Products/JIS G 3507-2:2005

MATERIAL DATA · COLD FORMING

SWCH8A Cold heading wire

Technical data for SWCH8A wire rod for cold forming, compliant with JIS G 3507-2:2005. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

SWCH8A Cold heading wire
SWCH8A · Cold heading wire
01Applicable standardJIS G 3507-2:2005
02Material gradeSWCH8A
03Product formCold heading wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Composition source and applicability

Reference composition for the stated standard edition, not heat analysis. Confirm the order standard and the separate requirements for feedstock and finished product.

Source: JIS G 3507-2:2005 → JIS G 3507-1:2021 · SWRCH8A · p.7

ElementMass fraction / %
C0.05~0.10
Si≤0.10
Mn≤0.60
P≤0.030
S≤0.035
Cr≤0.20
Ni≤0.20
Cu≤0.30
Al≥0.02
For all steel grades in this table, Cu shall not exceed 0.30%, Ni 0.20%, and Cr 0.20%.

2. Mechanical properties of wire rod

Table 2 Mechanical properties of wire rod resulting from Process D

GradeWire diameter range mmTensile Strength N/mm²Reduction of Area %(Reference) Hardness HRB
SWCH8A≤3≥540——
SWCH8A>3–4≥440≥45—
SWCH8A>4–5≥390≥45—
SWCH8A>5≥340≥45≤85
Notes: 1. For wire diameters exceeding 20 mm, the tolerance is the value in Table 2 minus 5. No tolerance is specified for diameters of 3 mm or less. 2. 1 N/mm² = 1 MPa

Table 3 Mechanical properties of wire rod resulting from the DA process

GradeTensile Strength N/mm²Reduction of Area %(Reference) Hardness HRB
SWCH8A≥290≥55≤80
Notes: 1. For SWCH6R to SWCH27K grades, when the product is used as heat-treated wire, the lower limit of tensile strength may be set below the values in Table 3 upon agreement between supplier and purchaser. 2. For wire diameters exceeding 20 mm, the tolerance is the value in Table 3 minus 5. No tolerance is specified for diameters of 3 mm or less. 3. 1 N/mm² = 1 MPa

3. Depth of decarburized layer

Table 4 Permissible limits for average decarburized layer depth

Unit: mm
Wire diameterFerrite decarburized layer depthTotal decarburized layer depth
≤15≤0.02≤0.15
>15~25≤0.03≤0.20
>25~32≤0.04≤0.25
For SWCH30K to SWCH50K wire, when specified by the purchaser, the test in 10.3.1 shall be performed. The permissible limit for the average decarburized layer depth shall be in accordance with Table 4. However, for wire with a diameter exceeding 32 mm, the limits shall be agreed upon between the supplier and the purchaser.

4. Tolerance on wire diameter and out-of-roundness

Table 5 Tolerance on wire diameter and out-of-roundness

Wire diameterPermissible deviationOut-of-roundness
≤3+0 / −0.025≤0.013
>3–6+0 / −0.030≤0.015
>6–10+0 / −0.036≤0.018
>10–18+0 / −0.043≤0.022
>18–30+0 / −0.070≤0.035
>30–40+0 / −0.100≤0.050
>40–50+0 / −0.150≤0.070
Note (4): Diameter deviation refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — SWCH8A

Basis: JIS G 3507-2:2005

Chemical composition source: JIS G 3507-2:2005 → JIS G 3507-1:2021

Transcribed from the cited standard

Original source wording

Table 2

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.0500–0.2733

Missing elements: Mo, V

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.0500–0.1617

Missing elements: Mo, V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Known-element contribution, not a complete value: 0.0500–0.1900

Missing elements: Mo

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group