Products/JIS G3505

MATERIAL DATA · COLD FORMING

SWRM22 Wire Rod for Cold Forming

SWRM22 Wire Rod for Cold Forming – Technical Data compliant with JIS G3505. View the chemical composition, mechanical properties, and related technical requirements for the current grade.

SWRM22 Wire Rod for Cold Forming product image
SWRM22 · Cold forming wire rod
01StandardJIS G3505
02GradeSWRM22
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 – Chemical composition, unit: %

GradeCMnPS
SWRM220.20-0.250.30-0.60<0.040<0.040
Elements not listed in this table shall not be intentionally added, except as required for steelmaking purposes. However, B may be added upon agreement between the supplier and the purchaser. In such cases, refer to Appendix JA.3. a) When killed steel is specified, add K to the end of the grade designation, e.g., SWRM10K. b) JA.2 may also apply upon agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →