Products/JIS G4804

MATERIAL DATA · COLD FORMING

SUM42 Steel for cold forming

Technical data for SUM42 Steel for cold forming, compliant with JIS G4804. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

SUM42 Steel for cold forming
SUM42 · Steel for cold forming
01Applicable standardJIS G4804
02Material gradeSUM42
03Product formSteel for cold forming
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 -- Chemical Composition, %

GradeCMnPSPb
SUM420.37~0.451.35~1.65<0.0400.08~0.13
Note a) Si is not specified. However, upon agreement between supplier and purchaser, limits or ranges such as ≤0.10%, 0.10%–0.20%, or 0.15%–0.35% may be established.
b) Elements not specified in this table shall not be intentionally added to the steel, except for the purpose of completing the steelmaking process, unless agreed upon by the supplier and purchaser.
c) For SUM22 and SUM22L, the upper limit for Mn may be set at 1.10% upon agreement between the supplier and the purchaser.
d) When product analysis for lead in leaded steel is conducted at the purchaser's request, the lead content shall be 0.07–0.35%.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — SUM42

Basis: JIS G4804

Chemical composition source: JIS G 4804:2008

Transcribed from the cited standard

Original source wording

Table 1

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.5950–0.7250

Missing elements: Cr, Mo, V, Ni, Cu

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.4375–0.5325

Missing elements: Si, Cu, Cr, Ni, Mo, V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Known-element contribution, not a complete value: 0.5050–0.6150

Missing elements: Mo, Cr, Cu, Ni

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group