1. Chemical Composition
Table 1 – Chemical composition, unit: %
| Grade | C | Mn | P | S |
|---|---|---|---|---|
| SWRM10 | 0.08-0.13 | 0.30-0.60 | <0.040 | <0.040 |
MATERIAL DATA · COLD FORMING
Technical data for SWRM10 cold heading wire rod, compliant with JIS G3505. View the chemical composition, mechanical properties, and related technical requirements for the current grade.
Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

STANDARD & PROPERTIES
Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.
Enquire this grade| Grade | C | Mn | P | S |
|---|---|---|---|---|
| SWRM10 | 0.08-0.13 | 0.30-0.60 | <0.040 | <0.040 |
Engineering Knowledge
TECHNICAL NOTE
Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.
RFQ CHECKLIST
RELATED CAPABILITIES
Basis: JIS G3505
Chemical composition source: JIS G 3505:2017
Transcribed from the cited standard
Table 1
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.1300–0.2300Missing elements: Cr, Mo, V, Ni, Cu
IIW/CEV: carbon and low-alloy steel weldability screening.
Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.0950–0.1600Missing elements: Si, Cu, Cr, Ni, Mo, V, B
Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.
CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Known-element contribution, not a complete value: 0.1100–0.1900Missing elements: Mo, Cr, Cu, Ni
CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.
A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.
Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.
Method reference: TWI
Carbon equivalent calculator →View watermarked sample-test reports. Results do not replace the delivery-batch inspection certificate.
Find and preview reports →Same-grade reference does not establish standard equivalence, supply or substitution approval.