Products/JIS G3508

MATERIAL DATA · COLD FORMING

SWCHB526 Wire Rod for Cold Forming

Technical data for SWCHB526 wire rod for cold forming, compliant with JIS G3508. View the chemical composition, mechanical properties, and related technical requirements for this grade.

SWCHB526 Wire Rod for Cold Forming product image
SWCHB526 · Cold forming wire rod
01StandardJIS G3508
02GradeSWCHB526
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 – Chemical composition, unit: %

For all steel grades in this table, Cu shall not exceed 0.30%, Ni 0.20%, and Cr 0.20%. Note a) The lower limit for Si may be set to less than 0.10% by agreement between supplier and purchaser. b) The B content may be 0.0005% or higher by agreement between supplier and purchaser.

2. Hardenability

Table 3 Distance from quenched end and hardness

3. Mechanical properties of wire rod

Table 4 Mechanical properties of wire rod resulting from process D

Notes: 1. For wire diameters exceeding 20 mm, the tolerance is the value in Table 2 minus 5. No tolerance is specified for diameters of 3 mm or less. 2. 1 N/mm² = 1 MPa

Table 5 Mechanical properties of wire rod resulting from the DA process

Notes: 1. For wire diameters exceeding 20 mm, the tolerance is the value in Table 2 minus 5. No tolerance is specified for diameters of 3 mm or less. 2. 1 N/mm² = 1 MPa

4. Decarburized layer depth

Table 6 Permissible limits for average decarburized layer depth

Average decarburized layer depth
Wire diameter (mm)Ferrite decarburized layer depthTotal decarburized layer depth
≤15<0.02<0.15
15<d≤25<0.03<0.20
25<d≤32<0.04<0.25
For SWCH30K to SWCH50K wire, when specified by the purchaser, the test in 10.3.1 shall be performed. The permissible limit for the average decarburized layer depth shall be in accordance with Table 4. However, for wire with a diameter exceeding 32 mm, the limits shall be agreed upon between the supplier and the purchaser.

5. Wire diameter tolerance and out-of-roundness

Table 7 Tolerances and out-of-roundness for wire diameter

Table 7 Wire diameter tolerances and deviations
Unit: mm
Wire diameterPermissible deviationOut-of-roundness
≤30-0.0250.013
3<d≤60-0.0300.013
6<d≤100-0.0360.013
10<d≤180-0.0430.013
18<d≤300-0.0700.013
30<d≤400-0.1000.013
40<d≤500-0.1500.013
Note (3) Out-of-roundness refers to the difference between the maximum and minimum diameters within the same cross-section of the wire.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.