SWRM17 Wire Rod for Cold Forming

SWRM17 Wire Rod for Cold Forming – Technical Data compliant with JIS G3505. View the chemical composition, mechanical properties, and related technical requirements for the current grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

SWRM17 Wire Rod for Cold Forming product image
SWRM17 · Cold forming wire rod
01Applicable standardJIS G3505
02Material gradeSWRM17
03Product formCold forming wire rod
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 – Chemical composition, unit: %

GradeCMnPS
SWRM170.15-0.200.30-0.60<0.040<0.040
Elements not listed in this table shall not be intentionally added, except as required for steelmaking purposes. However, B may be added upon agreement between the supplier and the purchaser. In such cases, refer to Appendix JA.3. a) When killed steel is specified, add K to the end of the grade designation, e.g., SWRM10K. b) JA.2 may also apply upon agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — SWRM17

Basis: JIS G3505

Chemical composition source: JIS G 3505:2017

Transcribed from the cited standard

Original source wording

Table 1

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.2000–0.3000

Missing elements: Cr, Mo, V, Ni, Cu

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.1650–0.2300

Missing elements: Si, Cu, Cr, Ni, Mo, V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Known-element contribution, not a complete value: 0.1800–0.2600

Missing elements: Mo, Cr, Cu, Ni

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.