Products/JIS G3507

MATERIAL DATA · COLD FORMING

SWCH15R cold heading wire rod

Technical data for SWCH15R cold heading wire rod, compliant with JIS G3507. View chemical composition, mechanical properties, and related technical requirements for this grade.

SWCH15R cold heading wire rod product image
SWCH15R · Cold forming wire rod
01StandardJIS G3507
02GradeSWCH15R
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 – Chemical composition, unit: %

For all steel grades in this table, Cu shall not exceed 0.30%, Ni 0.20%, and Cr 0.20%.

2. Mechanical properties of wire rod

Table 2 Mechanical properties of wire rod resulting from Process D

GradeWire diameter range mmTensile Strength N/mm²Reduction of Area %(Reference) Hardness HRB
SWCH12R SWCH15R SWCH12A SWCH15A SWCH10K SWCH12K≤3≥590--
>3~4≥490≥45
>4~5≥410
>5≥360≤90
Notes: 1. For wire diameters exceeding 20 mm, the tolerance is the value in Table 2 minus 5. No tolerance is specified for diameters of 3 mm or less. 2. 1 N/mm² = 1 MPa

Table 3 Mechanical properties of wire rod resulting from the DA process

GradeTensile Strength N/mm²Reduction of Area %(Reference) Hardness HRB
SWCH12R SWCH15R SWCH12A SWCH15A SWCH10K SWCH12K≥340≤83
Notes: 1. For SWCH6R to SWCH27K grades, when the product is used as heat-treated wire, the lower limit of tensile strength may be set below the values in Table 3 upon agreement between supplier and purchaser. 2. For wire diameters exceeding 20 mm, the tolerance is the value in Table 3 minus 5. No tolerance is specified for diameters of 3 mm or less. 3. 1 N/mm² = 1 MPa

3. Depth of decarburized layer

Table 4 Permissible limits for average decarburized layer depth

Unit: mm
Wire diameterFerrite decarburized layer depthTotal decarburized layer depth
≤15≤0.02≤0.15
>15~25≤0.03≤0.20
>25~32≤0.04≤0.25
For SWCH30K to SWCH50K wire, when specified by the purchaser, the test in 10.3.1 shall be performed. The permissible limit for the average decarburized layer depth shall be in accordance with Table 4. However, for wire with a diameter exceeding 32 mm, the limits shall be agreed upon between the supplier and the purchaser.

4. Tolerance on wire diameter and out-of-roundness

Table 5 Tolerance on wire diameter and out-of-roundness

Wire diameterPermissible deviationOut-of-roundness
≤30-0.025≤0.013
>3 ≤60-0.030≤0.015
>6 ≤100-0.036≤0.018
>10 ≤180-0.043≤0.022
>18 ≤300-0.070≤0.035
>30 ≤400-0.100≤0.050
>40 ≤500-0.150≤0.070
Note (4): Diameter deviation refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →