not interchangeable; this page does not guarantee supply or forming performance.

Illustrative product photograph randomly selected from company photos; it does not identify this grade, heat or batch.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — 20CrMnTi

Basis: GB/T 3077-2015 / Q/BQB 517-2023 / BEXG 021-2020

Chemical composition source: Original standard not yet verified

Original standard not yet verified

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →